IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1068 documents. Displaying 25 entries per page.


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


Selection of Wood-Rotting Basidiomycetes for Inoculation of an Accelerated Soil Bed Test
2014 - IRG/WP 14-20543
There is a need for a test method that guarantees exposure of treated wood to soil and preservative-tolerant wood-rotting basidiomycetes as standard field tests do not do this reliably. The ability of a range of selected wood-rotting basidiomycetes to grow through unsterile forest soil was investigated in a Mason jar test assembly. None of the white-rot fungi in test grew through this soil. Fou...
P I Morris, A Uzunovic, J Ingram


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Screening method to test efficacy of fumigants against fungi and preliminary data on the efficacy of sulfuryl fluoride
2014 - IRG/WP 14-20551
Methyl bromide is being phased out and there is an urgent need to find a suitable replacement that is effective in reducing exotic pest establishments via trade in wood products. Efficacy data for established phytosanitary fumigants were mostly developed for arthropods and nematodes, and limited information exists for plant pathogens. Increased interest in developing a fast screening process for f...
A Uzunovic, A Mukherjee, R Mack, P Elder, S Myers


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Laboratory investigation of fire protection coatings for creosote-treated timber railroad bridges
2014 - IRG/WP 14-30639
As the incidence of timber railroad bridge fires increases, so has the need to develop protective measures to reduce the risk from accidental ignitions primarily caused by hot metal objects. Of the six barrier treatments evaluated in the laboratory for their ability to protect timbers from fires sourced with ignition from hot metal objects only one intumescent coating provided adequate fire prote...
C A Clausen, R H White, J P Wacker, S T Lebow, M A Dietenberger, S L Zelinka, N M Stark


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Using Commercial Water Repellent Chemicals on Wood Protection
2014 - IRG/WP 14-30656
Lately, researchers have been looking for process and products that use environmental friendly technologies in wood protection. These sorts of innovations on wood protection should be carried out for wood evaluated at outdoor conditions. Using water repelling chemicals is one of those innovations which improve wood durability and dimensional stability by decreasing content of moisture. In this ...
G Köse, A Temiz, S Demirel, O E Özkan


Fire resistance of wood treated with potassium carbonate and silanes
2014 - IRG/WP 14-30657
This paper reports on the effect that organosilicon compounds and potassium carbonate and urea (PCU) have on wood flammability. The study focus on reducing wood flammability by promoting char formation through manipulation of the condensed phase decomposition chemistry. Potassium carbonate is known as an effective fire retardant, however it is easily leached out from wood and increases its hygrosc...
B Mazela, M Broda, W Perdoch


Field performance of wax treated wood
2014 - IRG/WP 14-30649
The durability and outdoor performance of wax treated Scots pine sapwood was investigated in above ground field tests. Therefore wood impregnated with three different waxes was exposed in horizontal lap-joint test which is running since eight years. Durability, wetting resistance and the susceptibility to checking has been investigated. In summary, all wax treated wood performed better compared to...
C Brischke, E Melcher


Resistance to Decay Fungi of Scots Pine Impregnated with Natural and Chemical Preservatives
2014 - IRG/WP 14-30650
In this study, heart-wood and sap-wood specimens of the Scots pine which is naturally grown in Turkey were treated with natural (valex) and some chemical preservatives such as CCA - C (Copper / Chrome / Arsenic), CBA - A (Copper / Boron / Azole). The wood protective efficacies of these preservatives were investigated by means of fungi decay test (EN 113). As a result of the study it was found t...
S Yildiz, U B Şimşek


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


Comparison of untreated plywood and untreated LVL in a field trial against Coptotermes acinaciformis and in laboratory trials against Tyromyces palustris and Coniophora puteana
2014 - IRG/WP 14-40671
In Australasia, efficacy data obtained on plywood is generally acceptable for laminated veneer lumber (LVL) and vice versa. This is particularly the case with glueline treatment approvals. The rationale is that the two wood products have predominately the same basic structure with the key difference being orientation of the veneer. LVL typically has all veneers in parallel while plywood typical...
A Siraa, K Day, S Millward, P Lobb


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong


Field Performance of Old-Growth and Second-Growth Western Red Cedar Fence Posts with and without Barrier Wraps
2015 - IRG/WP 15-10838
Many authors have suggested natural durability may be lower in second-growth western redcedar than in old-growth. One potential means of offsetting a decline in durability is use of physical barriers to separate the wood from soil. In the present work we compared the durability of old-growth and second-growth western red cedar posts, with and without barrier wraps, in a field test. After ten year...
P I Morris, J K Ingram, R Stirling


Durability of treated wood Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla against subterranean termite
2015 - IRG/WP 15-20563
This work aimed to analyze the durability of woods against termite Nasutitermes corniger Motsch. Fence posts from this study were collected in Pinheiros, north of Espírito Santo state, Brazil. Used the Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla species with 11 and 9 years, respectively and plant spacing of 3.00 x 2.00 m. Were used 72 samples from discs removed the 0.50 m of...
D Junior Verly Lopes, J Benigno Paes, P N de Medeiros Neto, G dos Santos Bobadilha


The combined effect of wetting ability and durability on field performance – verification of a new prediction approach
2015 - IRG/WP 15-20565
Comprehensive approaches to predict performance of wood products are requested by international standards and the first attempts have been made in the frame of European research projects. However, there is still an immanent need for a methodology to implement the durability and moisture performance of wood in a performance classification system. The aim of this study was therefore to establish an ...
C Brischke, G Alfredsen, P-O Flæte, M Humar, T Isaksson, L Meyer


Introduction of the COST FP 1303 Cooperative Performance Test
2015 - IRG/WP 15-20567
COST Action FP 1303 “Performance of bio-based building materials” successfully started in October 2013 and an ambitious program was set up for the four year programme. COST Actions provide an excellent opportunity for collaborative research, e.g. in the frame of Round Robin tests. The idea of this respective test was to distribute a fairly simple test set up to as many places in Europe as poss...
M Humar, C Brischke, L Meyer, B Lesar, N Thaler, D Jones, S Bardage, C Belloncle, J Van den Bulcke, J M Abascal, G Alfredsen, D Baisch, B Brunnhuber, G Cofta, E Grodås, E Frühwald Hansson, M Irle, H Kallakas, J Kers, M Klamer, P Larsson Brelid, A B Maider, K C Mahnert, E Melcher, R Möller, M Noël, L Nunes, G A Ormondroyd, S Palanti, N Pfabigan, A Pilgård, A O Rapp, P Schumacher, E Suttie, T Teppand, M Touza, J Van Acker


Above ground field testing: results of experiments in Brazil after one year
2015 - IRG/WP 15-30660
After the development of new products they need to be field-tested to assess their efficacy under diverse conditions of climate, comparing them with a preservative with proven efficacy. In some testing sites, decay occurs very slowly. The solution would be to bring these tests to locations that are conducive to biodeterioration, like tropical climates. Tropical sites provide higher temperature and...
M F Natale, J M Vidal


Potential of teak heartwood extractives as a natural preservative against Nasutitermes corniger termite
2015 - IRG/WP 15-30666
Most low durability timber are treated with waterborne preservatives consisting of metallic salts, however, these substances make the process expensive and are harmful to man and the environment, requiring cares with handling, dosing and leaks. Due to these facts, several researches have shown the use of natural substances, extracted from the wood of various naturally durable species, as potential...
V Fassina Brocco, J Benigno Paes, L Gonçalves da Costa, S Brazolin


The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with preservatives is unavoidable to ensure the desired service life. However, chemical treatment of wood can result in changes of its mechanical ...
M Humar, D Kržišnik, C Brischke


Biological Performance of Triadimefon in combination with Tebuconazole in laboratory and field tests
2015 - IRG/WP 30668
The usage of Triazole-combinations for wood preservatives is common practice in several countries. Especially the combination of Tebuconazole and Propiconazole is preferred for this application due to its broad spectrum of efficacy against wood destroying fungi. 1-(4-Chlorphenoxy)-3,3-dimethyl-1-(1,2,4-triazol-1-yl)-butanon, also known as Triadimefon provides a good efficacy against the wood destr...
P Meckler, T Jaetsch


Previous Page | Next Page