Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Above ground field testing: results of experiments in Brazil after one year
2015 - IRG/WP 15-30660
After the development of new products they need to be field-tested to assess their efficacy under diverse conditions of climate, comparing them with a preservative with proven efficacy. In some testing sites, decay occurs very slowly. The solution would be to bring these tests to locations that are conducive to biodeterioration, like tropical climates. Tropical sites provide higher temperature and...
M F Natale, J M Vidal


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Global survey on durability variation – on the effect of the reference species
2016 - IRG/WP 16-20573
Climate change due to anthropogenic emissions is the largest environmental challenge of our time. Forest-based value chains play an important role in reducing the accumulation of CO2 in the atmosphere. Maximizing the use of wood to tackle climate change requires improved understanding of the service life of timber products. This information can best be obtained from field testing and while there i...
R Stirling, G Alfredsen, C Brischke, I De Windt, L P Francis, E Frühwald Hansson, M Humar, J Jermer, M Klamer, M Kutnik, P Laks, I Le Bayon, S Metsä-Kortelainen, L Meyer-Veltrup, P I Morris, J Norton, T Singh, J Van Acker, J Van den Bulcke, T M Venås, H Viitanen, A H H Wong


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Comparative studies on the durability of English oak (Quercus robur L.) under in-service, field and laboratory conditions
2017 - IRG/WP 17-10881
The durability of many wood species varies due to differences in extractive content, anatomical features, growth conditions, and not at least in dependence of the respective exposure conditions either under test or in real life applications. And so does the durability of English oak (Quercus robur L.), which has recently been considered in the revised European standard EN 350 (2016) and is now cla...
C Brischke, L Meyer-Veltrup, A Soetbeer, M Höpken, E Melcher, J Trautner


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Resistance of modified wood to termite attack assessed in laboratory and field testing: A review of internal research
2018 - IRG/WP 18-40824
Within the past decades, new wood modification technologies have been investigated in order to improve certain wood characteristics and enable the use of timber products for outdoor applications. Some of these non-biocidal technologies have been developed and commercialized recently. Thus, various material properties were studied intensively and shown to be improved. To a great extent, previous re...
L Emmerich, P Gascón-Garrido, H Militz


Performance of field cut preservatives above-ground and in ground contact exposures
2019 - IRG/WP 19-30742
Field cut preservatives are needed to protect cut ends and drill holes that expose the untreated interior of preserved wood. A series of field cut preservatives were assessed in ground contact and above-ground exposures. After 10 years in ground contact exposure, all of the untreated controls had failed or exhibited very advanced decay. In contrast, the copper naphthenate (2% Cu in mineral spirits...
R Stirling, D Wong


Performance of naturally durable decks after 15 years of field exposure
2020 - IRG/WP 20-10963
A decking test of Canadian species considered to be naturally durable was inspected after 15 years of exposure at test sites in Ontario and British Columbia. Based on the materials used in this experiment, Douglas-fir and yellow cypress had the greatest decay resistance, followed by eastern white cedar and western redcedar, and then by western larch and tamarack. All materials tested were more dur...
R Stirling, D Wong


Post-layup protection of mass timber elements in above ground protected exposures: 2-year results
2022 - IRG/WP 22-30766
Mass timber has seen increased use as a building material for low and mid-rise construction in recent decades. The durability of mass timber elements has not been fully examined and the effects of wood destroying organisms on this these materials merits attention. The effectiveness of currently labeled soil termiticides and passively applied biocides at post-construction or as remedial agents need...
M E Mankowski, T G Shelton, G T Kirker, J J Morrell


Above-Ground Termite Resistance of Naturally Durable Species in Ontario and Mississippi
2022 - IRG/WP 22-30767
A collaborative above-ground protected termite field test was initiated by FPInnovations and the USDA Forest Service at sites in Ontario and Mississippi. The aims of the experiment were to compare the rate of attack in protected, above-ground exposures by the subterranean termite species, Reticulitermes flavipes, between northern (Ontario) and southern (Mississippi) test sites and to generate perf...
R Stirling, M Mankowski


Glued laminated poles - Progress report after 43 years of testing
2023 - IRG/WP 23-20692
In 1979, a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse in Uppsala, in the Simlångsdalen test field in south-western Sweden and in a power lane in Vuollerim in northern Sweden, in order to study their resistance against biological degradation. The test poles were treated in a two-step process. All laminations of Scots pine (Pinus sylvestris) were first...
J Jermer, M Westin, N Terziev


Field durability testing of wood above ground - Part 1: 15 years’ experience with the Bundle method
2023 - IRG/WP 23-20695
A ‘jack of all trades’ method for above-ground wood durability testing has been sought for decades, but until now no method has found its way into standardization. The method of choice shall be applicable for untreated and treated wood – ideally also for wood composites. It shall be reproducible, objective, fast, easy, and inexpensive. Finally, it shall provide high predictive power. This s...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Field durability testing of wood above ground - Part 2: The full guideline of the Bundle method
2023 - IRG/WP 23-20696
To determine the biological durability of wood above ground, numerous approaches for test methods have been pursued and tried out in the field in the past. So far, no method has managed to find its way into a European standard. During the last 15 years, experience with the Bundle method has been gained. As described in Part 1 of this paper, the method is recommended as a suitable tool for determin...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Challenges in managing very long-term field tests
2023 - IRG/WP 23-30779
Field testing of wood preservatives has been on-going in Petawawa, Ontario, Canada since at least 1937. Many of the treated roundwood posts from these early experiments are still in test, and include preservatives still used today, including creosote, copper naphthenate, pentachlorophenol and CCA. Performance data from selected experiments more than 50 years old are reported and we discuss some of...
R Stirling, D Wong


Long-term field performance of a carbon-based preservative in ground contact test conditions
2023 - IRG/WP 23-30781
Carbon-based preservatives have demonstrated reasonable long-term field performance in above ground testing. This study examines the performance of a carbon-based preservative formulation containing quaternary ammonium compounds and tebuconazole as a treatment for three softwood species exposed in ground contact at two sites in Canada. The treatment was associated with improved decay resistance an...
C Wilson, J Zhang, R Stirling


Field performance of MCA-treated wood in ground contact
2023 - IRG/WP 23-30782
Micronized Copper Azole (MCA) was evaluated for its ability to resist biodegradation at two Canadian test sites using Pacific silver fir and white spruce stakes, and lodgepole pine and red pine roundwood posts. After 12 years of exposure the treated stakes exhibited low to moderate levels of decay while the untreated controls had failed. When stakes were moved to an active termite site, the untrea...
C Wilson, J Zhang, R Stirling


Field performance of preserved shakes and shingles
2024 - IRG/WP 24-41000
Wood shakes and shingles are used in applications where they are at risk of decay, either in sidewall (UC3.1) or roofing (UC3.2) applications. Material durability may come from using the heartwood of naturally durable species, using preservative treatments, or both. Through a series of long-term field tests, this paper explores the performance of naturally durable and preserved shakes and shingles...
R Stirling, S Kus


A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Proposed method for out-of-ground contact trials of exterior joinery protection systems
1981 - IRG/WP 2157
Methods for testing the efficacy of preservative treatments for exterior joinery are described using the format of a European Standard. Commercially used treatments applied to jointed test units (L-joints) which are then protected by conventional finishes are exposed to normal outdoor hazards out of ground contact. Assessment is made a) by determining eventual failure through decay and b) by destr...