Effect of wood decay on the proportional limit of thin wood samples stressed in the bending mode
2006 - IRG/WP 06-20334
When using bending stiffness as a measure of wood decay it is advantageous to repeatedly test individual samples after they are exposed to decay fungi for varying periods of time. In order to obtain reliable results, variation in modulus of elasticity (MOE) values of the test samples that are repeatable bent to a given deflection must be considered. In this study it was shown that sound 3mm thick ...
G Li, D Nicholas, T Schultz


Re-sealing cut ends of envelope-treated softwood framing timber to protect against damage by the Australian subterranean termite Coptotermes acinaciformis: A revisitation
2006 - IRG/WP 06-20335
The claim that Australian Coptotermes acinaciformis (Froggatt) do not appear to initiate damage on timber from the end grain, thereby negating the need for treating exposed cut ends of softwood framing material (35 ? 90 mm) which has a repellent Tanalith? T envelope, was further investigated. Specimens of commercial Pinus radiata D.Don framing timber (untreated) and Pinus elliottii Englem. (untrea...
B C Peters, M Lenz, J W Creffield


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Field Tests on Poles. A report from practice
2006 - IRG/WP 06-20343
A routine field inspection of some 1000 creosote poles during summer 2005 in northern Jutland, Denmark. The routine inspection was done by hammering, Pilodyn testing and taking core samples with a Matson Borer. Additionally a drill resistance measurement was done with a device consisting of the drill machine with a long, flexible steel needle with 1,5mm diameter and the measuring computer/battery-...
A Peylo, C-G Bechgaard


Performance of boron-treated radiata pine in above ground field tests in New Zealand
2006 - IRG/WP 06-30406
Boron treatment was approved for exterior, above ground use in New Zealand in 1958, provide treated commodities were painted with a three-coat paint system. Above ground tests of rail units and L-joints were established at the NZ Forest Research Institute (now Scion) between 1967 and 1980 to monitor performance of boron treatment in relation to that of untreated and CCA-treated timber. Results sh...
M Hedley, D Page


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


How to win friends and influence the market — Service Life Prediction and performance-based durability assessments of wood products in construction
2006 - IRG/WP 06-20348
Due to direct and implied demands from the market and from e.g. the EU Construction Products Directive, the need to supply service life estimates for building products is growing. For several years, a development of Service Life Prediction (SLP) methodologies has been going on, but the awareness of this development has hitherto reached only a very limited extent in the wood sector. For materials w...
F Englund


Standard Test Methods for Wood Preservatives by Laboratory Agar-Block Test
2006 - IRG/WP 06-20350
Wood is one of the most valuable and versatile resources for all sorts of constructional purposes. But timber in its various forms is subjected to several types of deterioration. This standard lays down the method for the laboratory determination of threshold value of wood preservatives against fungi. Most chemicals are initially tested for their ability to control decay fungi in agar-block tests....
P K Sarker, M A Rahman, M R Bulbul, T Das, G N M Ilias


Preliminary screening of a boron based wood preservative for biological efficacy (fungicidal) in treated timber
2006 - IRG/WP 06-30396
The resistance of Pinus radiata D.Don sapwood blocks, treated with a boron based preservative, to attack by five wood destroying fungi (Fomitopsis lilacino-gilva, Coniophora olivacea, Gloeophyllum abietinum (boron resistant), Serpula lacrymans and Perenniporia tephropora) was investigated. A phenyl pyrazole termiticide (fipronil) was also incorporated into the formulation to examine if its presen...
S R Przewloka, J A Hann, P Vinden


One year performance of graveyard stakes in the Northern Territory of Australia
2006 - IRG/WP 06-30398
This paper presents the one year progress performance of in ground graveyard stakes exposed to numerous termite species and decay fungi in tropical field conditions. The field study examines the efficacy of a new timber preservative formulation developed at the University of Melbourne, Australia. The biocides used in the formulation are fipronil (a phenyl pyrazole) and trimethyl borate. The pre...
B Ahmed, J Hann, S Przewloka, P Vinden, P Blackwell, P Plews


Laboratory bioassay and field trial on imidacloprid and cypermethrin as glueline treatments for softwood plywood
2006 - IRG/WP 06-30405
The effectiveness of imidacloprid and cypermethrin as glueline treatments for protecting phenol formaldehyde (PF)-bonded Pinus radiata (radiata pine) plywood from attack by subterranean termites was evaluated both in the laboratory and field. Imidacloprid was evaluated in two plywood constructions (19 ply x 1.6 mm-thick veneers and 5 ply x 3.2 mm-thick veneers) whereas cypermethrin was evaluated i...
J W Creffield, D K Scown


Further discussion of biological durability assessments of acetylated wood from several European institutes
2006 - IRG/WP 06-40340
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000-03, the European Commission funded the "Thematic Network on Wood Modification". This paper features a re-evaluation of work undertaken...
D Jones, W Homan, F Bongers


Effect of fumigation with Sulfuryl Difluoride on wood inhabiting fungi, a laboratory test
2006 - IRG/WP 06-30410
Special methods are necessary for the control of wood destroying organisms in the preservation of monuments and historic buildings because of the conservation of their originality and uniqueness. The control of wood destroying organisms can be realized with conventional liquid wood preservatives or alternative methods. One of these methods is the fumigation. One fumigant, which was in the past of...
A Pfeffer, W Unger, G Fröba, G Binker


Wood-Plastic Composites and the Durability Dilemma: Observations from the Field
2006 - IRG/WP 06-40351
Wood-Plastic Composites (WPCs) used for decking, window & door moldings have experienced dramatic growth in North America over the last several years, with annual production increasing at rates greater than 20% per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being t...
M J Manning, F M Ascherl, M E Mankowski


Wood plastic composites from modified wood. Part 2 - Durability in laboratory decay tests
2006 - IRG/WP 06-40353
The decay resistance of wood plastic composites, WPCs, was tested according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils, terrestrial microcosms, TMCs). The WPC materials were conically extruded profiles with 30% polypropylene content. The 70% wood content was untreated Scots pine sapwood, acetylated pine and heat treated Norway spruce, respective...
M Westin, P Larsson Brelid, M L Edlund, G Alfredsen


Resistance of DMDHEU-treated pine wood against termite and fungi attack in field testing according to EN 252. Results after 30 months
2006 - IRG/WP 06-40354
The aim of this study was to determine the effectiveness against decay and termite attack of pine sapwood treated with pure and modified DMDHEU in a field test according to European Standard EN 252. Some of the treatments tested were able to increase, within the period of the test reported (30 months), the resistance of the wood both to micro-organisms and termites. The curing process seems to be ...
S Schaffert, L Nunes, A Krause, H Militz


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


Leaching of CCA from Paraserianthus falcataria panels exposed to field conditions at Krishnapatnam harbour, Andhra Pradesh
2006 - IRG/WP 06-50241
This study assessed the leaching of copper, chrome and arsenic (CCA) from Paraserianthus falcataria (=Albizia falcataria) panels exposed to marine condition at Krishnapatnam harbour on the east coast of India. Metal loss was assessed in test panels after 6, 12, 24 and 36 months of exposure using Atomic Absorption spectrophotometer (AAS). The metal loss was found slightly higher in panels treated ...
B Tarakanadha, K S Rao


Current state of world standardization in the toxicometric methods for testing of wood preservatives
2007 - IRG/WP 07-20354
The paper presents an outline of the history of forming standardized toxicometric methods for testing of wood preservatives in the world during last 100 years. Numerous studies resulted in three main methods which are currently used for official and basis assessment of biocides: - agar-block method in Europe (EN 113); - soil-block method in the USA and Pacific countries (ASTM D 1413); - modifi...
J Wazny


A roadmap for performance-based specification of wooden components based on service life prediction
2007 - IRG/WP 07-20351
The need for an unified and harmonised system for performance classification and specification of wood and wood-based products in Europe emanates from requirements of users and the European Construction Products Directive, CPD. A road to a feasible specification system is outlined. Exposure-related performance prediction was worked out as a key task on the way to product specification. Therefore s...
C Brischke, A O Rapp


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Molecular methods as a tool within the field of wood protection – available methods and new possibilities
2007 - IRG/WP 07-20361
The area of wood protection is in a period of change. New tools are needed to understand the mode of action, and to further improve the new wood protection systems. A set of useful tools are found among the molecular methods. This paper presents an overview of some of the tools available, and the methods are exemplified by papers within the frame of wood protection issues. However, there is stil...
G Alfredsen, A M Hietala, C G Fossdal, H Solheim


Comparison of laboratory termite test methods
2007 - IRG/WP 07-20365
Seven standardized laboratory tests with termites were evaluated. The bioassays were made in accordance with EN 117, SAA32 E08, SAA32 E09, Ebw 02, the American Wood-Preservers’ Association (AWPA) Standard E1-97, the Japan Wood Preserving Association (JWPA) Standard 11 (1) and The Protocols for Assessment of Wood Preservatives. Two different wood preservatives each in three concentrations and add...
H-U Kruschinski, W Unger, A F Preston


Predicting the decay resistance of timber above-ground: 2. When can reliable field data be obtained?
2007 - IRG/WP 07-20368
Application of modern performance-based engineering and design requires building products that are thoroughly characterised in terms of their ability to perform as expected over time. The engineering community is attempting to use this information to provide predicted service-lives for various building elements. Increasingly, this service-life prediction must be based on objective measurement coup...
L P Francis, A J Swain, J J Morrell