IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 805 documents. Displaying 25 entries per page.


Evaluation of white-rot fungal growth on Southern Yellow pine wood chips pretreated with blue-stain fungi
2000 - IRG/WP 00-10349
White-rotting basidiomycetes do not colonize on southern yellow pine. This study seeks to reduce the resinous extractive content of southern yellow pine by treating it with blue stain fungi. The mycelial growth of wood-inhabiting ligninolytic white-rot fungi can be achieved on pretreated southern yellow pine wood. Aureobasidium, Ceratocystis, and Ophiostoma spp. removed 70% to 100% of the extracti...
S C Croan


Inorganic preservative levels in soil under treated wood decks after 8 years natural exposure in Borås, Sweden
2005 - IRG/WP 05-50233
Inorganic preservative components (Cu, Cr and As) were measured to a depth of 150 mm under deck structures made with Scots pine lumber treated with several different wood preservatives and installed in Borås Sweden 8 years ago. Higher contaminant levels were observed mainly under the drip lines and in the top 50 mm of soil. Under CCA treated decks, soil arsenic concentrations increased from ba...
P A Cooper, Y T Ung, M-L Edlund, J Jermer


Enzyme immunoassay to detect Postia placenta in field tests: Comparison of plate ELISA with hydrophobic cloth and cotton dipstick
1991 - IRG/WP 2378
Standard indirect enzyme-linked immunosorbent assay in polystyrene 96-well plates was compared to hydrophobic polyester cloth and cotton dipstick for detection of wood-derived antigens from the brown-rot fungus Postia placenta. The ease of handling, larger surface area, and economics of the latter two adsorbents were surveyed for application as field tests for detection of early decay. At high ant...
C A Clausen


Performance of water-borne pressure treated fence posts - A practical application of the new Canadian field test data base
1988 - IRG/WP 2305
50 years of test plot data acquisition have been recently set up as a computerized database. The new database which contains information on the service life of a great number of non durable Eastern Canadian wood species treated with various preservatives and many application processes is presented. As an example for its use, a summary of the performance of fence posts treated with waterborne prese...
E E Doyle, R Dubois, J P Hösli


Control of wood biodeterioration by fungal metabolites
1992 - IRG/WP 92-1527
Treating wood with different conventional preservative chemicals for protection and economic utilisation is well known. Tough some of these chemicals are toxic to skin, their use as wood preservative is unavoidable as they should be toxic to biodeteriorating organisms also. Recent advances in chemistry of natural products enabled the use of wood extractives as biocidal compounds against biodeterio...
H S Ananthapadmanabha, H C Nagaveni, V V Srinivasan


Chemical treatment of chips for outdoor storage. Evaluation of sodium N-methyldithiocarbamate + sodium 2,4-dinitrophenol treatment
1980 - IRG/WP 2134
Fresh slash pine chips were treated by spraying them with a dilute aqueous solution of sodium N-methyldithiocarbamate and sodium 2,4-dinitrophenol. The were then formed into an experimental chip file 10 feet high, and the pile was maintained for seven months. The treatment effectively slowed heat release and retarded losses in wood substances, tall oil, pulp yield, and pulp strenght. Under certain...
E L Springer, M Benjamin, W C Feist, L L Zoch, G J Hajny


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


Laboratory versus field tests for evaluating wood preservatives: A scientific view
1995 - IRG/WP 95-20076
The relative merits of field tests versus laboratory tests for evaluating wood preservatives are discussed. Many of the problems involved in interpretation of the results are similar for both types of test. One major problem is to select field sites or laboratory tests that are representative for the practical use of treated timber in ground contact. Decay tests with treated wood in unsterile soil...
T Nilsson, M-L Edlund


Accelerated testing for out of ground contact using natural biological preconditioning
1996 - IRG/WP 96-20088
Small blocks made of Scots pine sapwood were treated, buried in vermiculite and exposed to natural microbial colonisation during outdoor exposure prior to laboratory decay testing. Periodic microbial isolations, moisture content, permeability and weight loss tests were also conducted. Bacteria and moulds colonised the vermiculite and miniblocks well. Aureobasidium pullulans was common on TnBTO tre...
S Molnar, D J Dickinson, R J Murphy


Performance criteria for approving new wood preservatives for ground contact
1994 - IRG/WP 94-20021
Protocols for testing novel formulations prior to approval or registration as wood preservatives are being developed in a number of countries, e.g. Australia, New Zealand, USA. One aspect which must be addressed is the effectiveness in tests relative to that of currently approved formulations which would be acceptable to approving authorities. It is assumed that natural exposure testing is a prere...
M E Hedley


Laboratory evaluation of JB-TB003 as potential bait toxicant against the subterranean termite, Coptotermes acinaciformis in Australia. subterranean termite, Coptotermes acinaciformis in Australia
1997 - IRG/WP 97-10214
In this laboratory evaluation, Coptotermes acinaciformis actively attacked in the first week of testing Pinus radiata wood blocks (50 x 25 x 15 mm3) treated with concentrations of JB-TB003 (i.e. 25, 50, 100, 200 and 400 ppm); the blocks with highest concentration were the most attractive. Results were similar whether blocks were leached or unleached. The earliest mortality occurred in the 400 ppm ...
B M Ahmed, J R J French, A R Valcke, P Blunt


Isolation and identification of the fungal flora in treated wood. Revised technique
1977 - IRG/WP 159
At the 8th Annual Meeting in Wildhaus a paper was presented for discussion on the isolation of fungi from treated wood.·Since then work of this nature has been undertaken at Imperial College and as a result a revision of that document has been made and is presented here. The main alterations are: 1) To streamline the isolation procedure 2) Modification of the benomyl agar 3) The inclusion of a st...
C P Clubbe, J F Levy


Evaluation of tropolone as a wood preservative : activity and mode of action
2002 - IRG/WP 02-30282
The fungicidal activity of 2-hydroxy cyclohepta-2,4,6-trienone (tropolone) analogue of b-thujaplicin a natural product responsible for the durability of heart wood of several cupressaceous trees was investigated in vitro on growth of white and brown rot fungi. Results obtained show that tropolone, easily prepared from commercially available products, possesses strong fungicidal activity similar ...
P Gérardin, M Baya, N Delbarre, P N Diouf, D Perrin, P Soulounganga, E Gelhaye, J P Jacquot, C Rapin


Comparison of three methods of quantitative evaluation of sapstain in rubberwood
2000 - IRG/WP 00-20188
Assessing the extent of fungal stain on wood during laboratory trials is a subjective process and is subjected to considerable variation between individual evaluators and specimen. The purpose of this paper was to explore the potential of three quantitative methods of wood surface measurement of rubberwood specimens degraded by sapstain and mould fungui (Botrydiplodia theobromae, Aureobasidium pul...
A J Ashari, J W Palfreyman, A H H Wong


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


Development and field trials of Evotek 230, a new antisapstain product
1997 - IRG/WP 97-30140
Laboratory and greenhouse studies, using freshly sawn pine boards, demonstrated that the fungicidal properties of prochloraz and carbendazim were complementary for protection from sapstain and mould under extreme conditions of close stacking and high humidity. Analysis of dip bath solutions before and after dipping 20 boards showed no evidence of any stripping of the active ingredients. Neither fu...
A Adams, J Oudenweyer, J L Lindars


A field test on susceptibility of wood-based board materials to moulds
1989 - IRG/WP 3545
A field test on susceptibility of wood-based board materials to mould growth was carried out under practical, but severe, service-conditions. A total of 19 commercially available composite boards were investigated. It was found that all board materials tested were not completely immune to mould attack. Test results revealed that among the three main categories of wood-based boards involved, partic...
Qiao Wang, B Henningsson


International standardisation: a hypothetical case study with stand-alone borate wood preservatives
1998 - IRG/WP 98-20147
The possibility of developing wood preservation standards with a global remit has a number of obvious advantages as well as far reaching ramifications, many of which are undefined as yet. The commercial implications of adopting international standards are clearly considerable, but equally, such a development is likely to focus attention on the conceptual differences in the way that different regio...
M W Schoeman, J D Lloyd


Fungus cellar and antisapstain field trial studies of six triazole fungicides
1995 - IRG/WP 95-30077
The efficacy of six triazole fungicides was compared using a fungus cellar soil bed test, a rapid antisapstain laboratory trial and a 36 week antisapstain field trial. After 21 months in the fungus cellar the mean soundness of radiata pine treated with 1.5 kg/m³ of cyproconazole, azaconazole, hexaconazole, tebuconazole, propiconazole and flusilazole in combination with 1.0 kg/m³ didecydimethyl a...
R N Wakeling, J G Van der Waals, R D Narayan, J B Foster, B E Patterson, P N Maynard


The wood preservative performance of biocide mixtures containing chlorpyrifos
1994 - IRG/WP 94-30055
Chlorpyrifos (O,O-diethyl[3,5,6trichloro-2-pyridyl]phosphorothioate) was evaluated as a wood preservative insecticide in two long term field tests. In the first project, pine sapwood blocks treated with chlorpyrifos (CPF) were exposed to Coptotermes formosanus using an above-ground test format. CPF is effective in protecting wood from attack by this termite, but its activity appears to decrease wi...
P E Laks


Protection for whole-of-house timbers from subterranean termites in Australia
2005 - IRG/WP 05-20315
A field study was designed to increase maximum protection of whole-of-house timbers against subterranean termites. Concrete slab and suspended floor simulated houses were constructed using untreated and treated (slow acting toxicants) timber frames. The treated and untreated timber structures within the simulated houses were exposed with or without soil chemical and/or physical barriers in the fie...
B M Ahmed, J R J French, P Vinden, P Blackwell, J Hann


Biological control of internal decay in Scots pine poles: A seven year experiment
1992 - IRG/WP 92-1529
The interactions between key fungi were monitored, by non-destructive and destructive sampling methods, during the course of an experiment on the effectiveness of Scytalidium sp. and Trichoderma spp. for eliminating established infections of Lentinus lepideus (Fr. ex Fr.) Fr. in creosoted Pinus sylvestris poles. Although extensively isolated at the beginning and end of the experiment, Trichoderma ...
P I Morris, D J Dickinson, B Calver


Comparison of laboratory tests and field experiments for the estimation of emissions from treated wood
2005 - IRG/WP 05-50224-6
The authorisation procedure for biocidal products according to the European Biocides Direc¬tive in¬cludes the assessment of possible environmental risks by the emission of ac¬tive ingre¬dients. This needs an input of data on the expected emissions of biocides into environmental com¬part¬ments. The procedures for the estimation of these emissions should be harmonised. La¬boratory test proceÂ...
U Schoknecht


Evaluation of the permeability of fast grown wood species
1995 - IRG/WP 95-40042
The low natural durability of certain species of wood, implies the need for applying a protecting treatment to increase its life in service. Because of this, a knowledge of the permeability properties of the wood is desired. In this work, a simple and reliable method to evaluate the wood permeability is presented. For that, we have been used fast grown species, with low natural durability, Poplar ...
M T De Troya, A M Navarrete, E Sanchez, J E Garcia de los Rios, E L Rodríguez Trobajo


Limitations of the Pilodyn when assessing decay in graveyard test stakes
1982 - IRG/WP 2168
The following examination was designed to evaluate more precisely the usefulness of the Pilodyn for routine, objective assessments of the condition of field test stakes and to examine its limitations, particularly in respect to: 1.) The importance of variables other than extent of decay which may affect Pilodyn readings; 2.) Practicality of obtaining multiple readings in decayed and non-decayed re...
M E Hedley


Previous Page | Next Page