IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 644 documents. Displaying 25 entries per page.


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Field Liners as physical barriers to prevent wooden utility pole decay in soil: An accelerated field simulation trial
2008 - IRG/WP 08-20384
Field Liners (FL’s), plastic sleeves used to protect in-ground wooden poles from fungal and termite damage, have been tested before as physical barriers to prevent contact between soil and wood and to retain wood preservative treatment. These earlier studies concentrated mostly on creosote preserved poles and early generation FL’s which were cumbersome in their application. The newer generatio...
A R Howgrave-Graham, L J Cookson, T Hale


Field Stake Tests with Copper-based Preservatives
2008 - IRG/WP 08-30459
The performance of field test stakes derived from commercially produced ground contact retention copper quat preservatives based on either soluble copper complexed with ethanolamine, or from a water-based suspension of particulate micronized copper compounds, as well as untreated southern yellow pine controls, is compared at two decay test sites. After less than one year in field test some of t...
A Preston, L Jin, D Nicholas, A Zahora, P Walcheski, K Archer, T Schultz


Above and Below-Ground Copper-Azole and Copper, Chrome Arsenate Depletion from Pinus radiata and Fagus sylvatica at Thirteen New Zealand & Australian Sites
2008 - IRG/WP 08-30460
The objective was to determine the significance of site on preservative depletion from Pinus radiata D. Don and Fagus sylvatica L. 20 x 20 x 500 mm field test stakes treated with a ground contact retention of copper amine plus tebuconazole (CuAz) and copper chrome arsenate (CCA) after approximately 5 years exposure to widely different soil and climate conditions. Site, wood species and their inter...
R Wakeling


Field Tests of naturally Durable North American Wood Species
2008 - IRG/WP 08-10675
There has been little field test performance data published on North American naturally durable species in general, and no published data on second growth material in particular. Yellow cedar (Callitropsis nootkatensis), western red cedar (Thuja plicata), eastern white cedar (Thuja occidentalis), and three wood species reputed to be moderately durable were installed in ground-contact (stakes) an...
P E Laks, P I Morris, G M Larkin, J K Ingram


To decay or not to decay: An accelerated field test of the validity of the Scheffer index
2008 - IRG/WP 08-20392
The Scheffer Index was introduced in 1971 to predict the relative decay hazard of untreated wood exposed above-ground. Precipitation and temperature parameters are used in the calculation. A higher Scheffer Index value implies a greater risk of decay. An accelerated 18-month study using seven field sites with Scheffer Indices ranging from 35 to 400 and two wood types (Populus tremuloides and Pi...
G M Larkin, P E Laks


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Field testing in Colombia: Three years of evaluations and experiences
2008 - IRG/WP 08-20394
Two field test sites have been established in Colombia for the evaluation of fungal and termite resistance of treated wood. The combination of elevated temperature, high and stable humidity and high rainfall at the two test sites accelerates microbial and insect activity (Scheffer, 1971; Thornton et al, 1994; Freitag et al, 1995). Tests established include above ground termite tests, ground contac...
Y Cabrera, A Preston


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Utilidad práctica de mini estacas en ensayos de campo
2009 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks


Field Stake Performance of Parallel Strand Lumber Treated with Waterborne Copper Naphthenate
2008 - IRG/WP 08-40435
Wood and wood products have been considered a premium building material for residential and industrial structures for many centuries. More recently, structural composite lumber (SCL) products have played an increasing role in satisfying the needs of the building industry. However, both wood and wood composites are naturally biodegradable materials which require enhanced durability when used in ce...
G P Merrick, M H Freeman, J A Brient


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Accelerated H3 above-ground decay trials in Australia
2009 - IRG/WP 09-20411
An above-ground H3 fungal field trial was installed at five sites (3 in Australia, 2 in New Zealand), with the aim of finding a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter of the H3 preservative retentions were mostly installed, as first results suitable for registration occur when these reach 70% soundness. Chemical analysis of ...
L J Cookson, J Carr


Review of candidate graded particle barrier testing methods in Australian Standard (AS 3660.3 – 2000): Assessment criteria for termite management systems
2009 - IRG/WP 09-20417
The Australian Standard (AS. 3660.3 – 2000) for assessment of candidate graded particle termite barriers is reviewed and suggestions for amendments are made. Areas requiring amending in light of current biological knowledge involve the inclusion of proprietary or patented systems rather than generic types; selection of test termites in the genus Coptotermes; duration of test periods; and inadequ...
J R J French, B M Ahmed (Shiday), B L Schafer


Laboratory and field evaluation of Laminated Strand Lumber treated with Borogard® ZB against termites
2009 - IRG/WP 09-30498
A laboratory bioassay and subsequent field trial was undertaken to determine the termiticidal effectiveness of a Laminated Strand Lumber (LSL) composite when treated with Borogard® ZB. The bioassay and field trial were conducted against two of Australia’s most economically important species of termite, Mastotermes darwiniensis and Coptotermes acinaciformis. Against both species of termite, LSL ...
D K Scown and J W Creffield


Effectiveness of a superficial treatment of bifenthrin to protect softwood framing from damage by subterranean and drywood termites in Indonesia
2009 - IRG/WP 09-40443
Various experimental testing procedures were undertaken in Indonesia to determine the effectiveness of a superficial (envelope) treatment of bifenthrin to protect softwood framing from damage by two species of subterranean termite (Macrotermes gilvus and Coptotermes curvignathus) and one species of drywood termite (Cryptotermes cynocephalus). Lengths of framing (Pinus radiata sapwood) were commerc...
P Sukartana, J W Creffield, A Ismanto, N E Lelana


Termite Resistant Properties of Wood and Natural Fiber Plastic Composites - AWPA E1 Test Data
2009 - IRG/WP 09-40466
This paper deals with resistance properties of wood plastic composites against Formosan Subterranean Termites (FSTs) based on the AWPA E1 test standard. Sixteen laboratory WPC formulations, four WPC commercial materials, and southern pine (Pinus sp.) wood control were tested for termite mortality, sample weight loss, and sample damage rating. The results show that FSTs did attack WPC products in ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


Utilidad práctica de mini estacas en ensayos de campo
2008 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Observations on colony collapse in Reticulitermes flavipes (Kollar) in laboratory and field settings in Wisconsin
2010 - IRG/WP 10-10709
Parallel strategies were designed to eliminate Reticulitermes flavipes (Kollar) from a field site in Endeavor, Wisconsin and a simulated field test setup of approximately 20,000 workers in the laboratory. Indoor and outdoor colonies of R. flavipes were baited with commercial cellulose monitoring stations and rolled cardboard stations. If the commercial cellulose baits were attacked, they were repl...
F Green III, R A Arango, G R Esenther


Seasonal shifts of fungal community structure at the interface of treated or untreated wood and soil
2010 - IRG/WP 10-10721
Many wood species are degraded rapidly in soil by the fungal community. In order to preserve wood and structures in which it is used, chemical preservatives are used. Little is known about the interaction of treated wood and the surrounding soil fungal community. For this work, presented at IRG 41, wooden specimens (Pinus sylvestris sapwood, sizes 25 mm x 50 mm x 500 mm (longitudinal)) were treate...
M Noll, I Stephan


Estimating the age of subterranean termite attack and damage in buildings
2010 - IRG/WP 10-10727
This paper describes physical and experimental methods and a mathematical model (Rotramel 2003) to assist in estimating the age of subterranean termite attack and damage to building structures. Timber, building and termite management industries have to develop new strategies to assess and estimate termite attack and damage in the current climate of global warming. A case study will be used as an e...
J R J French, B M Ahmed Shiday, J Thorpe


Natural durability of African Padauk and Niove. Comparison of new trials and former data from the CIRAD database
2010 - IRG/WP 10-10743
African Padauk (Pterocarpus soyauxii) and Niove (Staudia kamerunensis) were tested in laboratory against Basidiomycetes. The results were calculated according to the requirements of EN 350-1 (1994) and XP CEN/TS 15083-1 (2006). Padauk samples showed a high durability and very small variations between trees and within tree. Niove presented a high durability, but with notable differences according ...
Y N N’Kolo Meze’e, N Leménager, C Baudassé, M-F Thévenon


Glued laminated poles - Progress report after 30 years testing
2010 - IRG/WP 10-20427
In 1979 a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and in a power lane in Vuollerim in northern Sweden in order to study their resistance against biological degradation. The tests have shown that the best performance will be obtained if each lamination is treated with a water-borne pre...
Ö Bergman, J Jermer


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


Previous Page | Next Page