Decay resistance of Scots pine (Pinus sylvestris) heartwood against brown rot
2002 - IRG/WP 02-10433
Natural decay resistance of wood is mainly restricted in the heartwood and based on wood microstructure and chemical composition. The genetic variation in the durability of Scots pine (Pinus sylvestris L.) wood against decay and the relationship between resistance and chemical composition was studied. The laboratory tests of 6 and 8 weeks were carried out with a brown rot fungus Coniophora puteana...
H Viitanen, A M Harju, P Kainulainen, M Venäläinen


Effect of permeability and extractives on the decay rate of southern pine sapwood in above grund exposure
2005 - IRG/WP 05-20310
The effects of wood permeability and hydrophilic and hydrophobic extractives on the decay rate of southern pine sapwood in above ground exposure were investigated. Permeability was determined by water sorption measurements, and the effect of extractives was studied by pre-extracting the test samples prior to outdoor exposure using water to extract hydrophilic extractives or sequential methanol/cy...
D D Nicholas, T Schultz, L Sites, D Buckner


A summary of work carried out to compare natural and artificial weathering for preconditioning test specimens in testing anti-stain chemicals for wood in service
1976 - IRG/WP 266
Since 1972 work has been in progress within CEN to establish a European standard for the testing of wood preservatives designed to prevent blue-staining of wood in service. The method is based on the Butin test and involves pre-weathering of the samples prior to biological testing. The weathering regime employed is 6 months outside exposure from March to October. This imposes severe limitations on...
D J Dickinson, A F Bravery


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Laboratory evaluation of chlorothalonil formulation for stain and mold control on rubberwood and maple
1998 - IRG/WP 98-30175
We evaluated the efficacy of several chlorothalonil and carbendazim fungicides (F1 and F2), etc. in the control of mold and stain fungi on rubberwood and maple. The results showed that these formulations effectively inhibited the selected fungal species such as Aspergillus niger, Penicillium sp., Trichoderma sp. (P71H), Aureobasidium pullulans, Ceratocystis minor (C-188), Ceratocystis pilifera (RW...
Mingliang Jiang, T L Highley, L Ferge, T L Woods


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...
O Encinas, G F Daniel


Relationship between bond strength and surface characteristics of CCA-treated Douglas-fir
1993 - IRG/WP 93-30008
Chromated-copper-arsenate (CCA) treated Douglas-fir was laminated using a commercial phenol-resorcinol resin. CCA treatment enhanced the water repelleney of wood espeeially in the presence of extractives. However, the shear strength of CCA treated wood was 12% lower in dry condition and 38% lower in wet condition after six cycles of vacuum-pressure test than that of untreated wood. Slight removal ...
K Yamamoto, J N R Ruddick


UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Bioassays of extracts from scaly ash (Ganophyllum falcatum B1) against the subterranean termite Coptotermes acinaciformis (Froggatt)
1983 - IRG/WP 1206
Scaly ash, Ganophyllum falcatum B1. wood shavings were extracted by methanol, and fractionated with ethyl acetate, diethyl ether and water, and the anti-termitic properties of these materials bioassayed against the subterranean termite Coptotermes acinaciformis (Froggatt). Laboratory techniques were developed to overcome the problem of limited extractive materials. The results of the various bioas...
J R J French, J P Robinson, J W Creffield


Resolution from IRG Working Group II Sub-group 4 'Stain in timber in service'
1984 - IRG/WP 2230
Sub-group 4 of IRG Working Group II has completed a series of studies of artificial weathering as an alternative to natural weathering in relation to testing the efficacy of chemicals in preventing blue stain in service. The Sub-group reports that within the limits of the equipments studied and described in its report Document No: IRG/WP/2215 the extent of blue stain varied little as a direct cons...
D J Dickinson


Effectiveness of a newly registered antisapstain preservative in preventing stain of Eucalypt timber in Australia
2000 - IRG/WP 00-30229
An antisapstain trial was conducted on two sites (Alexandra and Trentham) in order to establish the concentration of a newly registered antisapstain preservative (consisting of benzalkonium chloride (BAC) & 3-iodo-2-propynyl butyl carbamate (IPBC) & disodium octoborate (boron)) needed to prevent stain of Eucalypt timber. After 20 weeks of exposure at the Trentham site, the water treated bo...
J Snow, P R S Cobham, N Ryan


Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson


Attempt for developing a new method for above ground field testing of wood durability
2000 - IRG/WP 00-20199
Field testing remains the most appropriate way for evaluation of wood preservatives or natural durability of wood species. Above ground tests are designed to answer specific questions concerning the outdoor utilisation of wood. Such methods supply additional information and confirm or reject preliminary laboratory results. The European standard (ENV 12037, "lap-joint") for assessment of the durabi...
N Terziev, M-L Edlund


Variation in infection rates of blue-stain, mould and white rot tropical fungi on mixed light Malaysian woods
2000 - IRG/WP 00-10334
The modified 3-week FRIM laboratory method for screening of anti-sapstain formulations against three representative tropical fungi causing blue-stain (Botryodiplodia theobromae), mould (Paecilomyces variotii) and white rot (Schizophyllum commune) infection of sapwood species was used to examine the relative resistance of the sapwood of eight mixed light Malaysian woods, Scots pine (Pinus sylvestri...
A H H Wong, S Ahmad


Preventive effectiveness of petroleum derivatives against blue-stain fungi. Part 2
1993 - IRG/WP 93-30001
Solvex-Tar, a product derived from the distillation of petroleum could be suitable for the treatment against blue-stain fungi in wood used in exterior carpentry, due to its effectiveness as a fungicide. The aim of this work has been to optimize the application of this product, modifying it as necessary, so as to improve its physical characteristics without interfering with its preventive effective...
E Sanchez, M T De Troya, A M Navarrete, A Guijarro


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


The influence of the natural extractives of opepe (Nauclea diderrichii) and African padauk (Pterocarpus soyauxii) timbers on their durability
1996 - IRG/WP 96-30098
Many timbers contain chemical extractives that undoubtedly play a key role in the timber's natural durability. Opepe (Nauclea diderrichii) and padauk (Pterocarpus sp.) are both very durable timbers (class 1), yet they are described as being moderately permeable. This suggests the presence of biocidal chemicals within these timbers, rather than simple blocking agents. Initial trials on the...
E D Suttie, R J Orsler


Using image analysis to rate wood stain trials
1993 - IRG/WP 93-10034
Assessing the extent of fungal discoloration on wood during laboratory trials is a subjective process which provides an opportunity for considerable variation between individual evaluators of specimens. The development of reliable systems for automatically assessing discoloration would minimize evaluator bias and permit comparisons between results from different laboratories. The use of image anal...
C M Sexton, A G Maristany,C C Brunner, J J Morrell


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


Preventive effectiveness of petrol derivatives against blue-stain fungi
1992 - IRG/WP 92-3716
A possible application of fractions obtained on petrol pyrolysis is their use as a wood preservative against wood-decay and sap-stain fungi. From two of these fractions were prepared three different products (ST, STL and SST). The aim of this work has been the possibility of utilizing these products in the treatment of wood used for external joinery, determining their effectiveness against blue-st...