Intraspecific variability of durability of Wapa courbaril (Eperua grandiflora) against Antrodia sp. and Coriolus versicolor: effect of radial and height position in the stem
2004 - IRG/WP 04-10531
The variation of a lesser-used species, Eperua grandiflora attacked by brown and white rot has been examined. Trees of this specie showed differences in their behaviour against the type of rot used and also showed evidence of intra and inter tree variation. The “tree” effect is very significant concerning natural resistance. In the same way, there is variation of durability observed according ...
N Amusant, J Beauchêne, M Fournier


Results on field stake tests against termite – Maximum for 8 years examination at Kumamoto in Japan
2003 - IRG/WP 03-10463
Various preservative treated or modified wood and charcoal painting stakes were tested in field, maximum for eight years in Kumamoto, distributed two main termite species, Coptotermes formosanus and Reticulitermes speratus. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservative treated stakes were observed no signif...
K Suzuki


Assessing the importance of degradation mechanisms on the loss of effectiveness of wood preservatives
2000 - IRG/WP 00-20193
Accelerated ageing systems developed for application to samples in the laboratory prior to biological tests, should reflect those natural deterioration processes that are likely to occur in the hazard classes defined in EN 335-1. Losses through evaporation or the effects of leaching have been recognised, however their importance, relative to other mechanisms has not been quantified. Degradation me...
E D Suttie, R J Orsler, T Dearling


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz


Microwave digestion of preserved wood for the determination of Cu, Cr, As, B and P in quality control
1991 - IRG/WP 2364
A microwave digestion method for the determination of copper, chromium, arsenic, boron and phosphorus in preserved woods is described. Samples were digested with nitric acid in pressure-relief type teflon PFA vessels by microwave heating in a commercial laboratory microwave oven. Fast, efficient and complete digestion was achieved within 29 min for 12 samples. The digestion time compared favourabl...
N Bernth, L B Sheard


Bacterial degradation of Pinus radiata compression wood
1996 - IRG/WP 96-10153
An inspection of twelve year old, CCA-treated Pinus radiata wood from an industrial cooling tower showed extensive surface decay of wood. Electron microscopic examination of decaying compression wood indicated that compression wood cells were attacked exclusively by bacteria, which were of erosion and tunnelling types. As compared to the normal wood, compression wood appeared to be more resistance...
A P Singh, R N Wakeling


Effect of humidity fluctuations on mould growth on pine wood
1989 - IRG/WP 1412
Most studies on mould development on wood material have been made at constant moisture conditions during the experimental period. As a consequence of such studies, a maximum permittable humidity level to avoid mould problems in wood constructions has been recommended. In the practical situation, the constructions are seldom subject to constant humidity or temperature. In the present paper, we repo...
J Bjurman


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Second update
1995 - IRG/WP 95-10117
As was agreed by members at the termite workshop at the 24th annual meeting of IRG in Orlando, USA, in May 1993 to initiate an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists was initiated. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives (CCA and Cu-naphthen...
J R J French


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Effects of heat treatment on modulus of elasticity of beech wood
2002 - IRG/WP 02-40222
Heat treatment is the oldest, simplest and cheapest method for reducing hygroscopicity of wood. The heat treatment protects wood against to biological organisms as well as giving wood dimensional stabilization without damaging environment. The effects of heat treatment on modulus of elasticity (MOE) of beech wood (Fagus orientalis Lipsky) naturally grown and intensively used in forest products in...
S Yildiz, G Çolakoglu, Ü C Yildiz, E D Gezer, A Temiz


Formation of polychlorinated dibenzo-p-dioxins (PCDD) and polychlorinated dibenzofurans (PCDF) during the combustion of impregnated wood
1995 - IRG/WP 95-50040-19
Wood waste and industrial wood residues often contain various preservatives. The waste management for these residuals can be recycling, deposition or combustion. Among the three possibilities, combustion seems to be the most efficient way of disposal. To obtain detailed information about emissions of organic compounds with environmental impact, especially polychlorinated dibenzo-p-dioxins (PCDD) a...
T Salthammer, H Klipp, R-D Peek


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner


Effect of point of preservative addition on the mechanical and physical properties of strandboard treated with Tanalith 3485
2000 - IRG/WP 00-40152
Preservative has been added to a PF bonded strandboard at various different stages in the manufacturing cycle and the physical and mechanical properties of the boards have been evaluated (modulus of elasticity, modulus of rupture, thickness swelling, water absorption, internal bond strength, and shear strength). Preservative addition has been examined at five different stages namely green strand d...
G J Goroyias, M D C Hale


Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Organic nitrogen in wood: Growth substrates for a sapstain fungus
1993 - IRG/WP 93-10019
The nitrogen content of mature wood from lodgepole pine was 0.046% as determined by micro-Kjeldahl. Low molecular weight proteins between 14 and 21 kDa were identified in mature wood, branch wood and sap pressed from wood chips. Amino acids were quantified in acid-hydrolyzed wood samples and accounted for between 19 and 35% of the nitrogen in wood. The sapstaining ascomycete Ophiostoma piceae stra...
L D Abraham, C Breuil


Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu


Evaluation of copperised Cashew nut shell liquid and Neem oil as wood preservatives
2005 - IRG/WP 05-30368
An effort has been made to develop eco-friendly wood preservatives using naturally available plant by-products with less toxicity. Copper was incorporated into Cashew nut shell liquid (CNSL) and Neem seed oil. Rubber wood samples were treated with these solutions employing dipping and pressure techniques in 3 different levels. These samples have been evaluated to find out the effectiveness as wood...
D Venmalar, H C Nagaveni


Biological control of wood decay
1992 - IRG/WP 92-1531
This paper provides a general discussion of the principles underlying the concept of using biological control agents for the protection of wooden materials from decay. The rationale for the current upsurge in interest in biological control is discussed and a critical appraisal of the technology compared with the use of chemical wood preservatives is included. The advantages and limitations associa...
A Bruce


Diffusion modeling of inorganic wood preservative leaching in service
2005 - IRG/WP 05-50224-5
To evaluate the potential environmental and health implications of leaching of inorganic wood preservatives in service under different conditions, there is a need for a predictive model that provides estimates of the rate and extent of leaching over a wide range of product dimensions and exposure conditions. In this paper, we show that the leaching behavior of inorganic preservative components fr...
L Waldron, P A Cooper, Y T Ung


Biological Safety Evaluation of Animal Contact of Preservative-Treated Wood
2003 - IRG/WP 03-50196
Biological safety of preservative-treated woods that could be contacted to human and animal was evaluated for rat and rabbit exposed to CCA-, ACQ- and CCFZ-treated woods. The accumulation of preservatives ingredient in the rat’s plasma and viscera, and the transforming function of replacing preservatives were examined in this study. The result indicated that preservative-treated wood did not bri...
Dong-heub Lee, Dong-won Son, Myung Jae Lee, Chang Ho Kang, Cheon Ho Kim, Eui-Bai Jeung


Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner