IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 140 documents. Displaying 25 entries per page.


COST Action FP0904 – Increasing the Understanding of Thermo-Hydro-Mechanical Wood Behaviour and Processing
2013 - IRG/WP 13-40646
The polymeric components of wood and its porous structure allow its properties to be modified under the combined effects of temperature, moisture and mechanical action – so-called Thermo-Hydro-Mechanical (THM) treatments. Various types of processing techniques, including high temperature steam with or without an applied mechanical force, can be utilised to enhance wood properties, to produce eco...
D Jones, P Navi


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


How to Increase the Lifespan of Exterior Wood Coatings
2015 - IRG/WP 15-40700
In addition to aesthetic appeal, coatings are designed to protect the wood from weathering degradation in outdoor conditions. This paper gives an overview of the effects of main components of coating, coating properties, and wood treatments on coating performance. Understanding how different type of resins (alkyd, acrylic or polyurethane), amount of pigments, type of solvents (organic or water), a...
M Nejad


Termite Management and the U.S. Experience: A Case for Wood Treatment & Integrated Control
2015 - IRG/WP 15-30678
A brief overview of termite control is given using specific experiences from the U.S.A. Five major types of termite treatment now prevail: soil applied chemical barriers, in-structure chemical barriers (in-situ applied wood and foundation treatments), physical barriers, treated wood and termite baits. In general, ‘stand-alone’ pretreatments or ‘primary’ treatments are often discussed and ...
J D Lloyd, K van den Meiracker


Foundation piles: analysis of beech wood decay in service life conditions
2016 - IRG/WP 16-10858
Wood piles foundation system was largely used over decades. Thus, numerous buildings over the world are based on this constructive system. In the context of reduction of CO2 emissions in the building field of constructions, substitution of concrete by wood as material for foundation piles seems to be a promising alternative. However, fluctuation of the water table level in soil may promote fungal ...
Q Kleindienst, A Besserer, M-L Antoine, C Perrin, J-F Bocquet, L Bléron


Production of reactive oxygen species in the presence of oxidized iron and oxalate under conditions mimicking brown-rot fungal degradation of wood
2016 - IRG/WP 16-10861
The biochemical role of oxalate in the fungal solubilization of iron is well known, but additional information is needed on the role that oxalate plays in the brown-rot decay of lignocellulose. In this study iron sequestration from iron and iron oxide-hydroxides was assessed with regard to the function of a chelator-mediated Fenton (CMF) reaction and the generation of reactive oxygen species (ROS)...
Yuan Zhu, Liangpeng Zhuang, B Goodell, Jinzhen Cao, J Mahaney


On the effect of climate and exposure conditions on durability indicators and their potential for service life prediction of wood-based products
2016 - IRG/WP 16-20576
In order to encourage increased use of wood, different user groups need to be better informed regarding the variation in performance between different wood materials and the effect of different use classes. It is also important to provide good empirical data on the service life of wood products as input to for example life cycle assessment studies. In the current study the effect of temperature an...
G Alfredsen, C Brischke, P-O Flæte, M Humar, L Meyer-Veltrup


Variation in moisture content in field trials according to use class 3.2 conditions
2016 - IRG/WP 16-20580
Different test methods to determine the durability of wood in use class 3 (EN 335:2013) are available. Fungal degradation of wood requires liquid water. Different Standards (EN 335-1:2006; DIN 68 800:2011) specify the risk for decay with moisture content (mc) of above 20%. EN 335 (2013) does not specify moisture content but rather defined limited wetting conditions (use class 3.1) or prolonged wet...
S Bollmus, A Gellerich, H Militz


Engineering for Rural and Civil Development. Uni Performance of wood exterior structures above ground contact in Spain built with softwood species. The situation of cases in northern Spain
2016 - IRG/WP 16-20597
Across Europe is very common to find exterior structures build in sawn and glue-laminated wood. Most of these exterior structures used softwood wood species such as fir, spruce, larch and pine. In Spain wood exterior structures, as for example bridges, became more and more popular since eighties, when sawn and glue-laminated wood were utilized for building exterior wooden structures in overall Spa...
D Lorenzo, J Fernández-Golfín, M Touza


Performance of 3-iodo-2-propynyl butyl carbamate (IPBC) in L-joints under tropical conditions
2016 - IRG/WP 16-30688
The ability of 3-iodo-2-propynyl butyl carbamate (IPBC) to protect wood against fungal decay out of soil contact was evaluated using ponderosa pine L-joints at two exposure sites over a 12 year period. IPBC tended to provide better protection when formulated in an organic solvent and when applied using a double vacuum treatment. Performance also tended to be better when systems contained a water...
J J Morrell


Thermoplastic Plywood at Moderately Increased Thermal Conditions
2016 - IRG/WP 16-40735
New thermoplastic plywood material so-called GradaTM manufactured by UPM has vast potential in production of wooden products with new approach of manufacturing. This paper examines possibilities of including GradaTM material in skateboard deck production as a large use of plywood type construction in this manufacturing sector. Bending strength (BS) and tensile strength perpendicular to the surface...
R Réh, M Guoth


Optimising wood chemical modification with lactic acid oligomers by screening of processing conditions and chemical additives
2016 - IRG/WP 16-40741
Oligomer systems based on lactic acid (OLA), were impregnated in wood and polymerised in-situ by heat treatment to improve the properties of the treated wood especially regarding anti-swelling efficiency (ASE), hygroscopicity, water leaching resistance and durability. This article relates the optimisation of the heat treatment conditions and the consideration of selected chemicals for improvement ...
C Grosse, M-F Thévenon, M Noël, P Gérardin


Exterior birch plywood: potentiality of the thermo-hydro treatment
2016 - IRG/WP 16-40743
It has been found in the present study that, in laboratory fungi tests after leaching with water (EN 84), exterior birch (Betula spp.) plywood, as birch solid wood, is subjected to degradation by rot fungi. This limits the use of such plywood outdoors or in building structures in high humidity conditions. The possibility to improve the birch plywood fungal resistance was investigated in two ways: ...
B Andersons, I Andersone, A Meija-Feldmane, I Irbe, A Janberga, J Grinins


Comparative studies on the durability of English oak (Quercus robur L.) under in-service, field and laboratory conditions
2017 - IRG/WP 17-10881
The durability of many wood species varies due to differences in extractive content, anatomical features, growth conditions, and not at least in dependence of the respective exposure conditions either under test or in real life applications. And so does the durability of English oak (Quercus robur L.), which has recently been considered in the revised European standard EN 350 (2016) and is now cla...
C Brischke, L Meyer-Veltrup, A Soetbeer, M Höpken, E Melcher, J Trautner


An experimental study of mould growth and wood decay in timber frame walls
2017 - IRG/WP 17-20623
This paper deals with parameters related to the occurrence of mould growth and wood decay in timber frame walls. In a first part, the hygrothermal conditions inside a timber frame wall finished with brick veneer cladding are analysed to get an idea of possible moisture related problems. It is shown that, based on the VTT mould prediction model, there is a mould risk on the interface between the in...
M Vanpachtenbeke, J Van den Bulcke, I De Windt, J Langmans, S Roels, J Van Acker


Exterior paint for the future - Will there be any dry-film preservatives left?
2017 - IRG/WP 17-50332
Wooden houses have a long tradition in several of the Nordic countries. Wood can be protected in various ways; constructional, chemically and by surface treatment. The use of various types of exterior paints as a surface treatment is a common way to prolong the durability of the wood. To further protect the painted surface against growth of fungi and algae, dry-film biocides remains an essential p...
H Jensen, M Sandve, S M Lystvet


Superior kempas hardwood protection with two proprietary microemulsion termiticdes based on permethrin and cyermethrin against Coptotermes termite attack under H2 an H3 weathered conditions found in buildings
2018 - IRG/WP 18-10931
SARPECO® and AXIL® solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping treatment but also for vacuum pressure tr...
D Messaudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy


In-line quality control of the film thickness in industrial coating processes for exterior cladding
2018 - IRG/WP 18-40835
The production of industrially coated wood cladding has been strongly increasing in Scandinavia during the last years. In the beginning of this development, industrial coating processes included solely the application of pigmented primers; these however provide only a short protection of the wood surface and the application of a top coat is required during the first 6 to 12 months after mounting t...
U Hundhausen, M Slabohm


Performance of wood exterior structures above ground in Spain built with softwood species. The situation case of a shelter bridge
2018 - IRG/WP 18-40844
Across Europe is very common to find wood exterior structures build in sawn and glue-laminated wood. Most of these exterior wood structures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood structures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood structures in overall Spain. This paper s...
D Lorenzo, M Touza, J Fernández-Golfín, A Lozano, J Benito


Polyesterification of wood using sorbitol and citric acid under aqueous conditions
2018 - IRG/WP 18-40851
The aim of this research is to determine if the polyesterification of sorbitol and citric acid in wood has a future potential as a wood modification process. Pine wood was impregnated with an aqueous solution containing citric acid and sorbitol and was thereafter cured at 103, or 140°C for 18 hours. The dimensional stability and leaching resistance were studied for both modification temperatures....
E Larnøy, A Karaca, L R Gobakken, C A S Hill


Exemplary aboveground hardwood protection from Coptotermes curvignathus under weathered conditions conferred by proprietary microemulsion-based cypermethrin (SARPECO®) and permethrin (AXIL®) biocides
2019 - IRG/WP 19-30749
SARPECO® (with cypermethrin) and AXIL® (with permethrin) solutions are water-based wood preservatives approved for dipping treatment providing 25 years of termite protection for solid wood and wood-based products in Europe and for more than 10 years in Indonesia. SARPECO® and AXIL® solutions are patented formulations based on concentrated microemulsions (ME) diluted with water as a dipping tre...
D Messaoudi, A H H Wong, C A D Tawi, N Bourguiba, O Fahy


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Protecting wood exterior infrastructures above ground in Spain. The importance of protection by design in the performance
2019 - IRG/WP 19-40874
Across Spain is very common to find wood exterior infrastructures build mainly in sawn and glue-laminated wood. Most of these exterior wood infrastructures use softwood wood species such as: fir, spruce, larch and pine. In Spain exterior wood infrastructures, became more and more popular since nineties, when sawn and glue-laminated wood were utilized for building exterior wood infrastructures in o...
D Lorenzo, M Touza, J Fernandez-Golfín, A Lozano, J Benito, M T Troya, L Robertson


Moisture and temperature conditions in an old, highly moisture-loaded timber building in the Røros municipality, Norway
2020 - IRG/WP 20-10966
A 150 years old log building near Røros, Norway, has been in active use as a cowshed since its erection. The animals are kept inside the cowshed all winter and this causes a situation of a high moisture load on the wooden floor, wooden walls and ceiling. Logging of temperature and humidity over one year shows that there are favourable levels of moisture in the wood and air for development of moul...
M Sand Austigard, J Mattsson


Previous Page | Next Page