The use of plastic meshes in soft rot monoculture testing
1990 - IRG/WP 2353
Plastic meshes were introduced between the wood blocks and agar medium in a miniaturised soft rot monoculture test in order to minimise transfer of the preservative from the wood and mineral salts from the agar. Although several different sizes and types of mesh were used and the blocks were wetted up to an appropriate moisture content for soft rot attack the amount of decay was substantially redu...
S M Gray


Effects of artificial UV weathering and soft rot decay on heat treated wood
2005 - IRG/WP 05-40302
Oil and inert gas oven heat treated pine wood strips 100 µm thick were mildly heat treated (200°C, 30 mins linseed oil, 120 mins oven). Following treatment, specimens were exposed to UV weathering (300 hours) and decay by the soft rot fungus, Chaetomium globosum. The effects of each treatment were assessed by zero span tensile testing, microscopy and by FTIR. Tensile testing of heat treated s...
M D C Hale, S C Ghosh, M J Spear


Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker


Evaluation of New Zealand staining fungi for degradation of radiata pine
1999 - IRG/WP 99-10310
This investigation sought to determine the potential of selected NZ staining fungi to induce weight loss and changes in toughness (impact bending strength) and composition in unseasoned radiata pine sapwood. Furthermore, assays were performed to eveluate enzyme production by staining fungi. Sets of side-matched specimens were inoculated with Ophiostoma floccosum, Sphaeropsis sapinea and O. plurian...
A Schirp, R L Farrell, B Kreber


Immunogold localisation of catalytic domain of endocellulase in the cellulosic substrates
1997 - IRG/WP 97-10205
The reaction of catalytic domain of endocellulase on the cellulosic substrates was visualised by using immunogold labelling procedures to obtain a better understanding of the mechanism of enzymatic cellulose hydrolysis. Polyclonal antibody was produced against the catalytic domain of endo-l, 4-ß-glucanase (EGI) from a ruminal anaerobic bacterium Ruminococcus albus F-40. Immuno-TEM works showed th...
Yoon Soo Kim, Seung-Gon Wi, Kyu Ho Myung, K Ohmiya, S Karita


Alternative technologies for wood wastes recycling - Part B: Biotreatment of PCP- and creosote-treated wood
1998 - IRG/WP 98-50101-18 b
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
S Legay, P Marchal, G Labat


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Physiologic response of Phanerochaete chrysosporium to exposure to triazole fungicides
1994 - IRG/WP 94-10066
Triazoles are increasingly important fungicides which are employed for a variety of applications included wood protection. Several recent studies suggest that white rot fungi are more tolerant of triazole compounds than other wood degrading fungi. Cultural studies using a white rot fungus, Phanerochaete chrysosporium, and 0.2 or 0.8 ppm of tebuconazole or propiconazole suggested that mycelial dry ...
J J Morrell, R K Velicheti


Polyflavonoid tannins - From a cause of CCA soft-rot failure to the "missing link" between lignin and microdistribution theories
1986 - IRG/WP 3359
Polyflavonoid tannins are proven to be fast-reacting with CCA solutions and hence, to be strong competitors of the structural wood constituents for fixation of CCA preservatives. The consequence of this effect is that even relatively small amounts of tannin cause severe undertreatment of the structural wood constituents which in turn badly affects the long term durability of CCA-treated timber. Th...
A Pizzi, W E Conradie, M Bariska


Soft rot decay of Eucalyptus maculata Hook. in different soils from Queensland, Australia
1980 - IRG/WP 1113
In the present work, different Queensland soils were chosen and their gross effects on the decay of treated and untreated Eucalyptus maculata examined. The soils were also amended with various levels of phosphate to study the response of the wood decay mycota to an increasing supply of this nutrient. Phosphate amendment was chosen because of the wide-scale use of superphosphate on Queensland soils...
L E Leightley, I W Russell


Examination of the Pilodyn as a non-destructive test method for detecting decay in CCA treated eucalypt poles
1982 - IRG/WP 2177
Below groundline condition of 274 CCA treated eucalypt poles comprising 13 different species was examined using 6 and 12 Joule Pilodyn units with 2 and 2.5 mm diameter pins. The data obtained was used to calculate regressions of density on pin penetration. A decrease in density was accompanied by an increase in pin penetration. The best correlation was found using the 6 Joule, 60 x 2.5 mm² diamet...
L E Leightley


Soft rot fungi as possible sources of odor in impregnated wood in buildings
1993 - IRG/WP 93-20013
Wood preservatives are frequently used inside houses. In several cases impregnated wood, particularly when used in crawlspaces or other near-ground constructions, has been found to be a source of odor. Mold fungi, soft rot fungi actinomycetes or bacteria growing on impregnated wood are possible producers of the odor. Analyses of volatile emissions from impregnated wood with odor and pure cultures ...
J Bjurman, J Kristensson


Role of cell wall structure in soft rot decay of bamboo
1995 - IRG/WP 95-10133
Models of soft rot hyphal penetration of bamboo cell walls are proposed. Soft rot hyphae show an interesting capability of penetrating the bamboo cell wall in different forms; typical longitudinal penetrating hyphae and tangentially orientated penetrating hyphae. The second form of penetration was found to be different from that normally associated with wood cell walls. The differences can be attr...
O Sulaiman, R J Murphy


Bioassays for rapid assessment of heavy metal toxicity in seawater
1998 - IRG/WP 98-50112
In evaluating the effect of CCA leachate on the establishment of fouling communities on wood exposed in the sea, three organisms were assessed as biological indicators of heavy metal toxicity. These were two macroalgae, Fucus serratus and Undaria pinnatifida. and the motile protist thraustochytrid, Schizochytrium aggregatum. The choice of these organisms for the tests carried out was based on the ...
C J Brown, R L Fletcher, R A Eaton


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


The performance of CCA treatment in bamboo against decay fungi
1993 - IRG/WP 93-30027
Samples of culm wall material from young (< 6 month age) and mature (> 3 years age) culms of the bamboo, Phyllostachys virideglaucescens were treated to equivalent% w/w retentions of a CCA preservative. After fixation and leaching the treated samples were exposed to decay by Chaetomium globosum FPRL S70K, Coriolus versicolor FPRL 28A and Coniophora puteana FPRL 11E. Thin section samples of u...
O Sulaiman, R J Murphy


Photo-discoloration and Degradation of Wood and its Stabilisation by Modification with Benzoyl Chloride
2004 - IRG/WP 04-40274
Photo degradation of Pinus roxburghii (chir pine) and Hevea brasiliensis (rubber wood) was studied under artificial accelerated weathering conditions in a Xenon test chamber. The irradiated samples were analyzed for color changes and chemical changes. Analysis of colour changes in wood surfaces by UV-Vis. irradiation was carried out using a colour measuring (CIELAB) system and chemical changes ...
K K Pandey


The evaluation of the occurrence of soft rot in creosoted wooden poles
1988 - IRG/WP 1368
The occurrence of soft rot decay in creosoted wooden poles for overhead power lines was investigated by collection of field samples, their subsequent microscopic examination and statistical analysis of the data collected. Examination of samples collected from 296 poles revealed that approximately 15% of the pole population studied (Eastern Electricity Board) showed the presence of soft rot decay. ...
A Wylde, D J Dickinson


Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It&apos;s necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building&apos;s construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur


Screening of lignin peroxidase from white-rot fungi
1998 - IRG/WP 98-10274
Since lignin peroxidase was first found in the ligninolytic culture of Phanerochaete chrysosporium, it has been regarded as an enzyme responsible for the lignin biodegradation and studied comprehensively. As the results of these studies its unique characteristics have been revealed. On the other hand, the features of lignin peroxidase produced by other white-rot fungi have not been studied so much...
I Momohara


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Novel observations on the micromorphology of soft rot attack of wood
1996 - IRG/WP 96-10176
Electron microscopic examinations of decaying Pinus radiata horticultural posts which had been treated with CCA preservative prior to being placed in service about nine years ago showed the presence of soft rot fungi and tunnelling bacteria. Some novel observations on the micromorphology of the soft-rotted areas of tracheid walls are described here. The micromorphology of soft-rotted areas was hig...
A P Singh, R N Wakeling


High CCA retentions and the protection of eucalypt power poles
1983 - IRG/WP 3226
Tasmanian power pole material treated to high retentions, was analysed to accurately determine the amount of CCA preservative in the timber. Material from the same disc was subsequently exposed in unsterile soil in order to determine the effectiveness of treatment. Results showed that even at high retention levels, soft-rot attack was not prevented. Fourteen further poles were sampled, but this ti...
L E Leightley, J Norton


Soft rot tests
1983 - IRG/WP 2206
At the IRG meeting in Turkey it was proposed that developments in testing preservative-treated wood in unsterile soil according to techniques variously described as "fungus cellar", "soil-bed", or "accelerated field simulation" be considered along with conventional laboratory procedures as the basis for a standard test. Before formulating any co-operative test programme it is essential to examine ...
J A Butcher


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...