Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Effects of the sulfuric acid modification of CCA treating solution
1987 - IRG/WP 3415
Sulfuric acid modification of CCA treating solution is often used to control the formation of sludges and undesirable deposits on the surface of treated wood. The consequences of sulfuric acid addition are examined in this work and negative effects are shown to far outweigh any benefits. Major risks include the loss of copper due to leaching from treated wood and the accelerated corrosion of treat...
R F Fox, H J Fry, E A Pasek, A S Ross


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


Evaluation of rapid methods for detecting wood preservatives in waste wood
1994 - IRG/WP 94-50024
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Several analytical methods are available for the detection of most elements in wood preservatives. Industrial process conditions, however, demand methods with very short turn around times. In this research several methods of analysis were judged on their speed and accuracy. A num...
W J Homan, H Militz


Survey of practical methods for conditioning of forest products before preservative treatment
1971 - IRG/WP 39
The seasoning of forest products is undertaken for a wide range of end uses and is becoming increasingly required for applications and building construction and secondary manufacturing industries. A wide range of applications of new technology and specifically required seasoning schedules is being actively developed for such requirements, but less attention has been given to the means by which woo...
J Rak, T S McKnight


Blue Staining of Coated Modified and Unmodified Wood
2006 - IRG/WP 06-10589
We investigated resistance of unmodified, DMDHEU modified and oil heat treated uncoated and coated Scots pine wood against blue stain fungi. Both EN 152-1 and the reverse exposure tests showed excellent resistance of DMDHEU and especially of oil heat treated wood against blue staining. It is not needed to add any additional protective coating layers to prevent modified wood from staining. However,...
M Petric, M Pavlic, M Humar, M Tomažic


Termite Response to Oil-Heat-Treated Norway spruce, Scots Pine and Eucalyptus Wood
2006 - IRG/WP 06-20325
The work here presented focused on the behaviour of subterranean termites (Reticulitermes grassei Clément) towards Oil-Heat-Treated (OHT) Norway spruce (Picea abies L.), Scots pine (Pinus sylvestris L.) and eucalyptus (Eucalyptus globulus Labill) wood, with a particular interest in the development of simple methods adequate to study the resistence of these materials to termite attack. Small test ...
L Nunes, T Nobre, C Welzbacher, A O Rapp


Re-sealing cut ends of envelope-treated softwood framing timber to protect against damage by the Australian subterranean termite Coptotermes acinaciformis: A revisitation
2006 - IRG/WP 06-20335
The claim that Australian Coptotermes acinaciformis (Froggatt) do not appear to initiate damage on timber from the end grain, thereby negating the need for treating exposed cut ends of softwood framing material (35 ? 90 mm) which has a repellent Tanalith? T envelope, was further investigated. Specimens of commercial Pinus radiata D.Don framing timber (untreated) and Pinus elliottii Englem. (untrea...
B C Peters, M Lenz, J W Creffield


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Laboratory methods for assessing the resistance of wood plastic composites to fungal attack.
2006 - IRG/WP 06-20340
Wood plastic composites (WPC’s) have many attractive material features including dimensional stability and resistance to moisture, but the wood in these materials remains susceptible to fungal attack. Assessing WPC decay resistance in laboratory trials has proven difficult because the slow moisture sorption characteristics of this material do not allow for sufficient fungal attack over the trad...
J J Morrell


Testing durability of treated wood according to EN 252. Interpretation of data from Nordic test fields
2006 - IRG/WP 06-20341
To evaluate the effectiveness of new wood preservatives intended for treated wood in ground use there is a European standard, EN 252. The test shall run for five years before any formal interpretation of the results can be made. Due to environmental concerns, the use of wood preservatives based on copper, chromium and arsenic (CCA) has been restricted in recent years. As a consequence of restrict...
M L Edlund, F G Evans, K Henriksen, T Nilsson


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


How to win friends and influence the market — Service Life Prediction and performance-based durability assessments of wood products in construction
2006 - IRG/WP 06-20348
Due to direct and implied demands from the market and from e.g. the EU Construction Products Directive, the need to supply service life estimates for building products is growing. For several years, a development of Service Life Prediction (SLP) methodologies has been going on, but the awareness of this development has hitherto reached only a very limited extent in the wood sector. For materials w...
F Englund


Standard Test Methods for Wood Preservatives by Laboratory Agar-Block Test
2006 - IRG/WP 06-20350
Wood is one of the most valuable and versatile resources for all sorts of constructional purposes. But timber in its various forms is subjected to several types of deterioration. This standard lays down the method for the laboratory determination of threshold value of wood preservatives against fungi. Most chemicals are initially tested for their ability to control decay fungi in agar-block tests....
P K Sarker, M A Rahman, M R Bulbul, T Das, G N M Ilias


Protection of hard and softwood through Neem leaves extracts and oil - A direction towards development of eco-friendly wood preservatives
2006 - IRG/WP 06-30394
Conventional wood preservatives like CCA and CCB are facing lot of criticism all over the world. It is essential to address the problem in view of environment protection. Eco-friendly wood preservatives may be considered as one option. The present study is an expolartion of neem leaves and seed oil against wood decaying fungi and termites. Azadirachta indica A. Juss, commonly known as neem is one ...
S Dhyani, S Tripathi


The commercialisation of ThermoWood® products
2006 - IRG/WP 06-40339
The concept of thermally modifying timber is well established, which has achieved a limited market breakthrough to date. Commercial application has mainly occurred within Finland, though recent years has seen market gain in several other European countries. This paper reviews the known properties of ThermoWood® timber, based on the combined work of the Finnish ThermoWood® Association, alongside ...
D Jones, E Suttie, J Ala-Viikari, N Bergstrom, D Mayes


Effect of fire retardants (monoammonium phosphate and diammonium phosphate, mixture of monoammonium phosphate and borax and ammonium sulphate) on beech wood with dipping and Lowry methods
2006 - IRG/WP 06-40350
In this study, the possibilities of using four kinds of chemicals as fire retardants with 12% concentration for beechwood (Fagus orientalis Lipsky) was surveyed. Providing testing samples that are related to the measurement of fire resistance properties according to JIS A-1321-1975 standard were evaluated. Wood samples were impregnated with Lowry and dipping methods. In this study, samples impregn...
M Akhtari, D Parsapajouh, M Arefkhani


Effect of fire retardants (monoammonium phosphate and diammonium phosphate, mixture of monoammonium phosphate and borax and ammonium sulphate) on beech wood with dipping and Lowry methods
2006 - IRG/WP 06-40350
In this study, the possibilities of using four kinds of chemicals as fire retardants with 12% concentration for beechwood (Fagus orientalis Lipsky) was surveyed. Providing testing samples that are related to the measurement of fire resistance properties according to JIS A-1321-1975 standard were evaluated. Wood samples were impregnated with Lowry and dipping methods. In this study, samples impregn...
M Akhtari, D Parsapajouh, M Arefkhani


Criteria for environmentally and socially sound and sustainable wood preservation industry
2006 - IRG/WP 06-50237
This paper is dealing with critical criteria for environmentally and socially sound and sustainable wood preservation industry. A research study supported by past experience, knowledge and training on relevant topics and consultation of relevant appraisal manual, training module and technical guideline revealed concise widespread checklists for sustainable establishment of wood preservation indust...
A K Lahiry, M Hasan, M A J H Chowdhury


Current state of world standardization in the toxicometric methods for testing of wood preservatives
2007 - IRG/WP 07-20354
The paper presents an outline of the history of forming standardized toxicometric methods for testing of wood preservatives in the world during last 100 years. Numerous studies resulted in three main methods which are currently used for official and basis assessment of biocides: - agar-block method in Europe (EN 113); - soil-block method in the USA and Pacific countries (ASTM D 1413); - modifi...
J Wazny


Methods for Determining the Role of Extractives in the Natural Durability of Western Redcedar Heartwood
2007 - IRG/WP 07-20356
The durability of western redcedar heartwood is influenced by a number of different extractives operating by different mechanisms. In order to guide a systematic isolation of extractives with high fungal toxicity, a micro-bioassay has been developed for measuring the fungal toxicity of extractive fractions. Two additional assays quantify the anti-radical and metal chelating properties of cedar ext...
R Stirling, C R Daniels, J E Clark, P I Morris


Comparison of laboratory termite test methods
2007 - IRG/WP 07-20365
Seven standardized laboratory tests with termites were evaluated. The bioassays were made in accordance with EN 117, SAA32 E08, SAA32 E09, Ebw 02, the American Wood-Preservers’ Association (AWPA) Standard E1-97, the Japan Wood Preserving Association (JWPA) Standard 11 (1) and The Protocols for Assessment of Wood Preservatives. Two different wood preservatives each in three concentrations and add...
H-U Kruschinski, W Unger, A F Preston


Photo-degradation of modified and non-modified wood, coated with water borne acrylic coatings during artificial light exposure
2007 - IRG/WP 07-30416
A series of experiments were carried out to investigate photo-degradation of thermally modified (at 210oC and – 0.9 bars for two hours) and non-modified spruce wood (Picea abies L (Karst)), coated with transparent and semitransparent (with 3% pigment content) acrylic coatings during artificial UV light irradiation for 200 hours. Photo-degradation was evaluated in terms of colour changes througho...
M Deka, M Tomažic, M Petric


Microwave curing of furfuryl alcohol modified wood
2007 - IRG/WP 07-40371
Furfurylated wood has shown to have promising properties for a wood modification agent during the last years. In this paper, an alternative curing method for furfuryl alcohol modified pine sapwood by means of microwave radiation was investigated. Different process parameters of microwave treatment such as output power, exposure time to microwave radiation, initial wood moisture content and evapor...
A Treu, E Larnøy, H Militz


Effects of heat treatments on decay resistance and material properties of ponderosa pine and yellow poplar
2007 - IRG/WP 07-40374
The potential for using heat treatment to improve the properties of North American fenestration species was evaluated on ponderosa pine (Pinus ponderosa L) and yellow poplar (Liriodendron tulipifera L) treated using the ThermoWood process at various treatment temperatures and times. Soil block tests using Gloeophyllum trabeum, Postia placenta, or Trametes versicolor showed that durability was enh...
C Vidrine, C Freitag, J Nicholson, J J Morrell