Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Life Cycle Assessment of treated timber: methodological aspects and first results
2009 - IRG/WP 09-50264
Environmental information on products is more and more required as a key to the market, and the building sector in Europe is certainly advanced in that direction. In France, Environmental Product Declarations are becoming very common for construction products. Therefore, the CTB P+ and CTB B+ certification comity as commissioned FCBA to perform the Life Cycle Analysis of treated timber in order to...
E Vial, M Bertrand, C Cornillier, G Deroubaix


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Service life prediction of wooden components – Part 2: Impact of material, exposure and design details
2010 - IRG/WP 10-20440
Dose-response functions permit to estimate the moisture and temperature induced decay potential for any wooden building component and exposure, and thus the service life to be expected. In part 1 of this series dose-response functions were established as a result of double layer field trials carried out at 24 European test sites over up to eight years. Using them makes it no longer necessary to co...
C Brischke, B Lauenstein, M Bilstein, T Bornemann, A O Rapp


Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot


Drying Rates and Mold Growth on Various Building Materials under Different Environmental Conditions
2010 - IRG/WP 10-20454
Mold growth on building materials is a major problem for homeowners. The most suitable method to control mold growth on building materials is to utilize design features, construction tools and practices that prevent moisture accumulation, and keep the wood as dry as possible. In order to achieve this, engineers and homebuilders have to know the effects of various temperature and moisture conditi...
Dian-Qing Yang


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


A comparative study and evaluation of methodologies used for determining wood preservative penetration
2011 - IRG/WP 11-20475
A series of methods for determining penetration of wood preservatives into the wood structure have been developed for either quality control (QC) or research and development purposes. QC methods range from monitoring the solution uptake, applying colour indicators or sampling specific wood samples followed by wood acid digestion/atomic absorption spectroscopy (AAS) or solvent extraction/chromatogr...
R Craciun, R Moeller, J Wittenzellner, T Jakob, J Habicht


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Environmental safeness of 60% and 72% concentrated CCA-C solution and paste for wood treatment
2012 - IRG/WP 12-50284
In this study 30-years practical and observational experience of the present author about using of 72% concentrated CCA-C paste for preparing treating solutions and for treating wooden poles, anchor logs and cross arms has revealed that the 60% concentrated CCA-C solution is superior to the 72% concentrated CCA-C paste regarding solubility, homogeneity, cleanliness, treatability, sludge formation,...
A K Lahiry


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and imported Russian spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer


Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant. • Less En...
AquAeTer, Inc.


Conclusions and Summary Report on an Environmental Life Cycle Assessment of Borate-Treated Lumber Structural Framing with Comparisons to Galvanized Steel Framing
2013 - IRG/WP 13-50296
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of borate (disodium octaborate tetrahydrate)-treated lumber structural framing and galvanized steel framing using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood framing are significant....
AquAeTer, Inc.


Conclusions and Summary Report Environmental Life Cycle Assessment of Highway Guard Rail Posts
2013 - IRG/WP 13-50297
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood and galvanized steel highway guard rail posts using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood guard rail posts are significant. • Less Energy & Resource Use: ...
AquAeTer, Inc.


Conclusions and Summary Report Environmental Life Cycle Assessment of Marine Pilings
2013 - IRG/WP 13-50298
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood, concrete, galvanized steel, and plastic marine piles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood piles are significant. • Less Energy & Resource Use: Tre...
AquAeTer, Inc.


Conclusions and Summary Report on an Environmental Life Cycle Assessment of Utility Poles
2013 - IRG/WP 13-50299
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of pentachlorophenol-treated wood, concrete, galvanized steel, and fiber-reinforced composite utility poles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood poles are significant. ...
AquAeTer, Inc.


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar