IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 600 documents. Displaying 25 entries per page.


Screening wood preservatives: Comparison of the soil block, agar block and agar plate tests
1993 - IRG/WP 93-20001
Several test procedures have been developed over the years to screen potential biocides for their value as wood preservatives. Each test has inherent advantages and disadvantages. In this paper the relative merits of the soil block, agar block and agar plate tests are compared. Eight commercially available biocides encompassing inorganic and organic systems were tested against four basidiomycete d...
K J Archer, D D Nicholas, T Schultz


Implications for comparability of laboratory experiments revealed in studies on the effects of population density on the vigour in groups of Coptotermes lacteus (Frogatt) and Nasutitermes exitiosus(Hill) (Isoptera: Rhinotermitidae, Termitidae)
1983 - IRG/WP 1194
The vigour - survival. and wood consumption - of groups of Coptotermes lacteus and Nasutitermes exitiosus was measured when termites were kept at different population densities (g termites/mL) by changing group size and/or volume of the holding container. A characteristic pattern emerges for subterranean-like termite species. At low population densities (<0.01 g/mL) performance of termites impr...
M Lenz, R A Barrett, E R Williams


Efficacy of waterborne copper naphthenate as preservative for northern hardwood species
1995 - IRG/WP 95-30091
Northern red oak (Quercus rubra) and red maple (Acer rubrum) cubes pressure treated with waterborne formulation of copper naphthenate were evaluated for resistance to attack by brown fungi Gloeophyllum trabeum (Pers. ex Fr.) Murr. (Madison 617 ATCC 11539) and Poria placenta (Fr.) Cooke (Madison 698, ATCC 11538), white rot fungi Trametes versicolor (L. ex Fr.) Pilat (R-105 from Jeff Morrell), Irpex...
D P Kamdem, R Fair, M H Freeman


A laboratory bioassay method for testing preservatives against the marine borers Limnoria tripunctata, L. quadripunctata (Crustacea) and Lyrodus pedicellatus (Mollusca)
1990 - IRG/WP 4159
A laboratory culture and bioassay method is described for the marine borers Limnoria tripunctata, Limnoria quadripunctata, and Lyrodus pedicellatus. The methods were tested in a bioassay using established marine preservatives. The attack produced on blocks treated with CCA or creosote in some ways paralleled the attack found in the sea. Limnoria tripunctata attacked treated and untreated pine bloc...
L J Cookson


Report on the efficacy and performance of the insecticide candidate termiticide in H2 field trials
2004 - IRG/WP 04-10516
This paper explains the field results of phenol pyrazole treated timber against in an above ground mound colonies of Coptotermes acinaciformis (Froggatt). C. acinaciformis (‘termites’) are the major pest of human structures throughout tropical and sub tropical regions, causing billions of dollars in damage to timber-in-service worldwide. The result of this field test have shown that candidate ...
B M Ahmed, P Vinden, J Hann, J R J French


New methods for nondestructive inspection of timber in buildings
1995 - IRG/WP 95-20070
In these years older buildings are renewed in most European countries on a large scale, and new techniques are needed for both inspection and eradication of fungal attacks. Heat treatment as a means of eradicating the dry rot fungus has been used in Denmark during the last decade. This technique minimises the structural damage to the building, whilst at the same time reducing costs by up to 50%. T...
B Madsen, O V Frederiksen


Evaluation of bending strength by non-destructive methods of Ezomatzu with white pocket rot
1991 - IRG/WP 2371
The possibility of application of three non-destructive methods was examined for evaluation of bending strength of ezomatsu (Picea jezoensis CARR.) with white pocket rot. As non-destructive methods, the measurements of ultrasonic wave propagation time, impact-induced stress wave propagation time and penetration depth of pin of "PILODYN Wood Tester" were applied to compare with visual evaluation of...
T Tanaka


Accelerated weathering test for the evaluation of wood preservative efficacy
2003 - IRG/WP 03-20262
Wood samples treated with ammonium copper quat (ACQ-1900 and ACQ-2200), Chromated copper arsenate (CCA), Tanalith E 3491 and Wolmanit CX-8 have been studied in accelerated weathering experiments. The weathering experiment was performed by cycles of 2 hours UV-light irradiation followed by water spray for 18 minutes. The changes on the surface of the weathered samples were characterized by FTIR Sp...
A Temiz, M Eikenes, Ü C Yildiz, F G Evans, B Jacobsen


Development of a mini-block test method for the rapid evaluation of preservative performance against Basidiomycte fungi
1991 - IRG/WP 2379
Screening procedures for new biocides used as wood preservatives can be a time consuming process using conventional Basidiomycete assay procedures. This is due mainly to the long exposure periods required to achieve adequate levels of decay (weight loss) in the test blocks. A number of alternative methods have been developed but most utilise artificial substrates such as filter paper or agar in wh...
J Brown, S Caswell, G R Williams


The potential application of rapid gas-chromatographic assay of microbial respiration to the monitoring of wood decay in field trial situations
1983 - IRG/WP 2196
Gas chromatographic detection of microbial activity (C02 production) within stakes in a field trial situation would appear to provide a sensitive, non-destructive and relatively rapid method for the quantitative assessment of preservative treatments. Most consistent results were obtained when stakes were removed from the soil, washed, saturated with water and incubated in sealed PVC tubes at 25°C...
M A Line


The efficacy of preservatives into the glue-line of plywood
1993 - IRG/WP 93-30002
This research is anti-termite/decay preservatives mixed with resin to produce the plywood. Thereafter, anti-decay/termite plywood were produced by the ordinary methods. To produce suitable plywood in the utilization and certified performance, the preservatives should be 0.3 to 0.4 kg/m³ of Chlorpyrifos; 0.88 and 1.10 kg/m³ of mix preservatives of Chlorpyrifos + IF-1000. Laboratories decay test (...
S Fushiki, T Saito, Y Katuzawa, Y Imamura, S Yusuf, B Subiyanto


Chemical Analysis of Southern Pine Pole Stubs Thirteen Months Following Treatment with Three Methylisothiocyanate Based Commercial Fumigants
2002 - IRG/WP 02-30294
Agricultural fumigants have been commercially used in the United States for over 20 years to control internal decay in utility poles and other wooden structures. Of the four fumigants which are currently used in the remedial treatment of utility poles, three are based on methylisothiocyanate (MITC) as being the principal fungitoxic component. Two of these MITC based fumigants, liquid metham sodi...
R J Ziobro, T C Anderson, D J Herdman, J Guzzetta, T Pope


Comments on leaching in view of accelerated testing
1977 - IRG/WP 294
We developed an accelerated test for leaching at elevated temperatures (75-85°C). This test was used for the examination of 11 preservative formulations containing Cu, Zn and As. The data obtained from these experiments were compared with data on some formulations tested by ASTM standard leaching test. The method consists in making a large surface to volume ratio of wood from a treated block by c...
J Rak


Effect of post-treatment drying schedule on the modulus of elasticity of CCA-treated southern pine dimension stock using nondestructive methods
1987 - IRG/WP 3413
This paper describes the results from the nondestructive testing for modulus of elasticity (MOE) of southern pine (Pinus sp.) 2 x 6&apos;s treated with chromated copper arsenate and redried using three commercial kiln schedules. The data indicate that redrying CCA-treated southern pine dimension stock treated to above-ground retentions (4 kg/m³) has no deleterious effect on the MOE, regardles...
H M Barnes, S Moore


Comparison of the anti-fungal efficacy of Cobra with drill perforation on oscillating pressure treated spruce transmission poles -Laboratory test
1988 - IRG/WP 3469
A laboratory method for measuring the depth of penetration of the fungicidal concentrations effective against basidiomycetes (brown rot) was developed. The tests on CCB oscillating pressure treated spruce transmission poles have shown that the depth of salt penetration can be increased by about 10 mm by a drill perforation before the impregnation. An even better penetration is reached, however, if...
E Graf, B Zgraggen


Determination of corrosive effect of liquid wood preservatives to metals – First experiences with a National Standard which is in revision
2006 - IRG/WP 06-20321
The development of standards is an essential tool to characterise different kind of materials and products. An important aspect during the development of a new product is to check the corrosion behaviour with other materials. Corrosion can cause several problems like pitting corrosion. Consequently the knowledge concerning the corrosive effect of liquid wood preservatives is important due to the s...
E Melcher


Reappraisal of some fungicides by the amended JWPA method
1992 - IRG/WP 92-3689
Organoiodine compounds which have been commercialized these years in Japan poorly performed as fungicides in the amended JWPA decay test (Standard 1, 1989) when applied to superficial treatment of timber. Because some parts of active ingredients seemed to disappear from the treated timber surface mainly due to the severe leaching cycles. This was prominently true for beech (Fagus crenata Blume) sa...
K Tsunoda


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


Untersuchungen zur Prüfung mit Moderfäulepilzen im Vermiculit-Eingrabe-Verfahren
1972 - IRG/WP 214
Im Hinblick auf die Entwicklung eines Prüfverfahrens für die Bestimmung der moderfäulewidrigen Wirksamkeit von Holzschutzmitteln wurden Versuche mit Reinzuchten von Pilzen und mit Vermiculit als Trägersubstanz sowohl mit unbehandelten als auch mit Schutzmittelgetränkten Holzproben durchgeführt. Dabei wurde die Eignung von handelsüblichen, eintachen Einweg-Kunststoffbechern anstelle der bish...
W Kerner-Gang, M Gersonde


The influence of carrier fluid type on the efficacy of a wood preservative against cavity forming soft rot
2000 - IRG/WP 00-30244
Propiconazole was applied to Scots pine sapwood (Pinus sylvestris) and beech (Fagus sylvatica) using three different carrier systems selected on their varying ability to swell timber. The effects of microdistribution on the activity of cavity forming soft rot fungi were examined to determine the practical benefits of using swelling and non-swelling carriers with this active ingredient. Efficacy of...
P A Hodges


FLUROX, a new breakthrough in insect control for wood preservation
1995 - IRG/WP 95-30079
FLUROX (flufenoxuron) is an acylurea insecticide which acts as a growth regulator in insects. FLUROX inhibits the production of chitin - the exoskeleton or &apos;skin&apos; of the insect. When the exposed larva attempt to moult to its next stage of development, it is unable to produce a new skin and dies. FLUROX has been found to be extremely active against wood borers, when applied in a p...
A R Valcke, M Pallaske


Collaborative soft rot tests: Final Report
1978 - IRG/WP 2106
Since preparation of Document No: IRG/WP/258 results have been received from the remaining collaborators. Thus there is a little further to add to the conclusions already derived, those in Document No: IRG/WP/251 being as follows: 1) the exposure system used sometimes resulted in excessive weight gains in the sterile check blocks. Consequently the corrected loss in weight of the test blocks could ...
J G Savory, J K Carey


Imaging fungal deterioration of wood using x-ray microtomography
1997 - IRG/WP 97-10240
Nondestructive tomographic images of solid Southern yellow pine (SYP) wood and SYP during deterioration by wood decay fungi were obtained by using a new class of synchrotron X-ray computed microtomography (CMT). The CMT images will provide information about spatial relationship between degrading fungi and wood structures. Wood samples were scanned with synchrotron-generated X-rays at high resoluti...
B Illman, B A Dowd


Leaching of copper-chrome-arsenic treated timber: Simulated rainfall testing
1996 - IRG/WP 96-50074
Six kiln dried radiata pine sapwood packs of timber were preservative treated with copper-chrome-arsenic preservative using a modified Bethell treatment schedule. The packs were then subjected to simulated rain leaching at specified periods after treatment. Higher chromium leachate was obtained when higher volumes of simulated rainfall were applied. Lower chromium leachate was obtained for timber ...
S Walley, P R S Cobham, P Vinden


Effects of chemical pretreatment of Douglas-fir heartwood on efficacy of potential bioprotection agents
1990 - IRG/WP 1440
Biological protection against wood decay fungi represents an environmentally attractive alternative to the use of chemicals; however, the process of identifying suitable candidates and the conditions that ensure successful protection pose major challenges. One critical aspect of this problem is to identify organisms that can rapidly and uniformly colonize the wood. Wood contains low levels of nutr...
B Dawson-Andoh, J J Morrell


Previous Page | Next Page