Your search resulted in 46 documents. Displaying 25 entries per page.
Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz
Acquisition of sorption isotherms for modified woods by the use of dynamic vapour sorption instrumentation: Principles and Practice
2010 - IRG/WP 10-40518
The complex wood-water relationship has been the topic of numerous studies. Sorption isotherms – in particular – have been derived for hundreds of wood species, their sap- and heartwood sections as well as for decayed, engineered and modified wood materials. However, the traditional methods for obtaining sorption isotherms are very time consuming. With new dynamic vapour sorption (DVS) instrum...
E T Engelund, M Klamer, T Mark Venås
Thermally modified timber (TMT) for decking applications – determination of relevant surface properties
2011 - IRG/WP 11-40544
In recent years thermally modified timber (TMT) entered various market segments. It is used for facades, horticultural equipment, garden furniture, and also for kitchen and bathroom cabinets. However, flooring turned out to be the most important application for TMT, either as interior parquet or as exterior decking. Besides durability and dimensional stability, which had been the initial target pr...
L Meyer, C Brischke, C R Welzbacher
Adsorption boundary curve influenced by step interval of relative humidity investigated by Dynamic Vapour Sorption equipment
2011 - IRG/WP 11-40547
The adsorption of water vapour from dry conditions by Norway spruce sapwood has been investigated using Dynamic Vapour Sorption (DVS) instrumentation. This equipment allows a fast and easy data acquisition as well as enables detailed studies of sorption properties using very small sample masses. In this study, particular focus was paid to the effect of step size on the sorption isotherms. Furtherm...
E Tang Engelund, M Klamer, T Mark Venås
Effect of an antioxidant on the efficacy of organic wood preservatives in an accelerated soil contact decay test
2012 - IRG/WP 12-30583
In comparison to inorganic wood preservatives, organic biocides in transient carriers are considerably less effective when the treated wood is exposed to soil contact. Various oils are used in some formulations with pentachlorophenol to improve the efficacy. However, use of these oils imparts unacceptable properties to products used in residential applications. Consequently, there is a need to de...
D D Nicholas, J Shi, T P Schultz, L Sites
Conclusions and Summary Report on an Environmental Life Cycle Assessment of ACQ-Treated Lumber Decking with Comparisons to Wood Plastic Composite Decking
2013 - IRG/WP 13-50295
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of ACQ (alkaline copper quaternary)-treated lumber decking and wood plastic composite decking using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood decking are significant.
• Less En...
AquAeTer, Inc.
Conclusions and Summary Report on an Environmental Life Cycle Assessment of Borate-Treated Lumber Structural Framing with Comparisons to Galvanized Steel Framing
2013 - IRG/WP 13-50296
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of borate (disodium octaborate tetrahydrate)-treated lumber structural framing and galvanized steel framing using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood framing are significant....
AquAeTer, Inc.
Conclusions and Summary Report Environmental Life Cycle Assessment of Highway Guard Rail Posts
2013 - IRG/WP 13-50297
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood and galvanized steel highway guard rail posts using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood guard rail posts are significant.
• Less Energy & Resource Use: ...
AquAeTer, Inc.
Conclusions and Summary Report Environmental Life Cycle Assessment of Marine Pilings
2013 - IRG/WP 13-50298
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of treated wood, concrete, galvanized steel, and plastic marine piles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood piles are significant.
• Less Energy & Resource Use: Tre...
AquAeTer, Inc.
Conclusions and Summary Report on an Environmental Life Cycle Assessment of Utility Poles
2013 - IRG/WP 13-50299
The Treated Wood Council has completed a quantitative evaluation of the environmental impacts associated with the national production, use, and disposition of pentachlorophenol-treated wood, concrete, galvanized steel, and fiber-reinforced composite utility poles using life cycle assessment (LCA) methodologies and following ISO 14044 standards. The results for treated wood poles are significant.
...
AquAeTer, Inc.
Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du
Dynamic mechanical analysis of viscoelastic properties of heat treated glycerol-impregnation poplar wood
2016 - IRG/WP 16-40732
The viscoelastic properties of glycerol-impregnated poplar wood after heat treatments at various temperatures were examined by dynamic-mechanical analysis. The spectra of storage modulus (E’) and loss tangent (tgδ) in the frequency at 10 Hz were measured at the temperature range from -100 to 300℃. Compared to no peak in E’ spectra and two relaxation processes in tanδ spectra of...
Li Yan
Wood Protection and Environmental Performance of Products - Impacts COST Action FP1407 Aims to Bring
2016 - IRG/WP 16-50323
Though many aspects of wood modification (chemical, thermal, impregnation) treatments are known, the fundamental influence of the process on product performance, the environment, and end of life scenarios remain unknown. To contribute to the low-carbon economy and sustainable development, it is essential to integrate interactive assessment of process parameters, developed product properties, and e...
A Kutnar
The sorption behaviour of wood
2017 - IRG/WP 17-20605
The use of dynamic vapour sorption to determine the sorption properties of wood has become an increasingly popular technique. The method has many advantages when compared with many other gravimetric methods. However, it is necessary to set an equilibrium condition in order to obtain data for an isotherm in a reasonable amount of time. An important recent finding has been that multiple sorption cyc...
C Hill
Analysis of Wood Industrial Pollutants Based on Emission Coefficients
2017 - IRG/WP 17-50325
Accurate calculation and estimation pollutants is one of the basic tasks of environmental protection .The low carbon economy put forward However,low carbon economy data of wood industry is lack. The paper research on emissions and pollution of Chinese wood industry. The results showed dust emissions from much to least is: fiberboard, plywood and particle board; the amount of industrial ...
Chu Jie, Ma Ji, Zhangjing Chen
Uncertainty in life cycle assessment of preservative treated wood – copper and freshwater ecotoxicity
2017 - IRG/WP 17-50331
Life cycle assessment (LCA) is a method for quantifying the environmental impacts of a product over the life cycle. In the last years, there have been a growing application of LCA in developments of environmental product declaration (EPD), which is utilised by professional procurement of materials for buildings. For legislative issues, LCA have also been used to assess application of creosote to t...
L G F Tellnes
Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz
Declaring life cycle inventory of toxicity related emissions in environmental product declarations of preservative treated wood products
2018 - IRG/WP 18-50339
Life cycle assessment (LCA) including impacts on toxicity for preservative treated wood has been shown to have large uncertainties. With the growing demand for verified LCA in environmental product declarations (EPD), the need for reliable data is crucial for realistic assessment of wood products. Uncertainty is caused by several issues such as service life prediction, leaching rates and calculati...
L G F Tellnes, C Askham, P-O Flæte, M Klamer
Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke
Moisture sorption behaviour of poplar and thermally modified poplar using dynamic vapour sorption (DVS)
2022 - IRG/WP 22-40947
The moisture sorption behaviour of wood has a critical impact on service life. In Europe, softwood is mostly used to manufacture engineered wood products such as cross-laminated timber (CLT) or glue-laminated timber (GLT or glulam). Yet fast-growing and widespread tree species such as hybrid poplar with or without modification, have potential to meet the increasing demand. This study shows the moi...
X Jiang, J Van den Bulcke, L De Boever, M Minsart, A Mignon, J Van Acker
Keeping wood greenest: Maximizing the unique benefits of preserved wood through end-of-life planning to realize carbon sequestration and a circular economy
2024 - IRG/WP 24-50387
While competitive fuels and different energy sources are a main driver of current difficulties with using end-of-life wood products for fuel, that is a potentially smaller problem than the rapidly changing carbon footprints of competitive materials, which can potentially be smaller than wood, if the wrong decisions are made at the end of life by users and waste generators. While users have several...
J D Lloyd, B Poe