Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


Moisture and Fungal Durability of Wood-Plastic Composites Made With Chemically Modified and Treated Wood Flour
2013 - IRG/WP 13-40648
Evaluating the fungal durability of wood-plastic composites (WPCs) is complicated by the influence of slow moisture sorption. Recently, the American Wood Protection Association (AWPA) Standard Method E10, Testing Wood Preservatives by Laboratory Soil-Block Cultures, was modified to incorporate not only solid wood, but also wood-based composites and WPCs. To simulate long term WPC performance, cond...
B K Segerholm, R E Ibach


Bio-based thermoset resins for bonding and eco-friendly preservation in the wood industry
2013 - IRG/WP 13-40650
Yellow dextrins and tannins were used in wood adhesives formulation to substitute resins based on formaldehyde. Several formulations were carried out in alkaline aqueous media by varying the weight fraction of two compounds from 10% to 30%. The cross-linking was performed using epichlorohydrin as a reticulant agent. Rheological behaviours and initial adhesion of three liquid formulations, before r...
C Motillon, A Allal, A Visse, F Charrier, B Charrier, A Baldé


Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


An Overview of Western Red Cedar as a Wood Pole Species
2014 - IRG/WP 14-10815
This paper reviews the characteristics of western red cedar, with particular emphasis on its use in utility poles. Western red cedar naturally grows primarily in British Columbia, Alaska, Washington, Oregon, California, Idaho and Montana. Compared to other commercial softwoods it has low density, increased corrosivity, weaker mechanical properties, high dimensional stability, and high natural dura...
M H Freeman, R Stirling


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Natural durability of plantation-grown coast redwood (Sequoia sempervirens) in New Zealand
2014 - IRG/WP 14-10817
There is wide variation in the wood properties of plantation-grown coast redwood in New Zealand. Contributing factors are the seed source, silviculture, growth and age of the trees in the plantation forests. Little is known about how these factors affect the variation of wood properties among and within the trees of New Zealand’s coast redwood forests. Heartwood of plantation-grown coast redwood...
D O’Callahan, T Jones, C Low, C Chittenden


Durability and Wood Protection for Historic Covered Bridges in the United States
2014 - IRG/WP 14-10829
A majority of the covered wooden bridges in United States were built in the mid -1800’s. These structures represent a unique cultural and technological heritage from that era. Over time, these bridges have been deteriorated by microorganisms and insects or damaged by acts of vandalism and arson. The National Historic Covered Bridge Preservation (NHCBP) Program sponsored by the Federal Highway Ad...
V W Yang, C A Clausen


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Thermal durability and biodegradation of tannin lignin adhesives
2014 - IRG/WP 14-40657
Mimosa tannins and lignosulfonates were used in wood adhesives formulation to substitute resins based on formaldehyde. Mimosa tannins were mixed with either glyoxalated sodium lignosulfonates or glyoxalated ammonium lignosulfonates. The ratios of mimosa tannins and sodium lignosulfonates varied from 20% tannins to 60% tannins. The thermal durability of the adhesives were analysed by thermogravimet...
L Chupin, B Charrier, A Pizzi, F Charrier


Termite resistance of wood modified with short- and long-chain siloxanes
2014 - IRG/WP 14-40660
Scots pine (Pinus sylvestris L.) sapwood specimens modified with short- and long-chain amino-functional siloxane emulsions were exposed to subterranean termites (Reticulitermes flavipes Kollar). Laboratory choice and no-choice tests following the standard EN 117 (2013) were conducted for 8 weeks in order to evaluate the influence of these silicon-based compounds on the termite resistance of treate...
P Gascón-Garrido, M-F Thévenon, H Militz, C Mai


Development of new wood treatments combining boron impregnation and thermo modification - Effect on decay and termites durability
2014 - IRG/WP 14-40666
Environmental pressures appeared in most European countries during the last decade has lead to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative methods during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important chemical mo...
S Salman, A Pétrissans, M-F Thévenon, S Dumarçay, B Pollier, P Gérardin


A guideline for sorting easy to impregnate Scots pine sapwood based on three treatability studies from Northern Europe
2014 - IRG/WP 14-40669
Scots pine sapwood is generally considered an easy to impregnate wood species, though it reportedly faces challenges towards a homogeneous impregnation and large variations in treatability are reported for the material. This study comprises the results of three treatability tests that were performed on Scots pine (Pinus sylvestris) sapwood. The material impregnated was originated from a large ...
K Zimmer, E Larnøy, A Treu


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Biological durability of natural fibre reinforced composites
2014 - IRG/WP 14-40681
Composite materials reinforced with wood or non-wood natural fibres have the potential to be a lighter and lower-cost alternative construction material. Until better availability and properties and a lower cost price of degradable polymers makes their use more prevalent, the application of natural fibre reinforcements in synthetic polymers is an intermediate step towards products that are complete...
N Defoirdt, I De Windt, J Van den Bulcke, J Van Acker


Influence of the moon phase on durability against wood decay fungi of Larix kaempferi and Pseudotsuga menziesii wood species
2015 - IRG/WP 15-10836
The analysis of the natural durability of wood is essential when establishing the level of protection required, depending on the designated end use of timber. On the other hand, there is a popular belief based on the influence of the moon phase in felling timber, recommending the waning moon as the optimum for felling trees. In fact, some companies now offer among their products, sawn timber felle...
M T Troya, M Conde, M J Barriola, F Llinares, V Dorronsoro


Field Performance of Old-Growth and Second-Growth Western Red Cedar Fence Posts with and without Barrier Wraps
2015 - IRG/WP 15-10838
Many authors have suggested natural durability may be lower in second-growth western redcedar than in old-growth. One potential means of offsetting a decline in durability is use of physical barriers to separate the wood from soil. In the present work we compared the durability of old-growth and second-growth western red cedar posts, with and without barrier wraps, in a field test. After ten year...
P I Morris, J K Ingram, R Stirling


Investigations on the durability of several Congo basin wood species
2015 - IRG/WP 15-10840
The sawdust of ten wood species was studied to assess their natural resistance to decay. The extractives and lignin contents were primarily determined (between 2.7-16.0% and 26.8-35.9% respectively) to give an overview of the chemical distribution. Then, a phytochemical screening (colorimetric methods) characterized the different chemical functional groups in all extracts studied. Antioxidant act...
S Mounguengui, J-B Tchinda Saha, M Kor Ndikontar, S Dumarçay, C Attéké, D Perrin, E Gelhaye,


Chemical composition of extractives of different wood compartments of Pinus merkusii and their potential implication in wood durability
2015 - IRG/WP 15-10841
Amounts and nature of extractives differ strongly according to the compartment of wood and to the nature of the wood species. Previous studies reported that knotwood of several European Pinus sp. contains extractives contents much higher than stemwood consisting mainly of lignans which may find valuable applications in cosmetic, nutraceutic or pharmaceutic sectors. Different explanations have been...
A Wijayanto, S Dumarçay, R Kartika Sari, W Syafii, P Gérardin, C Gérardin-Charbonnier


Natural durability of Chilean commercial wood exposed to the action of marine borers
2015 - IRG/WP 15-10849
Results of field experiences of natural durability of ten commercial wood, exposed to the action of Bankia martensi (Stempell) in the South coast of Chile are presented. Tested species were seven types of native wood and three types of exotic ones. Test specimens of standard dimension of 0.02 x 0.045 x 0.23 m with three replications by species were used. The degree of attack was determined accord...
R Carmona C, C Osorio, A Almuna