Report of activity of CEN/TC 38: Test Methods for Wood Preservatives
1987 - IRG/WP 2287
G Castan


Japanese Classification of Wooden Building Members for ISO Use Classes according to the Building Code in Japan.
2006 - IRG/WP 06-20337
Because of the international approve of use class system for the biological degradation of wood by ISO/DIS 21887 and ISO/DIS 21892, Japanese committee of ISO/TC165/SC1 asked to the JWPA for classify the wooden commodities by use class of these draft ISO. The JWPA was prepared a draft use class model in Japan. Japanese building code systems are described and Japanese draft use class system is also ...
K Suzuki


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Studies on the destruction by marine wood boring organisms of fishing boats in the Eastern Black Sea of Turkey
1977 - IRG/WP 427
The present paper concerns the problem of fishing boats which are attacked by wood boring organisms in the Black Sea of Turkey. The aims of this study are: 1) to identify the marine wood boring organisms attacking fishing boats in the Northern Black Sea of Turkey; 2) to identify the wood species that are used in boat building construction and assess their durability; 3) to assess the degree of att...
R Ilhan, O A Sekendiz


Chemical, physical and biological factors affecting wood decomposition in forest soils
2003 - IRG/WP 03-20281
Organic matter (OM) decomposition is an important variable in determining the potential of forest soils to sequester atmospheric CO2. Studies using OM from a particular location gives site-specific decomposition information, but differences in OM type and quality make it difficult to compare results among soils and forest ecosystems. By using a “standard” OM in decomposition studies, OM qual...
M Jurgensen, P Laks, D Reed, A Collins, D Page-Dumroese, D Crawford


Kinetic of the wood degradation produced by wood decay fung
1993 - IRG/WP 93-20016
The degradation degree of a wooden structure has a direct influence on its loss of mechanical strength. It's necessary to deepen in non destructive techniques which permit to extrapolate the results obtained in laboratory to structural timber used in the building's construction. This work studies the relationship existing between the pulse velocity of ultrasonic waves and the wei...
M T De Troya, A M Navarrete, A Sanchez, V Bucur


Flow charts for termite and decay tests to determine the natural durability of Japanese cedar (Cryptomeria japonica D. Don)
2008 - IRG/WP 08-20385
This paper deals with the experimental flow charts that were used for determination the effects of fungal decay and termite attack on Sugi heartwood during the course of the study of “Comparative studies of natural durability of Japanese cedar (Cryptomeria japonica D. Don) among the geographic cultivate”, which was carried out by Usta et al (2006)....
I Usta, S Doi


Natural Durability Classification Systems Used Around the World
2009 - IRG/WP 09-10694
Around the world natural durability is classified in different ways. The nature and rigor of the tests used to measure durability, the method of classification based on these data, and use of these classifications to specify end uses or predict service life all vary. This can lead to confusion among people not familiar with the various systems used. This review describes the methods used to classi...
R Stirling


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Bending creep test of plywoods under long term exposure to fungal attack
1981 - IRG/WP 2163
Bending creep test and decay test were coupled in order to evaluate the durability of structural plywoods and preservative efficacy. Experimental blocks, 5.0 x 1.2 cm² section x 35.0 cm length, were impregnated with distilled water and inoculated with mycelial fragments of test fungus. Polyethylene bags stretched with metal frame were used as decay chambers. The chambers containing inoculated blo...
M Takahashi


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


Data requirements for wood preservatives in the EU Biocides Directive
2001 - IRG/WP 01-50166-08
Directive 98/8/EC of the European Parliament and of the Council concerning the placing of biocidal products (the Biocidal Products Directive, BPD) lays down the requirements on data needed for authorisation of a biocidal product and approval of its active substance(s). The dossier must contain data needed for the proper risk assessment of the biocidal product. A detailed technical guidance documen...
H Braunschweiler


Chapter 1 - Introduction to bamboo
2007 - IRG/WP 07-10635-01
In this introductory chapter the botanical position, distribution, utilization, outlooks, production, research, importance, propagation, natural durability, preservative treatment, importance of preservative treatment, treating principles, research on preservative treatment of bamboos and the objectives of this book have been described briefly under individual caption....
A K Lahiry


A new model for wetting and drying of wood end-grain – with implications for durability and service-life
2011 - IRG/WP 11-20477
New experimental data for wetting and drying of wood end-grain, Sandberg (2009), imply that traditional models for moisture transport are not at all applicable. A new model is developed to consider the phenomenological behaviour of water transport in and out of end-grain, using the pore water pressure and sorption scanning properties. Modelling results are compared to experimental results and the ...
L-O Nilsson, K Sandberg


Soft rot tests
1983 - IRG/WP 2206
At the IRG meeting in Turkey it was proposed that developments in testing preservative-treated wood in unsterile soil according to techniques variously described as "fungus cellar", "soil-bed", or "accelerated field simulation" be considered along with conventional laboratory procedures as the basis for a standard test. Before formulating any co-operative test programme it is essential to examine ...
J A Butcher


The effect of ACC (Celcure) on durability of blue beech
1999 - IRG/WP 99-30209
Durability of the sapwood and heartwood of blue beech (Carpinus betulus) against white rot fungus (Coriolus versicolor) was studied. As treatment three concentrations of preservative (control or 0%, 3%, and 5% of ACC) were applied. The measuring 1.5x2.5x5cm3 as dimension of wood samples (sap and heartwood) was used. During 16 weeks exposure, untreated wood blocks were completely deteriorated by th...
S M Kazemi


Summarized comparison of four techniques for detecting defects in poles
1979 - IRG/WP 2126
Since our discussions in open session of Working Group II at Peebles, a number of workers in Australia have collaborated in comparing the efficacy of X-ray, sonic testing, or resistivity measurements for detecting internal defects in poles. The purpose of this circular is to draw to your attention some of the results, in summary form. No attempt has been made to compare techniques. More detailed a...
H Greaves


Correlation between different international standard assessment procedures with termites. Part 1: Field exposure
1983 - IRG/WP 1198
Ramin treated with copper-chrome-arsenic (CCA), pentachlorophenate and lindane, each at three retentions, and three other untreated timbers were assessed in the field against Coptotermes lacteus and Nasutitermes exitiosus. Replicate specimens were exposed around five mounds of each termite species over a period of five years in south-eastern Australia. The field results provided the basis for judg...
M Lenz, C D Howick, N Tamblyn, J W Creffield, M Westcott


Natural durability of Iranian saxual wood (Haloxylon persicum) against the fungal decay
1991 - IRG/WP 1515
Haloxylon persicum is vidly planted in the deserfic region of Iran. At the present time, in the age of 30, these small trees are ready for cutting for the different uses, specially for rural buildings. But there's any knowledge about its durability. In this study the laboratory tests were carried out in accordance to European Standard. 5 fungi were used as: Trametes versicolor, Coniophora...
D Parsapajouh, F H Schweingruber, K Richter


Study of the degradation of retified wood through ultrasonic and gravimetric techniques
1994 - IRG/WP 94-40030
One of the non-polluting processes that increase the natural durability of wood is a thermal treatment in an atmosphere poor in oxygen, producing what is normally denominated "retified wood". In this study the validity of a non-destructive technique (ultrasound) in order to determine the biodegradation suffered by wood across time has been studied. For this reason, the behavior of a wood species (...
D T De Troya, A M Navarrete


Resistance of Teak, Balau, keruing and Chengal Wood species against marine borers attack
2004 - IRG/WP 04-10513
Wood samples of Teak (Tectona grandis) , Keruing (Dipterocarpus alatus),Yellow Balau (Shorea laevis) and Chengal (Balanocarpus heimii) were treated by Creosote, using Ruping method. The dimension of samples were 200 x 75 x 20 mm and the retention were 188, 186, 331, 40 kg /m3 respectively. Both treated and untreated samples were installed in sea water (Mahshar in Persian gulf and Bandar Torkman an...
A Rezanejad


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


A comparison between the effects of ACC & CFK on the durability of beech, hornbeam and cottonwood by using Dipping & Bethel methods in the North of Iran
1997 - IRG/WP 97-40089
From the economical point of view, increasing the lumber durability by the application of preservative treatments is very important. In this study, samples were randomly selected from Fagus orientalis Lipsky., Carpinus betulus L. and Populus deltoides Bartr. in two forms (Board & Squared cross-section) and have been treated with ACC & CFK by using Dipping & Bethel methods. The matched ...
D Parsapajouh, V Etemad, K Pourtahmasebi


Evaluation of chlorpyrifos as an insecticidal component of a wood preservative
1984 - IRG/WP 3301
After two years of laboratory and field testing, chlorpyrifos is showing excellent potential as an insecticidal treatment to wood. In laboratory termite tests, retentions as low as 1-2 parts-per-million or approximately 0.0008 kg/m³ (0.00005 lbs/ft³) are effective against the Coptotermes formosanus. Laboratory leaching tests have shown no significant effect on the concentration of the retained c...
K Rose, J Kozuma, P Sparrow


European laboratory termite testing
1986 - IRG/WP 1299
As with all testing of wood preservatives the evaluation of the resistance to termites of treated wood requires methodology which is approriate to, and can be readily extrapolated to, the practical situation. Thus not only must the variations in possible treatment systems be taken into account (eg dip, brush or pressure application) so too must the range of termite species and the type of exposure...
R W Berry