Performance of treated and untreated sawn fence posts of Scots pine and Norway spruce
2000 - IRG/WP 00-30247
Sawn fence posts are a rather important product and the objective of this trial was to assess their durability. In 1985 a field trial with treated and untreated fence posts of Scots pine (Pinus sylvestris L.) and Norway spruce (Picea abies (L.) Karst.) was set out at the test field in Ultuna, Uppsala, Sweden. The posts had a dimension of 75 x 100 x 1400 mm3. The preservatives applied were a CCA, a...
Ö Bergman


Durable fibre for durable MDF – testing Tricoya®
2015 - IRG/WP 15-40704
The chemical modification of wood has been a commercial reality for a decade on release of technologies for the modification of solid wood including Accoya®. A challenge and an opportunity for the modification technologies which typically impart dimensional stability, water stability and enhanced biological durability was the adaptation of the technology to wood based panels. This paper presents ...
E Suttie, J Alexander, M Maes


Dimensional stability, biological resistance, and mechanical properties of phenol-resin-treated particleboard
1990 - IRG/WP 3622
Particleboards were treated with a low molecular-weight phenol-formaldehyde (PF) resin and their enhanced properties were evaluated. Besides dipping of particles in aqeous solutions of resin, and spraying of resin solutions before spray of the conventional phenol-formaldehyde resin for adhesive binder, one step treatment by spraying of the mixture of the low molecular-weight resin and the adhesive...
Y Imamura, H Kajita


Fungal resistance of smoke-dried Cryptomeria japonica wood
1998 - IRG/WP 98-40118
Performance of smoke dried wood on fungal resistance was studied. The maximum temperature of the smoke seasoning was 80-90°C in the drying room and 70-80°C within the wood for 6 days during the treatment for 15 days. Decay resistance of smoke-dried Cryptomeria japonica wood was evaluated using a brown rot fungus, Tyromyces palustris. Weight losses of untreated wood, smoke-dried wood, and smoke-d...
K Yamamoto, I Momohara, T Nishimura


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Evaluating the natural durability of a number of lesser known species of Ghanaian hardwoods using a short term laboratory assay
2004 - IRG/WP 04-10540
Resistance of a number of Ghanaian hardwoods to attack by the crustacean Limnoria quadripunctata was assessed by measuring the production of faecal pellets under forced feeding conditions over a two week period. Small sticks of commercially available, lesser known timber species, were leached in seawater for one week then placed in a cell culture chamber with one animal and 4 ml of seawater. At in...
J R Williams, S M Cragg, L M S Borges, B Shayler


Wood preservation in Thailand
1983 - IRG/WP 3265
The report gives a background to Thailand and its timber resources, production and consumption. The history of wood preservation in the country and its modern industrial development are described. Its 19 preservation plants are listed and the production figures of the two major ones given. The wood preservatives in use are noted and the costs of treating a railway sleeper in three different ways c...
A Rananand, R Cockcroft


Sustainability Through New Technologies for Enhanced Wood Durability. COST Action E37 – A New Action in the Forestry Domain
2004 - IRG/WP 04-40293
The main overall objective of the action is to concentrate on the contribution of wood durability on the sustainability through the development of systems for quality assurance and perfoamance of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeks to improve and consequently increase the cost-effective use of sustainably produced E...
R-D Peek


Novel wood modification processes for window and cladding products
2004 - IRG/WP 04-40285
Because of the low natural durability and low dimensional stability of European wood species, the usage of wood for window frames has decreased dramatically during the last decade. In a joint project of several German research institutes and the window industry, following wood modification systems were compared. heat treatment (3 different materials from 2 companies) acetylation (pine sapwood an...
A Krause, C Hof, H Militz


Stability and performance of tributyltin compounds
1984 - IRG/WP 3275
Based on the critical examinations of the disputable permanence of tributyltin compounds in wood, this paper deals with a number of examinations of the relative evaporation, thermal stability and oxidation stability of some TBT-compounds. While thermal and oxidative stability is high for all TBT-species, the relative evaporation at elevated temperature is highly variable, and lowest for the TBT-es...
F Imsgard, B Jensen, H A B Landsiedel, H Plum


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


Leaching of CCA preservative from treated timber in marine environment
2001 - IRG/WP 01-30254
Knowledge on the amount of preservatives leaching out of treated wood is essential to optimise the chemical loading in various species of timber required for different end uses. In order to gain more insight into this aspect, the residual CCA content in 40 treated timber panels belonging to 14 species removed on destruction by marine organisms from a series of durability tests conducted in Kochi w...
M V Rao, V Kuppusamy, K S Rao, L N Santhakumaran


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...
L Kervina


Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo


Information from the COIPM Wood Group
1986 - IRG/WP 4130
The Chairman outlined the progress of the co-operative work "testing the resistance to marine borers of heat shrinkable polyolefin sheathings and of wood treated by vacuum/pressure with polymers (polystyrene)". The first part of the work has been started: the samples of wood wrapped with shrinkable polyolefin sheathings have been prepared and sent to the stations participating. The second part of ...
A Gambetta


An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat


Natural durability of European wood species for exterior use above ground
2003 - IRG/WP 03-10499
The main interest in using more timber for exterior constructions is to protect the environment, where wood is considered an environmentally friendly material. However, chemicals for wood protection are getting more and more restricted, consequently, the focus on the natural durability of wood is increased. Good, well-documented data on the durability of wood species in ground contact exist, which...
B Lindegaard, N Morsing


A study of wood quality of Juglans nigra and hybrid walnut (MJ 209xRA) : durability against Coriolus versicolor, density and MOR
2004 - IRG/WP 04-10522
The study investigated possible effects of harvesting season on some wood properties of Juglan nigra (JN) and a hybrid walnut (MJ209xRA). The samples were taken from trees which were harvested in June July, August, November of the same year, and March in the year after to determine whether there were any significant differences in wood properties as regards the harvesting seasons. In order to test...
B Charrier, F Charrier, D P Kamdem, J B Aurel, G Janin


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Ammoniacal wood preservative for use in non-pressure treatment of spruce and aspen poplar. Part 1
1984 - IRG/WP 3273
End-matched lumber of Picea glauca (Moench)Voss (white spruce) and Populus tremuloides Michx. (aspen poplar) timbers was treated by a thermal diffusion process in open tank treating vessels using an ammoniacal copper-arsenate wood preservative. The process proved technically feasible with respect to controlling the vapourization of ammonia from open tanks during treatment at high temperatures. Tre...
C D Ralph, J K Shields


The dry rot fungus Serpula lacrymans, its growth and damaging of wood
2004 - IRG/WP 04-10511
The dry rot fungus (Serpula lacrymans) is one of the most dangerous wood rotting fungi, especially in the built environment. In our mycological laboratory more experiments with this fungus have been carried out aimed at:- its growth under stable and variable climatic conditions, - its possibility to attack either natural wood of different species and also modified wood primary pre-treated with ...
L Reinprecht


The effect of ACC (Celcure) on durability of blue beech
1999 - IRG/WP 99-30209
Durability of the sapwood and heartwood of blue beech (Carpinus betulus) against white rot fungus (Coriolus versicolor) was studied. As treatment three concentrations of preservative (control or 0%, 3%, and 5% of ACC) were applied. The measuring 1.5x2.5x5cm3 as dimension of wood samples (sap and heartwood) was used. During 16 weeks exposure, untreated wood blocks were completely deteriorated by th...
S M Kazemi


Assessing the performance of wood preservatives from biological tests - the European approach
1994 - IRG/WP 94-20040
The impetus for the European Standardisation Committee to undertake the development of a performance standard for characterising the effectiveness of wood preservatives from biological tests, lies in the Construction Products Directive. This is effectively the European Community law which provides the basis for Construction Products to be traded across all member states without technical or regula...
A F Bravery


Correlation between different international standard assessment procedures with termites. Part 1: Field exposure
1983 - IRG/WP 1198
Ramin treated with copper-chrome-arsenic (CCA), pentachlorophenate and lindane, each at three retentions, and three other untreated timbers were assessed in the field against Coptotermes lacteus and Nasutitermes exitiosus. Replicate specimens were exposed around five mounds of each termite species over a period of five years in south-eastern Australia. The field results provided the basis for judg...
M Lenz, C D Howick, N Tamblyn, J W Creffield, M Westcott