Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


Utilization of coconut timber from north Sulawesi, Indonesia. Part 1: Durability
1994 - IRG/WP 94-30044
Coconut timber from non-productive plantations is a byproduct of an agricultural crop and, by the same token, constitutes a renewable resource which may serve as a complement to or, at least in part, as a substitute for traditional timbers in local markets. Its more extensive utilization is expected to contribute to the conservation of tropical rain forests. Export of coconut timber and/or wood pr...
R-D Peek


Comparative natural resistance of eighty-two timber species to damage by marine borers at Goa (India)
1996 - IRG/WP 96-10139
Natural bioresistance of eighty-two species of Indian timbers to attack by marine wood-borers has been presented based on data collected from test panels exposed in Goa waters (west coast of India) for periods ranging from five to thirteen months. All the timber species, except Artocarpus gomeziana and Pterocarpus santalinus, were completely destroyed within a short period of three to six months. ...
L N Santhakumaran


A study of poplar LVL durability improvement:
1999 - IRG/WP 99-40148
The aim of this study was to optimise the durability of LVL panels by adding boron during the gluing process. Poplar veneers (2,6 mm thickness ) were selected by ISORY a French company . Two types of glue were tested : Phenol resorcine and Melamine Urea Formaldehyde. Each of them was mixed with various concentrations of borax (for the first one) and Boric acid(for the second one). Mechanical prope...
B Charrier, V Bridaux, N Fauroux, F Charrier


Termite resistance of Malaysian and exotic woods with plantation potential: Field evaluation
1998 - IRG/WP 98-10289
An in-ground resistance of selected Malaysian and exotic timbers to attack by a representative aggressive subterranean Coptotermes termite was evaluated as part of an on-going collaborative research between the Forest Research Institute of Malaysia and the University of Hawaii on termite control of building timbers under humid tropical conditions. A test site at FRIM, highly susceptible to the sub...
A H H Wong, J K Grace, L H Kirton


Field evaluation of the above-ground susceptibility of Pinus heartwood and untreated or treated sapwood to two species of Australian subterranean termites
1996 - IRG/WP 96-10147
Plantation-grown Pinus elliottii, Pinus caribaea and Pinus radiata specimens containing heartwood and untreated or preservative-treated sapwood were exposed above ground to the subterranean termites Coptotermes acinaciformis or Mastotermes darwiniensis near Sydney (NSW), Brisbane and Townsville (Qld), and Darwin (NT), using a variety of exposure techniques. Heartwood of Pinus elliottii and Pinus c...
M J Kennedy, J W Creffield, R H Eldridge, B C Peters


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


Durability aspects of (hydro)thermal treated wood
2000 - IRG/WP 00-40160
Samples of several wood species were treated in a two steps process, subsequently hydrothermal and dry heat-treated, by the so-called PLATO-process and analysed for their resistance against fungal attack. Both PLATO-treated and dry heat-treated specimen were prepared and analysed, in order to study the influence of moisture during hydrothermal treatment of wood. The resistance against all of the s...
B F Tjeerdsma, M Stevens, H Militz


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Preservative treatment of common timbers and bamboos of Bangladesh for rural electrification infrastructure
1998 - IRG/WP 98-40104
Researches revealed new treatment grades, treatment groups, grading groups, natural durability grades, strength groups and a new preservative combination for remedial treatment and sterilization of most common timbers and bamboos of Bangladesh. The obtained findings are applicable for equivalent timber species having equivalent climatic condition. Sapwoods are always perishable and timbers with wh...
A K Lahiry


Improvement of intrinsic properties of wood by chemical wood densification - Hydrophobic aspects and durability aspects
1999 - IRG/WP 99-40149
To improve the intrinsic properties of Scot pine wood ((1) hydrophobic surface and (2) durability), two ways of chemical modification have been tested. The first one is the chemical modification of hydroxyl groups by active substances like diisocyanate compounds with a copolymerization step. The second way is a densification by an impregnation of resins and a gamma polymerisation. This second way ...
G Labat, Q K Tran, I Le Bayon


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Introducing bamboos for their importance and conservation
2005 - IRG/WP 05-10546
Bamboo is a socio-economically, industrially and environmentally important forest and rural crop in Asia. It is an essential task for the people in this region to conserve the bamboos and preserve the bamboo products for their sustainable continuity. An earnest need for this task is to introduce a variety of important information on bamboos. In this research paper the botanical position, distribut...
A K Lahiry


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Preliminary studies of the performance of iron chelators as inhibitors of brown rot (Coniophora puteana) attack
1996 - IRG/WP 96-10185
This paper describes experiments to examine the proposal that the presence of iron is essential for brown rot fungi to utilize hydroxyl radicals remote from the hyphae as a means of converting the wood into a food source. reliminary test results are presented from trials using three different iron chelators impregnated into Scots pine (Pinus sylvestris) sapwood blocks. Their relative effects on th...
E D Suttie, R J Orsler, P M Wood


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


Field Trials with mini-stakes
2002 - IRG/WP 02-20244
In 1995 an extensive field test program with wood mini-stakes, 8 x 20 x 200 mm, was started. In these trials a large number of parameters are being evaluated, including several new wood preservatives, differently chemically modified woods and natural durability of various wood species. The test sites are three fields in Sweden for in-ground and “close to ground” testing, one subterranean termi...
M Westin, A O Rapp, Y S Hadi, T Nilsson


Chitosan for wood protection - state of the art
2005 - IRG/WP 05-30378
The aim of this paper was to give a state of the art description of chitosan as a wood protecting agent. Chitosan is a metal free natural compound derived from crustacean shells and is under evaluation as an environmentally benign wood protecting agent. Information from journals states that chitosan may act both fungistatically and at higher concentrations, as fungitoxic, but the mode of action is...
M Eikenes, G Alfredsen, E Larnøy, H Militz, B Kreber, C Chittenden


Evaluation of teak sawdayst Tectona grandis L Fil as a potential source to obtain a natural wood preservative in Colombia
2004 - IRG/WP 04-30356
Plantation Teak (Tectona grandis L. Fil) has been tested as a possible source of natural wood preservatives due to the known excellent durability of old-growth teak wood. Field tests (ground proximity termite and above ground simulated decking exposures) were established in Colombia in April 2003 at two different test sites with different climates (Tropical Dry and Rain forest). Teak heartwood ex...
A Castillo, Y Cabrera, A F Preston, R Morris


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


Reduction of preservatives leaching from wood by the application of animal proteins
2005 - IRG/WP 05-30387
The investigations consisted in the estimation of the effectiveness of protein borates and protein propionates in wood preservation against Coniophora puteana. The estimation was made on the basis of mass losses caused by the test fungus action against treated wood which was subjected to leaching with water. The investigations were performed for Scots pine wood (Pinus sylvestris L.) treated with p...
B Mazela, I Ratajczak, M Bartkowiak


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


An observation of seasoning, preservative treatment and storing of CCA treated 30 bangladeshi hardwood species for crossarms
1995 - IRG/WP 95-40058
Observed kiln seasoning, preservative pressure treatment and storing of CCA treated 30 Bangladeshi hardwood species for crossarms. It revealed that it was very difficult to kiln season and preservative pressure treatment of thirty species together in a single charge and found that when species of different specific gravity kiln season together there occur some objectionable seasoning degrades, and...
G N M Ilias, M D Rokib-ul-Hafiz


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...