IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 967 documents. Displaying 25 entries per page.


Tebuconazole - a new triazole fungicide for wood preservation
1991 - IRG/WP 3680
The great potential of Tebuconazole for wood preservation is demonstrated. Test carried out by official institutes shown that Tebuconazole is particularly effective against wood-rotting basidiomycetes strains. The efficacy of Tebuconazole against the brown rot Gloeophyllum trabeum is outstanding: the toxic value measured in accordane with EN 113, without·ageing, after leaching (EN 84) and after e...
O Exner


Developments in wood preservation processing techniques in New Zealand
1980 - IRG/WP 3143
P Vinden, A J McQuire


Japanese Classification of Wooden Building Members for ISO Use Classes according to the Building Code in Japan.
2006 - IRG/WP 06-20337
Because of the international approve of use class system for the biological degradation of wood by ISO/DIS 21887 and ISO/DIS 21892, Japanese committee of ISO/TC165/SC1 asked to the JWPA for classify the wooden commodities by use class of these draft ISO. The JWPA was prepared a draft use class model in Japan. Japanese building code systems are described and Japanese draft use class system is also ...
K Suzuki


Treatability and retainability of two important bamboo species - borak and jawa of Bangladesh
2002 - IRG/WP 02-40248
Preservative treatment has been carried out with five different concentrations, i.e. 3%, 4%, 5%, 6% and 7% and durations, i.e. 2 days, 4 days, 6 days, 8 days and 10 days, at different moisture content, i.e. green and air-dry, and different direction of penetration, i.e. radial and both radial and cross-section for jawa and borak. It has been observed that retention of CCB is always higher in jawa ...
M N Islam, A K Lahiry, M O Hannan


Fungal resistance of smoke-dried Cryptomeria japonica wood
1998 - IRG/WP 98-40118
Performance of smoke dried wood on fungal resistance was studied. The maximum temperature of the smoke seasoning was 80-90°C in the drying room and 70-80°C within the wood for 6 days during the treatment for 15 days. Decay resistance of smoke-dried Cryptomeria japonica wood was evaluated using a brown rot fungus, Tyromyces palustris. Weight losses of untreated wood, smoke-dried wood, and smoke-d...
K Yamamoto, I Momohara, T Nishimura


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Evaluating the natural durability of a number of lesser known species of Ghanaian hardwoods using a short term laboratory assay
2004 - IRG/WP 04-10540
Resistance of a number of Ghanaian hardwoods to attack by the crustacean Limnoria quadripunctata was assessed by measuring the production of faecal pellets under forced feeding conditions over a two week period. Small sticks of commercially available, lesser known timber species, were leached in seawater for one week then placed in a cell culture chamber with one animal and 4 ml of seawater. At in...
J R Williams, S M Cragg, L M S Borges, B Shayler


Flow charts for termite and decay tests to determine the natural durability of Japanese cedar (Cryptomeria japonica D. Don)
2008 - IRG/WP 08-20385
This paper deals with the experimental flow charts that were used for determination the effects of fungal decay and termite attack on Sugi heartwood during the course of the study of “Comparative studies of natural durability of Japanese cedar (Cryptomeria japonica D. Don) among the geographic cultivate”, which was carried out by Usta et al (2006)....
I Usta, S Doi


Natural Durability Classification Systems Used Around the World
2009 - IRG/WP 09-10694
Around the world natural durability is classified in different ways. The nature and rigor of the tests used to measure durability, the method of classification based on these data, and use of these classifications to specify end uses or predict service life all vary. This can lead to confusion among people not familiar with the various systems used. This review describes the methods used to classi...
R Stirling


Sustainability Through New Technologies for Enhanced Wood Durability. COST Action E37 – A New Action in the Forestry Domain
2004 - IRG/WP 04-40293
The main overall objective of the action is to concentrate on the contribution of wood durability on the sustainability through the development of systems for quality assurance and perfoamance of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeks to improve and consequently increase the cost-effective use of sustainably produced E...
R-D Peek


Novel wood modification processes for window and cladding products
2004 - IRG/WP 04-40285
Because of the low natural durability and low dimensional stability of European wood species, the usage of wood for window frames has decreased dramatically during the last decade. In a joint project of several German research institutes and the window industry, following wood modification systems were compared. heat treatment (3 different materials from 2 companies) acetylation (pine sapwood an...
A Krause, C Hof, H Militz


Stability and performance of tributyltin compounds
1984 - IRG/WP 3275
Based on the critical examinations of the disputable permanence of tributyltin compounds in wood, this paper deals with a number of examinations of the relative evaporation, thermal stability and oxidation stability of some TBT-compounds. While thermal and oxidative stability is high for all TBT-species, the relative evaporation at elevated temperature is highly variable, and lowest for the TBT-es...
F Imsgard, B Jensen, H A B Landsiedel, H Plum


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


The role of third party independent inspection agency for wood preservation industry in China
2009 - IRG/WP 09-20425
This presentation attempts to provide a brief historical background and a current status report on the wood preservation industry in China. In addition, it will briefly introduce the need for building the quality control procedures and China wood protection Quality Supervision and Testing Center, a third-party inspection agency. Besides, some suggestions of this industry are proposed for its furth...
Zhenzhong Tang, Changsheng Shen, Yujie Han, Changming Song


Bamboo preservation in Vietnam
2009 - IRG/WP 09-40457
This paper presents the current state of bamboo preservation in Vietnam. The report focuses on the importance of bamboo preservation in relation to the bamboo resource and utilization, the major methods for preservation (such as non chemical und chemical methods), and emphasises the today’s pressing problems of research, standards as well as information for the bamboo preservation industry in Vi...
Tang Thi Kim Hong


Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


Generic code of good practices for wood protection facilities. Part 1: Wood protection (antisapstain) facilities
1993 - IRG/WP 93-50003
In general, the potential of high toxicity (aquatic and human) of wood protection (antisapstain) chemicals dictates the need to protect the environment and humans from its harmful effects. This document is a compendium of recommendations for the design and operating practices of wood protection facilities. The suggested recommendations focus on achieving the objectives of protecting the environmen...
G Das, V N P Mathur


Amines – Promising Wood Preservatives
2002 - IRG/WP 02-30287
Environmental concerns require a new approach in the field of wood protection. Band of many traditional wood preservatives has lead to intense researches for new environmental-friendly wood preservatives. Amines seem to be promising substitutes for classical biocides. Fungicidal and leaching resistance as well as some other chemical analysis of beach and Norway spruce samples treated with ethanola...
M Humar, F Pohleven, Š Kesnar, P Kalan


Leaching of CCA preservative from treated timber in marine environment
2001 - IRG/WP 01-30254
Knowledge on the amount of preservatives leaching out of treated wood is essential to optimise the chemical loading in various species of timber required for different end uses. In order to gain more insight into this aspect, the residual CCA content in 40 treated timber panels belonging to 14 species removed on destruction by marine organisms from a series of durability tests conducted in Kochi w...
M V Rao, V Kuppusamy, K S Rao, L N Santhakumaran


The resistance of wood coated with different solvent-borne paints against colonisation by decay fungi
2009 - IRG/WP 09-40468
This paper examines different solvent-borne paints characteristics and their decay resistance when applied on pine wood surface. It was determined by the standard ENV 839 procedure. The part of samples were subjected to accelerated ageing according to the EN 84 standard. The discussed commercial paint systems were typical stains or penetrating oil-based products, with or without biocides....
B Mazela, P Hochmańska


Chapter 1 - Introduction to bamboo
2007 - IRG/WP 07-10635-01
In this introductory chapter the botanical position, distribution, utilization, outlooks, production, research, importance, propagation, natural durability, preservative treatment, importance of preservative treatment, treating principles, research on preservative treatment of bamboos and the objectives of this book have been described briefly under individual caption....
A K Lahiry


Chapter 9 - Preservation of borak bamboo
2007 - IRG/WP 07-10635-09
Adequate penetration and retention of CCA and CCB have been obtained in pre-dried Borak bamboo (Bambusa balcooa Roxb. See Fig. below), abundantly grown in Bangladesh, with full-cell pressure process. The treated bamboo can be used as building materials; the sufficient treatability ensured its long-term best utilization at ground contact and indoors. This will keep the environmental and socioe...
A K Lahiry


A new model for wetting and drying of wood end-grain – with implications for durability and service-life
2011 - IRG/WP 11-20477
New experimental data for wetting and drying of wood end-grain, Sandberg (2009), imply that traditional models for moisture transport are not at all applicable. A new model is developed to consider the phenomenological behaviour of water transport in and out of end-grain, using the pore water pressure and sorption scanning properties. Modelling results are compared to experimental results and the ...
L-O Nilsson, K Sandberg


Status of wood preservation in India
2005 - IRG/WP 05-30386
Wood, despite the advent of other modern materials, continues to play an important role in man’s day to day life. Usage of wood ranges from fuelwood to engineered wood products and demand for it is increasing which has resulted in depletion of forests and diminishing wood supplies. Future needs are required to be met from plantation timbers after adopting processing technologies for their life...
S C Gairola, P K Aggarwal


Upright capillary absorption behavior of five important timbers and one bamboo species of Bangladesh
2004 - IRG/WP 04-40273
The upright or vertical capillary absorption rate of five different timber and bamboo species namely mango (Mangifera indica), kalajam (Syzygium cumini), kanthal (Artocarpus heterophyllus), sissoo (Dalbergia sissoo), mahagoni (Swietenia macrophylla) and mulibamboo (Melocana baccifera) were measured in relation to their specific gravity and duration of immersion. It has been observed that there was...
M A Islam, A K M A Bosunia, A K Saha, A K Lahiry


Previous Page | Next Page