IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 234 documents. Displaying 25 entries per page.


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Treating Bambusa vulgaris with neem seed oil against basidiomycetic biodegradation
2012 - IRG/WP 12-30608
Realising maximum benefits from bamboo stems/culms in Nigeria are presently constrained by their almost non-acceptance for applications in most structural and construction purposes, except in comparatively low quality and some temporary applications, such as scaffolding, owing to their susceptibility to easy destruction by agents of biodegradation as a result of their poor inherent natural durabil...
A A Erakhrumen


Development of a quality control assessment method to predict properties of heat treated wood
2012 - IRG/WP 12-40611
Heat treatment has been used to improve properties of non durable European species. Chemical modification of some of the wood components provides improved dimensional stability and biological performance against decay fungi while mechanical properties such as modulus of rupture are reduced. Quality control of commercially made thermally treated wood is one of the major challenges to allow its indu...
M Chaouch, K Candelier, S Dumarcay, A Pétrissans, M Pétrissans, P Gérardin


Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products. In this study the efficacy of wood treated with micronized copper, zinc oxide and their mixture was compared to that of wood treated with soluble amine copper oxide with subterranean termites in a laboratory test. All of the formulations tested were effective in controlling wood degradation by the termites...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Utilization of TG-DSC to study thermal degradation of beech and silver fir
2013 - IRG/WP 13-40628
Thermal treatment of wood is, besides other wood modification system, used to improve the decay resistance and dimensional stability. However, the chemical changes that are caused by treatment process are still difficult to quantify, characterize and control. Previous studies have shown that thermodesorption coupled to GC-MS is an attractive tool to characterize and quantify products formed during...
K Candelier, A Treu, J Dibdiakova, E Larnøy, A Petrissans, S Dumarçay, M Pétrissans, P Gérardin


Comparison of moisture loss and its increment during the rehearsal process based on natural drying and water soaking application with or without sealing the trial discs of Common black poplar (Populus nigra L.)
2013 - IRG/WP 13-40639
This study was subjected to be set up to prove the pattern of moisture loss and moisture increment within the same wood samples prepared as the discs (30x23±3 cm diameter) with or without the bark intact during drying and in the duration of the water soaking application. In this concept, wood was exemplified by Common black poplar (Populus nigra L.) of the five 12 year old trees that are grown in...
I Usta


Effect of Nano and Micronized Particles as Wood Preservatives for Termite Control
2013 - IRG/WP 13-30620
Subterranean termites are a major factor in the biodegradation of wood constructor products. In this study the efficacy of wood treated with micronized copper, zinc oxide and their mixture was compared to that of wood treated with soluble amine copper oxide with subterranean termites in a laboratory test. All of the formulations tested were effective in controlling wood degradation by the term...
M Akhtari, D Nicholas, A Rowlen, M Arefkhani


Effect of Nano-silver and Nano-copper and Nano-zinc oxide on Paulownia wood exposed to white-rot fungus
2013 - IRG/WP 13-30635
Paulownia is known as a fast growing tree and it can be used in several applications. The present study investigated the effect of Nano-silver and Nano-copper and Nano- zinc oxide on resistance of Paulowina (Paulownia fortunei) wood against the white rot fungus (Coriolus versicolor). Wood specimens with a dry density of 0.37g/cm3 were impregnated with a 400 ppm aqueous suspension of micronized na...
M Akhtari, M Ganjipour


Nano-Zycosil in MDF. Part I: Gas and Liquid Permeability
2014 - IRG/WP 14-40652
Effects were studied of zycosil nanoparticles, with size range from 20 to 80 nm, on liquid and gas permeability of medium density fiberboard. Nanozycosil was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. The obtained results indicated that the addition of zycosil to the mat resulted in a significant increase...
H Reza Taghiyari, A Karimi, P M D Tahir, O Schmidt, E Bari, P Nouri , A Jahangiri


Effect of silver nanoparticles on the rate of heat transfer to the core of the medium-density fiberboard mat
2014 - IRG/WP 14-40653
Effect of silver nanoparticles on the rate of heat transferred to the core section of medium-density fiberboard (MDF) mat was studied here. A 400 ppm aqueous nanosilver suspension was used at three consumption levels of 100, 150, and 200 mL/kg based on the weight of dry wood fibers; the results were then compared with the control MDF panels. The size range of silver nanoparticles was 30-80 nm. Res...
H Reza Taghiyari, O Schmidt, E Bari, P M Tahir, A Karimi, P Nouri, A Jahangiri


Experiences with an industrial system for controlled thermal wood modification in pressurized unsaturated steam
2014 - IRG/WP 14-40678
Thermal wood modification in pressurized reactors has a long history, but these processes are to date industrially scarcely used, because of the relatively complicated process equipment, compared to the more common high-temperature processes in kilns at atmospheric pressure. However, based on our practical experience with the FirmoLin® process, supported by recent scientific findings, it is foun...
W Willems


Bio-friendly preservative systems for enhanced wood durability - the first periodic report on DURAWOOD
2015 - IRG/WP 15-30677
The objective of the paper is the DURAWOOD scientific project carried out within Polish-Norwegian Research Programme, which lasts from September 2013 till August 2016. The aim of the project concentrates on the developing of a new, eco-friendly and biocide-free wood protective systems as an alternative to traditional, commonly used preservatives or coatings, containing biocides. Several wood prese...
B Mazela, M Broda, W Perdoch, L Ross Gobakken, I Ratajczak, G Cofta, W Grześkowiak, A Komasa, A Przybył


A review of the analytical methods used in determining the decay resistance of heat treated wood
2015 - IRG/WP 15-40690
Heat treatment as a wood process is increasingly used because of its non-biocide behaviour and its low environmental impact. This sort of treatment is based on biopolymer chemical degradation by heat transfer. This process improves mainly the dimensional stability and the decay resistance of wood. Wood becomes darker after this type of treatment and thus gives it an aesthetic appearance. These i...
K Candelier, M-F Thévenon, A Pétrissans, S Dumarçay, P Gérardin, M Pétrissans


Effect of natural variability of European Oak wood on heat treatment process and potential implication on wood durability
2015 - IRG/WP 15-40693
Environmental pressures appeared in France and in most European countries during the last decade has led to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative method during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


High-frequency monitoring of mass loss due to brown rot degradation of modified wood
2016 - IRG/WP 16-10862
Fungi growing in liquid culture undergoes three separate phases in which they i) adapt to the new environment, ii) grow unrestrictedly and exponentially, and iii) are inhibited to increase in number/mass due to lack of nutrients etc. Filamentous fungi have been shown to exhibit similar growth phases in a solid food substrate and have been modelled to grow in this way also in solid wood. In modifie...
R Ringman, A Pilgård, K Richter


Durability of a willow/plastic composite mat
2016 - IRG/WP 16-20592
Developing uses for wood wastes could enhance utilization of low value renewable materials while creating opportunities for rural development. Small diameter willow stems have little use in China, but they could be combined with high density polyethylene to create wood plastic composite mats for decorative applications. These mats could be used in exterior, above ground exposures, but would still ...
Li Yan, Haiyan Duan, Beizhan Quan, J Cappellazzi, J J Morrell


Effect of Nano-Silane on Permeability in MDF as a Result of Susceptibility to Moulds and Fungi
2016 - IRG/WP 16-40716
Effects were studied of vapor chamber on specific gas permeability of nanosilane-treated medium-density fiberboards (MDF). Size range of nanoparticles was 20 – 80 nm. Nano-silane (NS) was used at four consumption levels of 0, 50, 100, and 150 g/kg dry wood fibers. Density of all treatments was kept constant at 0.67 g/cm3. Specimens were kept for 18 weeks in vaporized chamber; their specific gas ...
H R Taghiyari, J Norton, A Moradiyan, M Sadegh Taher Tolou Del, H Siahposht, B Moradi-Malek, M Noferesti


How intraspecific radial variability of the European Oak’s may influence mild pyrolysis process and durability of the material
2016 - IRG/WP 16-40725
Last decades wood is promoted as building material. Unprotected wood exposed to outdoor conditions undergoes a variety of degradation induced essentially by fungi attacks. Heat treatment of wood by mild pyrolysis (180°C T 240°C under inert atmosphere) is a preservation process with a weak environmental impact, and therefore, is viewed as an interesting alternative to the chemical impregnation me...
J Hamada, A Pétrissans, F Mothe, M Pétrissans, P Gérardin


Markers of quality in self-bonded beech boards
2017 - IRG/WP 17-40820
A self-bonding phenomenon takes place when five layers of beech (Fagus Sylvatica L.) veneers are pressed at temperatures higher than 200ºC. If the pressing temperature between veneer surfaces reaches at least 225ºC during pressing and if the pressure applied is optimal, water-resistant bonds are formed between veneers. This study investigates the relation of thickness reduction (marker of compre...
C Cristescu, D Sandberg, O Karlsson


Preliminary Investigation into the Natural Decay Resistance of Nigerian Grown Hevea brasiliensis and Mitragyna ciliata wood to Phanerochaete chrysosporium White-Rot Fungus
2018 - IRG/WP 18-10919
Wood is an important and versatile structural building material that finds applications in numerous uses. However, wood is also a biological material vulnerable to degradation by microbial activities; this is especially true in the tropics. Following the scarcity of highly durable species from our natural forests and the introduction of so many lesser used/durable wood species into the booming tim...
J M Owoyemi, U O Emmanuel


On the natural durability of RED MERANTI for window frames as a function of gross density wood
2018 - IRG/WP 18-10927
MERANTI is a wood species belonging to the family Dipterocarpaceae, in the genus SHOREA (Shorea spp.). The genus has approximately 196 species with four subgenera. The subgenus RUBROSHOREA is commonly named RED MERANTI (RM) and is found on the Malayan Island of Sarawak, Indonesia, with approximately 65 varieties (Symington 1943). According to Brazier (1956), the distribution of gross densities wi...
K Hasse, W Unger, T L Woods


Previous Page | Next Page