Resistance of modified wood to termite attack assessed in laboratory and field testing: A review of internal research
2018 - IRG/WP 18-40824
Within the past decades, new wood modification technologies have been investigated in order to improve certain wood characteristics and enable the use of timber products for outdoor applications. Some of these non-biocidal technologies have been developed and commercialized recently. Thus, various material properties were studied intensively and shown to be improved. To a great extent, previous re...
L Emmerich, P Gascón-Garrido, H Militz


Recent findings clarifying the mechanism of brown-rot decay protection in acetylated wood
2018 - IRG/WP 18-40827
This paper summarizes the findings obtained during my PhD research over the past three years. The results provide insights which help to understand the enhanced brown-rot decay resistance of acetylated wood with particular emphasis on the role of water. The protection acetylation provides is derived from moisture exclusion within the acetylated cell wall, but the exact mechanism by which water is ...
G Beck


Selection of heat flux value for wood fire retardants testing using MLC
2018 - IRG/WP 18-40846
One of more crucial elements of investigating treated wood combustion properties with the use of a cone calorimeter is a proper selection of heat flux (HF). The HF level is directly reflected in time to ignition and a thermal degradation degree. The ignition of raw wood or of wood ineffectively protected against fire occurs at a low HF level, i.e. 10-20 kW/m2. By contrast, the ignition of wood whi...
B Mazela, W Perdoch, W Grześkowiak, A Batista


Difference of wood decay manner between brown-rot species
2019 - IRG/WP 19-10938
Wood blocks (Cryptomeria japonica) which were decayed by a Polyporales white-rot fungus (Trametes versicolor) and brown-rot fungi (Fomitopsis palustris, F. pinicola, and Wolfiporia cocos), respectively, were analyzed by X-ray diffraction and infrared spectroscopic methods followed by multivariate analysis. In the analyses, the differences in the cellulose crystallinities and infrared spectral patt...
R Kondo, Yo Horikawa, S Nakaba, K Ando, M Yoshida


Performance of untreated timbers in above ground decking tests: Preliminary results from an international collaborative trial
2019 - IRG/WP 19-10940
The ability to accurately predict wood decay risks under varying environmental conditions has long been of interest to timber users. Accurate predictions are difficult owing to the myriad of variables associated with the decay process including wood species, wood inhabiting organisms, timber building element design and environmental conditions. Despite these difficulties, decay predictions have be...
L P Francis, J Norton, E Melcher, A H H Wong, J Kok Lai, M Klamer, M J Konkler, J J. Morrell


Decay and water resistance of Siberian and European larch wood
2019 - IRG/WP 19-10941
The occurrence of larch wood is rather frequent in civil engineering. Namely, in building façades, terraces and balcony fences. In Slovenia and other central European countries, the use of the Siberian larch is especially popular. In this research, the durability against decay fungi in laboratory conditions and water exclusion ability of plantation-grown and naturally grown Siberian larch (Larix ...
B Lesar, D Krzisnik, M Humar


Diversity of wood decay fungi isolated from ground-contact wood stakes in Korea
2019 - IRG/WP 19-10952
This study was conducted to investigate wood decay fungi from 5 different ground-contact wood stakes in Korea. A total of 73 basidiomycetes were isolated and identified into 20 genera and 22 species by using molecular method. Among all fungi, only 6 species were brown-rot fungi and the others were white-rot fungi. Pinus densiflora and Quercus variabilis showed high fungal diversity and isolation f...
S-M Yoon, M-J Kim, W-J Hwang, Y-S Choi, D-W Son


Performance of wood decking after 5 years of exposure: verification of the combined effect of wetting ability and durability
2019 - IRG/WP 19-20647
Wood is one of the most important construction materials and its use in building applications has further expanded in recent decades. In order to enable even more extensive and reliable use of wood, factors affecting wood’s service life need to be understood. More recently, a new concept to characterize the durability of wood-based materials and to predict the service lives of wood was proposed,...
M Humar, D Krzisnik, B Lesar, C Brischke


Durability by design – a case study of the performance of wooden decks after 9.5 years of natural weathering
2019 - IRG/WP 19-20648
The service life expected for wood decking manufactured with poorly durable wood species, left untreated and exposed to severe environmental conditions such as high humidity and active biological agents, is usually assumed to be short (less than 10 years). The current classification of wood’s natural durability is based on EN standardised tests which do not fully reflect the real end-use conditi...
M Kutnik, M Montibus


Quantifying the effect of microclimatic parameters on the moisture-induced decay risk of wooden structures
2019 - IRG/WP 19-20649
Wood exposed outdoors is prone to fungal degradation. Besides its material-inherent resistance, numerous factors are impacting on its service life with both, climate and design having a major effect. In addition, topography, shading, wind barriers, and other local parameters have an effect on the microclimatic conditions at site and therefore need to be quantified for service life prediction of wo...
L Emmerich, C Brischke


Visual assessment of longitudinal wheel timbers and assessing the feasibility of extending wheel timber service life in the UK railway network
2019 - IRG/WP 19-20651
Timber has been a versatile building material for centuries and during the start of the Railway Age in the nineteenth century it was in considerable demand for use in the railway network, particularly bridge building. Timber is still in service and widely used throughout the UK railway network. The resilience and favourable strength to weight ratio and its relative ease of fabrication make it an...
J R Williams


The Structural Performance of the Nail Driven into the Decayed Wood
2019 - IRG/WP 19-20652
In late years there are many actions to long-term excellent house realization. We have to consider repair or reinforcement for long-term and safety use of wooden house. There are various studies focused on structural performance of decayed wood. It is important for long-term use of wooden house that structural performance of nailed joint on decayed wood is accurately evaluated. However, there are ...
N Wada, H Isiyama


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Hydroxyl accessibility - A brief review of deuterium exchange studies on modified wood
2019 - IRG/WP 19-20656
Wood modification imparts dimensional stability and decay resistance. The mechanism(s) by which this occurs are thought to be related to the bulking of the wood cell wall and subsequent moisture exclusion. Hence, quantification of accessible hydroxyl (OH) groups is of great interest when evaluating and increasing the understanding of the performance of modified wood. The aim of this study was to b...
G Beck, C Hill, G Alfredsen


Impact of water holding capacity and moisture content of soil substrates on the moisture content of wood in terrestrial microcosms
2019 - IRG/WP 19-20662
Terrestrial microcosms (TMC) are frequently used for testing the durability of wood and wood-based materials as well as the protective effectiveness of wood preservatives. In contrary to experiments in soil ecology sciences, the experimental set-up is usually rather simple. However, for service life prediction of wood exposed in ground, it is of immanent interest to better understand the different...
C Brischke, F L Wegener


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Identification of Antifungal Compounds in Konjac Flying Powder and Assessment against Wood Decay Fungi
2019 - IRG/WP 19-30737
The antifungal activity of konjac (Amorphophallus rivieri) flying powder (a by-product produced during mechanical processing of konjac flour) ethanol extract was evaluated against wood decay fungi in culture. Compounds associated with antifungal activity in the extracts were isolated and purified by silica gel column chromatography. The antifungal active fractions were identified by ultra-high-per...
Z Bi, F Yang, Y Lei, J J Morrell, L Yan


Boron dual-treatments for Douglas-fir utility poles: Tracking boron migration over time
2019 - IRG/WP 19-30739
The potential for using boron pressure-treatment prior to over-treatment with conventional, heavy-duty wood preservatives to limit internal decay in-service was investigated in two field tests on Douglas-fir utility poles. Pole sections were pressure-treated with disodium octaborate tetrahydrate (DOT) and then over-treated with either pentachlorophenol or copper naphthenate in oil. Alternatively, ...
J Cappellazzi, M J Konkler, J J Morrell


Relative efficacy of various oxine copper formulations against brown-rot fungi
2019 - IRG/WP 19-30741
This paper investigates the relative resistance of three different oxine copper formulations (oil-borne, water-borne, water-borne with pH-adjustment) as a preservative treatment for wood against brown-rot fungi. Impregnated southern pine sapwood cubes were exposed to R. placenta and G. trabeum cultures in a soil-block test. After eight weeks, the weight losses of the cubes were examined in relatio...
M Petruch, J Lloyd, A Taylor


Performance of field cut preservatives above-ground and in ground contact exposures
2019 - IRG/WP 19-30742
Field cut preservatives are needed to protect cut ends and drill holes that expose the untreated interior of preserved wood. A series of field cut preservatives were assessed in ground contact and above-ground exposures. After 10 years in ground contact exposure, all of the untreated controls had failed or exhibited very advanced decay. In contrast, the copper naphthenate (2% Cu in mineral spirits...
R Stirling, D Wong


Effect ofNano-Copper Oxide on Decay Resistance of Pistachio Twig-Plastic Composite
2019 - IRG/WP 19-30750
The goal of our study was to investigate the decay resistance of pistachio twig-plastic composite treated with nano-copper oxide against the white rot fungus Trametes versicoloer and the brown rot fungus Coniophora puteana. For this purpose, wood–polypropylene composites (WPCs) containing different loadings of nano-copper oxide, namely 0, 1, 2 and 3 percent (W/W), were made from pistachio (Pista...
M R M Farahani,S Pourabdollah


Preservative Treatment of CLT: An Example at Shimojishima Airport
2019 - IRG/WP 19-30748
Cross laminated timber (CLT) is a relatively new construction method that allows multi-storey construction using solid wood instead of concrete or steel. It is a method favoured by progressive architects and recognized for its much lower environmental footprint. Wood is an excellent construction material and is a long-term carbon sink that also performs well in the event of earthquakes and fire....
J Lloyd, N Yamashita, A Taylor


Using X-ray scattering to elucidate the mechanisms behind the moisture and fungal decay resistance of epoxybutene modified wood
2019 - IRG/WP 19-40854
Chemical modification of the hydroxyl groups of wood can improve the properties of wood by providing moisture and biological resistance, as well as dimensional stability. Southern pine solid wood was chemically modified to various weight percentage gains (WPG) with epoxybutene (EpB, 8%-38% WPG). After modification, specimens were extracted with a toluene: ethanol (2:1) solution for 2 hours or wate...
R E Ibach, N Plaza


Development of beech wood thermo-chemical modification treatments based on different vinylic derivatives of glycerol and polyglycerol
2019 - IRG/WP 19-40855
In this study, a combination between chemical and thermal wood modification has been investigated. Seven types of a low concentration of 10% aqueous additive solution of vinylicglycerol [glycerol-maleic anhydride (Gly-MA), glycidyl methacrylate (GM), and Glycerol methacrylate-maleic anhydride (GM/MA(2eq))], vinylicpolyglycerol [polyglycerol-maleic anhydride (PG-MA), polyglycerol methacrylate (PGM...
M Mubarok, S Dumarcay, H Militz, K Candelier, M-F Thevenon, P Gerardin