Risk assessment for tomorrow
2001 - IRG/WP 01-50166-14
Under the Biocides Directive Competent Authorities will be responsible in conducting risk assessment strategies for 23 product types, of which wood preservatives are only one. All of these groups show further diversity in terms of use patterns and the type of application method of the different chemical products used to control a variety of natural organisms. This increases the problem associated ...
J Chadwick


Preservation of wood composites with zinc borate
1995 - IRG/WP 95-30074
Inorganic borates such as boric acid, borax, disodium octaborate tetrahydrate, and zinc borate can be incorporated into wood composites such as waferboard to impart decay and insect resistance to the final product. Zinc borate is especially well suited for this application due to its efficacy and leach resistance. The paper summarizes the work performed to date in this area. The effects on strengt...
P E Laks, M J Manning


Chemical and biological investigations of double-vacuum treated windows after 5 years in service
1983 - IRG/WP 3219
In 1980 The Swedish Wood Preservation Institute initiated an investigation to study the degradation of TBTO and possible fungal attack in double-vacuum treated window joinery in service during 5 years. A hospital in Gothenburg was chosen that was built during 1969 to 1976. Both untreated and double-vacuum treated windows of Pinus sylvestris were used. A brown alkyl oil type paint (Nordsjö system ...
J Jermer, M-L Edlund, B Henningsson, W Hintze, S V Ohlsson


Performance of Oriented Strandboard, Medium Density Fiberboard, Plywood, and Particleboard Treated with Tebuconazole in Supercritical Carbon Dioxide
2005 - IRG/WP 05-30364
The performance of oriented strandboard (OSB), medium density fiberboard (MDF), particleboard and plywood treated with tebuconazole using supercritical carbon dioxide was investigated over a 48 month exposure under harsh above ground conditions in Hilo, Hawaii. Samples treated to low retentions (<0.20 kg/m3) tended to experience decay at rates that were only slightly lower than those found wit...
J J Morrell, M N Acda, A R Zahora


The new method of detecting decay in poles
1984 - IRG/WP 2229
In 1982 the Swedish Telecoms Administration in corporation with the Swedish Dog Training Centre started to investigate the possibility of using dogs for detecting decay in poles. At present two German Sheppheards and two Labrador Retrievers are in operation and the results have up to now well fulfilled our expectations. The following results have been obtained: 1.) The dogs can with high reliabili...
A Ammer, B Svedberg


Environmental risk assessment of wood preservatives in the Netherlands
2001 - IRG/WP 01-50166-10
Before biocides can be introduced to the Dutch market, they have to be authorised under the Pesticides Act (1962). The criteria for authorisation of biocides have been laid down in the Dutch Decree on Environmental Requirements for the Authorisation of Pesticides Used in Fields Other than Agriculture. In 1998, the EU Biocides Directive (98/9/EC) entered into force, and it was implemented in May 20...
E Smit, P van der Zandt, J Appelman


Proceedings from the wood preservation symposium "The Challenge - Safety and Environment" 19-20 February 1990, Cannes, France
1990 - IRG/WP 3600
Contains the List of Participants and the following 29 Documents (IRG/WP/3562-3590): Canadian code of good practices - Recommendations for design and operation of wood preservation facilities. (IRG/WP/3582) Current models used by the European health authorities to evaluate the vililization of active ingredients from treated wood used inside dwellings. (IRG/WP/3565) Creosote and cancer. (IRG/WP/...
Anonymous


Stake test with ammoniacal copper in combination with different agents started in 1962
1997 - IRG/WP 97-30130
In 1962 a stake test was started with ammoniacal copper in combination with chromium, arsenic, pentachlorophenol, boron, salicylic acid, benzoic acid, sorbic acid, pyridine and tannin. Different concentrations of the copper component were used as well as the added agents. For each concentration and test site, ten stakes of Pinus sylvestris L. sapwood were treated. The stakes were set out at two te...
B Häger, Ö Bergman


Restrictions on the use of chlorosilanes as potential wood preservatives
1985 - IRG/WP 3345
The biological protection of wood by chemical modification with different types of chlorosilanes has been investigated. The impregnation of wood has been carried out by means of liquid phase and vapor phase treatments using pure silane and silane-solvent systems. The biological efficacy against wood rotting fungi, molds and staining fungi was determined in a number of screening trials, subsequentl...
M Stevens


Immunolocalization of extracellular metabolites from Poria placenta
1988 - IRG/WP 1361
Polyclonal antisera produced to Poria placenta extracellular metabolites was used in immuno-fluoresence microscopy and immuno-gold TEM studies. In the fluorescence work, labelling of Poria placenta hyphae in wet fixed wood material was observed but not in infected wood which was oven dried prior to sectioning and immunolabelling. TEM studies provided better resolution, with gold labelling detected...
B Goodell, G F Daniel, J Jellison, T Nilsson


Quantification des émanations de substances dans l'air ambiant a partir des bois traités
1993 - IRG/WP 93-50001-27
Pesticides on wood for the purpose of its protection may evaporate. Eventual toxicity of such emanations justifies risk assessment procedures for indoor air in building. This document describes bench scale tests based on the technique of chambers developped by CTBA/BIOTEC to determine the amount of pesticides and associated substances released to the ambient air. Results obtained with various pest...
H Sageot, M Lamour


The effect of added nutrients on growth rate and decay capacity of Serpula lacrymans
1990 - IRG/WP 1427
At the previous meeting a new technique was presented that enables both fungal growth rate and wood decay rate to be measured using the same timber specimen. The technique (IRG/WP/1384) has previously been carried out with 1% malt as the sole nutrient within the small jar that provides the inoculum for this method. Results presented here relate to an additional level of 5% malt, with or without a ...
J D Thornton, A McConalogue


EPR observation of Mn(II) in decayed wood
2002 - IRG/WP 02-10443
Preliminary Electron Paramagnetic Resonance (EPR) studies of copper/chromium (CC) treated spruce wood, subjected to laboratory soil decay test showed increased intensities of Mn(II) EPR signal in partially decayed specimens. Several reasons might be responsible for this phenomenon: Mn(II) could originate from the wood after being released from the typical ligand binding, from reduction of other Mn...
M Petric, M Humar, P Kalan, F Pohleven, U Schoknecht, M Šentjurc


Detection of increased metal cations after wood decay using Chromeazurol-S
1997 - IRG/WP 97-20112
Chromeazurol-S (CAS) is a dye used for the spectrophotometric determination of metals, mainly aluminum (Al), berillium (Be) and copper (Cu). CAS has been widely used for determining the penetration of copper containing preservatives like CCA (AWPA A3-96). Additional uses include: i) detection of utility pole decay (Esyln, 1979), ii) a chemical spot test for aluminum in wood (Kukachka and Miller, 1...
F Green III, U Srinivasan, R B Miller


Field study: Wood degradation pattern in buildings and utility poles in tropical climates of Nigeria
1992 - IRG/WP 92-1521
The paper is the result of five years field study of wood degradation patterns in three ecological forest zones (Guinea Savannah, Tropical rain forest and mangrove forest zones, respectively). It involved 800 residential buildings and 700 electric overhead transmission poles. The methodology used was a modified Eslyn (6) test. A high rate of Ascomycetes and Basidiomycetes attack especially on the ...
E O Onuorah


Evaluation of impact of CCA-treated wood on the marine environment
1995 - IRG/WP 95-50040-15
This paper reviews the literature relating to the potential of CCA-treated wood to affect the marine environment and outlines the compounds required for a model which could be used to predict the environemental impact of maritime construction using such timber. Marine pilings require high loadings of CCA to provide protection from marine borers. Though loadings of 32-48 kg/m³ provide long-term pr...
R M Albuquerque, S M Cragg


Occupational exposure risk assessment at a commercial treatment plant using copper azole preservative
1998 - IRG/WP 98-50101-15
Experience with traditional water-based preservatives such as chromated copper arsenate (CCA) applied in closed system vacuum pressure impregnation plants has shown that operator atmospheric exposure is low during normal operation. TANALITH E is a commercially available copper azole wood preservative introduced as a chrome and arsenic-free alternative to CCA based on the actives copper, tebuconaz...
A S Hughes, M Connell


Reappraisal of some fungicides by the amended JWPA method
1992 - IRG/WP 92-3689
Organoiodine compounds which have been commercialized these years in Japan poorly performed as fungicides in the amended JWPA decay test (Standard 1, 1989) when applied to superficial treatment of timber. Because some parts of active ingredients seemed to disappear from the treated timber surface mainly due to the severe leaching cycles. This was prominently true for beech (Fagus crenata Blume) sa...
K Tsunoda


A study of fungal biodeterioration in unseasoned, packaged hem-fir lumber
1978 - IRG/WP 2116
This study was undertaken to determine the extent of biodeterioration that could occur within British Columbia (BC) prior to the export of packaged Canadian Lumber Standard Hem-Fir (Tsuga heterophylla, Abies amabilis and small amounts of Abies grandis). By examining the anti-stain treatments received by the lumber and identifying and characterizing the organisms responsible for the biodeterioratio...
P W Perrin, A J Cserjesi


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


Untersuchungen zur Prüfung mit Moderfäulepilzen im Vermiculit-Eingrabe-Verfahren
1972 - IRG/WP 214
Im Hinblick auf die Entwicklung eines Prüfverfahrens für die Bestimmung der moderfäulewidrigen Wirksamkeit von Holzschutzmitteln wurden Versuche mit Reinzuchten von Pilzen und mit Vermiculit als Trägersubstanz sowohl mit unbehandelten als auch mit Schutzmittelgetränkten Holzproben durchgeführt. Dabei wurde die Eignung von handelsüblichen, eintachen Einweg-Kunststoffbechern anstelle der bish...
W Kerner-Gang, M Gersonde


Occurrence and importance of various types of fungal and bacterial decay in CCA-treated horticultural pine posts in New Zealand
1984 - IRG/WP 1234
A detailed microscopical examination has been carried out on samples taken from CCA-treated pine posts exposed in horticultural soils. The following decay types were observed: white rot, brown rot, soft rot, tunnelling bacteria, cavitation bacteria, and bacterial erosion. The occurrence and importance of the various decay types between different regions, and plots within a specific region, varied ...
T Nilsson


A biochemical explanation for the observed patterns of fungal decay in timber
1980 - IRG/WP 1111
Experiments designed to compare the degree of localization of the cellulase enzymes of some white, brown and soft rot organisms are described. The site and nature of binding of the enzymes is discussed. The technique is ellution of mycelium grown in liquid culture with a variety: of agents including acetate buffer, carboxymethyl cellulose solution, borate/glycerol buffer and urea. The mycelium was...
N B Green, D J Dickinson, J F Levy


Extracellular osmiophilic particles in connection with brown rot and white rot
1982 - IRG/WP 1157
The way of attack on Pine woodblocks of two brown-rot fungi (Fomitopsis pinicola, Coniophora puteana) differing in their cellulase activities, and one white-rot fungus (Trametes hirsuta) has been investigated by transmission electron microscopy. Even at early stages of decay, osmiophilic particles were found with all the fungi investigated. In the brown-rotted wood, the osmiophilic particles occur...
K Messner, H Stachelberger


International comparison of three field methods for assessing the in-ground resistance of preservative-treated and untreated wood to termites and fungal decay – Summary of observations after five years
2003 - IRG/WP 03-20261
Results are presented from a five-year study conducted in five locations in Australia, Thailand and the USA. Three methods of exposure were assessed (below-ground, graveyard and ground contact) for evaluating the in-ground termite and decay resistance of Pinus radiata D. Don sapwood stakes that had been vacuum pressure impregnated with CCA (Type C) and ACQ (Type D) each at two nominal retentions (...
M Lenz, J W Creffield, T A Evans, B M Kard, C Vongkaluang, Y Sornnuwat, A F Preston