Performance of wood-based composites in a protected aboveground test in southern Japan
2008 - IRG/WP 08-40391
Five kinds of untreated wood-based composites (medium density fiberboard, hardwood plywood=HP, softwood plywood, particleboard and aspen oriented strand board, hereinafter abbreviated as MDF, HP, SP, PB and OSB, respectively) were exposed to subterranean termites and microbial (decay) attack under protected aboveground conditions in a southern part of Japan (Kagoshima Prefecture) for six years. An...
K Tsunoda


Feasibility study on three furfurylated non-durable tropical wood species evaluated for resistance to brown, white and soft rot fungi
2008 - IRG/WP 08-40395
Furfurylation can protect non-durable wood species against biological degradation, but the method used today cannot fully protect the heartwood of Scots pine due to insufficient penetration. In order to test alternative wood substrates for furfurylation, three Malaysian grown wood species (Kelempayan, Rubberwood and Sena) were furfurylated and subjected to soil block decay testing. Their performan...
T Mark Venås, A H H Wong


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


The susceptibility of hardwood plywood to white rot
2008 - IRG/WP 08-40397
The subject of the tests was resistance of veneer hardwood plywood to activity of pure culture of white rot fungus Trametes versicolor. The tested plywood was made with the use of the following glues: urea-formaldehyde (UF), melamine-urea-formaldehyde (MUF) or phenol-formaldehyde (FF). 4, 12 and 15 mm thick plywood was tested. External veneer of the plywood was mostly alder and the inner veneer (c...
A Fojutowski, A Kropacz


The effects of zinc borate treatment of wood strands on some technological properties of oriented strandboard (OSB)
2008 - IRG/WP 08-40419
In this study, influences of zinc borate treatment on some technological properties of oriented strandboard (OSB), from aspen wood (Populus euroamericana cv.) were evaluated. Therefore, a total of nine panels with dimensions of 40 cm by 40 cm by 1.8 cm and with an average target density of 0.65 g/cm3 were manufactured under the laboratory conditions. Experimental panels were manufactured at two di...
A D Çavdar, H Kalaycioglu, G Nemli


Improvement of the Fungal Resistance of Japanese Cedar by the ThermoWood Process
2008 - IRG/WP 08-40422
The effect of the ThermoWood Process on sapwood of the Japanese cedar, Cryptomeria japonica, was investigated. Seven matched specimens were cut from a sapwood board of Japanese cedar and subjected to thermal treatments according to the ThermoWood Process. The decay resistance and chemical and physical properties of the treated specimens and untreated specimen were investigated. The decay test wa...
I Momohara, T Morita, S Shouho, A Yamaguchi


Natural durability and anatomical features of teak (Tectona grandis) from plantations in Costa Rica
2008 - IRG/WP 08-10671
Teak (Tectona grandis) possesses superior mechanical properties and durability and is thus frequently used as an alternative to impregnated timber in Europe. Demand on teak has resulted in severe exploitation of the tropical teak forests in recent decades, but today the imported timber originates mainly from plantations and is certificated according to the Forest Stewardship Council (FSC) policy. ...
U J Wolfsmayr, N Terziev, G Daniel


Field Tests of naturally Durable North American Wood Species
2008 - IRG/WP 08-10675
There has been little field test performance data published on North American naturally durable species in general, and no published data on second growth material in particular. Yellow cedar (Callitropsis nootkatensis), western red cedar (Thuja plicata), eastern white cedar (Thuja occidentalis), and three wood species reputed to be moderately durable were installed in ground-contact (stakes) an...
P E Laks, P I Morris, G M Larkin, J K Ingram


Wood Decay Research Using Molecular Procedures, What Can It Tell Us?
2008 - IRG/WP 08-10678
There are many unanswered questions in wood decay and protection research, and no single research technique will ever answer all of these questions. The process of wood decay is a very complex series of biochemical and chemical reactions that are heavily influenced by the hundreds of bacterial and fungal species found on environmental samples of wood. There are a variety of molecular techniques b...
S V Diehl, M. L Prewitt, Young-Min Kang, L Mangum, J D Tang


Aislamiento, identificación y evaluación enzimática de hongos de pudrición de madera de la Región de los Lagos
2008 - IRG/WP 08-10680
So far, systematic investigations have not been developed to determine the fungal diversity associated with wood in Chile. In addition, little is known about the mycoflora capabilities or their enzymatic processes in biotechnology although different research has hinted at the great potential of these microorganisms in various industrial processes. The aim of this work is to isolate, identify and e...
R Ortiz, J Navarrete, C Oviedo, R Blanchette


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


To decay or not to decay: An accelerated field test of the validity of the Scheffer index
2008 - IRG/WP 08-20392
The Scheffer Index was introduced in 1971 to predict the relative decay hazard of untreated wood exposed above-ground. Precipitation and temperature parameters are used in the calculation. A higher Scheffer Index value implies a greater risk of decay. An accelerated 18-month study using seven field sites with Scheffer Indices ranging from 35 to 400 and two wood types (Populus tremuloides and Pi...
G M Larkin, P E Laks


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Field testing in Colombia: Three years of evaluations and experiences
2008 - IRG/WP 08-20394
Two field test sites have been established in Colombia for the evaluation of fungal and termite resistance of treated wood. The combination of elevated temperature, high and stable humidity and high rainfall at the two test sites accelerates microbial and insect activity (Scheffer, 1971; Thornton et al, 1994; Freitag et al, 1995). Tests established include above ground termite tests, ground contac...
Y Cabrera, A Preston


A Comprehensive Review of Copper as a Biocide, with a Focus on Micronized Copper
2008 - IRG/WP 08-30486
This paper reviews the wood preservative biocide active ingredient copper and delvers into new and previously unpublished data regarding the new micronized formulations which are now in vogue and widespread use in N. America in all residential treated lumber markets. Included in this review is the overall discussion of copper containing formulations used for pressure treated wood used over the las...
M H Freeman, C R McIntyre


Effect of a biological treatment on below ground decay of Douglas-fir pole sections
2008 - IRG/WP 08-40433
The use of exogenous sugars to accelerate microbial growth and eventually limit available oxygen in soil surrounding wood in soil contact was investigated on untreated Douglas-fir poles exposed over a 3 year period in Western Oregon. Isolation frequencies differed markedly between treated and untreated poles and the treatment did appear to shift the frequency of some basidiomycetes. The treatment ...
C Freitag and J J Morrell


Effect of different ASAs (alkenyl succinic anhydrides) on the treatment of biological protection of wood in use class 4
2008 - IRG/WP 08-40440
The alkenyl suscinic anhydrides (ASAs) used in this work are adducts resulting from the maleinization reaction of fatty acid alkyl esters. Various products with different alkyl groups were synthesized from rapeseed (Brassica napus) oil esters, rich in oleic acid. The liquids obtained showed a viscosity similar to that of vegetable oils and a brown color. When applied into wood, a thermal treatment...
C Vaca-Garcia, O Pignolet


Evaluation of the natural durability of reed (Phragmites australis) originating in the Fertö region (Hungary) against wood decay organisms as material for use in a sustainable motorway noise barrier
2009 - IRG/WP 09-10685
This work presents the research carried out to determine the natural durability of reed from the Fertö region of Hungary against wood decay organisms. The final objective of this study is to obtain sufficient relevant data in order that the reed may be used as a constituent element in a viable and sustainable motorway noise barrier, which has been developed within the European research project, k...
M T Troya, F Rubio, M J Prieto, D Lorenzo, J L Fernández-Cabo, R Schöftner


Impact of decay and blue stain causing fungi on the structural integrity of wood
2009 - IRG/WP 09-10699
The potential influence of diverse decay patterns caused by different brown rot provoking basidiomycetes on the structural integrity of wood was investigated. Additionally the potential impact of blue stain on the structural integrity was examined. Therefore decayed Norway spruce (Picea abies Karst.) specimens representing a wide range of mass loss, caused by four different brown-rot fungi and one...
C Brischke, C Welzbacher, T Huckfeldt, F Schuh


Gene expression of selected decay enzymes produced during biodeterioration of three wood types
2009 - IRG/WP 09-10702
Comparative studies were conducted on the expression of several decay enzyme genes during the decay of pine, cedar, and ACQ treated pine over 10 months. Measurements of MOE, decay rating, and moisture control were monitored for physical properties. Identification of decay fungi and the detection of decay enzymes were carried out before gene expression levels were measured. The MOE of wood stakes d...
Young-Min Kang, L Prewitt, S Diehl


The involvement of hydroxyl-radical-producing glycoprotein from the white-rot basidiomycete Ceriporiopsis subvermispora in wood decay
2009 - IRG/WP 09-10688
White-rot decay can be divided into two subtypes. One type involves the simultaneous degradation of all wood components through the formation of erosion troughs with a progressive thinning of wood cell walls. This type of decay is consistent with a model in which several polymer-degrading enzymes act on the exposed surfaces of the wood cell walls, producing progressive erosion from the lumen to th...
H Tanaka, Y Inoue, T Morikawa, S Itakura, A Enoki


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz


Accelerated H3 above-ground decay trials in Australia
2009 - IRG/WP 09-20411
An above-ground H3 fungal field trial was installed at five sites (3 in Australia, 2 in New Zealand), with the aim of finding a method that would shorten the time required for evaluating new preservatives and protection systems. One-quarter of the H3 preservative retentions were mostly installed, as first results suitable for registration occur when these reach 70% soundness. Chemical analysis of ...
L J Cookson, J Carr


Previous Page | Next Page