Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Durability of some alternatives to preservative treated wood
2004 - IRG/WP 04-30353
The environmental discussion in Sweden has lead to an increasing use of naturally durable domestic wood species and wood treated according to alternative methods for use above ground. A number of these alternatives have been tested according to field- and laboratory tests and compared to wood treated with preservatives for above ground use. Seven untreated wood species, four alternative wood treat...
M-L Edlund


Degradation of resin constituents in various wood species by the white rot fungus Bjerkandera sp. strain BOS55
1999 - IRG/WP 99-10301
In previous studies, the white-rot fungus Bjerkandera sp. strain BOS55 was shown to cause extensive degradation of lipophilic extractives (resin) in Scots pine wood. Further research was carried out in order to investigate the ability of Bjerkandera sp. for reducing resinous constituents in various softwood (Douglas fir, larch and spruce) and hardwood species (birch, beech and poplar). The greates...
J Dorado, T A Van Beek, F W Claassen, R Sierra-Alvarez


The action of siderophores isolated from Gloeophyllum trabeum on the structure and crystallinity of cellulose compounds
1991 - IRG/WP 1479
Low molecular weight, high affinity iron-binding compounds (siderophores) were isolated from the brown-rot fungus Gloeophyllum trabeum. The compounds were shown to be inducible by iron starvation and could be purified by ultra-filtration, ethyl acetate extraction, column chromatography and preparative HPLC. The isolated compounds were shown by analytical and immunological techniques to be produced...
J Jellison, V Chandhoke, B Goodell, F Fekete, N Hayashi, M Ishihara, K Yamamoto


The influence of timber species and preservative treatment on spore germination of some wood-destroying Basidiomycetes
1988 - IRG/WP 2300
Basidiospores from six wood decay fungi exhibited varying germination rates on untreated softwood and hardwood blocks. Germination inhibition of all test fungi was recorded on pine sapwood. No preference for a certain timber species by a particular fungus was evident. Whereas almost complete inhibition of germination occurred on wood treated with a quarternary-ammonium based wood preservative, mos...
B M Hegarty, G Buchwald


Effect of fungal degradation on the chemical composition of acetylated beech wood
2003 - IRG/WP 03-40267
This study investigated the impact of fungal attack on the chemical composition of acetylated wood. Beech wood acetylated to different degrees was exposed to decay by the white-rot fungus Trametes versicolor under solid-state fermentation conditions. Laboratory soil-bed assays were also conducted to study the degradation of acetylated wood by soft rot fungi and other soil-inhabiting microorganisms...
H Militz, Dong-won Son, L Gómez-Hernández, R Sierra-Alvarez


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


The microbial ecology of treated birch stakes in a soil-bed
1983 - IRG/WP 1209
The microbial ecology of small birch stakes exposed in soil beds in two Fungus Cellars was investigated. Patterns of fungal colonisation and decay initiation are described in untreated birch and copper fluosilicate-treated stakes. Results are based on fungal isolation onto selective media and direct light microscopical observations of decay features. In untreated stakes there was a rapid build-up ...
C P Clubbe


A 53-year old field trial to evaluate the performance of a range of chemical treatments on eucalypt poles
1989 - IRG/WP 3526
Hardwood pole stubs of Eucalyptus maculata, Eucalyptus pilularis, Eucalyptus saligna and Eucalyptus paniculata were examined for termite attack and fungal decay after 53 years in ground contact. The trial compared eight different chemical treatments with untreated pole stubs of the four species investigated. Untreated Eucalyptus paniculata, a Class I durability species, performed particularly well...
R S Johnstone, R A Eaton


The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson


Shorter-term biological control of wood decay in pre-seasoning pine roundwood as an alternative to chemical methods
1992 - IRG/WP 92-1555
Previous studies on the long-term control of decay in creosoted transmission poles, using Trichoderma and other antagonistic moulds, have met with limited success. However, it is possible biological control is more suited to control of decay on shorter time scales. An earlier study, focusing on pre-seasoning treatment of transmission poles showed that favourable porosity increases could be brought...
M W Schoeman, D J Dickinson


Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli


Factors affecting decay rates in a fungus cellar
1985 - IRG/WP 2242
Birch and pine stakes treated with chromated copper arsenate and didecyldimethylammonium chloride were incubated in two soils in a "Fungus Cellar" test. At three month intervals, sets of stakes were inspected and assigned visual ratings or removed from the soil beds for weight loss determination. Preliminary results after nine months exposure have shown differences in the decay rates between birch...
P A McKaig


The use of fumigants for controlling decay of wood: a review of their efficacy and safety
1989 - IRG/WP 3525
Volatile agricultural chemicals (fumigants) such as chloropicrin (trichloronitromethane) and sodium n-methyldithiocarbamate have been used in the United States for controlling internal decay of large dimension wood products for over 20 years. This usage has been concentrated in the electric utility industry, but fumigants are increasingly applied to protect bridge timbers, marine piling, and even ...
J J Morrell


A Novel Type of Multiple Cavity Attack in Wood Cell Walls of Heat-treated Timber Exposed in Seawater – Preliminary Observations
2004 - IRG/WP 04-10523
Samples of untreated and heat-treated Norway spruce and Douglas fir were submerged in Langstone Harbour, Portsmouth for 4 years at a depth of ca. 0.3 metres. The heat-treated samples had been prepared using the Plato process. Samples were initially assessed for the severity of marine borer damage and were then examined microscopically for evidence of microbial decay. Longitudinal and transverse wo...
R A Eaton, C Björdal, T Nilsson


Effects of pre-harvest girdling on selected properties of red pine, red maple and Eastern larch
1999 - IRG/WP 99-40137
Trees of three species - tamarack (Larix laricina), soft maple (Acer rubrum) and red pine (Pinus resinosa) - were girdled immediately below the crown,one to two years before felling. The wood from these trees was compared with wood taken from un-girdled control trees felled at the same. Sapwood and heartwood, from the controls, and from above and below the girdle of treated trees, were examined fo...
A Taylor, P A Cooper


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Natural decay resistance of some lesser known /used timber species from the forests of Tanzania
2005 - IRG/WP 05-10557
In order to manage the Tropical forest in a sustainable manner and increase the resource base for their wood industries, many Tropical African timber producing countries including Tanzania are promoting the many lesser known/used timbers in their forests as alternative sources of wood to the over-exploited primary timber species. Four lesser known/utilized timber species from the forests of Tanzan...
S A Amartey, P R Gillah, R C Ishengoma, J Gabriel, D H Kitojo


The risk assessment process. Point of view of a biocide manufacturer [Évaluation du risque. Point de vue d'un fabricant de biocide]
1990 - IRG/WP 3568
Risk assessment is an inherent part of our everyday lives. The risk assessment equation combines Hazards and Exposure. For the Wood Preservation Industry, the hazards may be characterised by the toxicity a the ecotoxicity of chemicals and the exposure by the identification of exposed people, of the exposure routes and exposure frequency. To quantify the exposure, good co-operation is required betw...
D Baur


Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


The use of organic wood preservatives in ground contact and the suitability of laboratory test procedures to determine their efficacy
1999 - IRG/WP 99-20175
Organic fungicides, such as propiconazole, have proven to be highly effective when used as a co-biocide in recently developed wood preservative formulations. They have however been ineffective when used as a stand alone preservative, particularly when used in ground contact (European Hazard class 4). Previous research, using the test methods of ENV 807 (1993), provided conflicting evidence regardi...
I J Herring, D J Dickinson


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors