Correlation between modulus of elasticity, mass losses and FTIR spectra of copper treated decayed wood
2006 - IRG/WP 06-10580
The composition of copper-based preservatives will change from copper-chromium to copper-ethanolamine, due to environmental demands. The most important drawback of copper-impregnated wood is the presence of tolerant fungal organisms that have developed an ability to degrade such preserved wood. In order to elucidate these processes, specimens (0.5×1.0×15 cm) made of Norway spruce (Picea abies) w...
M Humar, B Bucar, F Pohleven


Evidence for Basidiomycete Tunnelling in Pinus radiata and Fagus sylvatica
2006 - IRG/WP 06-10587
Decay micromorphology was studied systematically for diversely preservative treated Pinus radiata and Fagus sylvatica 20 x 20 x 500 mm stakes across 13 in-ground field test sites, during a 6.5 year exposure. Sites were selected to maximise occurrence of a diverse range of decay types. Presence of clamp connections in close associated with tunnelling coupled with macroscopic features similar to whi...
R Wakeling


Isolation and characterization of hydroxyl-radical-producing glycopeptide genes from the white-rot basidiomycete Phanerochaete chrysosporium
2006 - IRG/WP 06-10588
During wood decay, the white-rot basidiomycete Phanerochaete chrysosporium secretes low-molecular-weight glycopeptides that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radical. This reaction accounts for most of the hydroxyl radical produced in wood-degrading cultures of P. chrysosporium. In combination with phenol oxidases, hydroxyl radical is believed to play a r...
H Tanaka, G Yoshida, Y Baba, K Matsumura, S Itakura, A Enoki


Decay resistance of coconut and rubber woods. Alternative wood species from Ghana
2006 - IRG/WP 06-10596
With the expanding local and world wide demand for tropical timbers, there is increased interest in the suitability of lesser–used timber species as alternatives for the forest based industries in order to ensure sustainable forest management. In the forests of Ghana, there are quite a number of timber species that are lesser known and have not been adequately used due to the absence of informat...
S Amartey, M Humar, B Donkor, F Pohleven


The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt


Comparing microbial colonisation and Decay Rates of Wood from Sound and Aphid-Killed Kenyan-Grown Mexican Cypress (Cupressus lusitanica)
2006 - IRG/WP 06-10599
Samples of wood from 10, 15, and 30-year old trees attacked and killed by the cypress aphid (Cinara cupressi) and sound Kenyan-grown Cupressus lusitanica trees were investigated for variations in moisture content, density and susceptibility to microbial decay. MC varied with tree age, a normal trend, and between samples from aphid-killed and sound trees. In samples from 10, 15 and 20-year old so...
R Venkatasamy


Study of new wood preservatives from biological origin and low toxicity against wood decay organisms (fungi and termites)
2006 - IRG/WP 06-10600
Wood as an organic material is likely to be attacked by living organisms if no protecting treatment is applied to improve its durability. The biological agents, which in Spain, due to its specific climatologic, cause major damage to wood, are the stain fungi, the rot fungi and the subterranean termites. The commercialisation of the products actually used to treat wood against fungi and to treat t...
M T Troya, M J Prieto, F Rubio, D Lorenzo, J J Teixidó


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


Effects of chlorothalonil (CTN) and butylated hydroxytoluene (BHT) on microbial communities involved in the deterioration of wood using T-RFLP I: Accelerated laboratory decay study
2006 - IRG/WP 06-20332
The effects of Chlorothalonil (CTN) and Butylated Hydroxy Toluene (BHT) on microbial species diversity in wood and the surrounding soil are being assessed by Terminal Restriction Fragment Length Polymorphism (T-RFLP). CTN was selected as a trial organic wood preservative, and BHT is being evaluated for its synergistic effects with CTN. Results from an accelerated decay test will be presented. The...
G T Kirker, M L Prewitt, S V Diehl


Effect of wood decay on the proportional limit of thin wood samples stressed in the bending mode
2006 - IRG/WP 06-20334
When using bending stiffness as a measure of wood decay it is advantageous to repeatedly test individual samples after they are exposed to decay fungi for varying periods of time. In order to obtain reliable results, variation in modulus of elasticity (MOE) values of the test samples that are repeatable bent to a given deflection must be considered. In this study it was shown that sound 3mm thick ...
G Li, D Nicholas, T Schultz


Investigation on a Wood Decay Biomarker
2006 - IRG/WP 06-20336
HPLC evolution of beech wood extractives was investigated with or without exposure to Coriolus versicolor during one month. The nature and the quantity of extracts depends on the extraction conditions, but were also strongly influenced by the wood drying temperature and time leading to an important modification for higher drying temperature. After two weeks of exposure to Coriolus versicolor, resu...
S Mounguengui, S Dumarçay, P Gérardin


The Use of Modulus of Elasticity and Modulus of Rupture to Assess Wood Decay in Laboratory Soil-Bed Test
2006 - IRG/WP 06-20338
The efficacy of wood preservatives were determined in a soil-bed test. Samples of alder wood sapwood (Alnus glutinosa subsp. barbata) (5x10x100 mm) were treated with Solutions of CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Modulus of Elasticity, modulus of rupture, mass loss and decay rate according to AWPA E7 wer...
A Temiz, Ü C Yildiz


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


Laboratory methods for assessing the resistance of wood plastic composites to fungal attack.
2006 - IRG/WP 06-20340
Wood plastic composites (WPC’s) have many attractive material features including dimensional stability and resistance to moisture, but the wood in these materials remains susceptible to fungal attack. Assessing WPC decay resistance in laboratory trials has proven difficult because the slow moisture sorption characteristics of this material do not allow for sufficient fungal attack over the trad...
J J Morrell


Testing durability of treated wood according to EN 252. Interpretation of data from Nordic test fields
2006 - IRG/WP 06-20341
To evaluate the effectiveness of new wood preservatives intended for treated wood in ground use there is a European standard, EN 252. The test shall run for five years before any formal interpretation of the results can be made. Due to environmental concerns, the use of wood preservatives based on copper, chromium and arsenic (CCA) has been restricted in recent years. As a consequence of restrict...
M L Edlund, F G Evans, K Henriksen, T Nilsson


Performance of boron-treated radiata pine in above ground field tests in New Zealand
2006 - IRG/WP 06-30406
Boron treatment was approved for exterior, above ground use in New Zealand in 1958, provide treated commodities were painted with a three-coat paint system. Above ground tests of rail units and L-joints were established at the NZ Forest Research Institute (now Scion) between 1967 and 1980 to monitor performance of boron treatment in relation to that of untreated and CCA-treated timber. Results sh...
M Hedley, D Page


Testing biological durability of wood-plastic composites
2006 - IRG/WP 06-20347
Testing biological durability is inherently different for wood-plastic composites (WPC) compared to solid timber. However there is clearly a need for more information on the durability of WPC’s, on the effect of decay on the material properties of WPC’s and on methods for assessing decay of WPC’s. For the emerging European WPC market there has been some discussions on how to work on these to...
J Van Acker


How to win friends and influence the market — Service Life Prediction and performance-based durability assessments of wood products in construction
2006 - IRG/WP 06-20348
Due to direct and implied demands from the market and from e.g. the EU Construction Products Directive, the need to supply service life estimates for building products is growing. For several years, a development of Service Life Prediction (SLP) methodologies has been going on, but the awareness of this development has hitherto reached only a very limited extent in the wood sector. For materials w...
F Englund


Qualitative and quantitative assessment of chemicals used for wood durability improvement by Near Infrared Spectroscopy
2006 - IRG/WP 06-20349
The Near infrared spectroscopy (NIRS) could be a suitable technique to assess chemicals used for wood durability improvement in the forest products industry. NIRS methodology can be used to obtain results more quickly, less costly and without damaging the wood. In this study, wood samples selected from heartwood and sapwood of Maritime Pine (Pinus pinaster) were prepared to assess the artificial d...
S Zahri, F Charrier, H Baillères, B Charrier


Preliminary screening of a boron based wood preservative for biological efficacy (fungicidal) in treated timber
2006 - IRG/WP 06-30396
The resistance of Pinus radiata D.Don sapwood blocks, treated with a boron based preservative, to attack by five wood destroying fungi (Fomitopsis lilacino-gilva, Coniophora olivacea, Gloeophyllum abietinum (boron resistant), Serpula lacrymans and Perenniporia tephropora) was investigated. A phenyl pyrazole termiticide (fipronil) was also incorporated into the formulation to examine if its presen...
S R Przewloka, J A Hann, P Vinden


Improvement of Grevillea robusta durability using heat treatment
2006 - IRG/WP 06-40333
Heat treatment of Grevillea robusta was carried-out under inert conditions to improve its durability. Resistance of heat treated samples was evaluated by malt agar block tests after three months of exposure to several wood rotting fungi. Results showed that the fungal durability was greatly improved after treatment. There was a good correlation between fungal resistance and mass loss which is a fa...
F Mburu, S Dumarçay, F Huber, M Petrissans, P Gérardin


Copper borate for the protection of engineered wood products
2006 - IRG/WP 06-40334
Copper borate was evaluated for use in protecting oriented strand board (OSB) from mould, decay, and termites. Aspen OSB bonded with either phenolic or isocyanate resin was treated with several formulations of copper borate at various loadings from 0.26 to 4 percent by weight. These panels were then tested to determine the impact of the preservative on mechanical properties as well as resistance ...
R Smart, W Wall


Tree crown architecture: a tool for decay resistance evaluation
2013 - IRG/WP 13-10793
The variability of natural durability contributes to the bad perception of some wood end-users. In our search, we need to adjust our methods and strategies to estimate natural durability and extract higher value from wood resources. Architectural analysis is essentially a detailed, multilevel, comprehensive and dynamic approach to plant development. Numerous biological process which impact some wo...
N Amusant, J-B Anouhé Say, A Amissa, J Beauchène, F Niamké, E Nicolinni


The commercialisation of ThermoWood® products
2006 - IRG/WP 06-40339
The concept of thermally modifying timber is well established, which has achieved a limited market breakthrough to date. Commercial application has mainly occurred within Finland, though recent years has seen market gain in several other European countries. This paper reviews the known properties of ThermoWood® timber, based on the combined work of the Finnish ThermoWood® Association, alongside ...
D Jones, E Suttie, J Ala-Viikari, N Bergstrom, D Mayes


Further discussion of biological durability assessments of acetylated wood from several European institutes
2006 - IRG/WP 06-40340
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000-03, the European Commission funded the "Thematic Network on Wood Modification". This paper features a re-evaluation of work undertaken...
D Jones, W Homan, F Bongers


Previous Page | Next Page