On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald


Nondestructive Evaluation of Oriented Strand Board Exposed to Decay Fungi
2002 - IRG/WP 02-20243
Stress wave nondestructive evaluation (NDE) technologies are being used in our laboratory to evaluate the performance properties of engineered wood. These techniques have proven useful in the inspection of timber structures to locate internal voids and decayed or deteriorated areas in large timbers. But no information exists concerning NDE and important properties of wood composites exposed to dec...
B Illman, V W Yang, R J Ross, W J Nelson


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


Types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand
1984 - IRG/WP 1226
The few reported failures of 11-12-year-old horticultural posts in New Zealand in 1982 were caused by brown-rot. A subsequent survey of CCA-treated posts in all the major horticultural areas has revealed decay of many posts. A microscopic examination of these posts has shown decay by brown-rot, white-rot, soft-rot and bacteria. Several types of bacterial decay have been observed....
J A Drysdale, M E Hedley


The dry rot fungus Serpula lacrymans. Examples of attack and remedial treatment
1988 - IRG/WP 1347
The film deals with several aspects of dry rot attack and eradication in buildings. The detailed biology and morphological charasteristics of the fungus are portrayed. The various forms of mycelial growth, the role of the strands in the nourishment and spread of the fungus, as well as the many types of fruitbody formation are outlined. Environmental and nutritional requirements of the fungus as we...
G Buchwald, B M Hegarty, W Metzner, R Pospischil, H Siegmund, P Grabow


Physical properties of ß-1,4-Xylanase produced by Postia (=Poria) placenta: Implications for the control of brown rot
1987 - IRG/WP 1318
The degradation of hemicelluloses is an early event in wood decay by brown-rot fungi. An understanding of the physical properties of hemicellulases may suggest target mechanisms for the development of new control agents. Endo-b-1,4-xylanase was partially purified by column chromatography from wood decayed by Postia (= Poria) placenta. The enzyme was extremely resistant to denaturing conditions; no...
J A Micales, F Green III, C A Clausen, T L Highley


The decay resistance of chemically modified aspen composites to the white rot fungus Coriolus versicolor (L.) Quelet
1998 - IRG/WP 98-40122
Chemical modification of Aspen wood (Populus tremula L.) in the form of solid wood, veneers and sawdust was undertaken by a two step procedure consisting of esterification with maleic anhydride (MA) and subsequent oligoesterification with MA and glycidyl methacrylate (GMA) or allyl glycidyl ether (AGE). Modified wood was thermoplastic and was thermally formed by hot-pressing to produce veneer or s...
M C Timar, A J Pitman, M D Mihai


Additions and corrections to recent names for some common decay fungi
1977 - IRG/WP 167
A Käärik


A summary of current information on actinomycetes and wood
1978 - IRG/WP 177
B King, R A Eaton, A A W Baecker


The dry rot fungus and other fungi in houses. Part 2
1993 - IRG/WP 93-10001
J Bech-Andersen


Valid names for some common decay fungi, their synonyms and vernacular names
1978 - IRG/WP 172
A Käärik


Wood preservation in Lithuania
2004 - IRG/WP 04-30363
This article is intended to give basic information on wood preservation activities in Lithuania and the main actors in wood preservations practice and research. Currently the main actors in practical Lithuanian wood preservation activity are enterprises of wood preservation industry united by the Lithuanian Wood Preservation Association. The most intensive activity in wood preservation practice an...
J Saladis


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell


Laboratory decay test of Burmese in and kanyin treated with three wood preservatives
1982 - IRG/WP 3210
Laboratory decay tests were performed on samples of In (Dipterocarpus tuberculatus Roxb.) and Kanyin (Dipterocarpus alatus Roxb. and Dipterocarpus turbinatus Gaertn f.) pressure treated with three wood preservatives - copper arsenic additive (CAA - a variation of ammoniacal copper arsenate), Arquad C-33 (a waterborne quaternary ammonium formulation), and tributyltin acetate (TBTA) dissolved in eth...
J N R Ruddick, R S Smith, A Byrne


Studies on accelerated ageing procedures with TBTO-treated wood
1985 - IRG/WP 2244
The efficacy of various procedures for accelerated ageing of organotin based wood preservatives in treated wood has been investigated. It was found that leaching of the treated wood samples in water according to the European Standard EN 84 was not satisfactory for organotin based preservatives and is probably also unsuitable even for other types of organic solvent preservatives. Keeping tributylti...
J Jermer, M-L Edlund, B Henningsson, W Hintze


A method of isolating actinomycetes from decayed wood
1974 - IRG/WP 126
This paper deals with a tentative method of isolating Actinomycetes from dacayed wood....
T Haraguchi


European standardization for wood preservation
1988 - IRG/WP 2321
G Castan


A laboratory method for assessing the effectiveness of fungicides in preventing the spread of decay fungi within packages of unseasoned lumber
1983 - IRG/WP 2202
To study the deterioration caused by decay fungi in the laboratory, a method for testing fungicides for their effectiveness in preventing spread of decay was devised. Some experiments using this method are reported here....
A J Cserjesi, E L Johnson, A Byrne


Discussion of diiodomethyl p-tolyl sulfone (Amical® 48) as a fungicide for wood preservatio
1987 - IRG/WP 3425
The effectiveness of diiodomethyl-p-tolyl sulfone (Amical® 48) as a fungicide for preservation of wood is supported by a discussion of results from the literature and current research programs....
J M Stamm, K J Littel, F M H Casati, M B Friedman


Interspecific variability of European oak durability against white rot fungi (Coriolus versicolor): Comparison between sessile oak and peduncle oak (Quercus petraea and Quercus robur)
2001 - IRG/WP 01-10393
The knowledge of wood natural durability against biologic predators enable its external use. The resistance of European oak wood was reported like durable according to the EN 350-2. However, some individuals may contain high durable wood. Our research was focused to understand this variability in oak population that represent the first french species (4.1 millions of ha). Natural durability of Eur...
N Ayadi, B Charrier, M Irmouli, J P Charpentier, C J Allemand, F Feuillat, R Keller


Successive collections of Basidiospores from wood decay fungi (in vitro) show variation in germination levels on common media
1978 - IRG/WP 191
In the course of various preliminary experiments in which spore germination levels of 6 decay fungi on malt and water agar were recorded as controls, it was noted that one could not reliably obtain an expected level of spore germination for any particular fungus. Inconsistent 'control' spore germination levels of a fungus greatly complicates large scale experiments in which compa...
E L Schmidt, D W French


Quantitative assessment of the condition of field specimens
1981 - IRG/WP 2154
Suggestions for a discussion on the desirability of an extension to the existing procedure of assessment of the condition of field specimens by adding more objective, reproducible methods in order to obtain earlier and more specific information than at present on the effect of biological attack on strength and other properties of the specimens as well as the time aspect....
H Friis-Hansen


Iron promotes decay capacity of Serpula lacrymans
1993 - IRG/WP 93-10008
The influence of iron and iron compounds on the decay capacity of Serpula lacrymans was studied. Mass losses of pine wood caused by dry rot fungus were increased when FeSO4 was added into the culture medium or when there were iron nails or stone wool on the culture medium. This supports the hypothesis that iron in stone-based building materials is one reason for the increased decay capacity of Ser...
L Paajanen