IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1504 documents. Displaying 25 entries per page.


Field trials of wood preservatives in UC3 retention. Part 1. Durability results after 13 years in and above ground
2010 - IRG/WP 10-30548
In 1996 an extensive field trial program was set up in order to obtain more data on wood treated with chromium and arsenic free preservatives in Use Class 3 retention. Apart from durability in and above ground, other features were also assessed, e.g. discoloration by staining fungi, depletion of active ingredients, weathering and corrosion of fasteners in con¬tact with the treated wood. Wood spec...
M Westin, J Jermer, M-L Edlund, P Larsson Brelid, I Johansson


Analysis of phenolic extractives from various Tunisian species trees -Study of its potential valorisation
2010 - IRG/WP 10-30552
Phenol extractives are naturally synthesized compounds taken from several trees. It is well demonstrated that the presence of phenol compounds is positively correlated with the durability of wood. This property is very interesting for outdoor uses of wood with a limited treatment. Phenol compounds may also be used in the formulation of glue. In the aim to improve the knowledge on Mediterranean tr...
I Oueslati, F Charrier, K Seffah, A Moubarik, N Ayed, A Zerizer, B Charrier


Fungal decay resistance and mechanical properties of plywood panels made from maritime pine (Pinus pinaster) and bonded with cornstarch-quebracho tannin-phenol formaldehyde adhesive
2010 - IRG/WP 10-40490
The aim of this work is to demonstrate the performances of cornstarch-quebracho tannin-based resins designed as adhesive in the plywood production. In this way, the cornstarch and quebracho tannin was introduced in the classic adhesive formulation in order to supply a part of phenol-formaldehyde (PF). In order to evaluate the mechanical performances of optimal cornstarch-quebracho tannin-PF, plywo...
F Charrier, A Moubarik, A Allal, A Pizzi, B Charrier


Decay and termite resistance of particleboard and MDF panels made from pinecones
2010 - IRG/WP 10-40493
Particleboard and medium density fiberboard (MDF) panels were produced by using pinecone from stone pine (Pinus pinea L.) tress and wood particles from pine and beech wood at various ratios. Specimens from the panels were subjected to slightly modified soil-block tests according to AWPA E10-06 standard method by using two brown-rot fungi, Gloeophyllum trabeum and Postia placenta and two white rot ...
C Köse, E Terzi, Ü Büyüksar, Erkan Avcı, Nadir Ayrılmış, S Nami Kartal, Y Imamura


Hydrothermal modification for upgrading the durability properties of soft deciduous wood
2010 - IRG/WP 10-40494
To extend the application potentialities of soft deciduous wood, upgrading the durability properties, hydrothermal modification (HTM) of aspen alder and birch wood was investigated. The treatment was conducted in a multifunctional laboratory device WTT. In the previous cases it has been found that the treatment at 160oC improves the durability insufficiently. The modification at 180oC ensured a hi...
B Andersons, I Andersone, V Biziks, I Irbe, J Chirkova, E Sansonetti, J Grinins, H Militz


Extruded wood plastic composites based on ACQ and MCQ-treated wood materials
2010 - IRG/WP 10-40495
This paper deals with wood plastic composites manufactured using ACQ and MCQ-treated wood fibers recovered from a wood treatment plant. The goal was to investigate the effect of coupling treatments on the properties of manufactured wood plastic composites (WPCs) through injection molding and to manufacture co-extruded WPC with treated wood fibers. The result demonstrated sound mechanical propertie...
Qinglin Wu, Fei Yao, K Ragon, J Curole, M Voitier, T Shupe


Ecological methods and products for wood protection used for restoration and conservation of built heritage cultural assets to increase natural durability and duration of exposure in open air museums
2010 - IRG/WP 10-40506
Wood is a perishable material, hygroscopic and fuel, which cause attention to selecting the wood species that is going to be exhibited in relation to humidity and soil. With variable depending on its humidity and moisture from the atmosphere or soil, wood is a good living environment for fungi and insects, but suffer biodegradation processes and dimensional changes. Observations over time on wood ...
M Pruna, D Purice, D Dumitru Copacean


Direct estimation of the durability of high-pressure steam modified wood by ESR-spectroscopy
2010 - IRG/WP 10-40508
Heat generated persistent free radicals have been detected by electron spin resonance measurement of thermally modified wood, prepared by high pressure superheated steam treatment. The specific density of these radicals have been correlated with the durability against basidiomycetes, as measured by the European standard EN113 test. In the lower range of specific radical densities, the found correl...
W Willems, A Tausch, H Militz


Durability of heat treated Malaysian bamboo Gigantochloa scortechinii strips
2010 - IRG/WP 10-40514
Bamboo is one of the fastest growing plants and can be used for various products. In tropical countries such as Malaysia bamboo is abundantly available at reasonable prices, therefore it is used for numerous purposes. However, bamboo (as a lignocellulosic material) is susceptible to fungal and insect attack and it is difficult to protect by preservative treatment. Heat treatment is an option to im...
N Kamarudin, K Sugiyanto


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Biological degradation of acetylated wood after 18 years in ground contact and 10 years in marine water
2010 - IRG/WP 10-40522
This paper addresses the resistance to biological degradation of acetylated wood. Firstly, it presents results from an EN 252 test after 18 years’ exposure. The test is still running in Nordic NWPC test fields, Simlångsdalen in Sweden and Viikki in Finland. Results from this test were presented after 5 years’ exposure ( IRG/WP 97-30139), and showed that the resistance of acetylated wood wit...
P Larsson Brelid, M Westin


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 1: Weathering Performance
2010 - IRG/WP 10-40526
Several different coated birch and spruce plywood types were investigated in Finland using outdoor weathering. The weather performance of the tested coated birch plywood was good compared with uncoated birch and spruce plywood. The paint base film coated and painted birch plywood performed well in outdoor testing at VTT's test site. Phenol film coated plywood was sensitive to UV light, but on...
A Nurmi, H Viitanen


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa


Fungal biodegradation of CCA-treated wood wastes
2011 - IRG/WP 10-50276
Fungal biodegradation could be employed as a pretreatment method to alleviate problems caused by landfill disposal of CCA-treated wood wastes (e.g. a shortage of landfill space and a release of leacheate). It could be used to decrease the volume of waste and to remove metals from waste simultaneously. We have screened hundreds of decay fungi, including fungi isolated from CCA-treated wood in servi...
Gyu-Hyeok Kim, Yong-Seok Choi, Jae-Jin Kim


Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans


Gene expression analysis of a copper-tolerant brown rot fungus on MCQ-treated wood
2011 - IRG/WP 11-10748
Most brown rot fungi are copper-tolerant, which makes them difficult to control with copper-based wood preservatives like MCQ. To better understand what biological processes are regulated, we used our model species, Antrodia radiculosa, to examine expression of genes on MCQ-treated wood. Our hypothesis was genes that decreased copper bioavailability would be up-regulated early, when wood showed ...
J D Tang, A Perkins, S V Diehl


Isolation and evaluation of Lactobacillus brevis from chilli waste for potential use as a wood preservative
2011 - IRG/WP 11-10749
Lactic acid bacteria were isolated from chilli waste and evaluated for their ability to arrest wood rotting basidiomycetes. In previous work a quick screening method using 96 well plates and measuring absorbance to determine fungal growth was developed specifically to investigate the efficacy of isolated bacteria against wood decay fungi. Using this method, one bacterium (isolate C11) was identif...
D O’Callahan, T Singh, I R McDonald


Decay resistance attributes of teak (Tectona grandis L. f.) wood: comparison of the fungicidal activities of quinones
2011 - IRG/WP 11-10752
The implication of quinones in decay resistance of teak wood is controversial. To better understand the role of individual quinone in this property, we studied the correlations between this latter and the content of 2-(hydroxymethyl)anthraquinone, tectoquinone, anthraquinone-2-carboxylic acid, 1,4-naphthoquinone, lapachol and the new compound 4’,5’-dihydroxy-epiisocatalponol found in teak wood...
F B Niamké, N Amusant, N Lemenager, G Chaix, M-F Thévenon, C Baudassé, S Kati-Coulibaly, A Amissa Adima, I Gossan Ado, C Jay-Allemand


Measuring fungal cellulolytic enzyme activity in degrading wood
2011 - IRG/WP 11-10753
An enzyme assay which measures enzyme activity directly from wood will assist in the fundamental understanding of the enzyme components of the decay mechanism of rot fungi and any changes in the presence of wood protectants. At present, to measure fungal carbohydrate degrading enzyme activity in the presence of wood, two methods are used: either 1) the enzyme is measured in the growth media contai...
S M Duncan, J S Schilling


Growth conditions for fungal decay in wooden constructions – practical experience versus literature
2011 - IRG/WP 11-10758
Data regarding moisture and temperature requirements of decay fungi found in literature have been compared to experience from observations in a large number of Norwegian buildings. A number of selected situations are discussed, among those exposure to high relative humidity, exposure to free water and decay in the supposedly adverse conditions on Svalbard. The moisture content in wood has to be at...
M Sand Sivertsen, J Mattsson


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Decay initiation in plywood, OSB and solid wood under marginal moisture conditions
2011 - IRG/WP 11-20469
Hygrothermal models are increasingly used as research tools by building scientists and and design tools by designers to simulate heat, air, vapour, and water movements within and through building envelope and even to predict the consequences in terms of mould/decay growth and metal corrosion. This work was designed to generate data on decay initiation under marginal moisture conditions to support...
Jieying Wang, P Morris


Performances of Douglas fir in real outdoor use conditions
2011 - IRG/WP 11-20472
The European standard EN 350-2 classifies Douglas fir as moderately resistant to fungal decay on the basis of standardized laboratory and field tests. However, the lifespan expectancy of outdoor structures such as cladding, decking and elements of wood construction carpentry may also vary according to environmental conditions (climate, exposure to weathering), maintenance and design. An investigat...
M Kutnik, S Lepetit, S Le Nevé


Non-destructive evaluation of wood decay
2011 - IRG/WP 11-20479
Evaluation of wood decay is often prone to subjective assessment. Standard rating scales are based on human perception of decay, often in addition to weight loss measurements. Especially the assessment of graveyard specimens or other long term testing material that has to be monitored regularly on a non-destructive basis, is challenging. In this paper two techniques are presented that can deliver ...
J Van den Bulcke, I De Windt, N Defoirdt, J Van Acker


Wood protection by nano silver against white rot
2011 - IRG/WP 11-30554
This research was done with the aim of investigation on the natural durability of poplar (populous deltoides) in natural situation and treated with nano silver against the white rot. Testing samples was treated with the method of modified soaking and nano silver in 3 treating level of 0,200 and 400ppm. In this study effect of coriolus versicolor fungus (identificated as white rot) on populous del...
V Tazakor Rezai, A Usefi, M Soltani


Previous Page | Next Page