Proposals for further co-operative studies on determining toxic values against wood-destroying basidiomycetes (1988)
1988 - IRG/WP 2316
This document sets out proposals for a further series of co-operative tests, based on previous discussions. A basic soil/block test is proposed, to be carried out by all participants using one preservative and four test fungi. Optional additional tests may be carried out using a range of other media (agar, vermiculite, rockwool) additional fungi of choice, additional preservatives of choice and pr...
A F Bravery, J K Carey


A laboratory evaluation of the fumigant, sulfuryl fluoride (VikaneR), against the Formosan termite Coptotermes formosanus Shiraki
1982 - IRG/WP 1164
A series of laboratory experiments showed that the fumigant sulfuryl fluoride (VikaneR) was effective against small groups of Coptotermes formosanus Shiraki exposed to the gas directly at temperatures from 20-40°C. At 10°C fumigations failed regardless of initial gas concentration. Very high or total mortality was observed at concentrations of 0.79 cc/L or higher. A second series of experiments ...
J P La Fage, M Jones, T Lawrence


Field test results for the elimination of subterranean termite (Coptotermes formosanus) colonies by a bait system containing the IGR hexaflumuron
1997 - IRG/WP 97-10222
Field studies were conducted at Chichijima (Ogasawara Islands, Tokyo) to determine the effectiveness of a termite bait system (commercial name: Sentricon* system) containing hexaflumuron (Insect Growth Regulator: IGR) in the elimination of subterranean termite (Coptotermes formosanus) colonies. The level of subterranean termite activity on Ogasawara Islands is high resulting in extensive damage to...
K Suzuki, Y Morita, K Yamauchi


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Changes in pore structure and cell wall volume in wood decayed by brown- and white-rot fungi
1991 - IRG/WP 1501
Sweetgum (Liquidambar styraciflua L.) wood blocks were decayed by Postia (=Poria) placenta or Phanerochaete chrysosporium in soil-block cultures. Decay was terminated at various weight losses, and the pore volumes available to probes of various molecular weight and diameter were determined by the solute exclusion technique (Stone, J.E. and A.M. Scallan. 1968. Cellulose Chem. Technol. 2, 343-358.)....
D S Flournoy


A study of the decay type potential of seven soils
1992 - IRG/WP 92-1539
The aim of this experiment was to determine the significance of the fungal inoculum potential and physico-chemical properties of five field trial test site soils, a garden compost known to cause white rot in copper treated fence palings, and soil from a zone between 2 and 15 centimetres from a CCA treated post with brown rot, in causing differential decay type in Pinus radiata and Poplus deltoides...
R N Wakeling


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


Performance of boron and fluoride based rods as remedial treatments in Douglas-fir poles
1995 - IRG/WP 95-30070
Boron and fluoride are widely used for remedial internal treatments, but their use in North America has been limited. Recently, however, interest in these chemicals has increased as the result of concerns about the risks of fumigant usage. The performance of boron or a boron/fluoride combination was assessed in Douglas-fir poles over 1 to 3 year periods. Both chemical formulations diffused well th...
J J Morrell, P F Schneider


The effect of different concentrations of polesaver rods on the survival of selected decay fungi in liquid culture
1998 - IRG/WP 98-30166
An in-vitro method was developed to determine the effect of solutions of Polesaver Rods on the survival of selected decay fungi. Polesaver Rods are a diffusing preservative treatment containing fluorine and boron designed for the internal remedial treatment of power poles. Two white-rot fungi, Perenniporia tephropora and Trametes versicolor, and two brown-rot fungi, Polyporus verecundus and Gloeo...
M A Powell, T Deldot, C McEvoy


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Preliminary studies of the decay mechanism of some brown-rot fungi
1989 - IRG/WP 1402
The importance of the enzymatic degradation of hemicellulose and cellulose by brown-rot fungi is still under discussion. Endo-ß-1,4-xylanase and endoglucanase activities of Coniophora puteana and Poria placenta cultures were measured by the increase in reducing groups. Enzymes were produced in liquid and solid sawdust based culture media. Enzyme activities were measured in two, four and eight wee...
A-C Ritschkoff, H Viitanen


Longterm monitoring of termite activity on multiple feeding sites: a laboratory method intended for the determination of attractant/repellent properties of wood preservatives and baits
2001 - IRG/WP 01-20225
A method is introduced allowing the continuous monitoring of the activity of a small laboratory termite- colony at 8 different feeding sites simultaneously. The test assembly consists of a small central polycarbonate-tube containing a colonie of Reticulitermes santonensis (de Feytaud) beeing connected with 8 external feeding sites by small glass-capillaries. The termites passing through the glass ...
M Pallaske, E Graf, H Takiuchi


Marine exposure assessment of the natural resistance of a number of lesser known species of tropical hardwoods to teredinid and limnoriid borers
2004 - IRG/WP 04-10520
Naturally durable species of timber are used as an alternative to preservative treated timber for marine structures, but many species have not been evaluated for their potential for use in this environment. EN 275 specifies a 5-year test period - too long a period for screening tests to be economically viable. In this study, candidate timber species were selected for testing in the sea on the basi...
J R Williams, S M Cragg, L M S Borges, J D Icely


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


A serial exposure technique for estimating probable service life of treated timber
1978 - IRG/WP 2111
This paper briefly describes part of our preliminary work aimed at developing a test procedure that culd be adopted as a standard method. A detailed version of the work has been submitted for formal publication. In both papers, the aim is to promote interest in extended laboratory testing of wood preservatives. It is believed that this work may provide the basis of a laboratory test procedure from...
J A Butcher


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


Effect of fumigant residue in aerated wood blocks on the spore germination of decay fungi
1991 - IRG/WP 2382
Fumigants are increasingly used in several countries for remedial treatments of transmission poles to increase the service life. The present study was initiated primarily to test the remaining toxic effects of spruce (Picea rubra) wood, fumigated with chloropicrin (trichloronitro methane) or MIT (Methyl isothiocyanate) after long period of aeration, on the spore germination of decay fungi. This st...
J Bjurman, B Goodell


BRE Experience in monitoring decay in out-of-ground exposure trials
1995 - IRG/WP 95-20077
The outdoor field trial has always been regarded as the ultimate test of performance for assessing the effectiveness of a wood preservative. For this reason, the Building Research Establishment (BRE) has invested much effort in such trials over many years. Emphasis in early trials was on ground contact tests which were the basis both for assessing the likely performance of a preservative in protec...
J K Carey, R J Orsler


Comparison of the effects of borate, germanate and tellurate on fungal growth and wood decay
1992 - IRG/WP 92-1533
The tetra-hydroxy borate ion is known to undergo complexation with polyols and has been shown to inhibit dehydrogenase enzymes in this way. It has been previously suggested that this complexation is responsible for the inhibition of fungal growth and the protection of boron treated timber. Other ions that have the ability to complex with polyols have also been shown to inhibit dehydrogenase activi...
J D Lloyd, D J Dickinson


A novel device for detecting internal defects in wooden poles
1989 - IRG/WP 2329
The diagnosis of internal defects caused by termites and decay in hardwood transmission poles has been investigated using a novel Automatic Feed Drill (AFD) pole testing device. Internal defects were recognised by changes in drill feed-rate as the automatic air-driven drill traversed its 100 mm working stroke. The instrument is portable, simple to operate and recognises defects instantaneously. Te...
R A Eaton, R S Johnstone


Soluble nutrient content in wood and its susceptibility to fungal discoloration and decay in above ground and ground tests
2000 - IRG/WP 00-10336
The objective of this comprehensive study was to reveal the impact of soluble nutrients in wood on its susceptibility to fungal discoloration and decay in various tests, which is important for the test methodology and standardisation. Seven tests were carried out including pure culture above and ground contact tests, above ground field test and laboratory ground contact tests. The samples containi...
O M Caballero, N Terziev


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


Biochemical aspects of white-rot and brown-rot decay
1987 - IRG/WP 1319
This paper presents an overview of the decomposition of wood by white- and brown-rot fungi - the most important and potent of known wood-decay fungi. These organisms are unique among cellulose destroyers because of their strong capability to enzymatically degrade lignified material. Special emphasis is given to the following aspects of wood decomposition by white- and brown-rot fungi: (1) effects...
T L Highley


Low polymer levels containing bioactive monomer polymerized in situ provide resistance to Gloeophyllum trabeum
1995 - IRG/WP 95-30066
Wood preservation based on in situ polymerization of potentially bioactive monomers has been studied. Tributyltin oxide acrylate (TBTOA) and pentachlorophenol acrylate (PCPA) were synthesized. Wood samples were treated at 2, 5, 10, 15 and 20% by weight solutions with varying amounts of crosslinker (trimethylolpropane trimethacrylate, TMPTM) and polymerized in situ in wood samples (2.54 x 2.54 x 0....
R E Ibach, R M Rowell