Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Temperature studies on two mounds of Coptotermes lacteus (Isoptera)
1986 - IRG/WP 1295
The temperatures within and around two Coptotermes lacteus mounds located in a cleared and shaded forest site in a dry sclerophyll forest in central Gippsland were monitored. Hourly temperature measurements were recorded at each mound over a 24 h period in spring, summer and winter respectively. Regardless of site, Coptotermes lacteus maintained the core temperatures in the nursery area much highe...
D M Ewart, J R J French


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


List of fungi in soft-rot tests
1975 - IRG/WP 105
This list gives information on the terrestrial and marine species and strains of fungi tested for soft-rot ability in pure culture with data on their decay activity in untreated wood. An index of the timber species tested is added. The compilation is based on 1) the list of soft-rot fungi of the former OECD Group (Doc.No. 27/DAS/CSI/M/559), Oct. 1968, prepared by R. Rösch and W. Liese, 2) informa...
G Seehann, W Liese, B Kess


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


The study of blue stain found in coniferous timber in SR Slovenia (Yugoslavia)
1983 - IRG/WP 1177
The report concerns the problems connected with blue stain in coniferous timbers stored in warehouses at wood-processing plants in SR Slovenia (Yugoslavia). The amounts of spruce-wood (Picea abies Karst.) found to have been infected with blue stain have been measured and some of the fungi causing the stain have been identified and their biology studied. It was found that the percentage of spruce-w...
R Benko


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


Effect of humidity and temperature on fastener withdrawal resistance from CCA and ACZA treated Douglas-fir
2000 - IRG/WP 00-20209
The effects of preservative treatment on fastener withdrawal was investigated in Douglas-fir lumber conditioned to two moisture regimes. In general, conditioning samples to 19% moisture content produced more substantial changes in withdrawal resistance of galvanized fasteners than did conditioning to 12%. Treatment had little or no effect on withdrawal resistance of stainless steel fasteners. With...
Sung-Mo Kang, J J Morrell


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


Effects of boron formulation on specific timber types used in ships of historical importance
1991 - IRG/WP 3676
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
B King, G M Smith, J W Palfreyman, S McCutcheon


Partial seasoning and preservative treatment systems for pine roundwood
1982 - IRG/WP 3187
Experimental trials at FRI, Rotorua showed that the steaming schedule normally used for steaming and venting is also suitable for steaming and vacuum seasoning. Applying vacuum of up to -84 kPa immediately after steaming did not increase the initial loss of wood moisture significantly in comparison to steam/venting. The main improvement to wood condition by using steam/vacuum appeared to be to dis...
A J Bergervoet


Microwave curing of furfuryl alcohol modified wood
2007 - IRG/WP 07-40371
Furfurylated wood has shown to have promising properties for a wood modification agent during the last years. In this paper, an alternative curing method for furfuryl alcohol modified pine sapwood by means of microwave radiation was investigated. Different process parameters of microwave treatment such as output power, exposure time to microwave radiation, initial wood moisture content and evapor...
A Treu, E Larnøy, H Militz


Copper fixation in ACQ-D treated Chinese fir at various temperature and relative humidity conditions
2007 - IRG/WP 07-30436
In this study, the effect of different conditions of temperature, relative humidity, and duration of post-treatments on accelerating copper fixation in ACQ-D treated Chinese fir wood blocks was investigated. The conditions include the combination of three temperatures (21, 50, and 70?) and two relative humidity levels (20% and 80%), also include four temperatures (50, 70, 90, and 110?) without con...
Jinzhen Cao, Lili Yu


In-service performance of wood depends upon the critical in-situ conditions. Case studies.
2008 - IRG/WP 08-20382
Wood is a unique building material, but is by nature designed to deteriorate. A detailed understanding of the factors and interactions involved are important when working with service life prediction of wooden components in buildings. Wood may experience exponential fungal degradation caused by variation in the climatic factors within a small limited area and by minor imperfection in the wooden ...
L Ross Gobakken, J Mattsson, G Alfredsen


High Temperature Treated Wood
2008 - IRG/WP 08-40429
High temperature can modify internal structure and physic-chemical properties of wood by a controlled pyrolysis process. Such treatment, among other changes in properties, modifies the wood color in a way that resembles exotic species, increasing its market value. The main objective of this work is to determine the changes in wood properties caused by the effect of temperature and time, in order t...
C C Borges, A L Barbosa, R Faber de Campos, S T Targas


Effects of concentration and temperature of CCA and CCB on wood strength of Turkish fir (Abies bornmulleriana Mattf.)
2009 - IRG/WP 09-40450
The purpose of this study was to present evidence for the effects of concentration and temperature of solutions of water-borne preservatives (chromated copper arsenate, CCA and chromated copper boron, CCB) on the static bending properties (modulus of elasticity, MOE and modulus of rupture, MOR) of Turkish fir (Abies bornmulleriana Mattf.). Wood samples were mechanically tested after a mild full ce...
I Usta, M Hale


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot


Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


Kinetic Water Vapour Sorption of Sitka Spruce at Variable Temperature Using the Parallel Exponential Kinetics Model
2010 - IRG/WP 10-40512
In this study the water vapour sorption of Sitka spruce (Picea sitchensis (Bongard) Carr.) was measured using a Dynamic Vapour Sorption (DVS) apparatus and then analysed using the parallel exponential kinetics (PEK) model. The water vapour sorption rate of wood quickly increased when the relative humidity was changed. With the elapse of time, the sorption rate gradually decreased within any specif...
Yanjun Xie, C Hill


Effects of global climate change on mould growth - Interactions of concern
2010 - IRG/WP 10-50270
An evident change in climate the last decades has been recorded, and combined effects of increased CO2, elevated temperature and altered precipitation regimes have been observed to represent a change to the fundamental drivers within ecosystems. Growth of moulds, both in nature and on man-made constructions and objects, will most likely increase due to changes in the climate. The survival, the rep...
L Ross Gobakken


Ambient-temperature borate dip-diffusion treatment of green railroad crossties
2011 - IRG/WP 11-40556
In the USA, borates are increasingly being applied prior to air seasoning and creosote treatment of railroad ties (railway sleepers). Borates are typically applied to green ties by vacuum pressure application at 1 to 10% disodium octaborate tetrahydrate (DOT) concentration or by traditional dip-diffusion treatments at elevated temperatures. Higher temperatures are used to maintain the 30 to 50% so...