IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1638 documents. Displaying 25 entries per page.


Antifungal activities of acetone-soluble Eusideroxylon zwageri and Potoxylon melagangai crude extracts against white rot
2012 - IRG/WP 12-30591
The development of natural wood extracts as a wood preservative is a potentially attractive prospect for the wood preservation industry. This study attempts to evaluate the toxicity of Eusideroxylon zwageri and Potoxylon melagangai extractives as potential wood preservatives. These two species are well-known as among the heaviest and very durable timbers. It has been established that natural durab...
I Jusoh, A Tida Henry, Z Assim, F Badruddin Ahmad, S Ujang


Termite resistance of copper-based preservative supplemented aspen strandboards
2012 - IRG/WP 12-30594
Termite resistance of aspen strandboards treated with various copper-based preservative systems was evaluated in field exposure tests. Five copper-based chemicals or zinc borate were blended into aspen furnish at three retention levels prior to pressing. Tebuconazole or 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (DCOI) were added as co-biocides to selected copper-based treatments. Sections from...
J J Morrell, C Vidrine, A Preston, L Jin


Mobilized copper(II) concentrations in earlywood and latewood of micronized copper treated red pine
2012 - IRG/WP 12-30596
Electron paramagnetic resonance (EPR) was used in conjunction with energy dispersive x-ray spectroscopy (EDX) to quantify total copper and mobilized copper retentions in MCQ and MCA treated red pine. The MCQ treated red pine was found to have higher copper retention than that of the MCA treated one. Earlywood in general had higher total copper content than latewood. The mobilized and complexed cop...
Wei Xue, P Kennepohl, J N R Ruddick


Performance of wood treated with linseed and tung oil against wood decay fungi and wetting
2012 - IRG/WP 12-30598
Most of the European wood species does not have durable wood. In order to use it in outdoor conditions nondurable material has to be protected. Nowadays, non-biocidal solutions for wood protection are attracting a lot of attention, particularly in use class 2 and 3 applications. One of the non-biocidal techniques is treatment of wood with water repellents like wax emulsions and oils. Linseed oil a...
M Humar, B Lesar


Analyses of premature failure of utility poles
2012 - IRG/WP 12-40584
In this study a total number of 18 utility poles of Scots pine (Pinus sylvestris) impregnated with a copper-chromium containing preservative were investigated. They were part of different lower voltage transmission lines in the western part of Germany and failed before predicted minimum service life. All poles in this study were less than 15 years in use. The type of decay and fungi were evaluated...
S Bollmus, N Rangno, H Militz, A Gellerich


A survey of factors affecting decay resistance of wood modified with acetic anhydride
2012 - IRG/WP 12-40594
From the range of information published, acetylation appears well suited to provide adequate protection against biological attack for materials derived from typically non-durable wood species. Acetylated wood is now commercially available both in Europe and in the USA. But still there are a lot of unanswered questions related to fungal decay mechanisms in acetylated wood. The paper summarize exist...
G Alfredsen, P O Flæte, H Militz


KERUING and APITONG: A Timely Review of the Perfect Choice Wood Species for Crossarms and Brace Arms, Including Data on Copper Naphthenate Treatments
2012 - IRG/WP 12-40603
Apitong or the wood species more commonly known as Keruing is an important tropical hardwood known for its high strength to weight ratio and its reasonable durability and preservative treatability. This wood has been exported from managed permanent forest estates in Malaysia into the United States for over 4 decades for its widespread use in wooden utility industry brace arms and crossarms, yet cu...
A Wong, M Freeman


Scale-up of a chemical process for copper-based preservative-treated wood wastes recycling
2012 - IRG/WP 12-50286
In recent years, the development of appropriate wood waste disposal options has been encouraged by severe regulations and expensive fees associated with wastes landfilling or burning. An efficient and economically attractive leaching process was developed at laboratory scale (200 mL) for CCA-, ACQ- and CA-treated wood wastes recycling. This leaching process consisted of three leaching steps of 2 h...
L Coudert, L Gastonguay, J F Blais, G Mercier, P Cooper, P Morris, A Janin, N Reynier


Efficiency of the Amazon Forest Oils as Preservatives to the Attack of cellulolytic fungi in Pine Wood
2012 - IRG/WP 12-30599
The bobbins of wood are used for storage and field installation of cables from the electricity and telecommunications sectors. There are legal requirements governing the Brazilian ways of treating the wood used in these sectors, aimed at preventing pollution and protecting nature. When exposed to severe environmental conditions in Brazil these products are degraded and occurs many operational prob...
S Silveira, I M S Mendes, R S Paiva, J E Volponi, R C G Comar, R S Cruz


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Copper naphthenate treatment for wood pols - a review and update
2012 - IRG/WP 12-30600
This paper reviews copper naphthenate (CuNap) and its utility as a treatment for wooden utility poles. One of the principal reasons that CuNap has gained market acceptance, in addition to its efficacy against decay fungi and wood-destroying insects, is its low mammalian toxicity. CuNap is a well-proven non-restricted use preservative, used extensively and specified for environmental reasons by ut...
J A Brient, M H Freeman


Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot


Hydrogels: a solution to reduce boron leachability without reduction of its biodisponibility to wood decaying fungi?
2012 - IRG/WP 12-30602
Products used today for wood protection must fulfill to more and more environmental constraints, such as being of low toxicity in answer to the Biocidal Product Directory, but also to involve waterborne treatments to limit rejection of volatile organic compounds in the atmosphere. Boron preservatives have been described as valuable alternatives for wood protection for non-ground contact applicatio...
F Obounou Akong, P Gérardin, M-F Thévenon, S Parant, C Gérardin-Charbonnier


Influence of a pulsed electric field on the growth of surface fungi
2013 - IRG/WP 13-10795
The colonization of mold and staining fungi are not only an aesthetical problem. Blue stain fungi are able to penetrate paint films. Maintenance of coatings on wood are time consuming and costly. A new approach uses a pulsed electric field (PLEOT) in order to protect wood against surface fungi. This technology is evaluated in non-sterile laboratory conditions on different coated and uncoated Scots...
M Starck, A Treu


Surface moulds and staining fungi on acetylated wood – effect of increasing acetyl content
2013 - IRG/WP 13-10797
Wood used in outside applications is susceptible to weathering and photo degradation, which often leads to surface discoloration, loss of brightness and surface deterioration. Research has shown that acetylated wood is more resistant against brown rot, white rot and soft rot, and more dimensionally stable than untreated wood. However, acetylated wood seems still to be disfigured by surface moulds ...
L Ross Gobakken, S Bardage, C J Long II


Preliminary evaluation of degradation patterns in wood samples from the Yenikapı shipwrecks
2013 - IRG/WP 13-10798
The uncovering of several shipwrecks during the excavation of the Marmaray Rail Tube Tunnel Project in Istanbul provides an important opportunity to evaluate waterlogged woods buried for centuries. Identification of these woods showed that a variety of species was used in the ships. One shipwreck (a galley) from the Yenikapı Marmaray was examined using electron microscopy. The micrographs rev...
C Köse, A M Taylor


Communities of mold fungi on flooded building materials
2013 - IRG/WP 13-10799
A small building built to residential code was flooded using farmland pond water to a depth of two feet at Tuskegee University. The building was drained and left enclosed for an additional three weeks. A total of 168 material samples were removed either immediately after opening (wet) or seven months after flooding (dry). Wall materials sampled included fiberglass batt insulation, gypsum wallboard...
F Skrobot III, H Aglan, S V Diehl


High-throughput sequencing highlighted contrasted pioneer fungal communities associated to coniferous and deciduous wood preservation assays
2013 - IRG/WP 13-10800
Studying the fungal communities in the wood, in particular during the first events of the colonization, and the factors that underlie the dynamics of fungal species assemblages remain a challenge in ecology, because of the absence of fructification during the pioneer steps of wood degradation. The use of Next-generation DNA sequencing methods, which produce massive volumes of data, provided new pe...
Y Mathieu, A Dassé, I Le Bayon, M Kutnik, L Harvengt, E Gelhaye, M Buée


An assessment of soft rot in preservative-treated poles in two test sites and two network areas in New South Wales
2013 - IRG/WP 13-10801
This document presents an extended summary of recent investigations into soft rot attack of preservative treated power poles from the re-inspection of samples selected from two field sites and two in-service trials located in New South Wales, Australia. The in-ground sapwood of selected poles was assessed by probing and, after core sampling, by microscopy to determine the severity and extent of s...
W D Gardner, M A Powell, C Kirton


Transferable Durability: Enhancing decay resistance of non-durable species with extractives from durable wood species
2013 - IRG/WP 13-10808
Extractive content and composition is a vital component of naturally durable woods; however, variability in extractives can limit their usefulness in the field. Two extractive-free, non-durable wood species were pressure treated with ethanol-toluene extractives from 8 durable wood species. Extracted Southern pine, Paulownia and unextracted Southern pine blocks were treated and challenged in soil b...
G T Kirker, A B Blodgett, S Lebow, C A Clausen


Resistance of Consolidated Deteriorated Wood to Wood Decay Fungi
2013 - IRG 13-10812
The main purpose of the experiment was to establish which consolidating products in impregnated wood are the most effective against wood decay fungi. Five different consolidators were tested: Paraloid B-72, Consolidating restaurateur, SG 715 BLANC (epoxy resin), R.712 polyester and the wood consolidant agent containing nano particles, which is still in development. From the already damaged wood ...
F Pohleven, A Valantič, M Petrič


The assessment by visual grading, change of color and ergosterol content ratings, the resistance to mould fungi of treated with wood preservative Scots pine sapwood
2013 - IRG/WP 13-20514
The filamentous (mould) fungi belonging to Ascomycetes, Deuteromycetes group are an cosmopolitan organisms which attacks wooden elements disfiguring them, dropping their value and causing environmental and health hazard. The fungi in a short time cause mainly disfigurement of wood does not effect on strength properties of wood, but with strong prolongation of duration of conditions favourable for ...
A Fojutowski, A Koziróg, A Kropacz


Image analysis for mould and sapstain detection on wood
2013 - IRG/WP 13-20519
Laboratory tests for mould growth on wood products are time consuming and rely on visual assessments of specimens utilizing subjective rating systems. Accelerated laboratory methods are needed that can provide rapid, quantitative assessment of mould and sapstain growth on solid and composite wood products. Image analysis of scanned spore imprints from southern pine or oriented strandboard (OSB) sp...
C A Clausen, V W Yang


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Previous Page | Next Page