The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Amine copper reaction with wood components: acidity versus copper adsorption
1997 - IRG/WP 97-30161
The bonding sites for copper in wood from CCA, as well as ammoniacal/amine based systems, has long been a topic of investigation. Both phenolic and carboxylic functional groups have been discussed as potential bonding sites for copper. However, no consensus on the adsorption mechanism has been realized. Thus, the selective adsorption of copper in southern yellow pine from ethanolamine-copper solut...
S M Thomason, E A Pasek


Impact of leachates from CCA- and copper azole-treated pine decking on soil-dwelling invertebrates
2002 - IRG/WP 02-50183
This study assessed the short-term effects on non-target soil invertebrates of leachates from a naturally durable hardwood and timber treated with two copper-based wood preservatives. Natural rainwater leachates from kwila decking, and radiata pine-decking treated with CCA or copper-azole, were collected and applied on mown lawn soil in Brisbane, Queensland. The soil study consisted of 5 treatment...
N Crumière, A House, M J Kennedy


Copper based wood preservative - A new approach using fixation with resin acids of rosin
2000 - IRG/WP 00-30249
Copper soaps with carboxylic acid groups of resin acids of rosin were shown to be potential long-term wood preservatives. The principle involved is the attachment of copper to the network formed by the inorganic part of the preservative (rosin) through the -COOH groups. The mechanisms of fixation have been studied, and it has been shown that this association could be obtained : (1) by forming the ...
C Roussel, J P Haluk, A Pizzi, M-F Thévenon


Soft-rot testing. Memo to CEN
1983 - IRG/WP 2206 A
1. Development of a single test procedure to assess performance of preservatives against soft rot fungi is an ideal that cannot be realised at present, if results are to be both reproducible between laboratories and pertinent to the practical requirements of individual countries. 2. Consensus opinion amongst members of Sub Group I - Soft rot tests, of Working Group II - Fundamentals of Testing, of the IRG, is that the immediate needs of CEN would be best answered by: (a) a code of recommended practice, (b) a multiplicity of test procedures, and (c) a degree of flexibility in test procedures. 3. The code of recommended practice should recognise the need for: (a) a pure culture, synthetic medium (sand or vermiculite + nutrients), single wood species test to be adopted by all laboratories as a common reference point of testing, (b) mixed inoculum and/or unsterile soil laboratory or fungus cellar tests which account for local variations in the fungal flora, (c) incorporation of a range of wood species where applicable (i.e. where mixed hardwoods comprise the main resource), (d) provision of local internal standards of known performance under field conditions, (e) incorporation of leaching procedures other than standard methods with deionized water (e.g. mild acid, milk alkali, ionic solutions of various salts) where applicable to local exposure conditions, (f) precise definition of the criteria used for establishing toxic thresholds (mass loss, strength loss, microscopic examination). 4. Initial screening tests should remain the province of the individual research worker. 5. The code of recommended practice should have the sole purpose of establishing provisional retention levels for subsequent confirmation by field trial. 6. IRG should list and approve test procedures considered adequate to establish toxic thresholds for preservatives against soft rot fungi. 7. It should be clearly understood that when using a series of test techniques, it is inevitable that a range of toxic thresholds will be obtained for the same preservative. 8. Guidelines should be drawn up for interpretation of test data for subsequent transformation to provisional retention levels. 9. Adoption of the broad principles outlines above is recognition of the dynamic nature of toxic thresholds. The additional information obtained by a more flexible, and complex, approach to testing may make interpretation more difficult but should provide data from which response of preservatives to varying biological and environmental hazards can be more realistically assessed. 10. It is recommended that CEN adopt, in principle, the basic philosophy of testing outlined above and move towards formulation of a Working Document in collaboration with IRG
J A Butcher, D J Dickinson


A spectroscopic investigation of copper ethylenediamine fixation in wood
1999 - IRG/WP 99-20160
The fixation reaction which take place between copper ethylenediamine (Cu-en) solution and wood were expolored using X-ray photoelectron spectroscopy (XPS) and Fourier Transformed Infrared Spectroscopy (FTIR). The FTIR spectra revealed that copper reacts with the carboxylic acid and phenolic groups in wood to form stable complexes. The copper ethylenediamine complexes formed in wood were identifie...
Xiao Jiang, J N R Ruddick


Comparative performance of copper azole and copper-chrome-arsenate treated rubber wood in Australian, Malaysian and New Zealand tests sites
2000 - IRG/WP 00-30213
Rubberwood (Hevea brasiliensis) has been used for non-structural products where appearance is important. It has rarely been used for structural uses where preservative treatment is required. In order to evaluate the in-ground durability of preservative-treated rubberwood, test stakes (20 x 20 x 500 mm3) were treated to four retentions of CCA and copper azole (Tanalith® E) and installed in test si...
J A Drysdale, M E Hedley, E Loh, L T Hong


Protection of cellulose string with biocide/water repellent mixtures
1997 - IRG/WP 97-30148
Protecting cellulosic materials in soil contact poses a formidable challenge. Many soil inhabiting bacteria and fungi that cannot degrade wood can nevertheless rapidly depolymerize cellulose once its protective lignin matrix is removed. As a result, cellulose based materials are rarely used in direct contact with soil. One exception, however, is the use of cellulose string to support climbing vine...
A B Chang, J J Morrell


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


A comparison of analytical and visual techniques used for assessment of weathering properties of chromium and copper azole treated timber
1994 - IRG/WP 94-20023
The weathering properties of preservative treated timber were studied by measuring surface lignin loss and by microscopic examination after weathering, and results were related to qualitative assessments of visual appearance after weathering. Measurement of relative rates of delignification of untreated and preservative treated timber obtained by FTIR analysis, and weight loss determined on thin v...
J A Cornfield, M D C Hale, G Fettis


The fixation of copper in Pinus sylvestris using the sodium salts of two polyhydroxycarboxylic acids
1992 - IRG/WP 92-3706
As part of the research concerned with the development of fixed, copper based preservatives, the salts of polyhydroxycarboxyIic acids, have been used in copper sequestration studies and fixation trials in Pinus sylvestris splinters. Selected compounds have been shown to be effective sequestrants at low concentrations allowing alkaline solutions to be formulated. Leaching trials following a 48 hour...
M Bacon, J A Cornfield


Copper tolerance of various Antrodia vaillantii isolates
2001 - IRG/WP 01-10406
Copper based preservatives have been extensively used in the field of wood preservation. However, several brown-rot fungi to be tolerant to copper and consequently, efficacy of copper based wood preservatives may not be sufficient. Copper tolerance is especially by some fungi that are closely aligned to or included in genus Antrodia. The highest copper tolerance was found at some strains of wood r...
F Pohleven, A Malnaric, M Humar, C Tavzes


Performance of Copper-Chrome-Arsenic (CCA) and Copper-Chrome-Boric (CCB) treated panels of Bombax ceiba and Paraserianthus falcataria against bio-deterioration at Krishnapatnam harbour, east coast of India
2003 - IRG/WP 03-30310
Results of investigations on the durability of light weight timber species (Specific gravity below 0.4) i.e., Bombax ceiba and Paraserianthus falcataria in treated and untreated condition conducted at Krishnapatnam harbour (Lat 13o28’ to 13o59’ N; Long: 80o10’ to 80o16’E) along the east coast of India are reported in the paper. Exposure trails were conducted with panels (Size: 30 x 3.8 x...
B Tarakanadha, N R Raveendra Prasad, K S Rao


Utilisation of carbohydrates by stain fungi in agar culture
1998 - IRG/WP 98-10248
Stain fungi are often defined by their ability to utilise the starch and free sugars found in ray parenchyma cells, and their inability to utilise other wood constituents. However, several species of stain fungi produce bore holes in wood cell walls. This suggests that enzymatic activity capable of degrading structural polysaccharides and/or lignin is associated with the growth of the appressorium...
J Snow, P Vinden, S M Read


Biological control of sapwood-inhabiting fungi by living bacterial cells of Streptomyces rimosus as a bioprotectant
1992 - IRG/WP 92-1564
The objective of this study is to evaluate the efficacy of antifungal activity of living bacterial cells for the protection of wood against sapwood-inhabiting fungi. The following sapwood-inhabiting fungi were selected: sapstain --Ceratocystis coerulescens, Ceratocystis minor, Ceratocystis pilifera, and Aureobasidum pullulans; mold fungi --Aspergillus niger, Penicillium spp, and Trichoderma spp. L...
S C Croan, T L Highley


Degradation of resin constituents in various wood species by the white rot fungus Bjerkandera sp. strain BOS55
1999 - IRG/WP 99-10301
In previous studies, the white-rot fungus Bjerkandera sp. strain BOS55 was shown to cause extensive degradation of lipophilic extractives (resin) in Scots pine wood. Further research was carried out in order to investigate the ability of Bjerkandera sp. for reducing resinous constituents in various softwood (Douglas fir, larch and spruce) and hardwood species (birch, beech and poplar). The greates...
J Dorado, T A Van Beek, F W Claassen, R Sierra-Alvarez


An audit of copper chrome arsenic timber treatment plants throughout Queensland
1995 - IRG/WP 95-50047
Thirty seven copper chrome arsenic (CCA) timber treatment plants in Queensland were assessed according to the operational criteria specified in Australian Standard 2843.2 - 1985, Timber Preservation Safety Code - Plant Operation. The criteria have been designed to provide information on the design and operational activities of a CCA plant. Design aspects that have an effect on the environment are ...
J Norton


The influence of timber species and preservative treatment on spore germination of some wood-destroying Basidiomycetes
1988 - IRG/WP 2300
Basidiospores from six wood decay fungi exhibited varying germination rates on untreated softwood and hardwood blocks. Germination inhibition of all test fungi was recorded on pine sapwood. No preference for a certain timber species by a particular fungus was evident. Whereas almost complete inhibition of germination occurred on wood treated with a quarternary-ammonium based wood preservative, mos...
B M Hegarty, G Buchwald


Effect of fungal degradation on the chemical composition of acetylated beech wood
2003 - IRG/WP 03-40267
This study investigated the impact of fungal attack on the chemical composition of acetylated wood. Beech wood acetylated to different degrees was exposed to decay by the white-rot fungus Trametes versicolor under solid-state fermentation conditions. Laboratory soil-bed assays were also conducted to study the degradation of acetylated wood by soft rot fungi and other soil-inhabiting microorganisms...
H Militz, Dong-won Son, L Gómez-Hernández, R Sierra-Alvarez


Interaction of copper-amine complexes with wood: Influence of copper source, amine ligands and amine to copper molar ratio on copper retention and leaching
1999 - IRG/WP 99-30203
The absorption and leachability of copper in copper amine (Cu-EA) treated wood are influenced by the formulation and the composition of copper amine treating solutions. The sources of copper used, Cu(OH)2, CuCO3, CuSO4 and Cu(NO3)2, in the copper amine complex formulation affect the leachability of copper. Data show that copper amine from CuSO4 and Cu(NO3)2 treated wood has less copper loss during...
Jun Zhang, D P Kamdem


Wood preservation in Japan
1982 - IRG/WP 3218
The report indicates the importance of wood preservation in Japan, which is the world's largest importer. The main hazards of timber are listed, fungi, insects and marine borers. Besides wood preservation fire protection treatments are also important in Japan. Classifications are given of the durability and treatability of the timbers used. In describing the wood preservation industry, th...
S Amemiya, R Cockcroft


Partial characterization of inhibitors extracted from pine (Pinus sylvestris) sapwood active against germination of wood rotting fungi
1988 - IRG/WP 1351
Germination inhibitors in pine sapwood could be extracted and separated with the aid of solvent partitioning and chromatography on silicic acid. The inhibitory action was tested by three different bioassays. Active fractions have been characterized by TLC and HPLC. Inhibitory activity could be correlated with phenolic compounds. The minimum active concentration of inhibitors have been determined....
J Bjurman


Limnoria quadripunctata Holthuis - a threat to copper-treated wood
1983 - IRG/WP 4100
This paper presents the first reported attack by the crustacean marine wood-borer Limnoria quadripunctata Holthuis of CCA treated eucalypt piles. The attack occurred after 12 years service of the piles in the River Derwent at Hobart, Tasmania. Attack by both this borer and Limnoria tripunctata Menzies is also reported in CCA treated softwoods and hardwoods over periods ranging from 5 to 22.9 years...
J E Barnacle, L J Cookson, C N McEvoy


Leaching of Copper from ACQ treated wood exposed above ground
2004 - IRG/WP 04-50219
The leaching of chemicals of ACQ Type C treated wood exposed above ground for 16 months was studied. Commercially treated Hem-fir boards (Tsuga heterophylla Raf. and Amabilis fir Forb) of 37.5 mm by 87.5 mm were used. The amounts of chemical leached monthly by the rainfall were determined and the leachate was collected and analyzed. Also, the environmental factors influencing the leaching were ...
P A Chung, J N R Ruddick


The use of low cost X-ray fluorescence instruments in the determination of copper chromium and arsenic in preservative treated wood
1987 - IRG/WP 2278
Internal quality control in timber treatment plants can be pursued by analysis of preservative treatment solutions and treated timber. Treaters must proceed with costly and lengthy analyses through analytical laboratories. An alternative approach for the timber treater, is to use low cost analysers (L.C.A.'s) based upon x-ray fluorescence. Detailed comparisons have been made between stand...
J Norton, L E Leightley