Reappraisal of some fungicides by the amended JWPA method
1992 - IRG/WP 92-3689
Organoiodine compounds which have been commercialized these years in Japan poorly performed as fungicides in the amended JWPA decay test (Standard 1, 1989) when applied to superficial treatment of timber. Because some parts of active ingredients seemed to disappear from the treated timber surface mainly due to the severe leaching cycles. This was prominently true for beech (Fagus crenata Blume) sa...
K Tsunoda


A study of fungal biodeterioration in unseasoned, packaged hem-fir lumber
1978 - IRG/WP 2116
This study was undertaken to determine the extent of biodeterioration that could occur within British Columbia (BC) prior to the export of packaged Canadian Lumber Standard Hem-Fir (Tsuga heterophylla, Abies amabilis and small amounts of Abies grandis). By examining the anti-stain treatments received by the lumber and identifying and characterizing the organisms responsible for the biodeterioratio...
P W Perrin, A J Cserjesi


Resistance of acrylic paints on wood against growth of the rot fungus Dacrymyces stillatus
1990 - IRG/WP 2345
In the last few years the presence of the rot fungus Dacrymyces stillatus has been repeatedly confirmed in external wood panels, particularly from wood painted with water based paints. A laboratory method for testing of the fungal resistance of paint films on wood has been developed.This method has been used to test the efficacy of the fungicides Parmetol DF 18 and Parmetol HF 25 against attack by...
J Bjurman


The growth and metal content of plants grown in soil contaminated by a copper/chrome/arsenic wood preservative
1977 - IRG/WP 3110
Salts of copper, chromium and arsenic are used together in water soluble formulations for the preservation of wood against insect and fungal attack. Copper/chrome/arsenic (CCA) preservatives are of proven efficacy and, used correctly, ensure a useful service life for timber for 30 years or more with little, if any, attendant threat to the environment from the treated wood itself. The preservative ...
C Grant, A J Dobbs


Determination of bis-(N-cyclohexyl-diazeniumdioxy)-copper in different matrices by photometer, thermal energy analyzer and HPLC
1999 - IRG/WP 99-20179
For the quantitative analysis of bis (N-cyclohexyl-diazeniumdioxy)-copper (Cu-HDO) three analytical methods are used. The employment of the different methods depends on the matrices involved. For several years now, the colorimetric determination of Cu-HDO by photometer has been applied to solutions and concentrates of wood preservatives. In principle, the technique consists of a quantitative conve...
J Wittenzellner, W Hettler, M Maier


Untersuchungen zur Prüfung mit Moderfäulepilzen im Vermiculit-Eingrabe-Verfahren
1972 - IRG/WP 214
Im Hinblick auf die Entwicklung eines Prüfverfahrens für die Bestimmung der moderfäulewidrigen Wirksamkeit von Holzschutzmitteln wurden Versuche mit Reinzuchten von Pilzen und mit Vermiculit als Trägersubstanz sowohl mit unbehandelten als auch mit Schutzmittelgetränkten Holzproben durchgeführt. Dabei wurde die Eignung von handelsüblichen, eintachen Einweg-Kunststoffbechern anstelle der bish...
W Kerner-Gang, M Gersonde


A biochemical explanation for the observed patterns of fungal decay in timber
1980 - IRG/WP 1111
Experiments designed to compare the degree of localization of the cellulase enzymes of some white, brown and soft rot organisms are described. The site and nature of binding of the enzymes is discussed. The technique is ellution of mycelium grown in liquid culture with a variety: of agents including acetate buffer, carboxymethyl cellulose solution, borate/glycerol buffer and urea. The mycelium was...
N B Green, D J Dickinson, J F Levy


The influence of carrier fluid type on the efficacy of a wood preservative against cavity forming soft rot
2000 - IRG/WP 00-30244
Propiconazole was applied to Scots pine sapwood (Pinus sylvestris) and beech (Fagus sylvatica) using three different carrier systems selected on their varying ability to swell timber. The effects of microdistribution on the activity of cavity forming soft rot fungi were examined to determine the practical benefits of using swelling and non-swelling carriers with this active ingredient. Efficacy of...
P A Hodges


Working plan: Second international collaborative field trial
1995 - IRG/WP 95-20056
This paper describes the scope, objectives, and approaches to be used in the second international collaborative field trial approved by the Scientific Programme Committee for partial funding in 1994. The trial is designed to develop a broad data base on causal mechanisms, interactions, and factor affecting the performance of treated wood in ground contact. The trial encompasses 12 different field ...
H M Barnes, T L Amburgey


The effect of concrete embedment on CCA treated hardwood and softwood timbers
1985 - IRG/WP 3340
Small size stakes of Eucalyptus maculata and Pinus elliottii were treated with CCA to various retentions and embedded in concrete collars containing varying amounts of a fungicide additive. During the 30 month trial period stakes were removed after 12, 18, 24 and 30 months and assessed for residual strength. Stakes which showed significant strength reductions were microscopically examined for the ...
L E Leightley, G A Willoughby


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1984 - IRG/WP 3318
Over a third of the treated stakes involved in this test have been mechanically damaged. As many of these stakes broke off at or near groundline they could not be reinstalled. So they have been removed from the study despite most exhibiting little or no decay. Because of the mechanical damage to a substantial number of the treated stakes, we propose to terminate the CSIRO part of this study after ...
G C Johnson, J D Thornton


Collaborative soft rot tests: Final Report
1978 - IRG/WP 2106
Since preparation of Document No: IRG/WP/258 results have been received from the remaining collaborators. Thus there is a little further to add to the conclusions already derived, those in Document No: IRG/WP/251 being as follows: 1) the exposure system used sometimes resulted in excessive weight gains in the sterile check blocks. Consequently the corrected loss in weight of the test blocks could ...
J G Savory, J K Carey


On the use of probit analysis for assessing the toxicity of wood preservatives
1974 - IRG/WP 244
To elucidate the general character of the action of the toxic material on the fungus, it is sufficient to carry out preservative tests using the previously described procedure, but in doing so, it is necessary somewhat to change the number of specimens and their arrangement in jars. Five concentrations of toxic material are tested simultaneously. For the testing of one preservative ten jars should...
D A Belenkov


Minimum inhibitory concentration of methylene bisthiocyanate towards selected wood inhabiting fungi in liquid culture and on radiata pine
2001 - IRG/WP 01-30261
The objective of the current study was to determine the minimum inhibitory concentration (MIC) of methylene bisthiocyanate (MBT) towards wood inhabiting fungi common on unseasoned radiata pine (Pinus radiata D. Don). The fungi used were Ophiostoma floccosum, Leptographium procerum, Sphaeropsis sapinea and Trichoderma viride. Fungi were individually inoculated into nutrient media spiked with differ...
T Singh, B Kreber, C Chittenden, R N Wakeling, A Stewart


Leaching of copper-chrome-arsenic treated timber: Simulated rainfall testing
1996 - IRG/WP 96-50074
Six kiln dried radiata pine sapwood packs of timber were preservative treated with copper-chrome-arsenic preservative using a modified Bethell treatment schedule. The packs were then subjected to simulated rain leaching at specified periods after treatment. Higher chromium leachate was obtained when higher volumes of simulated rainfall were applied. Lower chromium leachate was obtained for timber ...
S Walley, P R S Cobham, P Vinden


A comparison of the leaching resistance of copper 2-ethanolamine and copper ethylenediamine treated Scots pine
2000 - IRG/WP 00-30233
The depletion of copper from copper 2-ethanolamine and copper ethylenediamine treated Scots pine blocks was investigated. A greater leaching resistance was found for copper 2-ethanolamine, which retained ca. 86% and ca. 50% copper after water and buffer leaching, respectively. Leached amine treated blocks also contained significant residual amine. This was consistent with other observations linked...
Xiao Jiang, J N R Ruddick


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


Some fundamental thoughts on the prediction of field performance from lab-testing based on comparison of lab and field test results of some copper-free materials
2003 - IRG/WP 03-20269
In the paper results from lab testing (ENV 807 and EN 113) are compared with field results (EN 252) of differently treated wood. Depending on the type of the organic biocide containing material and depending on type of soil and type of decay differences were found in suitability of the lab methods to predict field performance. The attempt is made to interpret the found differences. Furthermore it ...
A O Rapp, U Augusta


The durability of wood polymer composites against fungi and insects
2000 - IRG/WP 00-40161
New materials such as wood polymer composites are used more in France. These materials are obtained by mixing wood and thermoplastics in different ratios. These kind of material must be considered as new materials and some characteristics such as durability must be evaluated for outdoor applications. On the other hand, some recycled fibers from wood waste could be used as raw materials. Some woodp...
G Labat, I Le Bayon, J Gerard, F Amin


Evaluation of the protective means of some wood preservatives by means of accelerated tests
1973 - IRG/WP 232
In site conditions of the eastern site in the forest-steppe part of the Krasnovarsk region, the relative effectiveness of a series of wood preservatives was obtained by means of field tests. To obtain a more accurate evaluation of the protective qualities of these accelerated tests were carried out in laboratory conditions. In 9 boxes filled with non-sterile soil taken from the site, 72 samples of...
I A Petrenko


The effect of acid rain on CCA treated timber
1990 - IRG/WP 3579
The effect of acid precipitation on the leaching of copper, chromium and arsenic from timber treated with different CCA preservatives was studied in the presence of three types of soil under simulated field conditions. Pine sapwood, embedded in soil, was subjected to simulated rainfall at three different levels of acidity. The CCA preservative formulations tested were:- American Wood Preservers&am...
R J Murphy, D J Dickinson


Development and Implementation of a DNA – RFLP Database for Wood Decay and Wood Associated Fungi
2004 - IRG/WP 04-10527
We are developing Restriction Fragment Length Polymorphism (RFLP) and Internal Transcribed Spacer (ITS) sequence databases for wood decay basidiomycetes and other fungi associated with wood. These databases currently house information for 39 fungal species consisting of 9 brown-rot basidiomycetes, 12 white rot basidiomycetes, 1 soft rot, 1 stain fungi, and 16 molds or other ascomycetes or imperfe...
S V Diehl, T C McElroy, M L Prewitt


Nondestructive assessment of biodegradation in southern pine sapwood exposed to attack by natural populations of decay fungi and subterranean termites
1994 - IRG/WP 94-20042
Field methods for evaluating decay resistance of experimentally treated materials lack a means for quantitative measurement of residual strength. Quantitative relationships between speed of impact-induced waves travelling parallel to the grain and residual compressive strength have been demonstrated in softwood attacked by brown rot-decay fungi, but the effects of termites have not been documented...
R C De Groot, R J Ross, W Nelson


Validation of the sapstain danger index
2000 - IRG/WP 00-10333
The Sapstain Danger Index (SDI) is a model that is used to indicate sites in the New Zealand forest where felled logs are more prone to sapstain, specifically it should indicate how soon after felling of a log should it be treated for sapstain. The validation of SDI has the goal to identify whether the SDI can be used to predict sapstain development and to eventually minimise loss of value of logs...
P A Cooper, S Downs, R l Farrell


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...