IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi


Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe


A novel technique for comparative toxicity studies of potential insecticidal wood preservatives
1983 - IRG/WP 2198
For some years now a device has been under development at the New Zealand Forest Research Institute, the purpose of which is to study the effects of sub-lethal amounts of stomach poisons (but also of fumigants and contact active materials) on the co-ordinative abilities of a cerambycid larva. This insect is Prionoplus reticularis - indigenous to New Zealand its larvae feed in decaying logs and are...
D J Cross


A combined method for drying and preserving wood in a single step process
2000 - IRG/WP 00-40183
Based on a convective dryer, this process allows to dry and treat wood blocks with diffusible preservatives in the same time. A boric acid solution (heated to fix the wet temperature of the system) is pumped and introduced in the flow system through a venturi, where the air coming back from the drying cell also arrives. The role of the venturi is to create a dispersion of boric acid solution micro...
O Colin, C Dupuis, E Mougel, A Zoulalian, M-F Thévenon


Bioefficacy of Cunapsol® treated western cedar and southern yellow pine
1996 - IRG/WP 96-30120
Western red cedar and southern yellow pine sapwood were dip treated with a new formulation of waterborne copper naphthenate (Cunapsol®) which complies with VOC regulations. Cunapsol dip treated samples were oven dried at 50°C for 48 hours and then water leached for two weeks. Decay resistance and leachability of preservatives from dip treated specimens were evaluated according to AWPA (American ...
D P Kamdem, M H Freeman, T L Woods


Environmental Impacts of CCA-Treated Wood: A Summary from Seven Years of Study Focusing on the U.S. Florida Environment
2003 - IRG/WP 03-50205
Wood treated with chromated copper arsenate (CCA) was identified in 1995 as the cause of elevated arsenic concentrations within wood fuel used for cogeneration within Florida. Since this time a research team from the University of Miami and University of Florida has evaluated the environmental impacts of CCA-treated wood within the State. Research has focused on two distinct areas: in-service l...
H M Solo-Gabriele, T G Townsend, J D Schert


Wood preservation in the Netherlands
1985 - IRG/WP 3324
This report gives some information on the production, import and use of timber in the Netherlands and, in more detail, about the country's wood preservation industry. As the country's production of wood that is useful for its manufacturing industries is very limited, the position of wood in the building industry is not too important. Architects think first in terms of bricks, con...
N Burgers, R Cockcroft, D De Jong


The influence of UV and IR radiation on leaching of copper and chromium from preservative-treated pine and spruce
1992 - IRG/WP 92-3687
The influence of artifical UV- and IR-radiation on the leaching of copper and chromium components of a CCB-preservative from freshly treated pine and spruce was evaluated. On small pinewood samples it could be shown, that the leaching of copper and chromium can considerabely be reduced by UV-radiation. A Philips HPA lamp type reduced the leaching most effective. IR-radiation lead to higher leachin...
H Militz


Chromated copper arsenate preservative treatment of hardwoods. Part 1: CCA fixation performance of seven North american hardwoods
1997 - IRG/WP 97-30131
There has been an increased interest in utilisation of hardwoods from eastern North America for exterior applications which require protection with preservatives such as CCA. We have examined CCA fixation at two selected temperatures of seven common North American species: red maple (Acer rubrum L.,), white birch (Betula papyrifera ), yellow poplar (Liriodendron tulipifera L.), trembling aspen (Po...
T Stevanovic-Janezic, P A Cooper, Y T Ung


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Evaluation of rapid methods for detecting wood preservatives in waste wood
1994 - IRG/WP 94-50024
For the disposal of wood waste under ecological sound conditions information about its hazardous potential is required. Several analytical methods are available for the detection of most elements in wood preservatives. Industrial process conditions, however, demand methods with very short turn around times. In this research several methods of analysis were judged on their speed and accuracy. A num...
W J Homan, H Militz


Evaluation of extractives from African Padauk (Pterocarpus soyauxii Taub.) for protection of non decay resistant species
2002 - IRG/WP 02-10419
The development of a wood preservative made up of natural extracts is a potentially attractive prospect for the wood preservation industry. In this study, organic solvents were used to remove extractives from African padauk wood samples. The solvent was removed by rotoevaporation, and the total content of the viscous extracts determined to be 54.4mg/ml. The toxicity of various extracts concentrat...
P Nzokou, D P Kamdem


Effects of hard water, sea water and humic acid on the release of CCA components from treated wood
2005 - IRG/WP 05-50228
Leaching medium is an important factor affecting release of preservative components from treated wood because physical and chemical characteristics of medium increase or decrease the solubility of fixed preservative components. This study evaluated the leaching properties of copper, chromium and arsenic elements from chromated copper arsenate (CCA)-treated wood specimens subjected to laboratory le...
S N Kartal, W J Hwang, Y Imamura


Acoustic technique for assessing decay in preservative treated wood
1998 - IRG/WP 98-20138
This study investigated the suitability of vibration techniques to assess the performance of wood preservatives in ground contact. Small stakes (10 x 5 x 100 mm3) of treated and untreated Scots pine sapwood were exposed to decay in lab-scale terrestrial ecosystems. Tests were conducted using three different soils including a garden compost soil, and soils obtained from a test field and a conifer f...
L Machek, M-L Edlund, R Sierra-Alvarez, H Millitz


Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar Part 1: Comparison of Results of Visual Assessments and Determinations of Static Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20319
With examples of routine in-ground stake tests differences are shown in the performance of wood preservatives at the BAM test fields Lehre and Horstwalde and in the BAM fungus cellar. Signs of attack of micro-organisms were assessed visually according to EN 252. Periodical determinations of static moduli of elasticity (MOE) revealed the influence of the attack on the elastic properties of the wood...
M Grinda, S Göller


Wood preservation sites polluted by CCA. Is potassium diphosphate incubation a catalyst for the electrodialytic remediation of these soils?
1998 - IRG/WP 98-50106
As part of an evaluation of a newly developed electrodialytic soil remediation technique, we investigated the incubation of a contaminated soil (from a Portuguese wood preservation site polluted with CCA) with potassium diphosphate as a possible catalyst for the removal of heavy metals and metalloids. A chemical sequential extraction scheme (SE) applied to the soil has shown that the potassium dip...
A B Ribeiro, G Bech-Nielsen, A Villumsen, A Réfega, J Vieira e Silva


Accelerating effects of the field biological attacks in a weather controled soil bed room
1997 - IRG/WP 97-20118
For the purpose of the accelerating the field evaluation of the material service life, a weather controlled soil bed room were designed. The room was controlled 30°C, 75%R.H. In this room, water was sprayed 15 minutes a day. The workers and soldiers of termite, Reticulitermes speratus, can be penetrated. The comparison results of preservative brushing coated treated stakes between field ones and ...
K Suzuki, I Momohara, T Nishimura


A physiological role of the glyoxylate and TCA cycles in fruitbody formation of the coppertolerant brown-rot fungus Fomitopsis palustris
2002 - IRG/WP 02-10430
Changes in activity of the representative enzymes involved in biosynthesis of oxalic acid (oxalate) and carbon metabolism of glucose were investigated in relation to the fruit body formation of the copper-tolerant brown-rot fungus Fomitopsis palustris. Changes in specific activities of the two glyoxylate (GLOX) cycle key enzymes (isocitrate lyase (ICL) and malate synthase (MS)), the two oxalate-fo...
Jeong-Jun Yoon, T Hattori, M Shimada


The role of oxalic acid in tolerance to N’N-naphthaloylhydroxylamine in Tyromyces palustris
2006 - IRG/WP 06-10584
Certain wood decay fungi exhibit tolerance to one or more wood preservatives. Copper tolerance of brown-rot fungi has been studied in our laboratory for the past six years. We have observed some degree of tolerance to N’N-naphthaloylhydroxamine (NHA), a recently patented termite bait, by the brown-rot fungus Tyromyces palustris TYP-6137. In an effort to try and confirm this tolerance in other is...
R A Arango, C A Clausen, F Green III


Study of new wood preservatives from biological origin and low toxicity against wood decay organisms (fungi and termites)
2006 - IRG/WP 06-10600
Wood as an organic material is likely to be attacked by living organisms if no protecting treatment is applied to improve its durability. The biological agents, which in Spain, due to its specific climatologic, cause major damage to wood, are the stain fungi, the rot fungi and the subterranean termites. The commercialisation of the products actually used to treat wood against fungi and to treat t...
M T Troya, M J Prieto, F Rubio, D Lorenzo, J J Teixidó


The role of chromium in wood preservatives - The situation and new results concerning biological efficacy
2006 - IRG/WP 06-30397
A heavy discussion about the status of chromium-containing compounds in wood preservatives has ensued in the European Union since the Biocidal Product Directive 98/8/EG has come into force.The origin of this discussion is the fact that according to the Biocidal Product Directive chromium trioxide and sodium dichromate have been identified as active ingredients and therefore the placement of wood p...
P Jüngel, H Härtner, E Melcher


Enhancing the Performance of Transparent Coatings by UV Protective Pre-treatments
2006 - IRG/WP 06-30399
Most industry observers anticipate a change from copper-based preservatives to metal-free combinations of organics for residential treated wood products in North America within the next one to five years. While the chromium copper provide considerable protection against UV, metal-free formulations will need UV protection in the form of additives or coatings. While transparent coatings can be made ...
P I Morris, S McFarling


Efficacy of some fungicides against mold on freshly cut beech sawn wood
2006 - IRG/WP 06-30403
The quality class of molded wood is lowered and this can result in financial losses due a decrease in its trade value. Currently beech wood is often used without steaming it first and it moulds in the course of drying. The aim of this study was to identify kinetics of beech wood molding and effectiveness of action of chosen modern pro-ecological wood preservatives applied in the protection of fres...
A Fojutowski, A Kropacz


Is Field Test Data from 20 x 20mm Stakes Reliable? Effects of Decay Hazard, Decay Type and Preservative Depletion Hazard
2006 - IRG/WP 06-20327
Effects of decay hazard, decay type and preservative depletion hazard on the performance of variously preservative treated 20 x 20 x 500 mm Radiata pine and Fagus sylvatica test stakes across 13 field test sites in New Zealand and Queensland Australia were determined. Radiata pine treated with an ammoniacal copper quaternary preservative (ACQ) (1.56% m/m a.i.) and copper chrome arsenate (CCA) (...
R Wakeling


EN 152: Is this Standard Relevant for today’s Wood Preservatives? A Critical Review.
2006 - IRG/WP 06-20331
The paper critically reviews the Blue stain test method described in EN 152 including possible test variables. Whereas EN 152 has been successfully used for solvent borne wood preservatives, it appears that the methodology is not suited for modern water borne products, where the majority fail. The paper will show that there exist different quality claims not concordant with EN 599-1 within diff...
B Jensen, F Imsgard, J Larsen