Investigation of new wood preservation formulations based on synergies between antioxidant, 2-HPNO and Propiconazole
2006 - IRG/WP 06-30401
Wood degradation by fungi is a complex phenomenon taking place in part through oxidative reactions involving many oxidizing agents like free radicals and hydroperoxide. In order to develop novel and more environmentally benign preservative systems, mixtures of Propiconazole and antioxidants with different stabilization mechanisms were investigated to detect possible synergies allowing to reduce th...
B Bakhsous, S Dumarçay, E Gelhaye, P Gérardin


Copper borate for the protection of engineered wood products
2006 - IRG/WP 06-40334
Copper borate was evaluated for use in protecting oriented strand board (OSB) from mould, decay, and termites. Aspen OSB bonded with either phenolic or isocyanate resin was treated with several formulations of copper borate at various loadings from 0.26 to 4 percent by weight. These panels were then tested to determine the impact of the preservative on mechanical properties as well as resistance ...
R Smart, W Wall


Ionic liquids with organic and inorganic anions as highly active wood preservatives
2006 - IRG/WP 06-30411
Quaternary ammonium tetrafluoroborates, nitrates(V), propionates, acetates and formates with alkoxymethyl substituents were prepared and tested on wood destroying and sapstaining fungi. These new compounds are ionic liquids (ILs), which penetrate very well into Scot pine wood. Alkoxymethyldecyldimethylammonium tetrafluoroborates and nitrates(V) show better microbial activity against Coniophor...
J Zabielska-Matejuk, A Skrzypczak


Surface and system treatments of wood for outdoor use
2006 - IRG/WP 06-30412
The project “Surface and system treatment of wood for outdoor use” was initiated the summer 2001. The project evaluates environmentally friendly preservatives and water borne coating systems, to find the best protection for timber indented for outdoor use. The wood species selected as test material were pine and spruce. The different treatments were exposed in several outdoor accelerated tests...
B Jacobsen, F G Evans


The Effect of Wick Action upon Moisture Distribution in Ellagate Treated Pinus radiata Wood
2006 - IRG/WP 06-40328
Sapwood stakes of Pinus radiata D. Don were treated with water-soluble tetraguanidinium, tetracholine and tetrakis-benzyltrimethylammonium ellagates. The effect of these treatments upon moisture distribution was investigated by wick action. Given that chemical reactions within the wood substrate between nutrients and treatment solutions may alter the properties of the wood with regard to moistur...
S R Przewloka, B J Shearer, J A Hann


Accelerated assessment tests of new termiticides
2007 - IRG/WP 07-20353
One of the biological agents, which cause major damage to wood in Spain, is the subterranean termites. The systems used for controlling termites don’t eradicate them, and the products presently used to treat wood against them, due to their toxicity and their persistence in the environment, could be prohibited in the near future in Europe as consequence of the 98/8/EC Directive (usually called t...
M T Troya, M J Prieto, D Lorenzo, F Rubio


Current state of world standardization in the toxicometric methods for testing of wood preservatives
2007 - IRG/WP 07-20354
The paper presents an outline of the history of forming standardized toxicometric methods for testing of wood preservatives in the world during last 100 years. Numerous studies resulted in three main methods which are currently used for official and basis assessment of biocides: - agar-block method in Europe (EN 113); - soil-block method in the USA and Pacific countries (ASTM D 1413); - modifi...
J Wazny


Detecting fungal DNA in treated and non-treated wood
2007 - IRG/WP 07-10621
Isolating fungi from wood has long involved culturing on selective media followed by identification using various keys. This process can be cumbersome, costly, and, most importantly, not always capable of detecting all of the fungi present. The recent development of molecular methods for isolation and identification of fungi has created tremendous opportunities for expanding our knowledge of the...
C Freitag, M Freitag, J Morrell


Accelerated Above-ground Testing of Wood Preservatives
2007 - IRG/WP 07-20358
The Canadian wood preservation industry is interested the introduction of new preservative formulations, some of which are intended only for above ground uses. Canada’s Pest Management Regulatory Agency requires data from field tests under Canadian conditions but these can take many years to generate results. Forintek has therefore developed an accelerated above ground test, under contract to a ...
P I Morris, S McFarling


Corrosion of metal fasteners in contact with copper preservative treated wood
2007 - IRG/WP 07-20370
The corrosion rates of metal fasteners in contact with alkaline copper quat (ACQ) treated wood with or without commercially available water repellent was compared to that of cedar. In this experiment, fasteners were sandwiched between two pieces of treated wood and exposed to a humid environment at a slightly elevated temperature. The use of a “sandwich” design allowed periodic examination of ...
BaekYong Choi, J N R Ruddick


Some textile auxiliaries as wood protective agents
2007 - IRG/WP 07-30417
This study evaluated some textile auxiliaries applicable for wood protection. Commercial alkoxysilane quarternary ammonium formulation and fluorocarbon based water-oil repellent were tested for their ability to provide hydrophobicity and antifungal effect to solid wood samples. Scots pine (Pinus sylvestris L.) sapwood samples were impregnated with 25, 50 and 100 % concentrations of the above menti...
E Dizman, A Temiz, N Terziev, Ü C Yildiz


Influence of ethanolamine on lignin depolymerization and copper leaching from treated Norway spruce and beech wood
2007 - IRG/WP 07-30423
Copper-ethanolamine based wood preservatives are replacing several classical copper-chromium based solutions, due to foreseen ban of chromium. Fixation of copper-ethanolamine based wood preservatives is not as good as fixation of copper-chromium ones. The main object of this manuscript was to prove, that ethanolamine is the prime reason for insufficient fixation of copper-ethanolamine formulations...
M Humar, B Bucar, M Zupancic, D Žlindra, F Pohleven


Amine Oxides for Use in Wood Protection: I. A Formulation Adjuvant and Performance Enhancer for Wood
2007 - IRG/WP 07-30425
Amine oxides have great potential for use in the area of wood protection. This paper highlights the advantages of using amine oxides as a formulation adjuvant and performance enhancer for different azoles. It was found that azoles are readily soluble in aqueous amine oxide solutions and form soluble concentrates. These azole/amine oxide concentrates have excellent storage stability and can be dilu...
Xiao Jiang, L Walker


Synthesis of boric acid ammonium oleate salt for wood preservation: Leachability and termite resistance test
2007 - IRG/WP 07-30435
A new chemical compound coupling boric acid and oleic acid through a joint of ammonium salt has been produced and its synthesis followed and validated by Fourier Transformed Infra Red (FTIR). This compound named ammonium borate oleate (BAO) combining biocidal properties of boron and water repellence of fatty acids has then been studied as a wood preservative. Synthesis of BAO involved different...
F Lyon, A Pizzi, Y Imamura, M F Thevenon, S N Kartal, J Gril


The effect of brighteners on wood surface aesthetics – exploring the use of various organo-phosphonates based precursors
2007 - IRG/WP 07-30441
Freshly cut hardwood lumber such as white oak, red oak, beech, or redwood are rich in mineral stain (mostly iron and calcium), which provides a strong discoloration of the wood surface significantly influencing the aesthetic of the wood surface and strongly affecting the cost of this lumber. The influence of mineral stain on soft wood discoloration (Southern Yellow Pine, Douglas fir, etc.) is les...
R Craciun, P Mitchell


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Effects of sodium hypochlorite on compression strength and copper retention of spruce wood treated with copper azole and alkaline copper quat
2007 - IRG/WP 07-40362
This work investigates the effects of sodium hypochlorite on compression strength values and copper retention ratios of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper Azole, (CBA-A, Tanalith-E 3492) and alkaline copper quat (ACQ-2200). Before the copper azole and alkaline copper quat treatment, the samples were immersed in 500 ml of sodium hypochlorite s...
S Yildiz, E Dizman, A Temiz, Ü C Yildiz


Refinement of emission values for preserved wood in the ‘Storage Scenario’, for use in the environmental risk assessment of Wood Preservatives under the Biocidal Products Directive
2007 - IRG/WP 07-50244
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes a scenario for the treated wood in storage after treatment, in which the predicted environmental concentration (PEC) in soil, surface water and groundwater is calculated, using emis...
E F Baines


The effect of additives on copper losses from alkaline copper treated wood
2007 - IRG/WP 07-50246
The replacement of chromated copper arsenate (CCA) by alkaline copper compounds has heightened awareness of the potential impact of copper losses on aquatic organisms. While there remains a healthy debate concerning the actual risk of copper leaching from wood preservatives into aquatic ecosystems, it is clear that reducing these losses will be necessary to avoid continued regulatory actions aga...
J Mitsuhashi, J J Morrell, L Jin, A F Preston


Evaluating the Process of ACQ-Treated Woods with TGAand CEM Analysis
2007 - IRG/WP 07-20374
To provide an understanding of the fundamental thermal behaviour and the disposal-end products of ACQ-treated woods, this study is comprised of two categories of examination. The first is related to the use of TGA under different thermal decomposition conditions (nitrogen or air, and 5 or 40 oC/min), and the use of EDX to examine certain residual elements of the char. The second applies the CEM ...
Han Chien Lin, Tsang-Chyi Shiah, Jung Ting Tsai


Evaluatiang the potency of cinnamaldehyde as a natural wood preservatives
2007 - IRG/WP 07-30444
Since cinnamaldehyde, the major constituent of leaf essential oil from Cinnamomum osmophloeum, has significant antifungal and antitermitic activities, it is worthy of understanding whether cinnamaldehyde has potential to be used as a natural preservative for improving the durability of wood. In this study, the fungi and termite resistance of cinnamaldehyde-treated wood (CTW) were evaluated accordi...
Chun-Ya Lin, Chi-Lin Wu, Shang-Tzen Chang


Validity of above ground testing according to ENV 12037
2008 - IRG/WP 08-20379
The standard ENV 12037 for testing of treated and untreated wood (lap-joint) exposed above ground was issued in 1996 by The European Committee for Standardization. A draft for the development of the standard was presented by CEN-TC 38/WG 25/DOC N 076 in 2002. For a test to become valid the median rating of decay for untreated control replicates (Scots pine sapwood) must be equal or greater than ...
Ö Bergman, U Råberg, N Terziev


Development of a Weatherometer to Accelerate the Surface Checking of Wood
2008 - IRG/WP 08-20388
There is significant interest in developing preservatives that are better at preventing wood from checking. Currently, however, there is no accepted test methodology for accelerating the development of checks in wood samples so information on the effectiveness of treatments at restricting checking can be obtained more quickly. This paper describes the development of a new type of weatherometer (Ac...
R Ratu, P D Evans


Influence of Polyvinyl acetate emulsion (PVA) on boron leaching and fungicidal properties
2008 - IRG/WP 08-30451
Boron compounds are very effective fungicides, but unfortunately they leach from wood. In order to improve boron fixation, boric acid, borax were combined with polyvinyl acetate emulsion (PVA). For comparison copper salts were included into this research as well. Selected preservative solutions were chosen for impregnation of Norway spruce wood specimens (Picea abies). Wood blocks were exposed to ...
M Humar, B Lesar, P Kralj


Preliminary evaluation of efficacy of copper in combination with boron and NHA (N'-N-(1, 8-naphthalyl) hydroxylamine) against wood decay
2008 - IRG/WP 08-30452
In this study, efficacy of various combinations of copper sulfate with either boric acid or calcium precipitating agent, NHA-Na (N'-N-(1, 8-naphthalyl) hydroxylamine) was evaluated. Wood specimens were treated with either 1%, 0.5%, or 0.1% concentrations of copper sulfate, boric acid, NHA-Na, copper sulfate + boric acid, or copper sulfate + NHA-Na mixtures. Treated specimens were subjecte...