Your search resulted in 3487 documents. Displaying 25 entries per page.


Natural durability of 9 tropical species suitable for round wood timber building: fungi and termites laboratory screening tests
2023 - IRG/WP 23-11013
In numerous tropical forest species, wood properties are poorly described and wood is under-valorized. Especially very few is known about small diameter trees although they may be used, directly as round wood, in construction timber building. A selection of abundant species was done and characterization tests were performed to assess their usability as building material. The aim of this work was t...
M Leroy, K Candelier, J Damay, J Bossu, R Lehnebach, M-F Thevenon, J Beauchene, B Clair


Isolation of the microbiota from wood decay insects and some of their enzymatic activities
2023 - IRG/WP 23-11014
Wood decay organisms have the ability to degrade wood components (cellulose, hemicellulose and lignin) by enzymatic capacities, but these enzymes can belong to the proper organism, or to the associated microbiota. The identification of the microorganisms, as well as their role in the digestion of many substrates not always is very well known. The wood decay insects produce big damages in wood str...
M T Troya, F Llinares, J Arranz, S Izpura-Luis, S M Santos, L Robertson


Assessing changes in hardness of furfurylated wood on a nano-scale to mimic levels experienced by the marine wood-boring crustacean, Limnoria
2023 - IRG/WP 23-11016
Wood-boring crustaceans and bivalves can cause severe damage to wooden structures in the marine environment, warranting the need for novel protection systems, such as chemical modifications. Furfurylation increases mechanical properties and resistance of timber species that would usually be susceptible to biodegradation by these borers, such as pine. In rapid laboratory and field testing, furfuryl...
L Martin, J Zekonyte, S Lande, M Westin, S Cragg


Reducing successful settlement by shipworm larvae on wood that has been modified using furfurylation
2023 - IRG/WP 23-11017
Shipworms are Teredinid bivalves that have a highly modified shell for boring into wood and an elongated, vermiform shape. Teredinids are marine wood-borers, utilising timber as both shelter and as a source of food. Wooden structures in the sea, such as piers and sea defences, are subject to severe damage by these borers, costing billions per year for maintenance and replacement. Traditionally, br...
L Martin, I Guarneri, S Lande, M Westin, S Cragg


Morphological observation of wood at the early stages of decay in brown rot and white rot
2023 - IRG/WP 23-11020
Wood rotting fungi, the fungal species causing biodeterioration for wood building, are generally classified into white-rot, brown-rot and soft-rot fungi based on their decay modes. Since white-rot and brown-rot fungi are known to reduce wood strength significantly, it is important to clarify the mechanisms of their wood degradation. White-rot fungi reduce wood strength as the decay progress and de...
R Tsukida, T Hatano, Y Kojima, Y Horikawa, S Nakaba, R Funada, M Yoshida


Effect of volatile organic compounds produced by wood rotting fungi on mycelial growth
2023 - IRG/WP 23-11023
Microorganisms such as fungi or bacteria produce volatile organic compounds (so-called MVOCs: Microbial Volatile Organic Compounds) as metabolites. Some MVOCs have been found to be biologically active, for example inhibition of spore germination, and when fungi of different species encounter each other, the MVOCs pattern change, suggesting that MVOCs play a role as a mediator for biological intera...
S Horikawa, R Konuma, M Yoshida


Comparison of culturable fungi found on two types of modified wood cladding
2023 - IRG/WP 23-11025
Modified woods are rapidly gaining popularity in the United States and are appearing on more public buildings. Because these are biocide-free products, they can support the growth of non-wood degrading fungi on their surfaces, many of which produce dark pigments and deface the cladding. Even growth of dark pigmented fungi on modified woods yields an even grey-black color, giving the materials a we...
G Presley, J Cappellazzi, B Held, R Blanchette


Mini-stakes – an alternative test method for EN 252?
2023 - IRG/WP 23-20691
Market approval of wood treatment products requires knowledge and prove of long-term durability. Efficiency of wood treatment with a specific product is evaluated based on variety of tests, including penetration evaluation, leaching studies as well as decay tests. EN 252 standard test is a core method for wood durability evaluation in a ground contact, both for commercial product approval and scie...
R Digaitis, P Larsson Brelid, N Terziev, M Klamer, A W Christof, J Stenaek, N Morsing


Glued laminated poles - Progress report after 43 years of testing
2023 - IRG/WP 23-20692
In 1979, a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse in Uppsala, in the Simlångsdalen test field in south-western Sweden and in a power lane in Vuollerim in northern Sweden, in order to study their resistance against biological degradation. The test poles were treated in a two-step process. All laminations of Scots pine (Pinus sylvestris) were first...
J Jermer, M Westin, N Terziev


Field durability testing of wood above ground - Part 1: 15 years’ experience with the Bundle method
2023 - IRG/WP 23-20695
A ‘jack of all trades’ method for above-ground wood durability testing has been sought for decades, but until now no method has found its way into standardization. The method of choice shall be applicable for untreated and treated wood – ideally also for wood composites. It shall be reproducible, objective, fast, easy, and inexpensive. Finally, it shall provide high predictive power. This s...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Field durability testing of wood above ground - Part 2: The full guideline of the Bundle method
2023 - IRG/WP 23-20696
To determine the biological durability of wood above ground, numerous approaches for test methods have been pursued and tried out in the field in the past. So far, no method has managed to find its way into a European standard. During the last 15 years, experience with the Bundle method has been gained. As described in Part 1 of this paper, the method is recommended as a suitable tool for determin...
C Brischke, G Alfredsen, L Emmerich, M Humar, L Meyer-Veltrup


Laboratory durability testing of preservative treated wood products – first attempts and observations
2023 - IRG/WP 23-20697
In the past, durability classes (DC) had been assigned to wood species, sometimes also to homogenously modified wood-based materials such as thermally modified wood. More recently, some standards allow for classifying the biological durability of chemically modified wood, preservative treated wood and wood composites. Even treated products may be subject to durability classification, but necessary...
C Brischke, M Sievert, M Schilling, S Bollmus


Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul


Sensitivity of copper indicators for detecting preservative penetration
2023 - IRG/WP 23-20701
Chrome azurol S (CAS), 1-(2-pyridylazo)-2-naphthol (PAN), and rubeanic acid (RA) are the three copper indicators currently used by the timber industry to assess preservative penetration. Although only the American Wood Protection Association (AWPA) standards specify indicator sensitivity, it is unclear how those limits were developed. The sensitivity of each copper indicator was determined in solu...
T Yi, J Norton, S Meldrum, J J Morrell


Simulations of microclimates for wood-decaying fungi in the built environment using environmental analysis
2023 - IRG/WP 23-20703
Simulations of fungal decay risk were run on two similar building geometries exposed to typical annual climate conditions of two different geographical locations, Brunswick (Germany) and Cairns (Australia). The simulations were conducted to capture the effect of wind-driven rain and solar irradiation exposure over nodes of the common building geometry. The moisture content and temperature variatio...
P B van Niekerk, J Niklewski, S H Hosseini, B N Marais, I Frimannslund, T Kringlebotn Thiis, C Brischke


Moisture performance of wooden shingles tested on the Golobar cable yarding
2023 - IRG/WP 23-20704
Wood is a traditional roofing material in Europe and other parts of the world. In the 17th century, wooden roofing was generally used on more important buildings, but today it is mainly used on huts and houses in the Alpine regions. As wooden roofing is expensive, we investigated the possibility of extending the service life of the roofing through material selection and details. The roof of the Go...
M Humar, B Lesar, D Kržišnik


A six-year ground proximity trial of TRU-CORE treatments at Innisfail, Queensland
2023 - IRG/WP 23-30775
This article describes an H3 (above ground outdoor) ground proximity field trial that compares the performance against decay fungi of TRU-CORE (also known as the Buffered Amine Oxide Enhancement System) Copper Quat (CQ) with CCA and commodity Alkaline Copper Quat (commodity-CQ) treatments, all in Pinus radiata. The retentions achieved reflected commercial practice, where higher mean retentions are...
L Cookson


Performance of a noise barrier with different wood materials – results from a service trial after 25 years of exposure
2023 - IRG/WP 23-30776
In connection with the construction of the railway connection between Stockholm Arlanda airport and Stockholm city, an 11 km long noise barrier made of untreated European larch was built along the railway line. This provided an opportunity to implement a full-scale study comparing different untreated wood species and preservative treatments. Thus, in March 1996 ten test sections including untreate...
J Jermer, M Westin


Improvement of durability of Scots pine against termites by impregnation with citric acid and glycerol followed by in situ polyesterification
2023 - IRG/WP 23-30777
Scots pine (Pinus sylvestris) sapwood samples were impregnated with solution containing citric acid (CA) and glycerol (Gly) followed by heating 140 °C according to already described procedure (L'hostis et al. 2018). The resulting modified woods were then used to evaluate the effect of chemical modification on the durability against termites. Two kinds of experiments were conducted for this purpos...
M Mubarok, J Damay, E Masson, E Fredon, Y S Hadi, I W Darmawan, P Gerardin


Suitability of boron preservative treatment of minor species as framing in New Zealand buildings
2023 - IRG/WP 23-30778
The inclusion of alternative species to radiata pine, predominantly exotic species, in the building code (NZS 3602) raises questions as to whether they require preservative treatment and, if so, whether they can be adequately treated using current industry processes. Early research with boron indicated that the dip/diffusion method for green timber would give adequate preservative retention in sa...
D Page, I Simpson, T Singh


Challenges in managing very long-term field tests
2023 - IRG/WP 23-30779
Field testing of wood preservatives has been on-going in Petawawa, Ontario, Canada since at least 1937. Many of the treated roundwood posts from these early experiments are still in test, and include preservatives still used today, including creosote, copper naphthenate, pentachlorophenol and CCA. Performance data from selected experiments more than 50 years old are reported and we discuss some of...
R Stirling, D Wong


Long-term field performance of a carbon-based preservative in ground contact test conditions
2023 - IRG/WP 23-30781
Carbon-based preservatives have demonstrated reasonable long-term field performance in above ground testing. This study examines the performance of a carbon-based preservative formulation containing quaternary ammonium compounds and tebuconazole as a treatment for three softwood species exposed in ground contact at two sites in Canada. The treatment was associated with improved decay resistance an...
C Wilson, J Zhang, R Stirling


Field performance of MCA-treated wood in ground contact
2023 - IRG/WP 23-30782
Micronized Copper Azole (MCA) was evaluated for its ability to resist biodegradation at two Canadian test sites using Pacific silver fir and white spruce stakes, and lodgepole pine and red pine roundwood posts. After 12 years of exposure the treated stakes exhibited low to moderate levels of decay while the untreated controls had failed. When stakes were moved to an active termite site, the untrea...
C Wilson, J Zhang, R Stirling


Recent studies into improved fire retardancy of wood undertaken at Luleå University of Technology
2023 - IRG/WP 23-30784
Modern construction is moving more towards engineered wood products, such as glulam and cross-laminated timber (CLT). This increase is driven by the aspiration to deliver high-rise buildings with enhanced environmental profiles and human well-being. This desire to use wood in construction is pushing the need for fire treatments capable of meeting a products service life. However, the use of wood ...
D Jones, C-F Lin, I Kim, E Garskaite, O Karlsson, D Sandberg


Reuse of discarded wood and alternative wood species to replace spruce in the development of wooden windows for complete disassembly – REWINNUSE
2023 - IRG/WP 23-30785
The REWINNUSE project focuses on the reuse of discarded wood and alternative wood species and on the development of wooden windows that can be easily disassembled into their basic components. In cooperation with the project partners (M Sora, the University of Ljubljana Biotechnical Faculty (BF), the Norwegian Institute of Bioeconomy - NIBIO and the Slovenian Forestry Institute (GIS)), the project ...
B Lesar, M Humar, J Levanič, A Treu, A Ugovšek, L Kramarič, B Štrakel, L Križnar, B Šubic, J Gričar


Previous Page | Next Page