Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Moisture Adsorption Behaviour of Rubber Wood Decayed by Brown and White rot Fungi
2005 - IRG/WP 05-40306
Moisture adsorption behaviour of rubber wood blocks decayed by each brown rot and white rot fungi was studied. The adsorption isotherms of decayed wood were compared with the isotherm of undecayed wood. The wood decayed by brown rot adsorbed less moisture as compared to sound or undecayed wood at all humidity levels. No significant difference was observed in adsorption behaviour of white rot dec...
S S Chauhan, H C Nagaveni


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Determination of thermal degradation of isothiazolone treated wood
1997 - IRG/WP 97-30154
Wood treated with 4,5-dichloro-2-n-octyl-4-isothiazolin-3-one was the subject of thermal degradation study. The study included burning isothiazolone treated wood under various temperatures with and without oxygen. The result showed that no harmful combustion products, such as polychlorinated dibenzo-p-dioxins, polychlorinated dibenzo-p-furans and polychlorinated biphenyls, were detected. These fin...
Bing Yu


The effects of pH on leaching of copper-chrome-arsenate (CCA) from pressure-treated Kenyan-grown Eucalyptus saligna and Acacia mearnsii: Initial findings.
2002 - IRG/WP 02-30298
The effects of pH on leaching of CCA from pressure-treated Kenyan-grown Eucalyptus saligna and Acacia mearnsii were tested under laboratory conditions. Small samples of the two species (100mm x 30mm x 40mm) were smooth sawn from 8-year old trees to represent equal amounts of both sapwood and heartwood, air-dried to 12% moisture content, end-sealed, and pressure-treated at a commercial treatment p...
R Venkatasamy


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Potential use of an emulsified tar oil fraction as a wood preservative: Preliminary technological and environmental assessment
1994 - IRG/WP 94-50028
In order to meet the recent environmental concern specifications of creosote are altered, the B[a]P content is limited and restrictions on the emission of volatile organic compounds (VOC) and higher polyaromatic hydrocarbons (PAH) are expected in some countries. Research has been conducted on an emulsion of a selected tar oil fraction. Using a waterborne formulation opens new perspectives for targ...
G M F Van Eetvelde, R Leegwater, M Stevens


Aggressiveness of Reticulitermes species in laboratory test
1993 - IRG/WP 93-10026
In European Standards concerned with the preventive action of wood preservatives against termites, i.e. EN 117, EN 118 the obligatory test species is Reticulitermes santonensis. It is argued that this species is more aggressive than the second European Reticulitermtes species, Reticulitermes lucifugus. Since Reticulitermes santonensis is confined to certain smaller areas in France and thus not rea...
H Hertel, S Pantos, D Rudolph


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Diagnostics methods and routes proposalsto define selective sorting of demolition wood wastes
2001 - IRG/WP 01-50177
Wood wastes are more and more often used in different wood waste valorisation industries (panels, wood energy, cement factories, ...). These industries are in progress to include in their processes, wood wastes coming from demolition wood. A state of the art and an analysis have been made to propose : (1) diagnostics methods to carry out a classification of wood wastes on demolition sites and in t...
G Labat, E Bucket, C Fréret, G Deroubaix


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Characterization and differentiation of wood rotting fungi by protein and enzyme patterns
1999 - IRG/WP 99-20177
Standardized tests for wood preservatives are performed with defined fungal strains to ensure comparability between laboratories. However, changes of virulence and variation of results are well known events. Suitable and reliable measures to control the stability of the test organisms are necessary.Comparison of protein patterns produced by SDS-electrophoresis was already described by several auth...
U Schoknecht


Wood preservation in Canada - Regulation and Registration
2001 - IRG/WP 01-50166-02
The Canadian wood preservation industry is at a critical juncture now as a number of initiatives converge on the industry over the next few years. Issues facing the industry include: Re-evaluation of the conventional wood preservative chemicals - inorganic arsenicals, creosote and pentachlorophenol targeted for July 2001. Delayed registration of new actives as a result of re-evaluation activity an...
P A Cooper


A determination of the toxic level of ACQ2100 wood preservative for the powder post borer Lyctus brunneus (Stephens)
1994 - IRG/WP 94-20029
The sapwood of two Lyctus susceptible Australian hardwoods, messmate (Eucalyptus obliqua L'Herit.) and black bean (Castanospermum australe A. Cunn. et Fraser ex Hook) were pressure impregnated with ACQ2100, a wood preservative, to produce replicates of a range of retentions. Preservative retentions were determined by solution weight uptake at treatment and chemical analyses of selected sa...
A R Moffat


Exclusion of anions from the wood cell wall
1991 - IRG/WP 3661
Anionic components of wood preservatives and fire retardants such, as arsenates and phosphates, equilibrate at much lower concentrations in the cell wall bound water than in the free solution in the cell lumens. A degree of anion exclusion is expected in wood, due to the Donnan membrane effect. Fixed anions in the wood cell wall, produced by pH-dependent dissociation of the weak acid groups in woo...
P A Cooper


A non-destructive testing technique for wood poles
1987 - IRG/WP 2293
A method has been developed to evaluate the stiffness and condition of a wood pole based on structural dynamics. This paper describes the results of tests performed on nearly 200 wood utility poles across Western Canada. A high correlation exists between the dynamic non-destructive test and direct mechanical tests. The need for an accurate non-destructive testing technique is demonstrated by the f...
W M Murphy, D E Franklin, R A Palylyk


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


A comparison of fatty acid and molecular profiles for identification of wood colonizing basidiomycota
2003 - IRG/WP 03-20278
Two methods that are currently being employed to detect and identify wood decay fungi are Fatty Acid Methyl Ester (FAME) analysis and Restriction Fragment Length Polymorphism (RFLP) analysis. A FAME library and RFLP library for 9 species and up to 10 strains within each species have been developed. The profiles generated by these methods have been compared for each species and strain to test for...
T C McElroy, L Prewitt, S V Diehl


A new process for in situ polymerization of vinyl monomers in wood to delay boron leaching
1998 - IRG/WP 98-40110
Efforts were accelerated on effective use of boron compounds in wood preservation owing to their environmentally safe characteristics and relatively low costs in addition to their well-known high bioactivity and fire resistant properties. Although having these unique favorable properties, they are readily leachable from treated wood at humid conditions. Therefore, they had limited market for exter...
M K Yalinkilic, W Dwianto, Y Imamura, M Takahashi


Creosote for wood preservation. (Reissued from earlier OECD draft)
1970 - IRG/WP III 1A
The literature on this subject is extensive and, to some extent, repetitive so that for pratical reference purposes it is essential that selective surveys and bibliographies be prepared. Many of these exist and, as an example, the reports issued by The Coal Tar Research Association (Numbers 0156, 0292 and 0396) may be quoted. The following bibliography, listing the more important sources of inform...
Anonymous


The chemical wood preservation in the former GDR - an overview
1995 - IRG/WP 95-50057
For the disposal of chemically treated wood waste and for the remedial treatment of contaminated soils in facility yards a profound knowledge is required concerning the kind of preservatives used and the degree of pollution. In order to record the production of wood preservatives and the location of impregnation plants in the former GDR, documents of the Office for Standardisation Measuring Affair...
E Melcher, R-D Peek


Production of fungal protoplasts from selected wood-degrading fungi
1991 - IRG/WP 1500
Studies of hyphal morphology and the effects of various chemicals on growth are often difficult to perform on filamentous fungi because of the difficulty of observing the protoplasm through the rigid hyphae wall and because most activity occurs in a limited region near the hyphal tip. As an alternative, hyphae can be reacted with certain cell wall degrading enzymes to remove the cell wall to produ...
C Rui, J J Morrell