A reliable spot test for TCMTB in wood
1992 - IRG/WP 92-2391
Test specimens of slash pine (Pinus elliottii) and spotted gum (Eucalyptus maculata) were treated with aqueous emulsions of Busan 30WB and Busan 31, containing the fungicide TCMTB (2-(Thiocyanomethylthio)benzothiazole), or with solutions of TCMTB in toluene. These and matching untreated specimens were subjected to a wide range of procedures in an attempt to reveal TCMTB penetration patterns. Most ...
D E Ferlazzo, M J Kennedy


Development of wood retification process at the industrial stage
1998 - IRG/WP 98-50101-16
Wood is a natural composite material which exhibits outstanding properties from the technical as well as from the ecological point of view. However, it is an anisotropic, hygroscopic material sensitive to biological attacks. We have to stabilise and preserve it if we want to ensure its market shares faced with competing synthetic material, whilst taking the new environmental rules into account. T...
P Gohar, R Guyonnet


Ecotoxicological behaviour of leachates from superficially treated timber as an approach for a test strategy of environmental risk assessment in wood preservation
1998 - IRG/WP 98-50101-09
At present for wood preservatives, which in Germany are subject to the quality mark of the RAL-Gütegemeinschaft Holzschutzmittel, health and safety as well as environmental aspects are evaluated by official authorities, as BgVV (Federal Institute for Consumer Health Protection and Veterinary Medicine) and the UBA (Federal Environmental Agency). From the environmental point of view to day there a...
H W Wegen, U J Lucks


Co-incineration of CCA-treated wood and Municipal Solid Waste in MSWI plant
2005 - IRG/WP 05-50224-19
The Norwegian Association of Energy Users and Suppliers (Norsk Energi) have carried out incineration tests with addition of 10 % by weight CCA-treated wood waste to municipal solid waste in a MSWI plant. The objective with the test was to determine emissions and composition of bottom ash. The incineration test was done at the Klemetsrud plant in Oslo The main conclusions are: -No significant inc...
D Borgnes, B Rikheim


Optimun storage period for the boron diffusion treatment of rubber wood
1996 - IRG/WP 96-30121
The study determined the maximum thickness of rubber wood that can be diffusion treated and the effect of diffusion storage period on the distribution of chemicals in treated wood of various thicknesses. Wood of thickness up to 50 mm can be easily diffusion treated with 10% boric acid equivalent (BAE) solution to adequate loading of chemicals. The optimum diffusion storage period to get uniform an...
T K Dhamodaran, R Gnanaharan


Confocal Laser Scanning Microscopy (CLSM) of decayed wood
1998 - IRG/WP 98-10273
Confocal laser scanning microscopy (CLSM) is currently being used to examine biodegraded wood and is proving to be a useful new technique in this area of work. Non-invasive optical sectioning within a thick specimen (20 - 50 µm), coupled with post image processing techniques allows manipulation of images and 3-D reconstruction from serial sections. Glutaraldehyde can cause cell autofluorescence,...
Ying Xiao, R N Wakeling, A P Singh


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Preservative treatment of different thatching materials for low cost housing
1999 - IRG/WP 99-40144
Preservative treatment were made in seven different roofing materials with Copper-Chrome-Boron (CCB) at different concentration by soaking process. These were paddy straw, wheat straw, jute stick, sungrass, ulu grass, sugercane leaf and Nipa fruticans. It was observed that retention of preservative chemicals varies from species to species at the same concentration. From the service test it was obs...
K Akhter, M Younusuzzaman, M H Chowdhury


The degradation of wood by metal fastenings and fittings
1972 - IRG/WP 302
As well as the hazards of biological decay, timber used in boat building is subject to the effects of chemical decay associated with the corrosion of metallic fastenings. The title has been deliberately chosen to emphasize that in wooden construction the troubles are not just those of corrosion of the fastenings, but also the destructive secondary effects on the wood caused by the products of the ...
L C Pinion


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


Physical and mechanical properties of wood-polymer composites prepared from alder wood (Alnus glutinosa (l.) gaertn. subsp. barbata (c.a.mey.) yalt)
2001 - IRG/WP 01-40201
In this study, the physical mechanical properties of wood-polymer composites prepared from alder (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey.) Yalt) wood were investigated. Three different monomers styrene, methyl methacrylate and styrene/methyl methacrylate (70/30) mixtures and two loading levels were used in preparation of wood-polymer composites. Of physical properties, the oven-dry s...
A Temiz, Ü C Yildiz, E D Gezer


Growth of selected wood decay fungi on various agar-supplemented media
2003 - IRG/WP 03-10456
The growth rates of a selection of wood decay fungi (brown and white rots) on various agar-supplemented media have been determined and compared. The agar media investigated were Malt extract agar (MEA), Potato dextrose agar (PDA), YMPG agar (yeast extract, malt extract, bacto-peptone, glucose, asparagine and thiamine), YMPG agar (without amino acids) and Beech wood powder agar (BWA). The tested wo...
S A Amartey, M Humar, F Pohleven


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


Recycling CCA-treated poles with Charterm
2005 - IRG/WP 05-50224-17
After 10 years of Research and Development, the first “Chartherm” industrial unit is now operating since nearly half a year, thanks to Thermya SA, engineering company, current owner of all the “Chartherm” process Patents and Rights. In accord with the recycling contracts signed with several French major companies, the “Chartherm” plant, located near Bordeaux, recycles every day severa...
J-S Hery


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


A comparison between different accelerated test methods for the determination of the natural durability of wood
1996 - IRG/WP 96-20099
According to the European standard EN 350-1 the natural durability of wood is defined as: "the inherent resistance of wood to attack by wood destroying organisms". This standard also describes how, for certain hazard classes, the durability is determined. The two methods described in this standard are the kolleflask method (EN 113) and the field-stake-test method (EN 252). The EN 113 test gives re...
H Militz, S G L Michon, J E Polman, M Stevens


An example of media response to perceived environmental problems with CCA-treated wood
1990 - IRG/WP 3564
A recent study suggested that CCA-treated wood exposed to acidic precipitation could lose significant amounts of copper chromium and arsenic resulting in loss of efficacy and possible environmental contamination. The study received wide newspaper and radio coverage in Canada, thereby heightening public concern about CCA use. Subsequent studies in our laboratory confirmed that the high losses were ...
P A Cooper


Borate diffusion in wood from rods and liquid product. Application to laminated beams
1988 - IRG/WP 3482
In the aim to use borate preservatives (fused rods and boracol) in fields of building construction other than external joineries, tests of diffusion of borate rods and secondary boracol, were carried out on different species of woods exposed to different moisture conditions. Tests were also applied on laminated beams very often subjected to high moisture contents and thus decay of rot fungi. Diffu...
D Dirol


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Preservative treatment of Golpata (Nypa fruticans) using CCA (Chromated Copper Boric Acid)
1999 - IRG/WP 99-40131
Golpata (Nypa fruticans) leaves provide a cheap but practical source of roof thatches. This study was carried out to determine whether the life span of Golpata could be extended by using CCB (Chromated Copper Boric Acid) treatment. Both leaves and midribs of Golpata , with different moisture contents ranging 16.63% to 70.67%, at the start of the experiment were treated with four different concentr...
G N M Ilias, F Abdullah, M O Hannan, S M Feroz


Oxine copper (NYTEK® GD) for the control of mould and sapstain on lumber in North America
1989 - IRG/WP 3517
NYTEK® GD is a new, water-based, micro-dispersible formulation of oxine copper registered in the United States and Canada for control of mold and sapstain-causing fungi. NYTEK GD is noncorrosive and of low hazard to applicators and people handling treated lumber, when used according to the label. The product is an effective wood protectant applied as a dip or spray treatment at concentrations of ...
D F Myers, J M Fyler, C H Palmer, G D Rosebery


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Bacteria are important degraders of cooling tower timbers: New Zealand experience
1995 - IRG/WP 95-10128
Microscopic examinations of CCA-treated Pinus radiata timbers in industrial cooling towers in New Zealand showed bacteria and soft rot fungi to be primarily responsible for the decay of these timbers. Of these micro-organisms, erosion bacteria appeared to be most widespread, attacking wood cell walls independently as well as together with tunnelling bacteria and soft rot fungi. Tunnelling bacteria...
A P Singh, R N Wakeling


Severe decay damages of bridges made of ekki (Lophira alata) wood known as a durable species
2000 - IRG/WP 00-10383
Bridges made of ekki (azobe, bongossi, Lophira alata Banks et Gaertn.) timbers were severely decayed only 10 years after the construction possibly caused from no maintenance for the periods. The reason of no maintenance is due to the misunderstandings on wood durability against wood-decaying fungi. Some civil-engineers and architectures understand "durable species" means "absolutely decay-durable ...