Laboratory tests on light organic solvent preservatives for use in Australia. - Part 6: Soft rot resistance of three fully formulated preservatives on different timber substrates
2000 - IRG/WP 00-30245
The above-ground soft rot resistance of substrates treated with three fully formulated light organic solvent preservatives (Cuprivac Green WR, Impresol WR 205 and Vacsol) was studied using a modified vermiculite burial method. The substrates were sapwood of Pinus elliottii and P. radiata and heartwood of Eucalyptus regnans, Pseudotsuga menziesii, Shorea sp. (a lower and a higher density source) an...
G C Johnson, M A Tighe, J D Thornton


An inclination incising technique for the preservative treatment of refractory timbers
1991 - IRG/WP 3664
An inclination incising technique for preservative treatment of refractory timbers was examined by changing cutting angle to the longitudinal direction of test specimen and by using different types of knife edge. Incised wood were impregnated locally into incisions with CCA solution by the specified local pressure process. Width and length of penetration areas of CCA solution were measured on long...
Y Nakamura, K Nishimoto


The new National Directive on wood preservation in the Netherlands
1998 - IRG/WP 98-50101-03
In the Netherlands the major part of treated timber is sold under the KOMO-certificate. The National Directive for vacuum pressure treated timber on which certification is based, is currently being revised. The new National Directive will contain a code of good practice including maximum leaching figures. It incorporates quality requirements for treated timber, existing legislative requirements an...
W J Homan, J K B Kwisthout, J Dubelaar


Volatile losses of wood preservatives
1973 - IRG/WP 236
The purpose of the work we have undertaken so far has been to try to quantify the volatile losses which occur in treated timber, and to examine some of the factors which influence these losses. The preservative compound chosen for the initial part of the programme was the contact insecticide g-BHC. This was attractive for several reasons, not the least of which was that specific and sensitive anal...
J W W Morgan, D F Purslow


Tanalith T - a new preservative system for protecting house frames in Australia from termite attack.
2003 - IRG/WP 03-30306
The sawn timber industry in Australia has expressed a desire for a new low cost termite treatment. The treatment needs to be on-line in the dry mill, minimising material handling costs and with a very fast processing time to meet timber flow through the dry mill. The preservative, Tanalith® T, forms an envelope on both Pinus radiata and Pinus elliotti sawn timber. Field trials conducted in Aus...
P R S Cobham, J Snow


Properties of plywood and Oriented Strand Board manufactured with an organic insecticide incorporated in the adhesive formulation
2000 - IRG/WP 00-40174
The efficacy of Fipronil as an insecticide has been established by laboratory and field experiments and commercial use against a broad range of insect pests for various crops. It can be used by either foliar or soil application. Development is underway for the non-agricultural uses of fipronil. Research is ongoing for the control of ants, cockroaches, fleas, ticks, houseflies, mosquitoes, termites...
D P Kamdem, J H Hope, A Jermannaud


Paper for discussion - Incising of spruce to improve preservative penetration
1973 - IRG/WP 318
Large quantities of whitewood or Norway spruce (Picea abies) are regularly imported into the United Kingdom from continental Europe. In addition, increasing amounts of Sitka spruce (Picea sitchensis) are likely to become available over the next decade from the Forestry Commission. In many ways spruce is a good structural timber, eg it is relatively cheap and easily available, it has adequate stren...
W B Banks


Copper leaching from Kemwood ACQ and Embalit CBC treated wood products
2000 - IRG/WP 00-50150
TNO has performed a study on the leaching of copper from Kemwood ACQ and Embalit CBC treated wood products, further referred to as ACQ and CBC. The sawn dry wood has been impregnated using an industrial vacuum-pressure process with ACQ (with or without Ultrawood 4) or with CBC, under supervision of Flexchemie B.V. After treatment samples have been transported and subjected to leaching tests at TNO...
P Esser, W L D Suitela, H Trompetter


Field tests of preservative-treated radiata pine in Japan
1995 - IRG/WP 95-30083
Test stakes of radiata pine treated with various alkyl ammonium compound (AAC) formulations and with copper-chrome-arsenate (CCA) as reference preservative were installed in 3 test sites in Japan in 1981-82. When inspected in 1995, CCA-treated stakes showed less decay at all three sites than stakes treated with other formulations. Ammoniacal copper quaternary (ACQ)- treatment was only slightly les...
M E Hedley, K Tsunoda, K Suzuki


Treatability problems - Relationships between anatomy, chemical composition and treatability
2001 - IRG/WP 01-40213
This report documents the results of phase 1 and 2 of a 3-phase research program. In phase 1, two hundred and fifty-six (256) Southern pine (pinus spp.) nominal 2 x 6's (38 mm x 140 mm) from a single mill in Georgia (southeastern US) were evaluated for treatability with CCA preservative. After treatment, 128 pieces representing a broad range of treatment characteristics were selected and ...
J E Winandy, F Green III, D Keefe


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Treatment of lumber with preservative/water repellent emulsions - The significance of shear stability on penetration
1997 - IRG/WP 97-20124
Currently, the treatment of lumber with a water repellent emulsion and a wood preservative formulation in combination is the most cost effective way to prevent decay and to maintain the appearance of uncoated lumber in service. Water repellents influence the movement of moisture into and out of wood and, by so doing, can decrease checking and splitting significantly. Adequate penetration of the em...
F Cui, K J Archer


The influence of soil pH on leaching of CCA elements from pressure-treated Eucalyptus saligna sapwood: environmental implication
2003 - IRG/WP 03-50203
Evidence is accumulating as to poor distribution and fixation of CCA in tropical hardwoods, and there is therefore a necessity to investigate the permanency of CCA in tropical hardwoods. The relationship between soil pH and leaching of Cu, Cr and As from CCA pressure-treated sapwood of Kenyan-grown Eucalyptus saligna was tested under laboratory conditions. Small sapwood samples were pressure-tre...
R Venkatasamy, D N Okwara


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Performance of CCA wood preservative and CCA treated wooden materials (pole, anchor log, cross-arm etc) with special reference to Bangladesh (Series 1)
2005 - IRG/WP 05-40318
Wood is an important renewable natural resources produced by plants which is without question oldest and versatile construction material. It is composed of cellulose, hemicelluloses and lignin. Cellulose and hemicelluloses accounts for about two-thirds of the dry weight of the wood which perform the major structural role. Lignin is the remaining one-third of the wood which holds the cellulose and ...
G N M Ilias


Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Investigation of temperature effect on fixation of Celcure preservative (ACC) in beech (Fagus orientalis)
2001 - IRG/WP 01-40200
In this research, the fixation speed of Celcure 2% (ACC) preservative salt, under temperature of 17°C, 27°C and 50°C, on intact and stained wood specimens of beech was investigated. For this purpose, blocks of wood with 5x5x7 cm dimensions were prepared and saturated with 2% ACC concentration by full-cell process. The specimens were put in three incubators at the above-mentioned temperatures. F...
A Karimi, M Ghorbani


Fungicidal activity of some new water borne copper octanoate based formulations
1999 - IRG/WP 99-30198
Four new water borne formulations for preservation of wood were prepared: the composition of Cu(II) octanoate, 2-aminoethanol (ethanolamine) and water; the composition of complex of Cu(II) octanoate with nicotinamide, 2-aminoethanol and water; the one of Cu(II) octanoate, organic boron complex, 2-aminoethanol, dimethyl sulfoxide and water and finally, the mixture of Cu(II) octanoate, diazene, 2-am...
M Petric, M Pavlic, F Pohleven, P Segedin, B Kozlevcar, S Polanc, B Stefane, R Lenarsic


Laboratory evaluation of metallic naphthenates as wood preservatives
1991 - IRG/WP 3654
Fungicidal and termiticidal efficacy of copper and zinc naphthenates was appraised according to Japanese standardized laboratory testing methods. Copper and zinc naphthenates succeeded in protecting wood from decay fungi at retentions of 0.5 and 1.0 kg/m³ as metal, respectively. [JIS A 9302 (1976)] when they were applied to vacuum/soak impregnation [JIS A 9301 (1976)]. With respect to the fungici...
K Tsunoda, M Sakurai


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Evaluating the performance of preservative/water repellent emulsion systems
1997 - IRG/WP 97-20127
Water repellent emulsions are being combined with wood preservatives to improve the weathering properties of treated wood in service. Unfortunately, few standard procedures are available to objectively compare the performance of these systems and as a result quality issues are almost completely neglected. The value of swellometer tests, water immersion tests and accelerated weathering regimes in t...
K J Archer, F Cui


Determination of total fluoride and boron in preservative-treated wood fluoride by ion selective electrode without steam distillation, and boron colorimetrically using azornethine-h
1998 - IRG/WP 98-20135
An analytical method was developed to determine total fluoride and boron in wood treated with aqueous or solid diffusing fluoride or borate-fluoride formulations. Ground wood was mixed with 30% sodium hydroxide solution and oven-dried for 2 hours before furnacing at 600° C for 1 hour. The cool fused product was dissolved in hot water, transferred to a plastic beaker and neutralised. Fluoride was ...
P A Collins, M J Kennedy


Some factors affecting the treatability of spruce roundwood with ammoniacal preservative solutions
1976 - IRG/WP 371
Permeable wood species for use in preservative-treated commodities are becoming depleted in Canada. Spruce can be a convenient replacement for them from local resources provided it can be treated to levels adequate for protection of commodities in ground contact. Basically, two approaches were taken to improve treatability of difficult-to-penetrate softwood species; first, to improve the permeabil...
J Rak