Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


Comparative performance of several ammoniacal copper preservative systems
1997 - IRG/WP 97-30151
The efficacy of several ammoniacal copper-based wood preservative systems was evaluated in this study. The selection of potential co-biocides was based on the results of an agar plate test. Following this, the most promising systems were evaluated in a standard field stake test. Good correlation was found between the agar plate and field stake test results. Of the preservative systems tested, copp...
D D Nicholas, T Schultz


Decay and mold resistance of borate modified oriented strandboard
2003 - IRG/WP 03-40260
Decay and mold resistance of zinc borate (ZB) and calcium borate (CB) modified oriented strandboard (OSB) from southern mixed hardwoods and yellow pine was investigated in this study. Tests were done with brown rot, Gloeophyllum trabeum, and white-rot, Trametes versicolar, fungi for 8 and 12 weeks, respectively. Wood species and fungus type had significant influence on the decay resistance. Decay...
Q Wu, S Lee, J P Jones


Evaluation of the corrosivity of the treated wood - Laboratory vs field test methodologies
2000 - IRG/WP 00-20211
The corrosivity of treated wood to fasteners has been evaluated using laboratory test procedures, including AWPA Standard E12-94. The standard method was modified in order to allow detailed study of commercial metal fasteners in terms of sample types, installation configuration and exposure conditions. Parallel field tests were also performed. The experimental results generated from these tests su...
L Jin, A F Preston


Copper leaching from Kemwood ACQ and Embalit CBC treated wood products
2000 - IRG/WP 00-50150
TNO has performed a study on the leaching of copper from Kemwood ACQ and Embalit CBC treated wood products, further referred to as ACQ and CBC. The sawn dry wood has been impregnated using an industrial vacuum-pressure process with ACQ (with or without Ultrawood 4) or with CBC, under supervision of Flexchemie B.V. After treatment samples have been transported and subjected to leaching tests at TNO...
P Esser, W L D Suitela, H Trompetter


Natural exposure weathering tests: Their role in the assessment of wood preservative efficacy
1993 - IRG/WP 93-20006
Previous work has demonstrated the potential and usefulness of natural ageing procedures in e evaluation of wood preservative efficacy. This results from the combination of physico-chemical influences and microbiological interactions with both substrate and wood preservative. In this paper, results are presented for a range of biocide types. Discussions are centred on the value of natural exposure...
G R Williams, J Brown


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


The influence of soil pH on leaching of CCA elements from pressure-treated Eucalyptus saligna sapwood: environmental implication
2003 - IRG/WP 03-50203
Evidence is accumulating as to poor distribution and fixation of CCA in tropical hardwoods, and there is therefore a necessity to investigate the permanency of CCA in tropical hardwoods. The relationship between soil pH and leaching of Cu, Cr and As from CCA pressure-treated sapwood of Kenyan-grown Eucalyptus saligna was tested under laboratory conditions. Small sapwood samples were pressure-tre...
R Venkatasamy, D N Okwara


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers
1991 - IRG/WP 2381
Standardized heartwood blocks of kempas (Koompassia malaccensis), keruing (Dipterocarpus sp.) and tualang (Koompassia excelsa) were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicola grisea, Petriella setifera and Trichurus spiralis in a containerized vermiculite-burial decay system according to draft CEN/TC 38 WG 4....
A H H Wong, R-D Peek


Fungicidal activity of some new water borne copper octanoate based formulations
1999 - IRG/WP 99-30198
Four new water borne formulations for preservation of wood were prepared: the composition of Cu(II) octanoate, 2-aminoethanol (ethanolamine) and water; the composition of complex of Cu(II) octanoate with nicotinamide, 2-aminoethanol and water; the one of Cu(II) octanoate, organic boron complex, 2-aminoethanol, dimethyl sulfoxide and water and finally, the mixture of Cu(II) octanoate, diazene, 2-am...
M Petric, M Pavlic, F Pohleven, P Segedin, B Kozlevcar, S Polanc, B Stefane, R Lenarsic


Laboratory evaluation of metallic naphthenates as wood preservatives
1991 - IRG/WP 3654
Fungicidal and termiticidal efficacy of copper and zinc naphthenates was appraised according to Japanese standardized laboratory testing methods. Copper and zinc naphthenates succeeded in protecting wood from decay fungi at retentions of 0.5 and 1.0 kg/m³ as metal, respectively. [JIS A 9302 (1976)] when they were applied to vacuum/soak impregnation [JIS A 9301 (1976)]. With respect to the fungici...
K Tsunoda, M Sakurai


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Studies on the mobility of arsenic, copper and chromium in CCA-contaminated soil
1990 - IRG/WP 3571
CCA contaminated soils from six Swedish preservation plants were investigated primarily to study the mobility of arsenic but also that of copper and chromium in the soils. The soil samples represented average types with different amounts of clay, organic matter, arsenic, copper, chromium and different pH. The total soluble amounts of the elements were measured. The pH dependent solubility and the ...
J Bergholm


Long-term efficacy of wood dip-treated with multicomponent biocides
2005 - IRG/WP 05-30379
Biocides designed for prevention of indoor mold growth on wood-based materials need to provide long-term protection under conditions of high humidity. Specimens of kiln-dried southern pine and unseasoned southern pine, aspen, and Douglas-fir were dip-treated with borate-dimethylcocoamine (DMCA) supplemented with voriconazole, thiabendazole, or thujaplicin and evaluated at 4-week intervals for inhi...
C A Clausen, V W Yang


Comparison of the effects of borate, germanate and tellurate on fungal growth and wood decay
1992 - IRG/WP 92-1533
The tetra-hydroxy borate ion is known to undergo complexation with polyols and has been shown to inhibit dehydrogenase enzymes in this way. It has been previously suggested that this complexation is responsible for the inhibition of fungal growth and the protection of boron treated timber. Other ions that have the ability to complex with polyols have also been shown to inhibit dehydrogenase activi...
J D Lloyd, D J Dickinson


A chemical and mycological evaluation of fused borate rods and a borate/glycol solution for remedial treatment of window joinery
1983 - IRG/WP 3225
The possibility of using fused borate rods (Impel Borpatron) and a borate/glycol solution (Boracol-40) for depot impregnation of window joinery has been examined in a co-operative project between The Swedish Forest Products Research Laboratory, The Swedish University of Agricultural Sciences and Prolignum AB. The fused Impel rod is a glassy rod composed of disodium octaborate which readily dissolv...
M-L Edlund, B Henningsson, A Käärik, P-E Dickèr


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Inorganic preservatives in wood dust - Cause of nasal cancer?
1997 - IRG/WP 97-50085
Since 1985 dust particles from beech and oak trees have been classified by the Senate Commission of the German Research Council (DFG) as being ,,working materials which are definitely carcinogenic to humans". All other wood dusts, including those from softwoods, are classified as being materials ,,with reasonable suspicion of carcinogenic potential". The carcinogenic principle of action continues ...
A O Rapp, K Brandt, R-D Peek, U Schmitt


Determination of absorption, accumulation and transport of copper in mycelium of some wood decay fungi
1999 - IRG/WP 99-10323
Copper compounds are common wood preservatives. However, tolerance of some wood decay fungi to copper compounds has been observed recently. Therefore, we tried to elucidate possible causes of this phenomenon. We investigated uptake, accumulation and secretion of copper in the mycelium of potentially copper tolerant fungi (Antrodia sp.) and non tolerant fungus Trametes versicolor. We observed that ...
F Pohleven, S Breznikar, P Kalan, M Petric


Fixation of copper-chrome-arsenic treated timber: A comparison of leaching methodologies
1996 - IRG/WP 96-50075
Five packs of kiln dried radiata pine heartwood were treated with copper-chrome-arsenic preservative treated, utilising a modified Bethell treatment schedule. Two methods of determining the level of preservative fixation were compared. These included the diphenylcarbazide method and simulated rainfall testing. The fixation levels were generally higher for tests involving simulated rain leaching. F...
S Walley, P R S Cobham, P Vinden


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Relative performance of copper/chrome/boron (CCB) and copper/chrome/arsenate (CCA) in ground contact
1992 - IRG/WP 92-3694
The performance of four retentions each of an oxide CCA formulation and a salt formulation of CCB in radiata pine and European beech was compared after 18 years' field exposure. In radiata pine CCA oxide was more effective (4 failures out of 40) than CCB (9 failures out of 40). However, in European beech CCB was substantially more effective (22 failures) than CCA oxide (all failed). Analy...
M E Hedley


Ability of chitosans to limit wood decay under laboratory conditions.
2004 - IRG/WP 04-30339
Chitosans have recently been explored for controlling a number of plant pathogenic fungi and have shown some promise for controlling stain fungi on wood. The potential for using chitosans either alone or in combination with copper sulfate to protect wood from fungal decay was explored using maple veneers. Chitosan treatment reduce weight losses caused by two brown rot and one white rot fungi, howe...