Mould growth on wood-based materials – a simulated in-service study
2012 - IRG/WP 12-20503
Ten different wood-based materials including preservative-treated wood, fire retardant-treated wood, modified wood, WPCs and untreated references of pine sapwood and spruce were placed in three different environments (an attic and two crawl spaces) for a period of 26 months. Mould growth was analysed at five to seven month intervals in an effort to map the growth development. The relative humidit...
G Bok, P Johansson, J Jermer


Triazole – based ionic liquids to protect of lignocellulosic materials against fungi
2012 - IRG/WP 12-30601
In presented paper we examined on biotic properties of novel structure of tebuconazole derivatieves: tebuconazole hydrochloride, allyltebuconazole chloride, methyltebuconazole iodide, tebuconazole dihydrocitrate. Our investigation against wood-degrading fungi were contained also the didecyldimethylammonium 3-aminotriazolate as well as didecyldime-thylammonium nitrate(V) with tebuconazole or wit...
J Zabielska-Matejuk, J Pernak, I Frąckowiak, A Stangierska, W Przybylska, M Kot


Communities of mold fungi on flooded building materials
2013 - IRG/WP 13-10799
A small building built to residential code was flooded using farmland pond water to a depth of two feet at Tuskegee University. The building was drained and left enclosed for an additional three weeks. A total of 168 material samples were removed either immediately after opening (wet) or seven months after flooding (dry). Wall materials sampled included fiberglass batt insulation, gypsum wallboard...
F Skrobot III, H Aglan, S V Diehl


Focus on the European standardization - Towards a revision of the EN 350 natural durability standard: a different approach to the inherent resistance and performance of wood and wood-based materials
2013 - IRG 13-10811
The European standard EN 350 “Natural durability of solid wood”, Parts 1 and 2, is one of the fundamental standards developed by the CEN/TC 38 “Durability of wood and wood-based products”. This standard is widely used by wood industries as the reference document which provides information on the resistance of wood species used in mainly the construction sector against decay fungi, wood-bor...
M Kutnik


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


A Vision of the Chilean Treated Wood Industry
2013 - IRG/WP 13-40619
Chile is an important actor in the world wide forestry industry, activity which represents 3,1% of the Gross National Product (GNP). The wood products sector, which includes pulp and paper, is the second source of export in Chile with USD 6,500 millions income per year. Native species are the main forestry source with 15,9 millions has., but the principal commercial activity is based on 2,3 mil...
F J Latorre, T A Hanke


Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Nondestructive Detection of Biodeterioration in Indonesian Traditional Wooden Construction of “Joglo”
2014 - IRG/WP 14-10834
To decide the repairing and reinforcement method for wooden constructions, it is necessary to get the enough and precise information on the status of the construction beforehand, especially the distribution and the degree of the biodeterioration, such as decay or insect attack (e.g. termite attack). In this study, damage of biodeterioration to teak wood used in Indonesian traditional wooden const...
Y Yanase, T Mori, T Yoshimura, Y P Prihatmaji, J Sulistyo, S Doi


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


Communities of mold fungi in moisture damaged building materials
2014 - IRG/WP 14-20542
The critical conditions needed for the development of mould and decay fungi have been modelled for different building materials. However, current knowledge of indoor microbes growing on building materials relies on culture-based methods and more advanced molecular biological techniques should be employed to study the complex microbial communities in building materials. In this paper molecular biol...
E Sohlberg, H Viitanen


Field performance of wood-based decking materials in the Western United States
2014 - IRG/WP 14-30645
While wood has long been used for the construction of decks and other outdoor features, a variety of wood-plastic composite (WPC) decking products have emerged over the past decade with claims of exceptional durability and low maintenance. There are relatively few long term comparative tests on these products. The performance of selected WPC decking products was compared with naturally durable we...
S Lipeh, C S Love, J J Morrell


Applicability of wood durability testing methods to bio-based building materials
2015 - IRG/WP 15-20561
It is well known that organic materials may be susceptible to attack from a range of fungal organisms and any bio-based material used in locations where there is the possibility of microbiological activity must be expected to be able to withstand or prevent such attack. There are a wide range of test methods and standards in place to test susceptibility although most of these test individual compo...
S F Curling, B K Stefanowski, E Mansour, G A Ormondroyd


Colonization of treated and untreated decking materials by bacteria, fungi and algae quantified by qPCR
2015 - IRG/WP 15-20568
The use of durable wood species for wood decking in outdoor applications, e.g. garden terrace (use class 3) is gaining more and more interest on the part of consumers and architects. To get detailed information on the practical use of deckings, a project was started in 2010. In total 71 different decking materials (0.03 m²) were installed and evaluated over 30 months. Beside other parameters, the...
E Stoyanova, B Schmöllerl, A Steitz, N Pfabigan, R Gründlinger


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...
D Jones


Evaluating the Effects of Post Dip-Treatment Laser Marking on Resistance to Feeding by Subterranean Termites
2016 - IRG/WP 16-10854
Dip-treatment of wood packing materials is often used instead of pressure treatment mainly because of issues relating to simplicity and cost. Packaging boxes fabricated for the United States Army are required to be dip-treated for at least one minute in an approved preservative solution prior to use. These boxes are expected to have a service life of up to 20 years in a wide variety of environment...
R A Arango, B Woodward, S Lebow


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Effects of fungal exposure on air and liquid permeability of nanosilver- and nanozincoxide-impregnated Paulownia wood
2016 - IRG/WP 16-30680
Effects of aqueous dispersion of silver and zinc-oxide nano-particles on air and liquid permeability of Paulownia wood exposed to T. versicolor were studied in the present research project. Specimens were also heat-treated at 100 and 150°C and compared with the control specimens. Permeability values were measured when the moisture content of the specimens was 12%. Results showed significant incre...
H R Taghiyari, A Kalantari, M Ghorbani Kookandeh, F Bavaneghi, M Akhtari


The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durability and reputation. This research was conducted to assess the decay resistance of CLT and OSB (oriented strand board) in an accelerated trial...
T Singh, D Page


Fabrication and characterization of MicroPCMs filled wood-plastic composites: Effects of polyethylene glycol on melamine–formaldehyde shell material
2016 - IRG/WP 16-40728
Microencapsulated phase change materials (MicroPCMs) containing dodecanol were fabricated using melamine-formaldehyde (MF) or polyethylene glycol 200 modified melamine-formaldehyde (PMF) resin as the shell materials by in situ polymerization. Wood flour/high-density polyethylene (WF/HDPE) composites with MF shell MicroPCMs (MF-MicroPCMs) or PMF shell MicroPCMs (PMF-MicroPCMs) were prepared, respec...
Xi Guo, Jinzhen Cao


The Environmental Impact of Timber Products Compared to other Building Materials - A Survey of Published Environmental Product Declarations
2016 - IRG/WP 16-50314
One of the positive aspects of using wood in construction is the environmental benefits that this can potentially bring. However, manufacturers of all construction products and materials make claims about the ‘environmental friendliness’ of their products, making it exceedingly difficult for the end user to make informed choices about the advisability of using one product over another. This st...
C Hill, J Dibdiakova


Lignin-Based Adhesive for Engineered Wood Products
2016 - IRG/WP 16-50319
Lignin as a naturally occurring polyphenolic compound has an excellent potential to replace petroleum-based phenol in formulation of phenol-formaldehyde adhesive that are used in manufacturing of engineered wood products. However, there are three major obstacles in application of polymeric lignin as phenol replacement: 1) low reactivity toward phenol, 2) high molecular weight, and 3) high polydisp...
I Kalami, M Arefmanesh, E Master, M Nejad


Efficacy of lignocellulosic materials for Removal of Cation and Anions from Industrial and Urban Wastewater
2016 - IRG/WP 16-50321
The adsorption of Ca, Zn, Na, Cd (II), Cr (III) and No3 ions from industrial and urban wastewater and aqueous solutions by poplar (Populusnigra) sawdust, cotton linter, zeolite and expanded perlite were examined on the basis of a batch adsorption technique. The results revealed that application of sawdust, cotton linter, perlite and zeolite are effective in improving elimination of Ca, Zn, Na ions...
M Akhtari, M Ghorbani Kohkandeh, H Borazjani


Effects of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger
2017 - IRG/WP 17-10878
Effect of wollastonite nanofibers on biological resistance of historical paper against Aspergillus niger was studied. Specimens from A4 papers were also prepared for comparison purposes. Paper specimens were dipped in aqueous nanowollastonite (NW) with 10, 20, 30, and 40% concentrations and compared with control specimens. In order the nanofibers be fixed on paper specimens, 5% of polyvinyl acetat...
H R Taghiyari, A Kalantari, A Ershad-Langroudi, A Kalantari


Evaluation of Particulate Materials as a Physical Barrier against Termites under Floor of Experiment House
2017 - IRG/WP 17-10900
In Japan, the damages by the subterranean termites (Coptotermes formosanus and Reticulitermes speratus) are more common. Recently the more attention is paid to the less- or non-chemical methods for termite control. As a non-chemical treatment, physical barriers using particles such as gravels were investigated in terms of environmental safety, cost effectiveness, and duration of performance, and t...
Y Yanase, Y Fujiwara, Y Fujii, T Mori, T Yoshimura, S Doi


Service Life Forecasting and Planning – Why, and Concepts to do it
2017 - IRG/WP 17-20625
The importance of the building and construction sector in society cannot be overestimated. It is globally the major industry sector, a main contributor to gross domestic products, a dominant employer, and the main consumer of material resources and energy. The environmental impact of constructing, running and demolishing the built environment is huge. The products of construction are normally long...
C Sjöström