Kinetic Water Vapour Sorption of Sitka Spruce at Variable Temperature Using the Parallel Exponential Kinetics Model
2010 - IRG/WP 10-40512
In this study the water vapour sorption of Sitka spruce (Picea sitchensis (Bongard) Carr.) was measured using a Dynamic Vapour Sorption (DVS) apparatus and then analysed using the parallel exponential kinetics (PEK) model. The water vapour sorption rate of wood quickly increased when the relative humidity was changed. With the elapse of time, the sorption rate gradually decreased within any specif...
Yanjun Xie, C Hill


Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Effect of Nano-Silver Treatment on Densified Wood Properties. Part One: Swelling, Recovery Set, Bending Strength
2010 - IRG/WP 10-40533
In this research the effect of Nano-Silver treatment on compressed wood properties, was studied. Wood specimens were cut from Popolus alba (poplar) and impregnated with Nano-Silver and water. Then the saturated samples were compressed through radial direction in a hot press under pressure of 6 MPa, for 1 and 4 hours. The temperatures of press were 150°C and 175°C. Swelling (24h), recovery set ...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khaje


Comparative Study of Heat Treatment of Beech Wood in Hot Water and Steam Medium
2010 - IRG/WP 10-40536
Heat treatment of wood is an effective method to improve the dimensional stability and durability against biodegradation. Heat treatments of beech wood in 2 different mediums (hot water and steam) in 180ºC were compared in physical, mechanical and anatomical properties. Mass loss in hydrothermally treated wood was higher than hygrothermally treated samples. Mechanical properties (MOR, MOE and CS)...
A Talaei, K Yaghoobi, A N Karimi


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Study of properties and application of Paulownia in wood industries
2011 - IRG/WP 11-40560
Important of required raw material supply regarding constraint in harvesting, increasingly population, change in consumption pattern and increasingly focus on wood products and per capita in consumption is obvious for anyone. Paulownia is a marvelous tree species with its characteristics of fast-growing, good Wood quality, multiple uses, wide-ranged distribution, easy propagation, deep root system...
M Akhtari


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Determination of Izod Impact Strength on Wood: A Suitable Method to Detect Fungal Decay in Protective Effectiveness-Screenings of Wood Preservatives
2012 - IRG/WP 12-20484
For testing a large number of different substances regarding fungicide properties, the reduction of the decay test duration is advantageous. In the present paper the suitability of a method for testing plastics using an impact testing machine was examined. The results clearly show that the fungal attack of European beech by the white-rot fungus Trametes versicolor leads to a decrease of izod imp...
H Delenk, M Zauer, A Wagenführ


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


KERUING and APITONG: A Timely Review of the Perfect Choice Wood Species for Crossarms and Brace Arms, Including Data on Copper Naphthenate Treatments
2012 - IRG/WP 12-40603
Apitong or the wood species more commonly known as Keruing is an important tropical hardwood known for its high strength to weight ratio and its reasonable durability and preservative treatability. This wood has been exported from managed permanent forest estates in Malaysia into the United States for over 4 decades for its widespread use in wooden utility industry brace arms and crossarms, yet cu...
A Wong, M Freeman


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Changes of fungicidal, mechanical and sorption properties of wood during above ground outdoor exposure
2013 - IRG/WP 13-20513
The aim of this preliminary study was to investigate differences in mechanical, fungicidal, and sorption properties of four different wood species (sweet chestnut (Castanea sativa), common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in the 3rd use class (CEN, 1992) for periods between 4 and 30 months...
N Thaler, M Humar


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Copper leaching from copper-ethanolamine treated wood during exposure to terrestrial microorganisms
2013 - IRG/WP 13-30621
Copper-ethanolamine based wood preservatives are still the most important solutions for protection of wood in ground applications in Europe. Wood in ground is exposed to variety of organisms, which can act synergistically. In order to simulate these conditions in laboratory, Scots pine (Pinus sylvestris) specimens impregnated with copper-ethanolamine preservative of three different concentrations ...
M Humar, N Thaler, B Lesar


Glue-bond strength of simul (Bombax ceiba) plywood made of Neem (Azadiracta indica) leaves treated veneers
2013 - IRG/WP 13-40647
The glue-bond qualities of plywood made of treated simul (Bombax ceiba) veneers were investigated. The veneers were treated with cold and hot water solution of neem (Azadiracta indica, A. Juss.) leaves of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated simul plywood ...
K Akhter, M A Hashem, S Akhter


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Douglas-fir PSL Treated with Oilborne Copper Naphthenate – Treatment Experience & Efficacy
2014 - IRG/WP 14-40687
Treating characteristics, field stake efficacy and the results from treatment trials for oilborne copper naphthenate (CuNap) and Douglas-fir parallel strand lumber (PSL) are summarized in this paper. Treatment with a P9 Type-C based solution in laboratory tests showed full cross section penetration of large cross sections could be achieved. Commercial treatment trials using a P9 Type-A solution ...
G P Merrick


The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with preservatives is unavoidable to ensure the desired service life. However, chemical treatment of wood can result in changes of its mechanical ...
M Humar, D Kržišnik, C Brischke


Investigation of Dimensional Stability and Coating Performance of Different Heat-Treated Poplar Wood Before and After Accelerated Aging
2015 - IRG/WP 15-40702
In this investigation, coating performance of heat-treated poplar wood (Populus tremuloioes) in different environments, before and after accelerated aging was studied. Specimens with 150×100×20 mm and 20×20×20 mm in dimensions were prepared. Heat treatments were performed in air, steam and linseed oil media. Specimens were coated by alkyd based stain. Adhesion strength before and after aging, ...
A Talaei, D Ansari Movahed, G Rassam


The influence of log soaking temperature and thermal modification on the properties of birch veneers
2016 - IRG/WP 16-40749
In veneer manufacture the logs are routinely soaked in heated water baths in order to soften the wood prior to peeling. The temperature of the water may vary greatly between batches; however, the influence of log soaking temperature on veneer properties has had little research attention. Uncontrolled moisture is known to cause problems in wood-based materials, while thermal modification offers a m...
S Källbom, K Laine, M S Moghaddam, A Rohumaa, K Segerholm, M Wålinder


Effect of Furfurylation on Shear Strength of Bond Line and Screw Withdrawal Resistance of Beech and Fir Wood
2016 - IRG/WP 16-40757
The aim of this study was to investigate the effects of furfurylation on shear strength of bond line and screw withdrawal resistance of beech (Fagus orientalis) and fir (Abies alba) species. In this regard, specimens with two different values of furfurylation i.e. low (fir 14% and beech 20%) and high (fir 38% and beech 65%) levels were prepared and evaluated in comparison with untreated specimens....
A Talaei, H Abdolzadeh, M Saleh Zare


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


Impact of heat treatment on physico-mechanical properties of torrefied Antholceistha djalonensis wood
2017 - IRG/WP 17-40811
Thermal modification at relatively high temperatures is an effective method to improve the dimensional stability and mechanical properties of wood. This study was carried out to investigate the impact of heat treatment on the physic-mechanical properties of torrefied Anthocleistha djalonensis wood. Thirty nine defect-free specimens of dimensions 20 mm × 20 mm × 60 were prepared for the determina...
E A Iyiola, B Olufemi, J A Fuwape, J M Owoyemi


Validation by micro-computed tomography of an assessment method to measure the residual strength of anobiids infested timber
2019 - IRG/WP 19-20650
In this article a quantitative correlation study of pine timber structural elements, which have been subject to attack by anobiids, is presented. The main objective of the study was to establish a valid empirical correlation between the lost material percentage (consumed by beetles) and original/residual apparent density. Since the beetles’ attack produces a diffuse damage with a set of tunnels ...
J L Parracha, M F Pereira, A Maurício, P Faria, L Nunes


Influence of weathering on the mechanical properties and performance of exterior wood coatings
2022 - IRG/WP 22-40951
Three commercial coatings were exposed to artificial (EN 927-6) and natural weathering (EN 927-3) on wood samples. Cracking was visually assessed as well as Persoz hardness. Free films of the same coatings were also exposed to the same weathering tests before their tensile properties were measured. Results show that artificial and natural weathering modified the overall mechanical properties of wo...
L Podgorski, J-D Lanvin


Previous Page | Next Page