Field Test Results after Nine Years for CCA and ACQ Preservative-treated Wood Fixed in Different Climates
2003 - IRG/WP 03-30303
During assessment of the ground contact stakes in the Norwegian test field, we have frequently found that the first visual rot attack is in the zone of the stakes, where the stakes have been in contact with each other during the fixation. These parts are usually light green, caused by the lack of light during fixation, compared to the rest of the stake surface, which has a darker colour. To inves...
F G Evans


Influence of bark damage on bluestain development in pine logs
1997 - IRG/WP 97-10197
Mechanized harvesting of conifers can lead to extensive bark damage, with the resulting wounds providing suitable entry points for bluestain fungi that are not associated with bark beetle vectors. However, the amount of bluestain colonisation can vary greatly between the different types of wound. To evaluate the effect of wound type seven different types of wounds were artificially created on fres...
A Uzunovic, J F Webber, D J Dickinson


Disposal of treated wood - Canada
1990 - IRG/WP 3563
It is estimated that treated wood removed from service each year in Canada contains about 16,000 tonnes of creosote, 1000 tonnes of pentachlorophenol and 245 tonnes of CCA or ACA. The amount of CCA treated wood for disposal is expected to increase more than ten-fold by the year 2020. At present, most treated wood is disposed of in landfills, burned (creosote only) or recycled as other products. Ot...
P A Cooper


A field test with Benzotar, an industrial residue, as a wood preservative
1985 - IRG/WP 3349
Benzotar, a residue of production of benzoic acid, was tested in field as a wood preservative. Results, after 6.5 years of exposure, showed that this product presents properties that improve the performance of wood in ground contact. This paper describes these results and presents a discussion an some aspects of its potential utilization in Brazil....
S Milano, L R Silva


Checking of sodium pentachlorophenate fixation in wood
1990 - IRG/WP 3620
In order to estimate the volatilization of sodium pentachlorophenate from treated wood, wood samples treated with pentachlorophenate were analysed after various durations of an EN 73 weathering The results giving no clear evidence of volatilization, treated wood samples were put in a test chamber with precise climatic conditions, the air used in the experiment being analysed. The pentachlorophenat...
M Lamour, H Sageot


Measurement of VOC emissions from curative treated wood: A new emission test chamber
2001 - IRG/WP 01-50166-13
A poor indoor air quality (IAQ) is now recognized as a potential factor affecting occupants health. There are three basic strategies to improve IAQ: source control, improvement of the ventilation and use of air cleaners. Usually, the most efficient way to improve IAQ is to eliminate the different pollutant sources or to reduce their emissions. In order to precisely measure emissions from building ...
F Maupetit, O Ramalho, C Yrieix


Bioconversion of wood wastes into gourmet and medicinal mushrooms
1999 - IRG/WP 99-50129
Increased wood wastes, including thinned material from stagnated and overstocked small-diameter forests, are a menace to forest health, to the sustainability of ecosystems, and to community economic viability. The objective of this study is to recycle wood wastes into value-added products, such as gourmet and medicinal mushrooms, by using the white-rot basidiomycetes, Pleurotus ostreatus, P. popul...
S C Croan


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen


The more important wood-destroying insects found in buildings in Poland
1974 - IRG/WP 128
In the different regions (voievodships) of the country Anobium punctatum and Anobium pertinax were to be found in the range of 47.7 to 63.5%. These insects were the main pests in urban buildings. In the second place came Hylotrupes bajulus occurring in the range of 25.9 to 45.1%. The other insects were to be found within the limits of 0.1 to 10.0%; only in a single instance did the amount reach 24...
J Dominik, J Wazny, M Czajnik


The First Annual Report of the International Research Group on Wood Preservation 1969-1970
1970 - IRG/WP A 7
IRG Secretariat


Cleaner prodiction and the wood preserving industry
1995 - IRG/WP 95-50040-29
H Carr-Harris, C R Coggins


Work program of CEN/TC 38 (January 1994). Durability of wood and derived materials
1994 - IRG/WP 94-20019
R Hüe


The most important wood-destroying insects in various countries (Results of questionnaire)
1981 - IRG/WP 1136
M-M Serment


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Standardisation of tests of toxicity of preservatives to soft rot fungi
1978 - IRG/WP 2119
J G Savory


Wood preservation in China
1989 - IRG/WP 3546
Huiming Zhou, Zhongwei Jin


Bacterial wood degradation by a pure culture
1995 - IRG/WP 95-10093
A single-celled bacterium isolated from lake water yielded cell wall degradation in Scots pine sapwood samples. The bacterium attacked all cell wall layers in one month of laboratory culture. It was identified as Aureobacterium luteolum....
O Schmidt


Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Environmental risk assessment of preservative treated wood
1998 - IRG/WP 98-50101-19
This paper reviews the status of the environmental risk assessment of preservative treated wood and confirms the distinction between the risks presented by wood preservatives and preservative treated wood. The paper proposes a tiered approach to risk assessment and discusses the rationale. Flowcharts are presented which summarise the tiered approach to risk assessment, show the tests required, and...
E F Baines, S J Davis


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


List of Members of IRG and contributing workers proposed for membership in IRG/WP/ - I - Sub-group 5
1976 - IRG/WP 154
S Cymorek


Wood-destroying Rhinotermitidae (Isoptera) in the oriental region
1984 - IRG/WP 1236
Species of the family Rhinotermitidae are important wood-destroying termites. From the Oriental zoogeographical region, 85 species of the family are reported of which some are wide spread and cause extensive damage to wood, wooden articles and other cellulosic products. The distribution, biology, ecology and pest status of the important wood-destroying species, in the Oriental region, are given in...
O B Chhotani


Preservative absorption response of planks of Anogeissus acuminata for plank-built catamarans
2002 - IRG/WP 02-40245
Due to shortage of timber coupled with other compelling factors, traditional fishermen along the east coast of India, especially of Andhra Pradesh, of late, are departing from conventional log type wooden catamarans. Instead, they are fabricating catamarans out of timber planks of hard woods and utilizing thermocol for buoyancy. Mostly, locally available timber of a Combretaceae species, Anogeis...
V Kuppusamy, M V Rao, M Balaji, K Rao


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek