Imaging fungal deterioration of wood using x-ray microtomography
1997 - IRG/WP 97-10240
Nondestructive tomographic images of solid Southern yellow pine (SYP) wood and SYP during deterioration by wood decay fungi were obtained by using a new class of synchrotron X-ray computed microtomography (CMT). The CMT images will provide information about spatial relationship between degrading fungi and wood structures. Wood samples were scanned with synchrotron-generated X-rays at high resoluti...
B Illman, B A Dowd


Minimum inhibitory concentration of methylene bisthiocyanate towards selected wood inhabiting fungi in liquid culture and on radiata pine
2001 - IRG/WP 01-30261
The objective of the current study was to determine the minimum inhibitory concentration (MIC) of methylene bisthiocyanate (MBT) towards wood inhabiting fungi common on unseasoned radiata pine (Pinus radiata D. Don). The fungi used were Ophiostoma floccosum, Leptographium procerum, Sphaeropsis sapinea and Trichoderma viride. Fungi were individually inoculated into nutrient media spiked with differ...
T Singh, B Kreber, C Chittenden, R N Wakeling, A Stewart


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


Comments on soft rot attack in timbers treated with CCA preservatives: A document for discussion
1982 - IRG/WP 1167
This paper is not based on any particular results but rather on several observations of soft-rot during many years of studies, and on a review of the existing literature. The short time available has unfortunately not permitted a detailed review of the literature. Data and knowledge of important facts are lacking for several aspects of soft-rot attack and for reactions occurring in the wood as a r...
T Nilsson


A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds
1989 - IRG/WP 2330
Thin veneers of Pinus radiata were treated with dilute aqueous solutions of chromium VI and iron III compounds and exposed to natural weathering for 35 days. Zero-span tensile strength and weight losses of treated veneers were compared with losses observed in untreated specimens In a study designed to demonstrate the applicability of strength and weight loss measurements to the rapid quantitative ...
P D Evans, K J Schmalzl


Co-operative studies on determining toxic values against wood-destroying basidiomycetes: Progress report to April 1990
1990 - IRG/WP 2357
This document reports progress on the co-operative study between nine laboratories, set up following the proposals contained in Document IPG/WP/2316 (1988). Results have been received from eight laboratories. Toxic values data have been established successfully for the test fungus Coniophora puteana with soil, malt agar and vermiculite methods and with the test fungi Gloeophyllum trabeum and Poria...
J K Carey, A F Bravery


Wood detection by the marine isopod Limnoria.markup
1995 - IRG/WP 95-10134
The search for alternative control methods for Limnoria, should perhaps focus on the most vulnerable stage during the isopod life cycle - during dispersal when adulls leave their tunnels to find new wood. Dispersal is known to be triggered by environmental conditions, although how Limnoria locate fresh wood is unknown. Literature available on Limnoria dispersal, their sensory capabilities during d...
S M Henderson, S M Cragg, A J Pitman


The natural history of teredinid molluscs and other marine wood borers in Papua New Guinea
1975 - IRG/WP 410
The teredinids, commonly known as teredos or shipworms, are bivalve molluscs adapted to boring into wood. They are most closely related to the Family Pholadidae, or piddocks, which bore into mud, stone and coral. The teredinids have a relatively small, hemi-spherically shaped shell, the elongated body extending beyond the posterior end of the shell valves. The soft body, protected by the wood and ...
S M Rayner


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 22: Report on the conditions of specimens at Sekondi, Ghana after 60 months
1986 - IRG/WP 4123
The results of the third inspection of CCA and CCB treated test panels exposed at Sekondi, Ghana in June 1980 are presented. None of the panels still in test, i.e. panels of Pinus sylvestris treated with CCA at 3 and 10%, Alstonia scholaris treated with CCA at 10%, Fagus sylvatica treated with CCA at 10%, and Erythrophleum ivorense and Mitragyna stipulosa both treated with CCB at 10%, shows any ex...
F F K Ampong, N Asare-Nyadu


The durability of wood polymer composites against fungi and insects
2000 - IRG/WP 00-40161
New materials such as wood polymer composites are used more in France. These materials are obtained by mixing wood and thermoplastics in different ratios. These kind of material must be considered as new materials and some characteristics such as durability must be evaluated for outdoor applications. On the other hand, some recycled fibers from wood waste could be used as raw materials. Some woodp...
G Labat, I Le Bayon, J Gerard, F Amin


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


Development and Implementation of a DNA – RFLP Database for Wood Decay and Wood Associated Fungi
2004 - IRG/WP 04-10527
We are developing Restriction Fragment Length Polymorphism (RFLP) and Internal Transcribed Spacer (ITS) sequence databases for wood decay basidiomycetes and other fungi associated with wood. These databases currently house information for 39 fungal species consisting of 9 brown-rot basidiomycetes, 12 white rot basidiomycetes, 1 soft rot, 1 stain fungi, and 16 molds or other ascomycetes or imperfe...
S V Diehl, T C McElroy, M L Prewitt


Metal plate fasteners in trussed rafters treated with preservatives or flame retardants - corrosion risks
1977 - IRG/WP 3104
In designing roof trusses employing metal plate fasteners it is generally assumed that the roof will remain dry in service. Whilst this is generally true, damp conditions do arise under some circumstances, although it is not possible to quantify the extent of the risk. It is only possible, therefore, to give general recommendations which must be interpreted in the light of local experience of serv...
R A Laidlaw, L C Pinion


Wood durability in the light of recent trends and research on the durability of building materials and components
2000 - IRG/WP 00-20195
Building-related research of today demonstrates a clear shift in focus from the design and production phases to usage and to the entire life time. A consequence is that the performance criteria of materials, components and of the entire building must be regarded over the life time rather than at the time of production or delivery. As one example can be mentioned the Building Construction Directive...
K Ödeen


Wood preservation requirements in Queensland, Australia
1983 - IRG/WP 3227
In Queensland the preservative treatment and utilization of timber must comply with the Timber Users' Protection Act. Preservative retention levels and penetration patterns must be complied with. Analytical zones are specified for removing samples for chemical analysis of preservative retention. The required retention levels have been expressed as percent weight of oven dry wood weight. T...
L E Leightley, M J Kennedy


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Proceedings of the 3rd international wood preservation symposium "The Challenge - Safety and Environment" 6-7 February 1995, Cannes-Mandelieu, France
1995 - IRG/WP 95-50040
Contains the following 35 Documents (IRG/WP 95-50040/1 - IRG/WP 93-50040/35), conclusions (summaries of the sessions chairmen) and some poster abstracts: Le pin: Matériau à contact alimentaire [Pine wood as a material for food contact] (IRG/WP 95-50040/1); The use of a physical field model to study the effects of remedially treated timber on the growth of perennial ryegrass (Lolium perenne) and...
Anonymous


Effect of post-treatment processing on leachability of ACZA-treated douglas-fir lumber
1998 - IRG/WP 98-50109
The effect of post-treatment procedures that more rapidly precipitate copper, zinc, and arsenic in douglas-fir treated with ammoniacal copper zinc arsenate (ACZA) on subsequent leaching resistance were investigated at two retentions (6.4 and 40 kg/m3). Total leaching was greater from boards treated to the higher retention. At both levels, copper was lost at the highest rate. Post-treatment process...
J J Morrell, C S Love, S Kumar, C M Freitag


Biological and chemical investigations for the assessment of the environmental impact of wood preservative components
1999 - IRG/WP 99-50127
This study was carried out in order to investigate the suitability of biological and chemical techniques to evaluate the environmental impact of wood preservatives depleted from impregnated wood. Small specimens (15*25*50 mm3) of Scots pine sapwood (Pinus sylvestris) were treated with a CCB salt. After fixation the treated and untreated samples were washed-out according EN 84, and the different le...
E Melcher, H-W Wegen


Surface characteristics of wood treated with various AAC, ACQ and CCA formulations after weathering
1991 - IRG/WP 2369
Wood samples treated with various alkylammonium compounds (AACs) as well as ammoniacal copper quat (ACQ) and chromated copper arsenate (CCA) have been studied in accelerated weathering experiments. Microscopic examination of the surfaces of these samples after exposure in a weatherometer revealed several different changes. Samples treated with didecyldimethyl ammonium chloride (DDAC) show consider...
L Jin, K J Archer, A F Preston


The involvement of extracellular substances for the generation of hydroxyl radical during wood degradation by white-rot fungi
1997 - IRG/WP 97-10218
The activities of one-electron oxidation, hydroxyl radical generation, and phenol oxidase during the incubation of cultures of four white-rot fungi containing either glucose or wood were periodically measured. Further, their degradation activities against wood were examined during the course of cultivation. The generation of hydroxyl radical was correlated to the activity of wood degradation and i...
H Tanaka, S Itakura, A Enoki


Wood preservation in Brazil
1984 - IRG/WP 3321
The report gives statistics on the wood products industries, the forest products exported, the production of treated sleepers, poles, crossarms, fence posts and other wood products in Brazil for the years 1977 to 1981. The total numbers of vacuum/pressure plants, through the years 1902 to 1984, indicate that from 1960 there has been a steady increase in treatment requirements. Most of the plants a...
M S Cavalcante, R Cockcroft


Effects of the specimen position on fungal colonisation and wood decay by en 113 test fungi
1998 - IRG/WP 98-20136
For testing wood preservatives according to EN 113 it is common practice to plant the test blocks on neutral supports in order to prevent (1) a diffusion of chemicals into the agar medium and (2) an excessive moistening of the specimens. The procedure was employed in EN 350-1 for testing the natural durability of solid wood. It turned out to be of problematic nature because of the individual requ...
G Kleist, M-T Lenz, R-D Peek


Wood preservation in Southern Africa
1984 - IRG/WP 3320
This report deals with the status of wood preservation in the countries of Southern Africa, namely Botswana, Lesotho, Mozambique, Namibia, South Africa, Swaziland and Zimbabwe. It includes some data on the timber production from the forests of these countries, as well as detailing the state of the timber products industries in South Africa which is the dominant country in the field in the sub-cont...
A Pizzi, W E Conradie, R Cockcroft