IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 160 documents. Displaying 25 entries per page.


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...
L Podgorski, G Grüll, M Truskaller, J D Lanvin, S Bollmus


Use of the durable species Coast Redwood as a reference system for field testing of Wood Protection systems
2012 - IRG/WP 12-20486
Data is provided and discussed for a number of field exposure tests where the naturally durable wood species Coast redwood, Sequoia sempervirens, was included along with untreated pine and standard preservative treatments. In general, there is potential for higher variability of results with this naturally durable species, but it does suggest that redwood can be a useful reference material for te...
A Zahora, A Preston, L Jin


Performance of Wood Protection Systems at Multiple Field Test Sites Using the Ground Proximity Test Method
2012 - IRG/WP 12-20499
A series of preservative systems were used to treat southern pine ground proximity test samples which were then exposed at a range of test sites located throughout the world. The sites were chosen on the basis of having vastly different Scheffer Climate decay indices. After almost 14 years exposure, distinct differences are apparent in how different preservative systems perform at the different ...
A Zahora, A Preston, L Jin


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


Inhibitory extractives or nutrients? Mould growth on coated heartwood and sapwood of Pinus sylvestris and Gleditsia triacanthos
2013 - IRG/WP 13-10806
Sometimes mould fungi grow over weathered coated sapwood, whereas the coated heartwood is not colonised. Two factors may be responsible for these differences: Either the larger content of nutrients in the sapwood, or the content of biocidal extractives in the heartwood. In this study the factors for the difference in mould growth on coated heartwood and sapwood of Pinus sylvestris (Scots Pine) and...
D Lukowsky, N Buddruhs


Copper Coating on Wood: a New Way of Protecting Wood
2013 - IRG/WP 13-30617
Thermal spray metal coating technology was used to apply a thin layer of copper on the surfaces of a number of wood species. The adhesion of metal coating to mahogany, oak, soft maple, spruce, white pine and medium density fibreboard (MDF) was evaluated by pull off adhesion test. The resistance of copper coated wood samples to mildew were assessed in the lab. Also, the decay resitance and water re...
M Nejad, R Shafaghi, L Pershin, J Mostaghimi, P Cooper


Performance of biocide-free preservative-protective systems modified with organosilicon compounds
2013 - IRG/WP 13-30628
The objective of the research was to determine the influence of organosilicon compounds in preservative-protective systems on the selected properties of pine wood aimed for outdoor use. The investigations were made for biocide-free systems based on alkyd resin and natural oils modified with alkylalkoxy-, amino- and glycidoxysilanes. The special attention was paid on the influence of hydrophobic pr...
B Mazela, P Hochmańska, T Krystofiak


Study of UV resistance and natural weathering of coatings on chemically modified wood
2013 - IRG/WP 13-40629
In this study, UV resistance and weathering performance of rubberwood (Hevea brasiliensis) and radiata pine (Pinus radiata) modified with benzoyl chloride and acetic anhydride was studied. Performance of polyurethane based wood coatings on modified wood was also evaluated. Unmodified and chemically modified specimens were exposed to accelerated and natural weathering. Modified and unmodified woo...
K K Pandey, K Srinivas


Protective effectiveness of antifouling coatings for wooden boats in the Northern Adriatic Sea
2013 - IRG/WP 13-40634
There are various conventional biocide containing antifouling coatings and some more environmentally friendly paints for boats on the market. However, the question of their performance in accordance with the manufacturers’ statements or guaranties arises. The aim of our preliminary investigation was to state which type of antifouling coating exhibits better effectiveness against fouling organism...
M Petrič, M Humar, J Adamek, B Kričej


Influence of coatings on water uptake of wood surfaces before and after natural and artificial weathering
2013 - IRG/WP 13-40641
Liquid water absorption of wood surfaces with and without coating, before and after exposure to artificial and natural weathering has been studied. Spruce, oak and sapele samples have been exposed to the cycle of EN 927-6, to the cycle of the Gardner wheel and to natural weathering. Five coatings were tested including solventborne and waterborne, semi-transparent and opaque products. Exposure to w...
L Podgorski, S Collignan, J-D Lanvin


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


CreoSub – New protection technology to substitute creosote in railway sleepers, timber bridges, and utility poles
2014 - IRG/WP 14-30644
Creosote oil is one of the oldest industrially used wood preservatives. Due to its toxic profile, the European Commission has restricted the use of creosote specific applications, but it is highly controversial within the European Commission. Its approval for use after 2018 is very questionable and may depend on derived research results until then, i.e., the viability of alternatives developed to ...
U Hundhausen, K-C Mahnert, A Gellerich, H Militz


Effect of polyurea coatings on performance of Douglas-fir in tropical above ground exposures
2014 - IRG/WP 14-40665
The potential for using polyurea barriers to limit fungal and termite attack was investigated on Douglas-fir lumber and timbers. Termites were capable of penetrating the barrier to attack non-treated wood as well as wood dip-treated with disodium octaborate. The coatings were also exposed above ground for 48 months in Hilo Hawaii. Samples were dissected to detect internal decay. Coated non-trea...
S Uysal, J J Morrell


Encapsulation Systems Combined with DOT Borate Treatments – The Future of Treated Crossties
2014 - IRG/WP 14-40670
Borates have been utilized in wood protection systems for many decades but only recently have been used in North America to treat crossties. This colorless, ordorless and very effective wood protection chemical has the ability to arrest and prevent the colonization of wood by both basidiomycete decay fungi and insects such as beetles and termites while ties are air seasoning or in service. Since ...
S C Kitchens, T L Amburgey


Lignin Modification to Produce Sustainable Polyurethane Resin for Wood Coatings
2014 - IRG/WP 14-40682
The use of lignin as the most abundant aromatic natural polymer has been evaluated for use in the production of lignin-based polyurethane resin for coating applications. Coatings are made of resins (ca. 50%), which today are mainly derived from petroleum-based polymers. This study is focused on the development of an environmentally friendly method of modifying lignin to be used as source of natura...
M Nejad, M Arefmanesh, S Chandra, J Mostaghimi, E Master


Buffered Amine Oxide Treatment Systems for Ammonical Copper Wood Preservatives
2014 - IRG/WP 14-40685
Wood is the most versatile, practical and sustainable building material in the world. In modern countries, wood is a well-managed renewable resource that has a small carbon footprint. Wood does suffer from a lack of durability against invasive organisms such as insects and fungi. Steel, aluminum and composites have emerged as viable alternative building materials. These sectors market the defi...
R W Clawson Jr


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


Bio-friendly preservative systems for enhanced wood durability - the first periodic report on DURAWOOD
2015 - IRG/WP 15-30677
The objective of the paper is the DURAWOOD scientific project carried out within Polish-Norwegian Research Programme, which lasts from September 2013 till August 2016. The aim of the project concentrates on the developing of a new, eco-friendly and biocide-free wood protective systems as an alternative to traditional, commonly used preservatives or coatings, containing biocides. Several wood prese...
B Mazela, M Broda, W Perdoch, L Ross Gobakken, I Ratajczak, G Cofta, W Grześkowiak, A Komasa, A Przybył


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


Application of nanoparticles of silver and nanoparticles of titanium dioxide in reinforcement of wood and coating for wood in Costa Rica
2015 - IRG/WP 15-40698
Wood is one of the most widely used materials in last 20 years by society in many applications, with a considerable proportion of this material coming from forest plantations. Plantations usually produce timber with reduced strength properties and low natural durability. On the other hand, nanotechnology applications have the potential to increase wood properties. Likewise, nanotechnology cannot o...
A Berrocal Jiménez, R Moya Roque, A Lucrecia Rodríguez, J R Vega Baudrit


How to Increase the Lifespan of Exterior Wood Coatings
2015 - IRG/WP 15-40700
In addition to aesthetic appeal, coatings are designed to protect the wood from weathering degradation in outdoor conditions. This paper gives an overview of the effects of main components of coating, coating properties, and wood treatments on coating performance. Understanding how different type of resins (alkyd, acrylic or polyurethane), amount of pigments, type of solvents (organic or water), a...
M Nejad


Previous Page | Next Page