IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 258 documents. Displaying 25 entries per page.


Using hyperspectral imaging to detect and quantify mould and blue stain on coated and uncoated wood
2014 - IRG/WP 14-10822
Hyperspectral imaging has been applied on the surface of samples of coated and uncoated Norway spruce (Picea abies) as a new technique to detect and quantify growth of mould and blue stain fungi. Principal Component Analysis of the hyperspectral images resulted in a clear visualization of the fungi and the amount of mould coverage could be estimated. This indicates that NIR hyperspectral imaging c...
L Ross Gobakken, I Burud, A Flø, K Kvaal, T K Thiis


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


Study of the effectiveness of wood products for permanent protection against Fusarium circinatum
2014 - IRG/WP 14-30655
In Europe there exist a number of quarantine organisms that affect conifer forests, including Fusarium circinatum Nirenberg et O'Donnell (telemorph: Gibberella circinata Nirenberg et O'Donnell), a quarantine organism in Europe producing the disease known as pitch canker of pines. For a decade, the European Union has taken steps to locate and eradicate the pathogen with the aim of elimina...
M T Troya, M Conde, R Raposo, F Llinares, M Elvira-Recuenco


Influence of Exposure Direction on Leaching of a Biocide from Painted Wood Surfaces
2014 - IRG/WP 14-50303
The objective of this project was to investigate the influence different exposure directions – North, East, South and West on the cumulative quantity of a biocide leached from painted wood surfaces due to rainfall and the consequences for the risk assessment. The study included a solvent-borne primer without biocides and a topcoat protected with a biocidal active substance. Both products were a...
M Klamer


Effect of polyurea coatings on performance of Douglas-fir in tropical above ground exposures
2014 - IRG/WP 14-40665
The potential for using polyurea barriers to limit fungal and termite attack was investigated on Douglas-fir lumber and timbers. Termites were capable of penetrating the barrier to attack non-treated wood as well as wood dip-treated with disodium octaborate. The coatings were also exposed above ground for 48 months in Hilo Hawaii. Samples were dissected to detect internal decay. Coated non-trea...
S Uysal, J J Morrell


Lignin Modification to Produce Sustainable Polyurethane Resin for Wood Coatings
2014 - IRG/WP 14-40682
The use of lignin as the most abundant aromatic natural polymer has been evaluated for use in the production of lignin-based polyurethane resin for coating applications. Coatings are made of resins (ca. 50%), which today are mainly derived from petroleum-based polymers. This study is focused on the development of an environmentally friendly method of modifying lignin to be used as source of natura...
M Nejad, M Arefmanesh, S Chandra, J Mostaghimi, E Master


Biocidal Products Regulation – Structure and Impact for Product Authorization and Testing in EU
2014 - IRG/WP 14-50308
Since September 2013 the Biocidal Products Regulations (BPR) has been in force in Europe. BPR replaces the Biocidal Products Directive (EC/98/8) and in some respect marks a turning point in the European legislation concerning registration of all types of biocides. BPR introduces some changes both for suppliers of active substances and for companies that produce and place biocide containing wood p...
M Klamer


Development of a rapid screening method to determine the susceptibility to mould growth of novel construction and insulation products
2015 - IRG/WP 15-20562
Wood-based materials are commonly used in building construction/insulation as a replacement for solid timber. However, these materials are susceptible to microbiological growth and different environmental conditions influence the vulnerability of wood-based materials. Moulds are a common problem found within homes and cause aesthetic damage, health problems and can increase material vulnerability ...
B K Stefanowski, S F Curling, E Mansour, G A Ormondroyd


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


The situation of the industrial protection of wood in Argentina (La situación de la protección industrial de la madera en Argentina)
2015 - IRG/WP 15-30675
Argentina holds 33 million hectares of native forests and 1.2 million hectares of cultivated forests, which make it the 3rd Latin American country with the largest surface of cultivated forests of the region. (Ministry of Industry, 2012). The industrial impregnation of wood through vacuum pressure was first implemented in our country in the year 1932, and currently there are over 100 active plants...
D A Gherscovic


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


Application of nanoparticles of silver and nanoparticles of titanium dioxide in reinforcement of wood and coating for wood in Costa Rica
2015 - IRG/WP 15-40698
Wood is one of the most widely used materials in last 20 years by society in many applications, with a considerable proportion of this material coming from forest plantations. Plantations usually produce timber with reduced strength properties and low natural durability. On the other hand, nanotechnology applications have the potential to increase wood properties. Likewise, nanotechnology cannot o...
A Berrocal Jiménez, R Moya Roque, A Lucrecia Rodríguez, J R Vega Baudrit


How to Increase the Lifespan of Exterior Wood Coatings
2015 - IRG/WP 15-40700
In addition to aesthetic appeal, coatings are designed to protect the wood from weathering degradation in outdoor conditions. This paper gives an overview of the effects of main components of coating, coating properties, and wood treatments on coating performance. Understanding how different type of resins (alkyd, acrylic or polyurethane), amount of pigments, type of solvents (organic or water), a...
M Nejad


Investigation of Dimensional Stability and Coating Performance of Different Heat-Treated Poplar Wood Before and After Accelerated Aging
2015 - IRG/WP 15-40702
In this investigation, coating performance of heat-treated poplar wood (Populus tremuloioes) in different environments, before and after accelerated aging was studied. Specimens with 150×100×20 mm and 20×20×20 mm in dimensions were prepared. Heat treatments were performed in air, steam and linseed oil media. Specimens were coated by alkyd based stain. Adhesion strength before and after aging, ...
A Talaei, D Ansari Movahed, G Rassam


Durability of reaction to fire performance of FRT wood products in different end use applications – Methods and results
2015 - IRG/WP 15-40705
Fire retardant treatments (FRT) may considerably improve the reaction to fire properties of wood-based products and the highest fire classifications for combustible products can be reached, but the maintained reaction to fire performance e. g. in exterior applications needs to be addressed in order to form a basis for new and reliable wood products with improved fire performance. A European Techn...
B Östman, L Tsantaridis


On the effect of climate and exposure conditions on durability indicators and their potential for service life prediction of wood-based products
2016 - IRG/WP 16-20576
In order to encourage increased use of wood, different user groups need to be better informed regarding the variation in performance between different wood materials and the effect of different use classes. It is also important to provide good empirical data on the service life of wood products as input to for example life cycle assessment studies. In the current study the effect of temperature an...
G Alfredsen, C Brischke, P-O Flæte, M Humar, L Meyer-Veltrup


Accelerated Weathering Performance of Impregnated Wood Samples Coated with Zinc by Means of Plasma-Assisted Particle Deposition
2016 - IRG/WP 16-30682
Many different methods are currently applied for wood protection against outdoor conditions. The most important of these is the process of impregnation with liquid substances. However, this kind of wood preservatives cannot provide a long-term protection of wooden surfaces. Weathering-resistant surfaces can be obtained by applying UV absorbing agents. In this study, the influence of zinc particles...
A Can, H Sivrikaya


The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durability and reputation. This research was conducted to assess the decay resistance of CLT and OSB (oriented strand board) in an accelerated trial...
T Singh, D Page


Variation in coating hardness during the EN 927-6 weathering test: influence of pigmentation
2016 - IRG/WP 16-40739
The objective of the SERVOWOOD project is to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. Within this project an extensive round robin exercise has been carried out by five partners to establish the repeatability and reproducibility of the EN 927-6 artificial weathering test. This round robin included the exposure of the I...
L Podgorski, L Malassenet, C Reynaud


Durability of Thermally Modified Engineered Wood Products
2016 - IRG/WP 16-40745
In this study, rated plywood, oriented strand board (OSB), laminated strand lumber (LSL), and laminated veneer lumber (LVL) were thermally modified as a post-treatment at 140 °C, 150 °C, 160 °C, 170 °C, and 180 °C using a closed, pressurized treatment method. Eastern larch OSB manufactured from heartwood and sapwood was also thermally modified as a post-treatment at 160 °C and 180°C. All ...
H M Barnes, M D Aro, A Rowlen


Development of methodologies to evaluate tanning blocking coatings
2016 - IRG/WP 16-40760
In Europe an increased interest in using home-grown hardwoods as sustainable and renewable construction materials started a few years ago. Amongst these species oak and chestnut are two interesting candidates as their heartwood contain a significant amount of tannins which contribute to their natural durability. To avoid wood greying and dimensional variations, oak and chestnut must be protected b...
C Reynaud, L Podgorski


The Environmental Impact of Timber Products Compared to other Building Materials - A Survey of Published Environmental Product Declarations
2016 - IRG/WP 16-50314
One of the positive aspects of using wood in construction is the environmental benefits that this can potentially bring. However, manufacturers of all construction products and materials make claims about the ‘environmental friendliness’ of their products, making it exceedingly difficult for the end user to make informed choices about the advisability of using one product over another. This st...
C Hill, J Dibdiakova


Decontamination of sludges, liquids and soils polluted by “class 1, 2 & 3a” and “temporary” wood treatment products from dipping tanks
2016 - IRG/WP 16-50315
Wood is one of the most widely used building materials as it is easy to find and process. As an organic material, time leads to a degradation of its substance, and even more so when it is exposed to pathogens such as fungi, bacteria and insects. In order to try and inhibit this phenomenon, several preservation treatments have been developed and applied thanks to the production of chemical biocides...
A Zaremski, E Wozniak, S Maman, C Zaremski, S Morel


Lignin-Based Adhesive for Engineered Wood Products
2016 - IRG/WP 16-50319
Lignin as a naturally occurring polyphenolic compound has an excellent potential to replace petroleum-based phenol in formulation of phenol-formaldehyde adhesive that are used in manufacturing of engineered wood products. However, there are three major obstacles in application of polymeric lignin as phenol replacement: 1) low reactivity toward phenol, 2) high molecular weight, and 3) high polydisp...
I Kalami, M Arefmanesh, E Master, M Nejad


Previous Page | Next Page