Ponding of radiata pine (Pinus radiata) - 1. The effect of bacteria on wood
1998 - IRG/WP 98-10265
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks were examined by light microscopy, confocal laser scanning microscopy (CLSM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) for bacterial colonisation of wood and degradation of pit membranes. After 2 weeks of ponding bacteria colonised the outer few cells of wood, ...
A P Singh, Y S Kim, U Schmitt, B S Dawson


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 5: Effect of wood species and preservative composition on the leaching during storage
1975 - IRG/WP 354
Conversion reactions during storage of CCA treated wood take place even at and below the fiber saturation point as long as ion transport is possible. Increase in drying temperature increases the final pH of the treated wood and the leachability of Cu and decreases slightly the leachability of Cr, while the leachability of As is not affected. This temperature effect is considered to be of no techni...
S-E Dahlgren


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Dimensional lumber model demonstrates the sensitivity of the particle capture immunoassay in early detection of brown-rot fungi
1995 - IRG/WP 95-20058
A dimensional lumber model was designed to test the sensitivity of the particle capture immunoassay (PCI) compared to traditional methods of culturing and microscopic examination for detection of brown-rot fungi. Southern yellow pine 2 x 4's (5.1x10.2 cm²), and 86.4 cm in length, were inoculated on one end with the brown-rot fungus, Postia placenta, and tested over the full length of the...
C A Clausen, L Ferge


Severe decay damages of bridges made of ekki (Lophira alata) wood known as a durable species
2000 - IRG/WP 00-10383
Bridges made of ekki (azobe, bongossi, Lophira alata Banks et Gaertn.) timbers were severely decayed only 10 years after the construction possibly caused from no maintenance for the periods. The reason of no maintenance is due to the misunderstandings on wood durability against wood-decaying fungi. Some civil-engineers and architectures understand "durable species" means "absolutely decay-durable ...
S Doi, T Sasaki, Y Iijima


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


The influence of fungi causing blue – stain on absorptiveness of Scotch pine wood
2005 - IRG/WP 05-10565
The blue-stain fungi cause discoloration of the wood. In the course of their development in wood may have an effect on wood structures and properties influenced on its use value. Investigation has been undertaken to clear the influence of blue-stain fungi on wood absorptiveness as indicators for the wood ability to impregnation with water diluted wood preservatives. The wet sapwood samples of fres...
A Fojutowski


Advances in understanding the mode of action of methylene bisthiocyanate against Sphaeropsis sapinea
2002 - IRG/WP 02-30284
The importance of arresting sapstain pre-infection in radiata pine in New Zealand, to prevent downstream sapstain in both logs and sawn timbers has been clearly demonstrated. Efforts are being made to improve the efficacy of diffusible antisapstain agents through improved understanding wood/fungicide/fungus interactions. The mechanism of action of methylene bisthiocyanate (MBT) was investigated u...
T Singh, R N Wakeling, B Kreber, A Stewart


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Effect of humic acid on leaching of CCA from treated wood
2000 - IRG/WP 00-50151
Laboratory studies indicate that relatively high concentrations (1.000 - 10.000 ppm) of humic acids can increase the leaching of chromium and copper from CCA-C treated wood, and that copper is most affected. They also show that leaching with natural water samples can result in higher leaching of all components than leaching with distilled water. Evaluation of CCA component retentions and mass bala...
P A Cooper, D Jeremic, J L Taylor, Y T Ung


Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen


On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson


A laboratory study on effect of coating materials on leaching of copper from CCA treated wood
2001 - IRG/WP 01-50176
Components of CCA preservatives can leach into surrounding soil and water and have some effect on germination and growth of some plants. In this report, the effect of coating materials in reducing chemical concentration in the leachate were evaluated. Rubber wood blocks (Hevea brasiliensis) treated with CCA were fixed at room temperature at high humidity. After air dried, they were painted with co...
A Veenin, T Veenin


Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger
1977 - IRG/WP 2125
Ziel der vorliegenden Arbeit war der Vergleich der in verschiedenen Ländern zur Bestimmung der pilzwidrigen Wirksamkeit von Holzschutzmitteln gegen Moderfäule-Erreger angewandten Methoden. Als Vergleichsmaterial dienten drei normierte Methoden: die britische (42), skandinavische (45) und die in der DDR angewendete (47) sowie wichtige, von verschiedenen Fachleuten ausgeführte Arbeiten experiment...
J Wazny


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Differential susceptibility of living and dead timber to colonisation by sapstain and mould fungi
1998 - IRG/WP 98-10288
Field studies have revealed that when timber is irradiated (i.e. killed) it is more susceptible to colonisation by mould fungi than sapstain fungi. By comparison, freshly sawn timber shows very little mould colonisation, tending to be colonised by sapstain fungi. It appears, therefore that the physiological state of the wood may influence the pattern of colonisation. A laboratory trial was underta...
J R Williams, D J Dickinson, J F Webber


Micromorphology of Schizophyllum commune attack in pine (Pinus sylvestris) wood
1983 - IRG/WP 1184
The decay pattern caused by Schizophyllum commune in pine latewood tracheids was studied using both light and transmission electron microscopy. The attack began as isolated concentric slits within the S2 layer with extensive lamellation and separation of individual wall layers observed in subsequent stages of decay. The slits resulting from attack appeared to be formed in thin, regular concentric ...
T Nilsson, G F Daniel


Effect of bioextracts on colonisation of radiata pine sapwood by three sapstain fungi
2003 - IRG/WP 03-10485
The objective of this study was to investigate the effect of aqueous bioextracts prepared following two-week incubation of forest soil, garden compost and chicken manure respectively, on the ability of Ophiostoma flocossum, Leptographium procerum and Sphaeropsis sapinea to colonise unseasoned radiata pine sapwood. The research showed that all bioextracts tested retarded the rate of fungal colonis...
J van der Waals, C Chittenden, B Kreber


Water-Borne Copper Naphthenate: An Emerging Wood Preservative
2002 - IRG/WP 02-30280
Waterborne copper naphthenate (WB Cu-N) was used to treat southern yellow pine (Pinus spp) and red maple (Acer rubrum) stakes. The treated stakes were exposed in test sites located in Florida, Michigan and Mississippi for 3 to 6 years. Copper Chromium Arsenate (CCA), Ammoniacal Copper Quat (ACQ) and Oil-borne Copper Naphthenate (OB Cu-N) were also used to treat some stakes for comparison. Results...
P Nzokou, D P Kamdem, M H Freeman


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


The Protection of Wood with Oxy-aluminium Compounds
2002 - IRG/WP 02-30286
Wood inorganic composites (WICs) containing aluminium compounds were developed and tested in relation to some essential requirements of preservative treated wood. Four different oxy-aluminium treatments were developed and identified according to the final insoluble compounds formed (sodium aluminate, aluminium hydroxide, magnesium aluminate and aluminium borate) in wood. Vacuum impregnation or dou...
F A Ximenes, P D Evans