Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


A study of the decay type potential of seven soils
1992 - IRG/WP 92-1539
The aim of this experiment was to determine the significance of the fungal inoculum potential and physico-chemical properties of five field trial test site soils, a garden compost known to cause white rot in copper treated fence palings, and soil from a zone between 2 and 15 centimetres from a CCA treated post with brown rot, in causing differential decay type in Pinus radiata and Poplus deltoides...
R N Wakeling


Investigation of temperature effect on fixation of Celcure preservative (ACC) in beech (Fagus orientalis)
2001 - IRG/WP 01-40200
In this research, the fixation speed of Celcure 2% (ACC) preservative salt, under temperature of 17°C, 27°C and 50°C, on intact and stained wood specimens of beech was investigated. For this purpose, blocks of wood with 5x5x7 cm dimensions were prepared and saturated with 2% ACC concentration by full-cell process. The specimens were put in three incubators at the above-mentioned temperatures. F...
A Karimi, M Ghorbani


Performance of boron and fluoride based rods as remedial treatments in Douglas-fir poles
1995 - IRG/WP 95-30070
Boron and fluoride are widely used for remedial internal treatments, but their use in North America has been limited. Recently, however, interest in these chemicals has increased as the result of concerns about the risks of fumigant usage. The performance of boron or a boron/fluoride combination was assessed in Douglas-fir poles over 1 to 3 year periods. Both chemical formulations diffused well th...
J J Morrell, P F Schneider


The implementation of restrictions on the use of arsenic and chromium based wood preservatives in Sweden
1995 - IRG/WP 95-50062
In 1992 the Swedish National Chemicals Inspectorate introduced restrictions on the use of wood treated with arsenic and/or chromium based wood preservatives. Such wood is now in principle only allowed for use in ground contact or in water. These restrictions have had considerable influence on the use of wood preservatives for sawn timber for the Swedish domestic market. Thus only 35% of the preser...
J Jermer, M-L Edlund, K Nilsson


Effect of angle of exposure on degradation of radiata pine during weathering trials
1988 - IRG/WP 2301
The importance of angle of exposure on the degree of weathering of materials has not been adequately resolved. In conventional tests, specimens are exposed at an angle of 45° facing the equator, but more recently experiments on polymeric materials have suggested that an angle of 0° may be preferable since this angle maximises levels of received ultra-violet radiation. In this paper the degradati...
P D Evans


Délavabilité de bois ronds traités avec un sel CCA dans des conditions réelles de stockage. Incidence pratique de la fixation accélérée par étuvage. Impact effectif sur l'environnement
1993 - IRG/WP 93-50001-23
Un essai de terrain a été organisé pour mesurer concrètement, dans des conditions aussi proches que possibles des conditions réelles de terrain, les pertes effectives en produit de traitement lorsque le bois traité est soumis à des intempéries. L'essai a été conduit sur des bois ronds (poteaux), traités en autoclave par procédé Bethell avec un sel CCA de type C, avec comme fi...
M Rayzal, F Larroze


Generic code of good practices for wood preservation facilities
1994 - IRG/WP 94-50037
Wood preservation chemicals are designed to be toxic to wood destroying organisms. This toxicity, however, may not be limited to target organisms but the use of these chemicals can potentially harm various biota and humans as well. This fact dictates that adequate precautionary measures be employed to prevent any harmful effects to humans and the environment. The extensive experience with wood tre...
V N P Mathur, G Das


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Industrial wood preservation in Kenya. Present status – future prospects
2005 - IRG/WP 05-30385
Although some 50 years old, industrial wood preservation in Kenya does not appear to have technically, scientifically, and commercially evolved and contributed to significantly extend service lives of timbers, protect health and the environment, and curb unnecessary over-exploitation of forests. The population of the country has increased by 530% over the past 50 years; regular excisions have red...
R Venkatasamy


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


Protection of rubberwood with modified creosote
1998 - IRG/WP 98-30165
Creosote is a renowned wood preservative but has certain disadvantages like obnoxius odour and colour, with its unpaintability and bleeding from wood surface may create environmental hazards. An effort has been made to isolate chemical fractions from creosote to obtain clean odourless preservative formulations by subjecting to steam distillation (SVC). Rubberwood treated with SVC and tested for it...
H C Nagaveni, H S Ananthapadmanabha, G Vijayalakshmi, M N Sharma, K H Shankaranarayana


Electrodialytic remediation of CCA-treated wood in larger scale
2005 - IRG/WP 05-50224-20
A pilot plant for the electrodialytic remediation of CCA-treated waste wood has been developed and tested at the Technical University of Denmark. Results from two experiments with different amount of wood chips are presented here. Prior to the electrodialytic remediation the wood was soaked in oxalic acid and phosphoric acid. The main purpose of soaking is to remove the most available fraction fir...
I V Christensen, L M Ottosen, A J Pedersen


Longterm monitoring of termite activity on multiple feeding sites: a laboratory method intended for the determination of attractant/repellent properties of wood preservatives and baits
2001 - IRG/WP 01-20225
A method is introduced allowing the continuous monitoring of the activity of a small laboratory termite- colony at 8 different feeding sites simultaneously. The test assembly consists of a small central polycarbonate-tube containing a colonie of Reticulitermes santonensis (de Feytaud) beeing connected with 8 external feeding sites by small glass-capillaries. The termites passing through the glass ...
M Pallaske, E Graf, H Takiuchi


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Preventive effectiveness of petrol derivatives against blue-stain fungi
1992 - IRG/WP 92-3716
A possible application of fractions obtained on petrol pyrolysis is their use as a wood preservative against wood-decay and sap-stain fungi. From two of these fractions were prepared three different products (ST, STL and SST). The aim of this work has been the possibility of utilizing these products in the treatment of wood used for external joinery, determining their effectiveness against blue-st...
A M Navarrete, M T De Troya, E Sanchez, A Guijarro


The growth and behaviour of Australian isolates of dry rot fungi, mainly Serpula lacrymans (Schum. ex Fr.) S.F. Gray. A comparision with the world literature
1983 - IRG/WP 1190
In Australia Serpula lacrymans occupies a rather unique environment, being restricted to growth within basal regions of buildings containing masonry. Its rate of timber attack in these situations appears to be far faster than that experienced in other parts of the world. Therefore the question arises as to how Australian isolates (particularly 16508 which has become a "standard" test fungus for so...
J D Thornton, O Collett


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Thermal modification of non-durable wood species 1. The PLATO technology: thermal modification of wood
1998 - IRG/WP 98-40123
The PLATO technology is an innovative upgrading technology with low environmental impact, which can be applied to fast grown and non-durable wood species. This technology is based on a thermal modification of solid wood without the addition of chemicals (e.g. preservatives), consisting of a hydrothermal treatment, followed by drying and curing. The PLATO technology results in a substantial improve...
M J Boonstra, B F Tjeerdsma, H A C Groeneveld


Fumigant movement in Canadian wood species
1984 - IRG/WP 3296
Pole sections prepared from seven Canadian wood species (Thuja plicata, Thuja occidentalis, Pinus contorta, Pinus resinosa, Pinus banksiana, Pseudotsuga menziesii, southern yellow pine) were fumigated with chloropicrin, methylisothiocyanate and Vapam and the rates of fumigant penetration determined. All three fumigants were applied directly into holes bored radially into the pole sections. Analysi...
J N R Ruddick


Determination of total fluoride and boron in preservative-treated wood fluoride by ion selective electrode without steam distillation, and boron colorimetrically using azornethine-h
1998 - IRG/WP 98-20135
An analytical method was developed to determine total fluoride and boron in wood treated with aqueous or solid diffusing fluoride or borate-fluoride formulations. Ground wood was mixed with 30% sodium hydroxide solution and oven-dried for 2 hours before furnacing at 600° C for 1 hour. The cool fused product was dissolved in hot water, transferred to a plastic beaker and neutralised. Fluoride was ...
P A Collins, M J Kennedy


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


A preliminary assessment of the penetration into wood achieved by bodied mayonnaise emulsion wood preservatives
1992 - IRG/WP 92-3725
Five different commercial formulations of bodied mayonnaise emulsions were applied to samples of Scots pine (Pinus sylvestris) sapwood as recommended by the manufacturers. Penetration and loading characteristics were determined by measuring the distribution profiles of the active ingredients after various intervals of time. The changes in the general appearance of the emulsions on the surface of t...
G E Holland, R J Orsler


Termite resistance of Malaysian and exotic woods with plantation potential: Laboratory evaluation
1998 - IRG/WP 98-10280
The resistance of selected Malaysian woods to attack by the representative aggressive subterranean termite Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae) was evaluated in four-week, no-choice laboratory tests. This is part of an ongoing effort between the Forest Research Institute Malaysia and the University of Hawaii to document the termite resistance of Malaysian timber species of po...
J K Grace, A A H Wong, C H M Tome