Factors affecting the sorption of preservative during diffusion treatment of wood
1988 - IRG/WP 3500
The sorption of preservative into wood during soaking in aqueous solution was found to comprise absorption as well as diffusion of solute. Absorption was increased by partially seasoning the wood prior to soaking and was characterised by (a) a very rapid initial rate of uptake and (b) an extended period of slow uptake, the rate of which varied with prior conditioning. It was concluded that some pa...
P Vinden


Spatial arrangement of lignin peroxidase in pine decayed by Phanerochaete chrysosporium and Fomitopsis pinicola
1988 - IRG/WP 1343
By applying immunoelectronmicroscopic methods, lignin peroxidase of the white rot fungus Phanerochaete chrysosporium has been localized in the cytoplasm of hyphae, close to the plasmalemma and on the plasmalemma. Infiltration of wood specimen with culture filtrates, concentrated 300-fold, gave clear information on the penetration of the enzyme into the wood cell wall. Penetration was restricted to...
E Srebotnik, K Messner


Oxalic acid production of fifteen brown-rot fungi in copper citrate- treated southern yellow pine
2001 - IRG/WP 01-10388
Non-arsenical copper-based wood preservatives have grown in number since the 1980's as a response to environmental concerns posed by arsenicals. Interest in copper tolerant decay fungi has increased accordingly. Oxalic acid (OA) production by brown-rot fungi has been proposed as one mechanism of copper tolerance. Fifteen brown-rot fungi representing the genera Postia, Wolfiporia, Serpula,...
F Green III, C A Clausen


Environmental risk assessment of preservative treated wood
1998 - IRG/WP 98-50101-19
This paper reviews the status of the environmental risk assessment of preservative treated wood and confirms the distinction between the risks presented by wood preservatives and preservative treated wood. The paper proposes a tiered approach to risk assessment and discusses the rationale. Flowcharts are presented which summarise the tiered approach to risk assessment, show the tests required, and...
E F Baines, S J Davis


The use, approval and waste management of industrial wood preservatives. A preliminary report
1994 - IRG/WP 94-50033
The structure on the wood preservation through the world is heterogenous. Environmental legislation, approval policy and application practices differ in each geographical region and in individual countries. This preliminary report gives a rough estimation of the production of treated timber, the use of wood preservatives and a bief summary of environmental status of wood impregnation in selected c...
A J Nurmi


Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Preservative absorption response of planks of Anogeissus acuminata for plank-built catamarans
2002 - IRG/WP 02-40245
Due to shortage of timber coupled with other compelling factors, traditional fishermen along the east coast of India, especially of Andhra Pradesh, of late, are departing from conventional log type wooden catamarans. Instead, they are fabricating catamarans out of timber planks of hard woods and utilizing thermocol for buoyancy. Mostly, locally available timber of a Combretaceae species, Anogeis...
V Kuppusamy, M V Rao, M Balaji, K Rao


A review of environmental emissions from building and construction materials in comparison with preserved wood
2005 - IRG/WP 05-50224-11
A review of the public domain literature concerning emissions to the environment from materials which are used in the construction of buildings (e.g. Concrete, Asphalt, Galvanised Steel), in comparison with preserved wood, and a review of the approaches taken by the construction sector in assessing the risk from environmental emissions, in comparison with the approaches taken by the wood preservat...
E F Baines


Disposal of treated wood - Canada
1990 - IRG/WP 3563
It is estimated that treated wood removed from service each year in Canada contains about 16,000 tonnes of creosote, 1000 tonnes of pentachlorophenol and 245 tonnes of CCA or ACA. The amount of CCA treated wood for disposal is expected to increase more than ten-fold by the year 2020. At present, most treated wood is disposed of in landfills, burned (creosote only) or recycled as other products. Ot...
P A Cooper


A field test with Benzotar, an industrial residue, as a wood preservative
1985 - IRG/WP 3349
Benzotar, a residue of production of benzoic acid, was tested in field as a wood preservative. Results, after 6.5 years of exposure, showed that this product presents properties that improve the performance of wood in ground contact. This paper describes these results and presents a discussion an some aspects of its potential utilization in Brazil....
S Milano, L R Silva


Checking of sodium pentachlorophenate fixation in wood
1990 - IRG/WP 3620
In order to estimate the volatilization of sodium pentachlorophenate from treated wood, wood samples treated with pentachlorophenate were analysed after various durations of an EN 73 weathering The results giving no clear evidence of volatilization, treated wood samples were put in a test chamber with precise climatic conditions, the air used in the experiment being analysed. The pentachlorophenat...
M Lamour, H Sageot


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Variation in Canadian bluestain fungi: Tolerance to DDAC and DOT
1999 - IRG/WP 99-10303
Bluestain in Canadian wood products results in significant and unpredictable losses each year. In order to develop rational methods to eliminate or reduce the sapstain problem, a more complete knowledge of the causal organisms must be gained. This includes a knowledge of the variability in tolerance of different fungal species and strains to commercially used chemicals. In British Columbia, the ma...
J Dubois, A Byrne, J E Clark, A Uzunovic


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


The more important wood-destroying insects found in buildings in Poland
1974 - IRG/WP 128
In the different regions (voievodships) of the country Anobium punctatum and Anobium pertinax were to be found in the range of 47.7 to 63.5%. These insects were the main pests in urban buildings. In the second place came Hylotrupes bajulus occurring in the range of 25.9 to 45.1%. The other insects were to be found within the limits of 0.1 to 10.0%; only in a single instance did the amount reach 24...
J Dominik, J Wazny, M Czajnik


The permanence of permethrin in wood preservation
1984 - IRG/WP 3288
The permanence of the synthetic pyrethroid permethrin in treated wood has been assessed for double vacuum and immersion treated Scots pine sapwood and whitewood using a 0.5% m/m solution of the insecticide in a hydrocarbon solvent. It is concluded that for all but the outermost 0.5 mm of the treated battens the distribution of the permethrin is relatively permanent. The outermost 0.5 mm appears vu...
R J Orsler, M W S Stone


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Timber Preservation and Sustainable Construction in Australia
2005 - IRG/WP 05-50224-14
Sustainable development has been described as meeting the needs of the present without compromising the ability of future generations to meeting their own needs. (Bruntland 1987) To achieve the sustainable development goal therefore, the maximum performance has to be obtained from existing resources (timber) so that the remaining resource is protected from over-exploitation. Clearly, wood preserva...
J Norton


Inspection of tropical hardwood window frames in Nigeria for decay presence
1987 - IRG/WP 2294
A method of in situ inspection of hardwood window frames for expression of decay is discussed in this paper. The results show that about 6% of the frames inspected or 23% of the volume of wood in all the frames sampled in buildings erected between 1920 and 1984, exhibited evidence of advanced decay. Protection by the length of the eaves, species of the framing timber used, length of exposure to se...
M A Odeyinde, M A Amakiri, E B Lucas, J O Eyenike, S Akanni


The First Annual Report of the International Research Group on Wood Preservation 1969-1970
1970 - IRG/WP A 7
IRG Secretariat


Cleaner prodiction and the wood preserving industry
1995 - IRG/WP 95-50040-29
H Carr-Harris, C R Coggins


Work program of CEN/TC 38 (January 1994). Durability of wood and derived materials
1994 - IRG/WP 94-20019
R Hüe


The most important wood-destroying insects in various countries (Results of questionnaire)
1981 - IRG/WP 1136
M-M Serment


The effect of service life and preservative treatment on the hardness of wooden poles
1989 - IRG/WP 3537
The surface hardness of utility poles is an important parameter which effects the acceptability of the pole as being safe to climb during line maintenance. The current investigation was designed to evaluate how the surface hardness of preservative treated utility poles is effected by the type of preservative, and the age of the poles. Chromated-copper-arsenate (CCA) treated red pine and jack pine ...