Acceleration of the fixation of chromated wood preservatives by UV-radiation
1989 - IRG/WP 3544
Preliminary laboratory tests demonstrated that the fixation of chromated water-borne wood preservatives may be accelerated by UV-radiation. The degree of fixation depends on the intensity of radiation and the prevailing temperature. Three hours radiation at 20°C in a device for artificial weathering diminished the leaching of chromium to 43% and of copper to 23% compared to not-radiated samples. ...
H M Illner, H Willeitner, K Brandt


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Leachability And Decay Resistance of Copper-Treated Wood
2004 - IRG/WP 04-30337
Samples of scots pine sapwood (Pinus sylvestris L.) were treated with solutions of (Copper II sulfat-5 hydro + fluoroboric acid) and (Copper II sulfat-5 hydro + fluoroboric acid + boric acid) in order to determining to leachability and decay resistance against brown rot fungus (Postia placenta) and white rot fungus (Coriolus versicolor). Results indicated that the copper in treated wood is less s...
A Temiz, T Nilsson, I Deemirtas, Ü C Yildiz


Sampling variation in a copper chrome arsenic treated power transmission pole
1990 - IRG/WP 2351
The Queensland Forest Service routinely samples poles treated at all treatment plants throughout the State. Each treatment plant is issued with a Certificate of Registration and the accompanying documents list the different levels of preservative retention required for performance in various service conditions. The posted levels represent the.minimum permissible, and it is to these concentrations ...
J Norton


Bioefficacy of boric acid grafted onto wood
1999 - IRG/WP 99-30202
The use of borate treated wood in outdoor is limited because of the migration of borate. The objective of this study is to investigate the fixation of boric acid in wood using polyethylene glycol (PEG-400) to form polyester borate and isocyanato group as coupling agent. FT-IR was used to monitor the reaction between boric acid and PEG. Elemental analysis was conducted to evaluate the C, H, and N v...
Weining Cui, D P Kamdem


Albumin borate: A new non-toxic, wide-spectrum, long-term wood preservative
1998 - IRG/WP 98-30167
Boron, widely recognized for its broad range of activity towards both fungi and insects and for its low mammalian toxicity, can not provide long term protection to treated timber due to its high leachability. Boron, in the form of boric acid, can be partially fixed to timber by the formation of an association with egg albumin, which is insolubilized by heat-induced coagulation. Chemical investiga...
M-F Thévenon, A Pizzi, J-P Haluk


Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


Anatomical Characteristics to the Distribution of Water-borne Copper Wood Preservatives in Wood
2004 - IRG/WP 04-40277
The objective of this study was to understand the micro-distribution of a copper-based preservative in wood in connection with anatomical morphology and to consider the fixation of copper in wood. Bulk specimens and semi-ultra thin sections (0.5µm) obtained from Japanese cedar were treated with a CuAz preservative solution. After fixation, SEM-EDXA was used to investigate the micro-distribution...
H Matsunaga, J Matsumura, K Oda


Leaching Characteristics of Copper in Copper Treated Wood
2003 - IRG/WP 03-30316
The leaching characteristics of copper in copper treated bamboo and other wood species such as slash pine and poplar has been conducted in this paper according to AWPA M11-87 standard, the result indicates that: --Copper fixation rate of salts from organic acids such as citrate and oxalate and malate is less than other non-organic acid formulations. --Copper fixation rate of oven-dried bamboo sa...
Mingliang Jiang, Junliang Liu, Daochun Qin, Yamei Wang, Zehui Jiang


Determination of fixation properties by bioassays - A proposal for the assessment of safety indexes in wood protection
1990 - IRG/WP 3566
In the determination of environmental effects of chemicals tests with fishes, daphnia and algae have proved to be practicable. With respect to wood protection such bioassays are suitable to control effects of treated timber against aquatic organisms. By using the fish-acute-toxicity-test the development of a laboratory test method is described for the checking of the fixation rate of a copper-chro...
H-W Wegen


A study of decay type variability in variously treated Fagus sylvatica and Pinus radiata field test stakes exposed at a vineyard for 30 - 45 months
1998 - IRG/WP 98-10271
Pinus radiata test stakes were treated with 10 kg/m3 of CCA plus 4 lower retentions in a geometric series of 1.5. Fagus sylvatica was treated with 15 kg/m3 and 2 lower retentions. Both timber species were also treated with equivalent retentions of various new generation preservatives (P. radiata was also treated with creosote). Whilst these stakes were exposed at 11 sites in New Zealand (NZ) and 2...
R N Wakeling, A P Singh


Leaching and fixation characteristics of chrome-copper-fluoride-zinc (CCFZ) treated wood
1996 - IRG/WP 96-30096
The leaching characteristics of radiata pine sapwood blocks treated with CCFZ were evaluated by the AWPA standard leaching test. The rate of fixation of the preservative components in CCFZ treated radiata pine were also evaluated by quantitative analysis of solution expressed from the treated wood. Both leaching and fixation characteristics of CCFZ were compared with CCA-Type C treated wood sample...
Gyu-Hyeok Kim, Jong-Bum Ra


Preliminary studies on cellulase production by selected Basidiomycetes and the effect of copper-chrome-arsenate on these enzymes
1980 - IRG/WP 1122
The growth of wood-destroying fungi on ligno-cellulosic materials depends on the production of many enzymes, of which probably the most important is the multi component cellulase system. Within this system, at least three different kinds of enzym are believed to be involved in crystalline cellulose decomposition. These are endo-1,4-glucanase, exo-1,4-ß glucanase and ß-glucosidase. Most of the re...
O Collett


Kiln drying of CCA-treated wood - Some safety and environmental considerations
1987 - IRG/WP 3443
Vapours and condensate from a condenser kiln in which CCA-treated wood was being dried have been collected and analysed. The concentrations of arsenic, copper and chromium found in the vapours from the drying process were well below Swedish threshold limit values. The contents of arsenic and chromium were also low in the condensate, although the copper content was fairly high. The latter result wa...
J Jermer, B Lundberg


Performance of copper-based wood preservatives in above ground and ground contact tests
1994 - IRG/WP 94-30057
The relative performance of a range of copper-based wood preservatives was compared using above ground and ground contact procedures. The data, accumulated after several years' testing, show that on an equivalent active ingredient basis, differences in performance of the preservative systems tested can vary quite markedly. The contribution of co-biocides to the overall performance of thes...
A F Preston, K J Archer, L Jin, W Metzner, D Seepe


Copper naphthenate: An analysis of the materials found in the worldwide marketplace using a new analytical technique
2000 - IRG/WP 00-30224
Naphthenic acid has been recovered from products of petroleum refining for well over 100 years. The metal soaps, specifically copper and zinc naphthenate, have been evaluated and used as commercial wood preservatives for in excess of 60 years. Most of the early data supporting the continued use of copper naphthenate as a wood preservative was based on materials manufactured from naturally occurrin...
J A Brient, R E Moyer, M H Freeman, H Jiang


Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano


Serviceability of copper naphthenate-treated poles
2000 - IRG/WP 00-30214
Copper naphthenate-treated poles in service were inspected for deterioration, penetration, retention, and serviceability. The study to date has included poles in all hazard zones in the United States. Poles installed by 12 different utilities and eight different treating companies are included in the survey. Both southern pine and Douglas-fir poles and distribution and transmission poles are inclu...
H M Barnes, M H Freeman, J A Brient, C N Kerr Jr


CCA modifications and their effect on soft rot in hardwoods. Part 2
1983 - IRG/WP 3244
The work outlined in this document is a continuation of that presented in Document No: IRG/WP/3201. The findings described in the previous paper are summarised below: a double treatment of CCB followed by arsenic (CCB+A) is more effective than a double treatment of boron followed by CCA (B+CCA) or a single treatment of CCA, CCB or CCAB in controlling soft-rot due to Chaetomium globosum in birch. C...
S M Gray, D J Dickinson


Corrosion of zinc-coated nails used with preservative-treated western red cedar shakes in service
1982 - IRG/WP 3197
The corrosion of metal fasteners used with certain wood species and with preservative-treated woods can be a serious problem. The chemical reactivity of western red cedar (Thuja plicata Donn) extractives to iron and copper is well documented and wood preservative treatments containing copper, chromium, and/or ammonium hydroxide can be expected to similarly attack some metals. This problem is compo...
R S Smith, E L Johnson, A J Cserjesi


The efficacy of remedial treatments for controlling fungal decay in window millwork used in the United States
1987 - IRG/WP 3432
Conventional window millwork was subjected to basidiomycete decay by inoculation and sampled for active growth of the decay fungus before and eight months after remedial preservative treatment with fused disodium octaborate rods (IMPEL) at boric acid levels of 1.5 and 4.0 kg/m³ or liquid bifluoride injections (IMPROSOL) at 1 kg/m³. The elimination of decay fungus after remedial treatment was nea...
M G Dietz, E L Schmidt


Effectiveness of a newly registered antisapstain preservative in preventing stain of Eucalypt timber in Australia
2000 - IRG/WP 00-30229
An antisapstain trial was conducted on two sites (Alexandra and Trentham) in order to establish the concentration of a newly registered antisapstain preservative (consisting of benzalkonium chloride (BAC) & 3-iodo-2-propynyl butyl carbamate (IPBC) & disodium octoborate (boron)) needed to prevent stain of Eucalypt timber. After 20 weeks of exposure at the Trentham site, the water treated bo...
J Snow, P R S Cobham, N Ryan


Incorporation of phenyl boronic acid treatment with vapor phase formalization
1997 - IRG/WP 97-40083
Phenylboronic acid (PBA) treatment was incorporated with vapor phase formalization (VPF) in order to increase dimensional stability and boron fixation as well as enhancement of biological resistance. Five and ten hours VPF were applied after PBA treatment as 0.34, 0.50, 1.00 and 2.00% concs. aqueous solutions. Anti swelling efficiency (ASE) attended to 71% in specimens impregnated with 0.50% PBA s...
M K Yalinkilic, S Yusuf, T Yoshimura, W-Y Su, K Tsunoda, M Takahashi


Effectiveness of copper/chromium salts as wood preservatives against Limnoria tripunctata Menzies in laboratory tests
1977 - IRG/WP 431
During the last joint meeting of IRG and COIPM a co-operative programme of tests with copper/chromium salts as wood preservatives against marine borers was discussed and agreed. In this connection the results of a laboratory test in the BAM with Limnoria tripunctata Menzies will be of interest. But as the respective paper is written in German (H. Kühne; G. Becker: Laboratoriumsversuche über die ...
H Kühne