IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3778 documents. Displaying 25 entries per page.


Depletion of boron and copper from CCB treated test specimens using different leaching protocols
2004 - IRG/WP 04-50208
The objective of this study was to measure the depletion of inorganic wood preservative components regarding the proposed OECD guideline "Estimation of emissions from preservative-treated wood to the environment: laboratory method for wooden commodities exposed in the use class 4 and 5" as part of the project "Investigations concerning the influence of test parameters on the release of biocidal ac...
E Melcher, R-D Peek, U Schoknecht, R Wegner


Field Testing of Copper Carboxylate Preservatives
2003 - IRG/WP 03-30322
This paper details our ongoing experience with field testing of copper naphthenate and other copper carboxylate preservative systems. Results from field stake tests at an AWPA Hazard Zone 4 test site are presented. In general, copper carboxylates made with ‘synthetics’ yielded results equivalent to or only slightly lower than systems with straight nap acids or nap acids amended with syntheti...
H M Barnes, M G Sanders, T L Amburgey


Influence of aliphatic acids on spore germination of wood decay fungi
1984 - IRG/WP 2224
Influences of eight saturated fatty acids (C5-C10, C12 and C16) on spores of four isolates of wood decaying basidiomycetes (white rot fungi: Poria tenuis and Trametes hispida; brown rot fungus: Gloeophyllum trabeum [two isolates]) were observed in-vitro. Spore response after 24 hr on malt extract agar containing 10, 10² , or 10³ ppm of each fatty acid included: no effect on normal germination, d...
E L Schmidt


Effect of protective additives on leachability and efficacy of borate treated wood
2002 - IRG/WP 02-30290
Borate preservatives have been used extensively in many countries as an effective means for protecting wood against fungal and insect attack especially in interior environments. Under exterior conditions, borate compounds have a main disadvantage as they can be leached from treated wood as a result of their water solubility. In this study, we compared the potential of different additives for re...
A Mohareb, J Van Acker, M Stevens


The registration of wood preservatives under the Pesticides Act of 1962 in the Netherlands
1976 - IRG/WP 364
J Van der Kolk


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 8: Panama test results
1980 - IRG/WP 458
Summary of damage to ITRG test stakes by pholadidae and teredinidae at the Panama test site - 8 Mar. '78 to 11 Oct. '79...
J R De Palma


Über Wespen als Holzverderber - Schäden, Ursachen, Bekämpfung
1978 - IRG/WP 189
Observations and a number of actual cases over recent years show that wasps have been associated more frequently with damage to wood. The nature of such damage and the agents involved are as follows: 1. Decay following infestation by Woodwasps (Siricidae). 2. Punctate marks caused by superficial gnawing and also boring into wood by larvae of the Dock sawfly (Tenthredinidae). 3. Damage due to super...
S Cymorek


Resistance of the wood of Eucalyptus saligna and Paulownia tomentosa against some wood rotting fungi
1997 - IRG/WP 97-10238
Paulownia tomentosa and Eucalyptus saligna are not autochthonous species in Slovenia and we determined the resistance of their wood against our most common wood rotting fungi. The resistance against Coniophora puteana, Gloeophyllum trabeum and Trametes versicolor was determined according to EN 113 and compared to the resistance of beech (Fagus sylvatica) wood. It was stated, that both paulownia an...
F Pohleven, M Petric


Collaborative soft rot tests: Programme and test method
1973 - IRG/WP 229
J G Savory, J K Carey


Agenda:Workshop CCA failures in horticultural soils
1983 - IRG/WP 3241
J A Butcher, H Greaves


Letter to the IRG meeting at Peebles, 1978
1978 - IRG/WP 181
J F Levy, R Cockcroft


Soil blocks versus field test for evaluating and standardizing wood preservatives: A commercial view
1994 - IRG/WP 94-20024
On the basis of technical considerations, experience, costs and applicability, the author concludes that the soil block test and other laboratory tests have little meaning in a wood preservative standardization process and almost no merit in the commercialization of a wood preservative system. Field tests at sites known to be aggressive to preservative treated wood are strongly recommended....
W S McNamara


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


Local preservation with difluoride pills: Life-time of preservative
1998 - IRG/WP 98-40127
A brief history of the situation in the Netherlands with respect to the preservation of joinery is given. Already in the eighties in the Netherlands many spruce window frames were treated with difluoride pills. One of the possible disadvantages of this kind of diffusing preservatives is the high leaching rate found in laboratory situations. The leaching rate in practice is influenced by many facto...
W J Homan, C Blom, B W Holleboom


Determination of the preventive efficacy against wood destroying basidiomycetes fungi, EN V 839 - CEN/TC 38 WG 9
1993 - IRG/WP 93-20015
The WG 9 of CEN TC/38 has presented to EC a mycological test to assess efficacy of preservatives applied by surface process. This method is now an experimental standard (EN V 839) which has to be approved by the different european delegations. The following paper is not the standard as it has been proposed but is a presentation of the principle of the method. The experimental standard specifies a ...
D Dirol


Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


AAC preservatives: Recent New Zealand and Australian experience
1982 - IRG/WP 3188
This paper outlines the present commercial situation in New Zealand, presents results of current research undertaken at FRI and CSIRO, Division of Building Research (DBR), and comments on parallel research carried out elsewhere. Finally, some general comments are made on the limitations of present technology....
J A Butcher, H Greaves


Accelerated fixation of CCA in borak bamboo (Bambusa balcooa Roxb.) of Bangladesh
2001 - IRG/WP 01-40193
CCA-C fixation study on impregnated (6% CCA solution), then boiled, oven-dried, normal, air-dried and steamed bamboo slices of air-dried borak bamboo (Bambusa balocca Roxb) of Bangladesh, revealed almost complete fixation in steamed (accelerated fixation) and air-dried (3 weeks, slow fixation) bamboo slices compared to moderate to slow fixation in boiled, oven-dried, normal and 24h air-dried slice...
A K Lahiry


Spore germination of Gloeophyllum trabeum on wood is related to the mass of the wood sample
1978 - IRG/WP 2118
E L Schmidt, D W French


Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood. Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz


The resistance of painting materials and consolidants against wood-destroying insects
1997 - IRG/WP 97-10239
Natural and synthetic adhesives, varnishes, painting materials and consolidants were used in investigations of bioresistance against newly hatched larvae and beetles of Hylotrupes bajulus (L.). Animal glues, casein, drying oils and natural resins such as dammar resin and shellac, were not resistant to attack by these larvae. Similarly, semi- and all-synthetic polymers tested including hydroxypropy...
W Unger, H Fritsche, A Unger


Wood preservation in the USA
1982 - IRG/WP 3215
This report is a comprehensive survey of the status of the wood preservation field in the U.S.A. at the start of the 1980s. The importance of wood preservation is discussed and its industry described. Various statistics and analyses regarding the use of treated wood have been compiled. Both pressure and non-pressure applications have been covered, as well as remedial treatments and pest control op...
D D Nicholas, R Cockcroft


Supplement to Document No: IRG/WP/56. Health and safety aspects of the use of wood preservatives
1975 - IRG/WP 356
H Willeitner


Wood preservation in France. "Bois plus" chain of quality. Description of the scheme early 1989
1989 - IRG/WP 3519
1989 - description of the French "CTB-BOIS PLUS" homologation scheme
G Ozanne


The Eighth Annual Report of the International Research Group on Wood Preservation 1976-1977
1978 - IRG/WP 569
IRG Secretariat