Laboratory studies of CCA-C-leaching: influence of wood and soil properties on extent of arsenic and copper depletion
2002 - IRG/WP 02-50186
The extent which a wood preservative leaches is important for efficacy studies and environmental concerns. However, little information exists on the effect soil properties have on leaching. This study investigated leaching of stakelets which had been cut from five different southern yellow pine (SYP) sapwood boards then treated with CCA-C to a target retention of 6.4 kgm-3 (0.4 pcf). All stakel...
D Crawford, R F Fox, D P Kamden, S T Lebow, D D Nicholas, D Pettry, T Schultz, L Sites, R J Ziobro


Antifeedant activities of flavonoids and their related compounds against the subterranean termite, Coptotermes formosanus Shiraki
1999 - IRG/WP 99-10305
Antifeedant activities of some flavonoids and their related compounds against the subterranean termite, Coptotermes formosanus Shiraki were examined with no-choice and two-choice tests. The activities of these compounds were considered in relation to their chemical structures. All flavonoids tested showed antifeedant activities whereas catechinic acid without A-ring and pyran ring in the molecule ...
W Ohmura, S Doi, M Aoyama, S Ohara


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


Wood kiln drying. Simple process of material treament or soft method of preservation? (Le séchage arificiel du bois. Simple opération de traitement du metériau ou méthode douce de préservation?)
1993 - IRG/WP 93-50001-14
Among the processes enabling to extend wood durability, kiln drying can be considered as a treatment and soft preservation method. Dry woods are naturally durable provided they are not subject to important retaking of the moisture. Drying thanks to the application of temperatures from 50 to120°C enable to execute a thermic treatment which kills grubs and mushrooms to ensure a sterilization that c...
F More-Chevalier


The identification of organic compounds in wood using thermal desorption GC-MS - possibilities and limitations
2001 - IRG/WP 01-20224
There is a clear need for the analytical characterisation and identification of organic compounds and their derivatives in different phases especially in timber. In this context the paper describes a rapid and powerful gas chromatographic method for the determination of insecticides, biocides and "other" organic substances in treated and/or modified wood. The main advantage of this procedure is th...
P Jüngel, E Melcher


Influences of the hydro-thermal treatment on physical properties of beech wood (Fagus orientalis)
2005 - IRG/WP 05-40303
Influences of the hydro-thermal treatment on physical properties of beech wood were studied. Wood specimens (2×2×2cm) were treated in two steps. At first step, samples were treated at 160,180 & 200ºC for 4, 5 & 6 hours. At second step, treated samples were cured based on their first step treatment temperatures (160,180 & 200ºC) for 16 hours. The treated samples were soaked in water...
B Mohebby, I Sanaei


An observation of seasoning, preservative treatment and storing of CCA treated 30 bangladeshi hardwood species for crossarms
1995 - IRG/WP 95-40058
Observed kiln seasoning, preservative pressure treatment and storing of CCA treated 30 Bangladeshi hardwood species for crossarms. It revealed that it was very difficult to kiln season and preservative pressure treatment of thirty species together in a single charge and found that when species of different specific gravity kiln season together there occur some objectionable seasoning degrades, and...
G N M Ilias, M D Rokib-ul-Hafiz


Applicability of supercritical carbon dioxide to the preservative treatment of wood-based composites
2001 - IRG/WP 01-40199
Treatability of five structural-use wood-based composites (medium density fiberboard, hardwood plywood, softwood plywood, particleboard and oriented strand board) was evaluated when supercritical (SC) carbon dioxide (CO2) was used as a carrier solvent. Treatments were conducted at three temperature 32 levels (25, 35 and 45°C) and two pressure levels [80 kgf/cm2 (7,845 kPa) and 120 kgf/cm2 (11,768...
M Muin, A Adachi, K Tsunoda


The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee


Thermal modification of non-durable wood species 2. Improved wood properties of thermal treated wood
1998 - IRG/WP 98-40124
Properties of wood treated in a new heat-treatment process called the PLATO-process have been studied. Several wood species have been treated using this new thermal modification process using a range of process conditions (mainly time and temperature). In this study the characteristics of the treated wood were determined using samples from whole planks treated on pilot plant scale. The modified ch...
B F Tjeerdsma, M J Boonstra, H Militz


Controlled envelope treatments of Pinus sapwood, achieved by modifications to impregnation process and carrier solvents
2003 - IRG/WP 03-40258
Specimens of slash pine or radiata pine were treated to a target retention of 0.02% m/m permethrin with conventional light organic solvent fluids or with oil-modified fluids (Tanalith® T). Best achievable envelopes from LOSP fluids were poorly controlled, penetrating not only the target outer 0-5 mm zone (mean 0.019%, RSD 28%), but also breaking through into the 5-10 mm zone (mean 0.013%, RSD 37%...
M J Kennedy, P R S Cobham


Effect of point of preservative addition on the mechanical and physical properties of strandboard treated with Tanalith 3485
2000 - IRG/WP 00-40152
Preservative has been added to a PF bonded strandboard at various different stages in the manufacturing cycle and the physical and mechanical properties of the boards have been evaluated (modulus of elasticity, modulus of rupture, thickness swelling, water absorption, internal bond strength, and shear strength). Preservative addition has been examined at five different stages namely green strand d...
G J Goroyias, M D C Hale


Properties of cellulose degraded by the brown rot fungus, Postia placenta
1988 - IRG/WP 1350
To gain further understanding of the nature of the cellulose depolymerizing agent or agents of brown-rot fungi, brown-rotted cellulose was chemically and physically characterized. Various culture conditions, such as low nitrogen and elevated oxygen levels, did not induce degradation of cellulose by Postia placenta in liquid cultures. Therefore, brown-rotted cellulose for analysis was prepared by a...
T L Highley, R E Ibach, T K Kirk


The influence of drying and chemical stress on the lignin degradation in aspen by Phanerochaete chrysosporium
1992 - IRG/WP 92-1573
Wood wafers of Populus tremuloides sapwood were incubated on common media with the white rot fungus Phanaerochaete chrysosporium (wild isolate) and subjected to cyclic drying or chemical agents (low levels of borate or trifluoperazine [a calmodulin antagonist]). After a mass loss of approximately 5.5%, wafers were dried and analyzed for acid-insoluble lignin. Those wafers containing chemical agent...
E L Schmidt, Y-L Lin


Microwave modification of wood properties - Improvements in wood permeability
2000 - IRG/WP 00-40181
A new method of microwave (MW) wood modification is described. Microwave irradiation of timber provides an improvement in wood permeability mainly in the radial and longitudinal directions. This is achieved by physically modifying ray cells and forming a large number of cavities in the radial - longitudinal planes. More extensive MW irradiation of different species transforms the wood into a new m...
G Torgovnikov, P Vinden


Deterioration of wood viewed from iron nail
1991 - IRG/WP 2368
Deterioration of nail was graded by a five - rank numerical - rating. The rating of nail moisture content and decay of wood were inspected in a mortal-wall of 34-year-old house. The wood was mostly in decay, when the rating of the nail was above about 4, and the moisture content was above about 20%. Nailed wood specimens kept in several humidity room of 20°C for 4 years showed that the rating of ...
H Imamura


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


Fungicidal properties of wood tar being a side product of pyrolysis of previously treated wood with preservatives
2004 - IRG/WP 04-30340
The objective of the paper was to estimate the limit of the fungicidal value of wood tar being a product of pyrolysis of wood previously treated with creosote oil or salt preservative of the CCB type. The effectiveness of wood tar in wood protection against fungi causing brown rot and soft rot was compared to the effectiveness of creosote oil (type WEI-B). Wood was impregnated with alcohol solutio...
B Mazela, M Kielczewski, W Grzeskowiak


Assessing the bioresistance conferred to solid wood by chemical modification
1997 - IRG/WP 97-40099
The chemical modification of wood using straight chain alkyl anhydrides can considerably enhance its durability. This paper presents an assessment of the effectiveness of these modifiers in improving the biological resistance of a susceptible softwood when exposed to four different basidiomycete fungi, soft rots and the larvae of the house longhorn beetle (Hylotrupes bajulus). It was clear that so...
E D Suttie, C A S Hill, D Jones, R J Orsler


Soft rot decay in CCA treated eucalypts in Queensland - A comment
1986 - IRG/WP 1301
A survey has been completed concerned with the distribution and severity of groundline soft rot decay in the CCA treated sapwood of eucalypt poles in Queensland. The survey encountered some 1000 poles of which 55% were slightly, 28% moderately and 17% severely decayed. Soft rot decay was more severe in urban than rural locations. Embedment of poles in concrete resulted in severe soft rot. No signi...
L E Leightley


New ways of chemical wood preservation
1997 - IRG/WP 97-40087
Synergistic effects pertaining to wood preservation have been investigated by combining different polymerizing agents with modifying chemicals, modifying chemicals with known preservatives and new types of preservative chemicals with each other. One of the investigated methods is the use of impregnating solutions based on furfuryl alcohol (produced from biomass), in which the chemicals polymerizes...
M Westin, T Nilsson, B Ohlsson, R Simonson


Silafluofen: Novel chemistry and versatility for termite control
1995 - IRG/WP 95-30069
A novel silicon - containing insectizide, HOE 084498 ('Silafluofen'), with a favourable toxicological profile, has shown activity against a broad spectrum of agricultural and environmental health pests. Results from laboratory and field studies around the world have demonstrated that silafluofen is effective at protecting timber from attack by various species of termite and wood-...
A J Adams, A Jermannaud, M-M Serment


A novel chemical barrier system, KORDON® TMB, for the protection of buildings against subterranean termites using a synthetic matrix as carrier for the chemical
1998 - IRG/WP 98-10264
Kordon TMB is a new chemical barrier system for installation beneath concrete slab-on-ground constructions using a matrix other than soil as carrier for the termiticide. The product consists of a synthetic foraminous web (blanket) carrying the synthetic pyrethroid deltamethrin. The blanket is laminated on the upper side to a standard 0.2mm thick moisture vapour membrane of low density polyethylene...
M Lenz, P Morrow, S Runko


Fire retardant treated wood and plywood: A comparative study Part III. Combustion properties of treated wood and plywood
2002 - IRG/WP 02-40236
The fire retardant treated and untreated plywood and alder wood samples were prepared with the aim to investigate the effects of the way of treatment on the combustion properties. Alder wood was used for the preparation of plywood. Boric acid and borax were used as fire retardant. The plywood samples were impregnated by using three different methods; first group samples were impregnated by soaki...
S Çolak, A Temiz, Ü C Yildiz, G Çolakoglu


The lasting dehydration of wood treated by bifluorides worked up in Diffusec noticed by a continual drying of the wood
1999 - IRG/WP 99-30196
After an immersion of sound wood in a solution of Diffusec, in which a combination of acid potassium and ammonium bifluorides = FHF- in dissociated form is present, their potassium and ammonium fluoride ions together with the bifluoride ion = (FHF-) diffuse into the wood. They make use of the woodmoisture available as O-H-O bonds directly attached to the cellulose in the wood fibres to attract the...
H F M Nijman